Computational and experimental search for potential polyanionic K-ion cathode materials

Discovering high-energy cathode materials is critical to construct K-ion batteries for practical applications. Owing to the great success of layered oxides in Li- and Na-ion systems, K layered cathodes have also been investigated in recent years. However, the much larger size of K + compared to Li or Na introduces strong K + –K + interaction within the layer, which results in a sloped voltage profile thereby limiting the specific capacity and operating voltage. In contrast, polyanionic materials with a three-dimensional K + arrangement can effectively mitigate K + –K + interaction. In this work, ten K polyanionic compounds with theoretical capacity >100 mA h g –1 are screened from the Inorganic Crystal Structure Database as potential cathode materials for K-ion batteries. Among the ten proposed compounds, K 2 MnP 2 O 7 , K 2 Mn 2 P 2 O 7 F 2 , K 2 Fe 2 P 2 O 7 F 2 , and K 6 V 2 (PO 4 ) 4 with average voltage <4.5 V are synthesized and evaluated electrochemically. While the re-insertion of K into these compounds is not fully reversible, it may be related to the very high migration barrier that we compute for K ions. In addition, we show the successful synthesis of a series of K 3 V 3–x Cr x (PO 4 ) 4 (x = 0, 1, 2, 3) compounds. Among these, K 3 V 2 Cr(PO 4 ) 4 exhibits the largest reversible capacity, as revealed by the in situ investigation. Lastly, we find that the redox couples in many of these compounds sit at remarkably high potential, even higher than in equivalent Li compounds, which brings both opportunities and challenges in the future research of K polyanion cathodes.

25 ENERGY STORAGE↗

Influences of Mg Ions and Al Ions on Deposition Behavior of Supersaturated Silicic Acid - 20261

Silicic acid can change into various species such as deposit, colloidal, and soluble form under certain conditions: for example, gradual pH changes around geological disposal repositories. In particular, silicic acid deposits narrow groundwater flow paths, thereby restricting the flow of groundwater. Such effects may contribute to a delay in radionuclide migration. Previous studies have reported that silicic acid supersaturated in sodium and calcium ions can narrow the flow paths. This study examined the effect of magnesium (Mg) and aluminum (Al) ions on the deposition of supersaturated silicic acid on the solid phase. The deposition behavior of supersaturated silicic acid on the solid phase was investigated in a batch system while changing the initial supersaturation concentration, the coexisting ion concentration, and the amount of added solid phase. In the presence of Mg ions, silicic acid precipitation increased with increasing Mg ion concentration due to the influence of the electrolyte, and crosslinking reactions. The coexistence of Al ions significantly suppressed silicic acid deposition due to the formation of a covering on the solid surface during Al ion hydrolysis under conditions of high Al concentration (1.4 mM). On the basis of these experimental results, the apparent deposition rate constant of silicic acid was estimated to be in the range from 10{sup -11} to 10{sup -10} m/s. The Damkoehler number (the dimensionless number expressed by the ratio of the characteristic time of mass transfer and the chemical reaction constant) was sufficient to cause the clogging of the host rock by deposition. This suggests that supersaturated silicic acid deposition, regardless of the presence of Mg ions (and Al ions), contributes to improving barrier performance against radionuclide migration in the host rock. (authors)

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Diffusion and migration in polymer electrolytes

Mixtures of neutral polymers and lithium salts have the potential to serve as electrolytes in next-generation rechargeable Li-ion batteries. The purpose of this review is to expose the delicate interplay between polymer-salt interactions at the segmental level and macroscopic ion transport at the battery level. Since complete characterization of this interplay has only been completed in one system: mixtures of poly(ethylene oxide) and lithium bis(trifluoromethanesulfonyl)imide (PEO/LiTFSI), we focus on data obtained from this system. We begin with a discussion of the activity coefficient, followed by a discussion of six different diffusion coefficients: the Rouse motion of polymer segments is quantified by D seg , the self-diffusion of cations and anions is quantified by D self,+ and D self,- , and the build-up of concentration gradients in electrolytes under an applied potential is quantified by Stefan-Maxwell diffusion coefficients, D 0+ , D 0- , and D +- . The Stefan-Maxwell diffusion coefficients can be used to predict the velocities of the ions at very early times after an electric field is applied across the electrolyte. The surprising result is that D 0- is negative in certain concentration windows. A consequence of this finding is that at these concentrations, both cations and anions are predicted to migrate toward the positive electrode at early times. We describe the controversies that surround this result. Knowledge of the Stefan-Maxwell diffusion coefficients enable prediction of the limiting current. We argue that the limiting current is the most important characteristic of an electrolyte. Excellent agreement between theoretical and experimental limiting current is seen in PEO/LiTFSI mixtures. What sequence of monomers that, when polymerized, will lead to the highest limiting current remains an important unanswered question. It is our hope that the approach presented in this review will guide the development of such polymers.

25 ENERGY STORAGE↗

Impact of Oxygen Non-Stoichiometry on Near-Ambient Temperature Ionic Mobility in Polaronic Mixed-Ionic-Electronic Conducting Thin Films

Enhanced ionic mobility in mixed ionic and electronic conducting solids contributes to improved performance of memristive memory, energy storage and conversion, and catalytic devices. Ionic mobility can be significantly depressed at reduced temperatures, for example, due to defect association and therefore needs to be monitored. Measurements of ionic transport in mixed conductors, however, proves to be difficult due to dominant electronic conductivity. This study examines the impact of different levels of quenched-in oxygen deficiency on the oxygen vacancy mobility near room temperature as measured by a novel dynamic current-voltage analysis. A Pr 0.1 Ce 0.9 O 2-δ film was grown by pulsed laser deposition and subsequently annealed, from 400-600° C, in various oxygen partial pressures to modify its oxygen vacancy concentration while minimizing microstructural growth and cation segregation. To monitor changes in film non-stoichiometry, we leverage the existence of an optical absorption center, related to the oxidation state of Pr ions in Pr0.1Ce0.9O2-δ. The oxygen vacancy migration enthalpy was found to exhibit a small increase from 0.73± 0.04 to 0.79 ± 0.02 eV with increasing oxygen deficiency, while the pre-factor was found to increase by a factor of 135. Here, a nearly 13-fold increase in ionic mobility at 60 °C for increases in oxygen non-stoichiometry from 0.032 ± 0.001 to 0.042± 0.001 was thereby detected. Raman spectroscopy was employed to rule out changes in strain as the primary cause for the significant change in mobility. Several factors potentially contributing to the large pre-factor changes are examined and discussed. Insights into how ionic defect concentration can markedly impact ionic mobility should help in elucidating the origins of variations seen in nanoionic devices.

36 MATERIALS SCIENCE↗

A Dual Anion Chemistry-Based Superionic Glass Enabling Long-Cycling All-Solid-State Sodium-Ion Batteries

Glassy Na-ion solid-state electrolytes (GNSSEs) are an important group of amorphous SSEs. However, the insufficient ionic conductivity of state-of-the-art GNSSEs at room temperature lessens their promise in the development of all-solid-state Na-ion batteries (ASSNIBs) with high energy density and improved safety. Here we report the discovery of a new sodium superionic glass, 0.5Na 2 O 2 -TaCl 5 (NTOC), based on dual-anion sublattice of oxychlorides. The unique local structures with abundant bridging and non-bridging oxygen atoms contributes to a highly disordered Na-ion distribution as well as low Na + migration barrier within NTOC, enabling an ultrahigh ionic conductivity of 4.62 mS cm −1 at 25 °C (more than 20 times higher than those of previously reported GNSSEs). Moreover, the excellent formability of glassy NTOC electrolyte and its high electrochemical oxidative stability ensure a favourable electrolyte-electrode interface, contributing to superior cycling stability of ASSNIBs for over 500 cycles at room temperature. The discovery of glassy NTOC electrolyte would reignite research enthusiasm in superionic glassy SSEs based on multi-anion chemistry.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Uranyl oxalate species in high ionic strength environments: stability constants for aqueous and solid uranyl oxalate complexes

Uranyl ion, UO 2 2+ , and its aqueous complexes with organic and inorganic ligands can be the dominant species for uranium transport on the Earth surface or in a nuclear waste disposal system if an oxidizing condition is present. As an important biodegradation product, oxalate, C 2 O 4 2– , is ubiquitous in natural environments and is known for its ability to complex with the uranyl ion. Oxalate can also form solid phases with uranyl ion in certain environments thus limiting uranium migration. Therefore, the determination of stability constants for aqueous and solid uranyl oxalate complexes is important not only to the understanding of uranium mobility in natural environments, but also to the performance assessment of nuclear waste disposal. In this work, we developed a thermodynamic model for the UO 2 2+ –Na + –H + –Cl – –ClO 4 – –C 2 O 4 2– –NO 3 – –H 2 O system to ionic strength up to ~11 mol•kg –1 . We constrained the stability constants for UO 2 C 2 O 4 (aq) and UO 2 (C 2 O 4 ) 2 2– at infinite dilution based on our evaluation of the literature data over a wide range of ionic strengths up to ~11 mol•kg –1 . We also obtained the solubility constants at infinite dilution for solid uranyl oxalates, UO 2 C 2 O 4 •3H 2 O, based on the solubility data over a wide range of ionic strengths. The developed model will enable for the accurate stability assessment of oxalate complexes affecting uranium mobility under a wide range of conditions including those in deep geological repositories.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Local control of perpendicular magnetic anisotropy of Pd/Co multilayers via ion bombardment

In this work, we have controlled locally the magnetic anisotropy of PdCo multilayers using ion beam modification. First, we have used techniques with different probing depths to confirm that cobalt is partially oxidized in the Pd/Co multilayers exhibiting PMA fabricated by sputtering, presumably due to the diffusion of atmospheric oxygen migrated through the Pd capping layer. Then, low energy ion bombardment has been employed to induce a structural disorder in the upper layers of the multilayer, gradually reducing the PMA at local scale with increasing ion doses. Medium ion doses lead to a marked decline in PMA, resulting in equivalent magnetic anisotropy directions and the loss of characteristic labyrinthine magnetic domain morphology. High ion doses completely suppress PMA, yielding a typical in-plane shape anisotropy. Furthermore, by combining controlled PMA reduction via lithographic techniques, we create elongated structures displaying distinct magnetic responses; bombarded regions exhibit reduced PMA, whereas adjacent regions maintain their PMA. Notably, regions with reduced PMA do not disrupt the distribution of perpendicular magnetic domains in neighboring PMA regions, even at widths as narrow as 500 nm, demonstrating the robustness of the PMA domain structure.

Sebastiani-Tofano, Eugenia [Universidad Complutens↗

Solution-Based, Anion-Doping of Li 4 Ti 5 O 12 Nanoflowers for Lithium-Ion Battery Applications

Solution–based, anionic doping represents a convenient strategy with which to improve upon the conductivity of candidate anode materials such as Li 4 Ti 5 O 12 (LTO). As such, novel synthetic hydrothermally–inspired protocols have primarily been devised herein, aimed at the large–scale production of unique halogen–doped, micron–scale, three–dimensional, hierarchical LTO flower–like motifs. Although fluorine (F) doping has been explored, the use of chlorine (Cl) dopants is the primary focus here. Several experimental variables, such as dopant amount, lithium hydroxide concentration, and titanium butoxide purity, were probed and perfected. Furthermore, the Cl doping process did not damage the intrinsic LTO morphology. The analysis, based on interpreting a compilation of SEM, XRD, XPS, and TEM–EDS results, was used to determine an optimized dopant concentration of Cl. Electrochemical tests demonstrated an increased capacity via cycling of 12 % for a Cl–doped sample as compared with pristine LTO. Moreover, the Cl–doped LTO sample described in this study exhibited the highest discharge capacity yet reported at an observed rate of 2C for this material at 143mAh g –1 . Overall, these data suggest that the Cl dopant likely enhances not only the ion transport capabilities, but also the overall electrical conductivity of our as–prepared structures. Furthermore, to help explain these favorable findings, theoretical DFT calculations were used to postulate that the electronic conductivity and Li diffusion were likely improved by the presence of increased Ti 3+ ion concentration coupled with widening of the Li migration channel.

25 ENERGY STORAGE↗

The nonexistence of a paddlewheel effect in superionic conductors

Since the 1980s, the paddlewheel effect has been suggested as a mechanism to boost lithium-ion diffusion in inorganic materials via the rotation of rotor-like anion groups. However, it remains unclear whether the paddlewheel effect, defined as large-angle anion group rotations assisting Li hopping, indeed exists; furthermore, the physical mechanism by which the anion-group dynamics affect lithium-ion diffusion has not yet been established. In this work, we differentiate various types of rotational motions of anion groups and develop quaternion-based algorithms to detect, quantify, and relate them to lithium-ion motion in ab initio molecular dynamics simulations. Our analysis demonstrates that, in fact, the paddlewheel effect, where an anion group makes a large angle rotation to assist a lithium-ion hop, does not exist and thus is not responsible for the fast lithium-ion diffusion in superionic conductors, as historically claimed. Instead, we find that materials with topologically isolated anion groups can enhance lithium-ion diffusivity via a more classic nondynamic soft-cradle mechanism, where the anion groups tilt to provide optimal coordination to a lithium ion throughout the hopping process to lower the migration barrier. This anion-group disorder is static in nature, rather than dynamic and can explain most of the experimental observations. Our work substantiates the nonexistence of the long-debated paddlewheel effect and clarifies any correlation that may exist between anion-group rotations and fast ionic diffusion in inorganic materials.

36 MATERIALS SCIENCE↗

NaGaS 2 : An Elusive Layered Compound with Dynamic Water Absorption and Wide‐Ranging Ion‐Exchange Properties

Abstract Most ternary sulfides belonging to the MGaS 2 structure‐type have been known for many years and are well‐characterized. Surprisingly, there have been no reports of the NaGaS 2 composition, which contains Na, a monovalent cation slightly larger in size than Li, found in LiGaS 2 , a compound known for its non‐linear optical properties. Now it is demonstrated for the first time that the unique reversible water absorption in NaGaS 2 has resulted in its absence from previous reports owing to difficulties encountered when characterizing this compound by SC XRD. The layered structure of this compound coupled with uniquely easy migration of water molecules between the layers allows for ion exchange with 3d and 5f metal cations. Some cations, for example, Ni 2+ , facilitate exfoliation of the layers, providing a facile synthetic route to a new class of 2D chalcogenide materials and furthermore demonstrating that NaGaS 2 can readily uptake uranyl species from aqueous solutions.

Klepov, Vladislav V.↗

NaGaS 2 - an Elusive Layered Compound with Dynamic Water Absorption and Wide-Ranging Ion Exchange Properties

Most ternary sulfides belonging to the MGaS 2 structure-type have been known for many years and are well-characterized. Surprisingly, there have been no reports of the NaGaS 2 composition, which contains Na, a monovalent cation slightly larger in size than Li, found in LiGaS 2 , a compound known for its non-linear optical properties. Herein we demonstrate for the first time that the unique reversible water absorption in NaGaS 2 has resulted in its absence from the literature due to the difficulties that one encounters when characterizing this compound by SC XRD. The layered structure of this compound coupled with uniquely easy migration of water molecules between the layers allows for ion exchange with 3d and 5f metal cations. We established that some cations, e.g. Ni 2+ , facilitate exfoliation of the layers, providing a facile synthetic route to a new class of 2D chalcogenide materials and, in addition, demonstrating that NaGaS 2 can readily uptake uranyl species from aqueous solutions.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Understanding and design of interstitial oxygen conductors

Highly efficient oxygen-active materials that react with, absorb, and transport oxygen is essential for fuel cells, electrolyzers and related applications. While vacancy-mediated oxygen-ion conductors have long been the focus of research, they are limited by high migration barriers at intermediate temperatures (400–600 °C), which hinder their practical applications. In contrast, interstitial oxygen conductors exhibit significantly lower migration barriers enabling higher ionic conductivity at lower temperatures. This review systematically examines both well-established and recently identified families of interstitial oxygen-ion conductors, focusing on how their unique structural motifs such as corner-sharing polyhedral frameworks, isolated polyhedral, and cage-like architectures, facilitate low migration barriers through interstitial and/or interstitialcy diffusion mechanisms. A central discussion of this review focuses on the evolution of design strategies, from targeted donor doping, element screening, to physical-intuition descriptor material screening and machine learning approach, which leverage computational tools to explore vast chemical spaces in search for new interstitial conductors. The success of these strategies demonstrates that a significant, largely unexplored space remains for discovering high-performing interstitial oxygen conductors. Crucial features enabling high-performance interstitial oxygen diffusion include the availability of electrons for oxygen reduction and sufficient structural flexibility with accessible volume for interstitial accommodation and migration. This review concludes with a forward-looking perspective, proposing a knowledge-driven methodology that integrates current understanding with data-centric approaches to identify promising interstitial oxygen conductors outside traditional search paradigms. These approaches are expected to significantly accelerate the development of high-performance interstitial oxygen conductors for a variety of oxygen-active applications, ultimately paving the way for more efficient and sustainable energy technologies.

Interstitial oxygen conductors↗

Stabilizing a Li–Mn–O Cathode by Blocking Lattice O Migration through a Nanoscale Phase Complex

Among all intercalation cathodes for Li-ion batteries, Li–Mn–O layered oxides offer the highest initial energy density at the lowest cost, due to the joint contribution from cationic and anionic redox chemistry. However, the poor cycling capability, resulting from the continuous lattice O loss at high potentials (>4.5 V), hinders practical applications. Herein, we employed phase complex engineering to obtain a new Li–Mn–O nanohybrid cathode featuring the uniform and coherent integration of layered nanodomains and spinel nanodomains. The combination of DFT calculations, synchrotron-based transmission X-ray microscopy, in situ differential electrochemical mass spectrometry, in situ synchrotron XRD, and electrochemical tests demonstrated that the O migration path in layered nanodomains was blocked by the neighboring spinel nanodomains with a higher oxygen vacancy migration energy, thus effectively suppressing the irreversible lattice O loss at high potentials and enhancing the cycling stability in both capacity and average voltage. Finally, the strategy is experimentally demonstrated to be effective and it leads to a new path for developing stable high-energy-density cathode materials.

25 ENERGY STORAGE↗

Factors Affecting the Electron Conductivity in Single Crystal Li 7 La 3 Zr 2 O 12 and Li 7 P 3 S 11

One of the serious challenges in all solid-state Li ion batteries is neutral Li intrusion into the solid-state electrolyte that can ultimately cause catastrophic failure. One possibility for this is due to n-type electron conductivity that induces the reaction Li + + e – → Li 0 at sites where the potential is less than the Li + /Li potential. This paper reports hybrid density functional theory calculations of the electronic conductivity in two prototype single crystalline solid-state electrolytes, cubic Li 7 La 3 Zr 2 O 12 (c-LLZO) and Li 7 P 3 S 11 (LPS). The formation energies of important point defects that can affect electron conductivity are determined, and we find that the mechanism of n-type electron conductivity for both solid-state electrolytes is via “small” electron polaron hopping, where the quotes signify that substantial Li ion rearrangement is associated with the polaron formation and its migration. In both electrolytes, the formation energies for the small polarons at the Fermi energy are too high to generate measurable electron conductivity at room temperature. For c-LLZO, the concentration of electron polarons necessary to ensure charge neutrality from positively charged oxygen vacancies formed in synthesis can be significantly higher. Hence, the electron conductivity could be significant when measured with ion-blocking metal electrodes, and we discuss how the synthesis conditions could affect this magnitude. However, in the solid-state battery, these polarons are replaced by negatively charged Li vacancies so that the electron conductivity should remain minimal. For LPS single crystals, the inherent minimal electron conductivity is independent of synthesis conditions. Here we also show that the cost of forming Li 0 in bulk c-LLZO is enormous due to strain effects so that it could only potentially form at voids, grain boundaries, or around vacancy defects which relax the lattice strain.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

A Nearly Zero-Strain Li-Rich Rock-Salt Oxide with Multielectron Redox Reactions as a Cathode for Li-Ion Batteries

Li-rich oxide cathodes are drawing increasing attention as next-generation cathode materials for the development of high-energy-density Li-ion batteries due to their strikingly high capacities. However, transition-metal migration, irreversible structural phase transformations, and the irreversible release of oxygen are responsible for rapid capacity and voltage decay. This study reports a Li-rich cation-ordered rock-salt oxide Li x V 0.4 Ti 0.4 O 2 (LVTO, x = 0.97/1.2) with space group Fd$\bar{3}$m that delivers a high capacity of over 250 mAh g -1 and capacity retention up to 89% after 50 cycles. A comprehensive experimental analysis confirms that the capacity can be attributed to the reversible V 3+ /V 5+ multielectron cationic redox reactions and a minor contribution from reversible anionic redox reactions. Importantly, LVTO exhibits nearly zero-strain behavior upon (dis)charge cycling cycles, which is associated with reversible V migration from octahedral to tetrahedral sites. Here our results demonstrate that Li-rich rock-salt oxide LVTO could be a promising cobalt-free cathode material for Li-ion batteries.

25 ENERGY STORAGE↗

Defect-Mediated Diffusion Pathways in Spodumene Accelerate Lithium Transport

Lithium extraction from naturally occurring α-spodumene is hindered by poor lithium diffusivity, necessitating high-temperature phase transformation to a low-density β polymorph. Although β spodumene exhibits up to 5 orders of magnitude higher lithium-ion diffusivity, both phases have diffusion activation energies between 0.8 and 1 eV, indicating that polymorph density is not the controlling factor over diffusivity. We show that aluminum vacancies facilitate lithium-ion diffusion in α-spodumene by reducing the migration barrier from 2.4 to 0.9 eV. Bond valence site energy and nudged elastic band calculations show a new lithium local minimum site which promotes a one-dimensional percolation network by reducing the lithium intersite distance from 4.5 Å to 2.9 Å. However, aluminum vacancies are energetically unfavorable to percolate through the whole structure, resulting in very low net lithium diffusivity and highlighting the critical role of nonstoichiometric defects in facilitating lithium transport in rigid aluminosilicate structures.

Chemical structure↗

Hydrogen migration in inner-shell ionized halogenated cyclic hydrocarbons

Abstract We have studied the fragmentation of the brominated cyclic hydrocarbons bromocyclo-propane, bromocyclo-butane, and bromocyclo-pentane upon Br(3 d ) and C(1 s ) inner-shell ionization using coincidence ion momentum imaging. We observe a substantial yield of CH 3 + fragments, whose formation requires intramolecular hydrogen (or proton) migration, that increases with molecular size, which contrasts with prior observations of hydrogen migration in linear hydrocarbon molecules. Furthermore, by inspecting the fragment ion momentum correlations of three-body fragmentation channels, we conclude that CH x + fragments (with x = 0, …, 3) with an increasing number of hydrogens are more likely to be produced via sequential fragmentation pathways. Overall trends in the molecular-size-dependence of the experimentally observed kinetic energy releases and fragment kinetic energies are explained with the help of classical Coulomb explosion simulations.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗