Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “tungsten”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 253 records · Page 14

Comparison of secondary neutron dose in proton therapy resulting from the use of a tungsten alloy MLC or a brass collimator system

Purpose: To apply the dual ionization chamber method for mixed radiation fields to an accurate comparison of the secondary neutron dose arising from the use of a tungsten alloy multileaf collimator (MLC) as opposed to a brass collimator system for defining the shape of a therapeutic proton field. Methods: Hydrogenous and nonhydrogenous ionization chambers were constructed with large volumes to enable measurements of absorbed doses below 10{sup -4} Gy in mixed radiation fields using the dual ionization chamber method for mixed-field dosimetry. Neutron dose measurements were made with a nominal 230 MeV proton beam incident on a closed tungsten alloy MLC and a solid brass block. The chambers were cross-calibrated against a {sup 60}Co-calibrated Farmer chamber in water using a 6 MV x-ray beam and Monte Carlo simulations were performed to account for variations in ionization chamber response due to differences in secondary neutron energy spectra. Results: The neutron and combined proton plus {gamma}-ray absorbed doses are shown to be nearly equivalent downstream from either a closed tungsten alloy MLC or a solid brass block. At 10 cm downstream from the distal edge of the collimating material the neutron dose from the closed MLC was (5.3 {+-} 0.4) x 10{sup -5} Gy/Gy. The neutron dose with brass was (6.4 {+-} 0.7) x 10{sup -5} Gy/Gy. Further from the secondary neutron source, at 50 cm, the neutron doses remain close for both the MLC and brass block at (6.9 {+-} 0.6) x 10{sup -6} Gy/Gy and (6.3 {+-} 0.7) x 10{sup -6} Gy/Gy, respectively. Conclusions: The dual ionization chamber method is suitable for measuring secondary neutron doses resulting from proton irradiation. The results of measurements downstream from a closed tungsten alloy MLC and a brass block indicate that, even in an overly pessimistic worst-case scenario, secondary neutron production in a tungsten alloy MLC leads to absorbed doses that are nearly equivalent to those seen from brass collimators. Therefore, the choice of tungsten alloy in constructing the leaves of a proton MLC is appropriate, and does not lead to a substantial increase in the secondary neutron dose to the patient compared to that generated in a brass collimator.

61 RADIATION PROTECTION AND DOSIMETRY↗

Results of high heat flux tests of tungsten divertor targets under plasma heat loads expected in ITER and tokamaks (review)

Heat loads on the tungsten divertor targets in the ITER and the tokamak power reactors reach ~10MW m{sup −2} in the steady state of DT discharges, increasing to ~0.6–3.5 GW m{sup −2} under disruptions and ELMs. The results of high heat flux tests (HHFTs) of tungsten under such transient plasma heat loads are reviewed in the paper. The main attention is paid to description of the surface microstructure, recrystallization, and the morphology of the cracks on the target. Effects of melting, cracking of tungsten, drop erosion of the surface, and formation of corrugated and porous layers are observed. Production of submicron-sized tungsten dust and the effects of the inhomogeneous surface of tungsten on the plasma–wall interaction are discussed. In conclusion, the necessity of further HHFTs and investigations of the durability of tungsten under high pulsed plasma loads on the ITER divertor plates, including disruptions and ELMs, is stressed.

36 MATERIALS SCIENCE↗

Deposition of tungsten metal by an immersion process

A new multi-step, solution-phase method for the spontaneous deposition of tungsten from a room temperature ethereal solution is reported. This immersion process relies on the deposition of a sacrificial zinc coating which is galvanically displaced by the ether-mediated reduction of oxophilic WCl 6 . Subsequent thermal treatment renders a crystalline, metallic tungsten film. The chemical evolution of the surface and formation of a complex intermediate tungsten species is characterized by X-ray diffraction, infrared spectroscopy, and X-ray photoelectron spectroscopy. Efficient metallic tungsten deposition is first characterized on a graphite substrate and then demonstrated on a functional carbon foam electrode. The resulting electrochemical performance of the modified electrode is interrogated with the canonical aqueous ferricyanide system. A tungsten-coated carbon foam electrode showed that both electrode resistance and overall electrochemical cell resistance were reduced by 50%, resulting in a concomitant decrease in redox peak separation from 1.902 V to 0.783 V. Furthermore, this process promises voltage efficiency gains in electrodes for energy storage technologies and demonstrates the viability of a new route to tungsten coating for technologies and industries where high conductivity and chemical stability are paramount.

36 MATERIALS SCIENCE↗

Effect of Tungsten L-PBF Feedstock Modification on Performance in Bending

Additively manufactured tungsten is a candidate refractory material for high-temperature aerospace and nuclear fusion/fission applications. The printability of pure tungsten is challenged by cracking defects arising from the metal’s high ductile-to-brittle transition temperature and low solubility of interstitial impurities. Furthermore, the cast microstructure inherent to the laser powder bed fusion (L-PBF) process has limited strength compared to worked microstructures common in wrought tungsten. Aside from process-related techniques to mitigate defects and increase strength (e.g., heated build chambers, multi-laser systems, low oxygen environmental control, etc.), micro-alloying additions can positively influence tungsten printability. In this work, pure tungsten L-PBF feedstock was modified with 1 wt% additions of ceramic compound nano-powders. Wrought and printed bars were evaluated in four-point bending. Flexural strength and fractography were primary means of comparison to assess the effect of the feedstock modification on printed tungsten mechanical performance.

Tungsten-based alloys↗

Bending Performance of Tungsten Printed Via Laser Powder Bed Fusion With Ceramic Dispersion Modified Powder Feedstock

Additively manufactured tungsten is a candidate refractory material for high-temperature aerospace and nuclear fusion/fission applications. The printability of pure tungsten is challenged by cracking defects arising from the metal’s high brittle-to-ductile transition temperature and low solubility of interstitial impurities. Furthermore, the cast microstructure inherent to the laser powder bed fusion (L-PBF) process has limited strength compared to worked microstructures common in wrought tungsten. Aside from process-related techniques to mitigate defects and increase strength (e.g., heated build chambers, multi-laser systems, low oxygen environmental control, etc.), micro-alloying additions can positively influence tungsten printability and strength. In this work, pure tungsten L-PBF feedstock was modified with 1 wt% additions of ceramic compound nano-powders. Wrought and printed bars were evaluated in four-point bending. Flexural strength and fractography were primary means of comparison to assess the effect of the feedstock modification on printed tungsten mechanical performance.

Additive Manufacturing↗

Comparison of Deuterium Retention for Ion-irradiated and Neutron-irradiated Tungsten

The behavior of D retention for Fe{sup 2+}-irradiated tungsten with a damage of 0.025-3 dpa was compared with that for neutron-irradiated tungsten with 0.025 dpa. The D{sub 2} thermal desorption spectroscopy (TDS) spectra for Fe{sup 2+}-irradiated tungsten consisted of two desorption stages at 450 and 550 K, while that for neutron-irradiated tungsten was composed of three stages and an addition desorption stage was found at 750 K. The desorption rate of the major desorption stage at 550K increased as the displacement damage increased due to Fe{sup 2+} irradiation increasing. In addition, the first desorption stage at 450K was found only for damaged samples. Therefore, the second stage would be based on intrinsic defects or vacancy produced by Fe{sup 2+} irradiation, and the first stage should be the accumulation of D in mono-vacancy and the activation energy would be relatively reduced, where the dislocation loop and vacancy is produced. The third one was found only for neutron irradiation, showing the D trapping by a void or vacancy cluster, and the diffusion effect is also contributed to by the high full-width at half-maximum of the TDS spectrum. Therefore, it can be said that the D{sub 2} TDS spectra for Fe{sup 2+}-irradiated tungsten cannot represent that for the neutron-irradiated one, indicating that the deuterium trapping and desorption mechanism for neutron-irradiated tungsten is different from that for the ion-irradiated one.

72 PHYSICS OF ELEMENTARY PARTICLES AND FIELDS↗

Survey of tungsten gross erosion from main plasma facing components in WEST during a L-mode high fluence campaign

An initial high fluence campaign was performed in WEST, in 2023, on the newly installed actively cooled tungsten divertor composed of ITER-grade monoblocks. The campaign consisted in the repetition of a 60 s long Deuterium L-mode pulse in attached divertor conditions, cumulating over 10000s of plasma exposure. A maximum deuterium fluence of approximately 5⋅1⁢026 m−2 was reached in the outer strike point region, representative of a few high performance ITER pulses. Gross tungsten erosion inferred from visible spectroscopy shows that the most eroded plasma facing component is the inner divertor target with rates ten times larger than on the outer divertor target. The outer midplane tungsten bumpers, located a few centimeters from the plasma, show gross erosion rates two times lower than at the outer divertor. We conclude that the outer midplane bumpers have a negligible contribution to the long range tungsten migration and deposition onto the lower divertor. The cumulated gross erosion rate on the inner divertor translates in an effective gross erosion thickness of about 20μ⁢m, while it is about 2μ⁢m for the outer divertor. Strikingly, these orderings coincide with the thickness of deposits found locally on the divertor: the exposed surfaces of high field side monoblocks are covered with several tens of μ⁢m tungsten deposits, while on the lower field side, few μ⁢m thin tungsten deposits are only found on the magnetically shadowed parts of monoblocks. The strong impact of those deposits on WEST operation, namely perturbation of surface temperature measurement with infra-red thermography, and the emission of flakes causing radiative perturbation of the confined plasma, calls for anticipating similar issues in ITER. In particular, the start of research operation shall consider the definition of a divertor erosion budget in order to anticipate the formation of deleterious deposits.

Fedorczak, N.↗

Effects of transition metal carbide dispersoids on helium bubble formation in dispersion-strengthened tungsten

Abstract The formation of helium bubbles and subsequent property degradation poses a significant challenge to tungsten as a plasma-facing material in future long-pulse plasma-burning fusion reactors. In this study, we investigated helium bubble formation in dispersion-strengthened tungsten doped with transition metal carbides, including TaC, ZrC, and TiC. Of the three dispersoids, TaC exhibited the highest resistance to helium bubble formation, possibly due to the low vacancy mobility in the Group VB metal carbide and oxide phases. Under identical irradiation conditions, large helium bubbles formed at grain boundaries in tungsten, while no bubbles were observed at the interfaces between the carbide dispersoid and tungsten matrix. Moreover, our results showed the interfaces could suppress helium bubble formation in the nearby tungsten matrix, suggesting that the interfaces are more effective in trapping helium as tiny clusters. Our research provided new insights into optimizing the microstructure of dispersion-strengthened tungsten alloys to enhance their performance.

36 MATERIALS SCIENCE↗

Discovering tungsten-based composites as plasma facing materials for future high-duty cycle nuclear fusion reactors

Abstract Despite of excellent thermal properties and high sputtering resistance, pure tungsten cannot fully satisfy the requirements for plasma facing materials in future high-duty cycle nuclear fusion reactions due to the coupled extreme environments, including the high thermal loads, plasma exposure, and radiation damage. Here, we demonstrated that tungsten-based composite materials fabricated using spark-plasma sintering (SPS) present promising solutions to these challenges. Through the examination of two model systems, i.e., tungsten-zirconium composite for producing porous tungsten near the surface and dispersoid-strengthened tungsten, we discussed both the strengths and limitations of the SPS-fabricated materials. Our findings point towards the need for future studies aimed at optimizing the SPS process to achieve desired microstructures and effective control of oxygen impurities in the tungsten-based composite materials.

21 SPECIFIC NUCLEAR REACTORS AND ASSOCIATED PLANTS↗

Thermal conductivity of tungsten: Effects of plasma-related structural defects from molecular-dynamics simulations

We report results on the lattice thermal conductivities of tungsten single crystals containing nanoscale-sized pores or voids and helium (He) nanobubbles as a function of void/bubble size and gas pressure in the He bubbles based on molecular-dynamics simulations. For reference, we calculated lattice thermal conductivities of perfect tungsten single crystals along different crystallographic directions at room temperature and found them to be about 10% of the overall thermal conductivity of tungsten with a weak dependence on the heat flux direction. The presence of nanoscale voids in the crystal causes a significant reduction in its lattice thermal conductivity, which decreases with increasing void size. Filling the voids with He to form He nanobubbles and increasing the bubble pressure leads to further significant reduction of the tungsten lattice thermal conductivity, down to ~20% of that of the perfect crystal. The anisotropy in heat conduction remains weak for tungsten single crystals containing nanoscale-sized voids and He nanobubbles throughout the pressure range examined. Analysis of the pressure and atomic displacement fields in the crystalline region that surrounds the He nanobubbles reveals that the significant reduction of tungsten lattice thermal conductivity in this region is due to phonon scattering from the nanobubbles, as well as lattice deformation around the nanobubbles and formation of lattice imperfections at higher bubble pressure.

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗

Hole formation effect on surface morphological response of plasma-facing tungsten

We report simulation results on the effect of helium (He) bubble bursting-mediated surface hole formation on the surface morphological response of tungsten plasma-facing components (PFCs) in nuclear fusion devices. Our analysis is based on an atomistically informed, continuum-scale model, which is capable of accessing the spatiotemporal scales relevant to the fuzz nanostructure formation process on the surface of PFC tungsten. Our simulations account, in an empirical fashion, for two types of subsurface bubble dynamical phenomena in the nanobubble region of PFC tungsten during He plasma irradiation, involving bubble bursting and surface crater formation. We demonstrate that the hole formation effect on the PFC tungsten surface accelerates the growth rate of nanotendrils and the onset of fuzz formation. As a result, the predicted incubation time for surface nanotendril growth is shortened, in agreement with experimental data of incubation fluence at comparable plasma exposure conditions. We also explore systematically the dependence of the PFC surface morphological response on the areal density of holes introduced at regular time intervals onto the He-implanted tungsten surface, a parameter in our analysis that serves as a proxy for the rate of He bubble bursting. More importantly, our simulations capture fine surface features in the PFC tungsten surface morphology and predict that the average spacing between nanotendrils is on the order of 100 nm, consistent with the experimental findings.

Chen, Chao-Shou (ORCID:0000000307910042)↗

The effect of ICRH and NBI on tungsten transport in neon edge radiation cooled discharges in TEXTOR

Tungsten is planned to be the plasma-facing material for the main chamber and divertor in future devices like ITER, SPARC, and DTT. To address risks associated with tungsten, R&D is being carried out on various toroidal confinement devices. One particular research question is related to the optimum heating mix for ITER. To investigate the influence of the heating scheme on the release and transport of tungsten, a comparison of neutral beam injection (NBI) and ion cyclotron resonance frequency (ICRF) heating was carried out in TEXTOR tungsten test limiter experiments. The experiments were performed under standard L-mode conditions and in radiative improved-mode operation with neon seeding and boronized walls covering the graphite plasma-facing components. The plasma was heated with hydrogen or deuterium NBI alone or with deuterium NBI in combination with H-minority, ion cyclotron resonance heating. A movable solid tungsten limiter was inserted through a limiter lock system into the edge plasma. The impurity release from this limiter was evaluated from visible spectroscopy. The tungsten concentrations in the plasma core were determined by extreme ultraviolet spectroscopy and bolometry. With deuterium NBI alone, strong central radiation and accumulation of W was observed. This can, however, be avoided by adding ICRF heating.

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗

Solute stabilization of nanocrystalline tungsten against abnormal grain growth

Microstructure and phase evolution in magnetron sputtered nanocrystalline tungsten and tungsten alloy thin films are explored through in situ TEM annealing experiments at temperatures up to 1000 °C. Grain growth in unalloyed nanocrystalline tungsten transpires through a discontinuous process at temperatures up to 550 °C, which is coupled to an allotropic phase transformation of metastable β-tungsten with the A-15 cubic structure to stable body centered cubic (BCC) α-tungsten. Complete transformation to the BCC α-phase is accompanied by the convergence to a unimodal nanocrystalline structure at 650 °C, signaling a transition to continuous grain growth. Alloy films synthesized with compositions of W–20 at.% Ti and W–15 at.% Cr exhibit only the BCC α-phase in the as-deposited state, which indicate the addition of solute stabilizes the films against the formation of metastable β-tungsten. Thermal stability of the alloy films is significantly improved over their unalloyed counterpart up to 1000 °C, and grain coarsening occurs solely through a continuous growth process. The contrasting thermal stability between W–Ti and W–Cr is attributed to different grain boundary segregation states, thus demonstrating the critical role of grain boundary chemistry in the design of solute-stabilized nanocrystalline alloys.

36 MATERIALS SCIENCE↗

Weldability, strength, and high temperature stability of chemically vapor deposited tungsten

Three types of CVD tungsten (fluoride-produced, chloride-produced and the combination of the two which is termed duplex) were evaluated to determine their weldability, high temperature strength and structural stability during 5000 hour exposure to temperatures of 1540 C and 1700 C. Each type of CVD tungsten could be successfully electron beam welded but the results for the chloride product were not as satisfactory as those of the other two materials. The high temperature strength behavior of the three materials did not differ greatly. However a large difference was noted for the grain growth behavior of the two basic CVD tungsten materials. Fluoride tungsten was found to be relatively stable while for the most part the grain size of chloride tungsten increased appreciably. The examination of freshly fractured surfaces with a scanning electron microscope revealed numerous bubbles in the fluoride material following its exposure to 1700 C for 5000 hours. Less severe thermal treatments produced relatively few bubbles in this material. Only at certain locations within the chloride material associated with the interruption of tungsten were bubbles noted.

Bryant, W. A.↗

Low-energy helium plasma effects on textured micro-porous tungsten

The effects of low-energy helium plasma on surface evolution and restructuring of micro-porous tungsten and tungsten-rhenium micro-engineered materials was experimentally investigated. Tungsten foam samples of 45 and 80 Pores Per Inch (PPI) of three types of textured surface architecture (nodular W, dense Re-pillars, and W-coated Re-pillars) were exposed to low-energy helium plasma at 80 and 200 eV to fluence levels of 1, 2, and 7 x 10 25 m -2 at 1123 K. The sidewalls of Re pillars exhibited surface holes due to trapped helium while their tips were found to form complex nano-scale web structures, 100's of microns across, rather than nano-tendrils (fuzz) that are often observed in flat W samples. A nano-necklace bead/string structure was observed for the first time on Re pillars, likely driven by a high density of nano-meter size helium bubbles crowded near pillar tips. W-coated Re pillars exhibited typical fuzz nanostructures seen on flat and untextured W-foam, albeit much shorter. While the height of W-fuzz was found to depend on the square root of ion fluence, the nano-web height was found to be linearly dependent on ion fluence. The fuzz was found to grow much slower on nodular foams as compared to planar tungsten, by as much as 25% slower in the W-coated Re pillar samples. Weight loss due to ion sputtering was found to be significantly reduced in nodular foam as compared to planar tungsten, but was found to be more pronounced with Re pillars. Surface coverage by nano-webs may provide insulation against plasma disruptions and act as a passive Thermal Protection System (TPS) that may be ablated during severe plasma disruptions, thus protecting the underlying surface. W-pillars or W-coated Re-pillars are found to allow trapped helium to diffuse out of the surface instead of building up sub-surface stress.

36 MATERIALS SCIENCE↗

Effects of Tungsten Oxide Addition on the Electrochemical Performance of Nanoscale Tantalum Oxide-Based Electrocatalysts for Proton Exchange Membrane PEM Fuel Cells

In the present study, the properties of a series of non-platinum based nanoscale tantalum oxide/tungsten oxide-carbon composite catalysts was investigated for potential use in catalyzing the oxygen reduction reaction (ORR) on the cathode side of a PEM fuel cell membrane electrode assembly. Electrochemical performance was measured using a half-cell test set up with a rotating disc electrode and compared with a commercial platinum-on-carbon (Pt/C) catalyst. Overall, all of the oxide-based composite catalysts exhibit high ORR on-set potentials, comparable to that of the baseline Pt/C catalyst. The addition of tungsten oxide as a dopant to tantalum oxide greatly improved mass specific current density. Maximum performance was achieved with a catalyst containing 32 mol% of tungsten oxide, which exhibited a mass specific current density ~8% that of the Pt/C catalyst at 0.6 V vs. the normal hydrogen electrode (NHE) and ~35% that of the Pt/C catalyst at 0.2 V vs. NHE. Results from X-ray photoelectron spectroscopy analysis indicated that the tungsten cations in the composite catalysts exist in the +6 oxidation state, while the tantalum displays an average valence of +5, suggesting that the addition of tungsten likely creates an oxygen excess in the tantalum oxide structure that influences its oxygen absorption kinetics. When the 32mol% tungsten doped catalyst loading on the working electrode was increased to five times that of the original loading (which was equivalent to that of the baseline Pt/C catalyst), the area specific current density improved four fold, achieving an area specific current density ~35% that of the Pt/C catalyst at 0.6 V vs. NHE.

08 HYDROGEN↗

Effect of tungsten addition on the toughness and hardness of Fe{sub 2}B in wear-resistant Fe-B-C cast alloy

The effects of tungsten additions of 0%, 1.12%, 2.04%, and 3.17% (in wt.%) on the morphology, fracture toughness and micro-hardness of Fe{sub 2}B in Fe-B-C cast alloy were investigated. The results indicate that, with the increase of tungsten addition, the morphology and distribution of Fe{sub 2}B have no change and a new W-containing phase, except the (Fe, W){sub 2}B with a certain tungsten solution, does not form, and that the fracture toughness of Fe{sub 2}B increases first and then decreases, while the hardness increases first and then has a little change. Compared with the fracture toughness (3.8 MPa{center_dot}m{sup 1/2}) of Fe{sub 2}B without tungsten addition, the toughness at 2.04 wt.% tungsten can be improved by about above 80% and achieves about 6.9 MPa{center_dot}m{sup 1/2}, and variation characteristics of hardness and toughness of Fe{sub 2}B were also testified by viewing the indentation marks and cracks on the Fe{sub 2}B, respectively. - Highlights: Black-Right-Pointing-Pointer Poor toughness of Fe2B decreases obviously the wear resistance of the alloy. Black-Right-Pointing-Pointer As W content increases, Fe2B's toughness increases first and then decreases. Black-Right-Pointing-Pointer As W content increases, Fe2B's hardness first increases and then has little change. Black-Right-Pointing-Pointer The toughness at 2.04 % W can be improved by above 80% more than that at 0% W.

36 MATERIALS SCIENCE↗

Tuning the morphology, stability and photocatalytic activity of TiO{sub 2} nanocrystal colloids by tungsten doping

Graphical abstract: - Highlights: • W{sup 6+}-doped TiO{sub 2} nanocrystal colloids were prepared by hydrothermal methods. • The properties of TiO{sub 2} nanocrystal colloids can be tuned by tungsten doping. • W{sup 6+}-doped TiO{sub 2} nanocrystal colloids show higher stability and dispersity. • W{sup 6+}-doped TiO{sub 2} nanocrystal colloids show higher photocatalytic activity. - Abstract: The effects of tungsten doping on the morphology, stability and photocatalytic activity of TiO{sub 2} nanocrystal colloids were investigated. The nanostructure, chemical state of Ti, W, O, and the properties of tungsten doped TiO{sub 2} samples were investigated carefully by TEM, XRD, XPS, UV–vis, PL and photocatalytic degradation experiments. And the structure–activity relationship was discussed according to the analysis and measurement results. The analysis results reveal that the morphology, zeta potential and photocatalytic activity of TiO{sub 2} nanocrystals can be easily tuned by changing the tungsten doping concentration. The tungsten doped TiO{sub 2} colloid combines the characters of high dispersity and high photocatalytic activity.

36 MATERIALS SCIENCE↗