A detailed study of the microstructure and thermal stability of typical SiC fibers

Highlights: • The cross-sectional microstructure and thermal stability of typical SiC fibers were characterized via SEM and TEM. • The SiC fiber with gradient microstructure has better properties than that with uniform microstructure. • The graphite exhibits straight planes on the fiber surface while they're turbostratic inside the fiber. Continuous SiC fibers have attracted increasing research interest for their significant application in aerospace and nuclear energy. Control of inhomogeneity and decrement of defects are crucial for improving the mechanical and high-temperature performance of SiC fibers. Thus an understanding of fine and detailed microstructural and microchemical distribution of SiC fibers is urgently needed. In the present work, the cross-sectional phase distributions, morphologies and defects of amorphous, non-stoichiometric and near-stoichiometric SiC fibers were well characterized. From surface to core, the amorphous and non-stoichiometric fibers exhibited uniform microstructures, but a gradient change along the radial direction was observed in the near-stoichiometric fiber. Nanosized SiC and turbostratic carbon (2–4 nm) were randomly distributed inside the amorphous fiber. A large amount of graphite surrounding SiC grains appears in the non-stoichiometric fiber which possess low strength and weak thermal stability. The near-stoichiometric fiber has transgranular fracturing, high strength and favorable thermal stability, and the graphite planes are turbostratic inside the fiber but straight on the surface. The results of both energy-dispersive X-ray spectrometry measurements and first-principles calculations demonstrate that Al atoms can occupy Si sites in the SiC grains. Our findings offer fine understanding for fabricating SiC fibers with superior properties.

77 NANOSCIENCE AND NANOTECHNOLOGY↗

Radiation defect dynamics in 3 C -, 4 H -, and 6 H -SiC studied by pulsed ion beams

Radiation damage behavior of SiC depends on its lattice structure. Here, we use a pulsed-ion-beam method to study defect interaction dynamics in 6H-SiC and damage buildup in 4H- and 6H-SiC irradiated at 100 °C with 500 keV Ar ions. These results are compared with previously reported data for Ar-ion-irradiated 3C- and 4H-SiC. We find that, for these irradiation conditions, damage buildup in 3C- and 6H-SiC is statistically indistinguishable and is significantly more efficient than in 4H-SiC. Within a stimulated amorphization model, 4H-SiC is described by a reduced amorphization cross-section constant, while the point defect cluster production cross-section is the same (within experimental errors) for the three polytypes studied. Moreover, 4H-SiC exhibits slower defect relaxation dynamics than 3C- and 6H-SiC. These results clearly demonstrate the importance of the lattice structure in damage buildup and defect interaction dynamics in SiC.

71 CLASSICAL AND QUANTUM MECHANICS, GENERAL PHYSIC↗

Thermal conductivity in nanocrystalline-SiC/C superlattices

We reported the formation of thin film superlattices consisting of alternating layers of nitrogen-doped SiC (SiC:N) and C. Periodically terminating the SiC:N surface with a graphitic C boundary layer and controlling the SiC:N/C thickness ratio yield nanocrystalline SiC grains ranging in size from 365 to 23 nm. Frequency domain thermo-reflectance is employed to determine the thermal conductivity, which is found to vary from 35.5 W m -1 K -1 for monolithic undoped α-SiC films to 1.6 W m -1 K -1 for a SiC:N/C superlattice with a 47 nm period and a SiC:N/C thickness ratio of 11. A series conductance model is employed to explain the dependence of the thermal conductivity on the superlatticestructure. Our results indicate that the thermal conductivity is more dependent on the SiC:N/C thickness ratio than the SiC:N grain size, indicative of strong boundary layerphonon scattering.

77 NANOSCIENCE AND NANOTECHNOLOGY↗

Role of Defects in Swelling and Creep of Irradiated SiC

Silicon carbide is a promising cladding material because of its high strength and relatively good corrosion resistance. However, SiC is brittle and therefore SiC-based components need to be carefully designed to avoid cracking and failure by fracture. In design of SiC-based composites for nuclear reactor applications it is essential to take into account how mechanical properties are affected by radiation and temperature, or in other words, what strains and stresses develop in this material due to environmental conditions. While thermal strains in SiC can be predicted using classical theories, radiation-induced strains are much less understood. In particular, it is critical to correctly account for radiation swelling and radiation creep, which contribute significantly to dimensional instability of SiC under radiation. Swelling typically increases logarithmically with radiation dose and saturates at relatively low doses (damage levels of a few dpa). Consequently, swelling-induced stresses are likely to develop within a few months of operation of a reactor. Radiation-induced volume swelling in SiC can be as high as 2%, which is significantly higher than the cracking strain of 0.1% in SiC. Swelling-induced strains will lead to enormous stresses and fracture, unless these stresses can be relaxed via some other mechanism. An effective way to achieve stress relaxation is via radiation creep. Although it has been hypothesized that both radiation swelling and radiation creep are driven by formation of defect clusters, existing models for swelling and creep in SiC are limited by the lack of understanding of specific defects that form due to radiation in the range of temperatures relevant to fuel cladding in light water reactors (LWRs) (<1000°C). For example, defects that can be detected with traditional transmission electron microscopy (TEM) techniques account only for 10-45% of the swelling measured in irradiated SiC. Here, we have undertaken an integrated experimental and modeling effort to discover the previously invisible defects in irradiated SiC and to determine the contributions of these defects to radiation swelling. Knowledge of the most stable defect structures and the rate controlling processes during defect evolution is essential for development of predictive models for swelling and creep as a function of temperature and radiation dose. This research has been enabled by state-of-the-art imaging techniques, such as the aberration corrected scanning transmission electron microscopy (STEM) (FEI TITAN) closely coupled with multi-scale models of stable defect clusters and their evolution.

22 GENERAL STUDIES OF NUCLEAR REACTORS↗

Mechanical and Thermophysical Properties of 3D-Printed SiC before and after Neutron Irradiation – FY21

This report presents the mechanical and thermophysical properties of 3D-printed SiC before and after neutron irradiation that have been evaluated to assess the fuel matrix material for the Transformational Challenge Reactor (TCR). The TCR fuel form consists of an additively-manufactured silicon carbide (SiC) matrix and uranium nitride tristructural isotropic (UN TRISO) fuel particles, which is manufactured through a newly developed processing route combining binderjet 3D printing, TRISO fuel particle loading, and chemical vapor infiltration (CVI). Because the fuel matrix is a primary component of the TCR core and its response to mechanical and thermal loads during operation is one of the most influential factors on the integrity of TCR core, testing and evaluation have focused on producing mechanical and thermophysical properties data for the binderjet/CVI SiC. Baseline mechanical and thermophysical properties were measured from the disk specimens printed for different and sizes orientations, which included equibiaxial flexural failure strength, elastic constants, thermal diffusivity and conductivity, density, and the coefficient of thermal expansion. Flexural failure strength datasets showed similar Weibull distributions regardless of sample variants including different orientations. The mean failure strengths of the 3D-printed SiC variants were in the range of 280–310 MPa, which are slightly lower than that of the chemical vapor deposition (CVD) SiC. Thermophysical test results showed that specific heat and thermal expansion are not sensitive to the build direction of SiC samples, while thermal conductivity is highly dependent on the build direction and can be correlated to the anisotropic character of the 3D-printed SiC. Neutron irradiation tests were carried out on the 3D-printed 6-mm diameter SiC disk specimens. Irradiation was carried to 2.3 dpa over a temperature range of 360–880°C. No significant degradation in strength was observed in SiC after irradiations in various conditions and with different orientations. Anisotropy that had been observed in the thermal conductivity of 3D-printed SiC prior to irradiation vanished after irradiation as the irradiation defect thermal resistivity accumulated in the material. Electron microscopy of the microstructure after neutron irradiation showed distinct defect morphologies in the heterogenous material, but no evidence for irradiation-induced cracking or degradation in the microstructure was observed.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

SiC cladding corrosion and mitigation

Silicon carbide (SiC) is a leading candidate for accident tolerant fuel. Testing of SiC in autoclaves at 360 C. degrees in simulated coolant resulted in little corrosion. However, testing of SiC tubes in the Massachusetts Institute of Technology (MIT) reactor manufactured in the same way had unacceptable corrosion levels. This in-reactor SiC corrosion issue is now being addressed by Westinghouse in tests being carried out at our Churchill, PA facility and in tests in the MIT reactor. The suspected driver for the excessive corrosion is the generation of oxidative water radiolysis products in the core. The MIT reactor was identified as running at H{sub 2} levels of ∼20 to 22 cc/kg coolant (cubic centimeters standard temperature and pressure per kilogram coolant) which were below those normally specified in operating pressurized water reactors (PWRs) of 25 to 50 cc/kg. Hydrogen is used to react with the radiolysis products to reduce them to water. The current MIT reactor tests will be run at H{sub 2} concentration levels of ∼50 cc/kg. The applicability of this approach has been supported by recent papers in the literature. Parallel testing at Churchill is being carried out to verify the efficacy of this approach using autoclaves operating at 345 C.degrees with H{sub 2}O{sub 2} injection to simulate the water radiolysis products. Various concentrations of H{sub 2} are being tested to determine the effect on SiC corrosion rate. Further studies are underway to investigate the effects of different SiC fabrication and structural parameters and to optimize for improved corrosion performance. This paper compares the results of the corrosion tests in the MIT reactor and the autoclave tests with H{sub 2}O{sub 2} injection and the effect of H{sub 2} injection on the SiC corrosion rate. The results of the autoclave tests with H{sub 2}O{sub 2} addition indicate that corrosion rates for SiC can be achieved that are much higher than those achieved in a reactor. It appears that the use of H{sub 2}O{sub 2} addition in flow through loops to simulate the corrosion rate of SiC samples in reactor is feasible. The use of H{sub 2} addition to reduce the corrosion rate in-reactor of SiC appears to be feasible.

21 SPECIFIC NUCLEAR REACTORS AND ASSOCIATED PLANTS↗

Preliminary Compendium of the Initial Conditions and Evolution of the Fundamental Interactions of SiC with Ag and Pd

Tri-structural isotropic (TRISO) particles are the fuel of choice for very-high temperature reactors. At the core, these spherical particles consist of an inner fuel kernel of UO{sub 2}, UC{sub 2} or a combination of both, which is coated radially outward by successive layers of low density pyrolytic graphite, an inner high density pyrolytic graphite layer, silicon carbide (SiC) and an outer high density pyrolytic graphite layer. SiC is the main diffusion barrier against the release of fission products due to its hardness and high melting point. Irradiation testing of TRISO particles indicates that trace amounts of metallic fission products can damage or potentially escape through the barrier layer. Surrogate experimental studies have previously been performed by various methods seeking to shed light on and explain the diffusion behavior of Ag and Pd. Although some of these experiments have yielded realistic diffusion coefficients the discrepancy of results between different groups is such that the essential details of the diffusive behavior are still to be fully understood. This work aims to understand the fundamental physical and chemical interactions that take place at the interface of SiC and Ag/Pd, and which give rise to the observed diffusion behavior of these metallic species in TRISO particles. Theoretical simulations of the diffusion of Ag through SiC have been exhaustive but typically yield bulk diffusion coefficients that due to the nature of bulk diffusion phenomena (i.e. slow diffusion) the diffusion coefficients are calculated to be orders of magnitude lower than what experimental observations suggest. This in part is due to the difficulty in simulating realistic models that include various polymorphs of SiC, and the dynamical structural transformations that SiC undergoes in the TRISO environment (which are also to be explained). The result is a particularly challenging problem to solve given that the initial conditions of the interactions of Ag and Pd with SiC are difficult to address, both in theoretical models and surrogate experiments. In order to improve these models the approach taken here is to consider fundamental interactions between Ag and SiC that take place in short time scales by varying the initial environmental conditions, i.e. annealing temperature and time, initial amounts of the metallic species (M) Ag, Pd in SiC/M/SiC multilayers. This work aims to understand the fundamental physical and chemical interactions that take place at the interface of SiC and Ag/Pd, and which give rise to the observed diffusion behavior of these metallic species in TRISO particles. In order to do so we have synthesized SiC/Ag/SiC and SiC/Pd/SiC multilayers of various thicknesses by PLD and characterized them using SEM/EDS. Initial results show that upon annealing Ag agglomerates and ruptures the SiC layer to be released. In the case of Pd a strong chemical interaction is deduced from the slow interlayer diffusion and limited release. Further studies using photoelectron spectroscopy and RHEED will be carried out in order obtain detailed information on the chemical and physical transitions that undergo upon annealing of these systems. (authors)

36 MATERIALS SCIENCE↗

Investigation of Fission Product Interaction with the SiC Containment Layer of High Turnup TRISO Fuel Particles

Tri-structural Isotropic (TRISO) encapsulated fuel particles are used in high-temperature gas-cooled nuclear reactors. Fuel performance is limited by the propensity of metallic fission products to be released under high temperature testing to simulate hypothesized accident scenarios. The current particle design consists of a 350 μm or 425 μm UO{sub 2} or UCO fuel kernel surrounded by a 100μm porous carbon buffer layer, a 40μm inner pyrolytic carbon (IPyC) layer, a 35μm high-density silicon carbide (SiC) layer, and a 40μm outer pyrolytic carbon (OPyC) layer. Of interest is the fission product interaction with the SiC layer, which provides the most structural support and is the main barrier to the diffusion of fission products. Previous laboratory examination studies have indicated the release of Ag through seemingly intact particles and the localized corrosion of the SiC due to Pd. Although a number of studies have been conducted, the specifics of both the Ag and Pd reaction mechanisms, in addition to U and Pu, through SiC are currently not well understood. This work aims to understand the pathways and kinetics of these interactions under normal operation as well as accident conditions. In order to improve our understanding of this, we have the unique opportunity to examine irradiated TRISO particles to study post-irradiation effects on these materials. Experimental data is necessary to constrain the current models used to predict the behavior of fission products in the SiC layer of TRISO fuels. This work aims to understand the interaction of fission products with the SiC containment layer in TRISO particles. We have systematically examined three SiC shells from irradiated TRISO particles using XAFS, TEM, and EDS. Results indicate the formation of palladium silicides, and uranium and plutonium carbides. Additionally, silver is seen to be metallic. Preliminary microscopy results indicate fission products throughout the SiC layer of the TRISO particles, and microstructural changes have been observed between the as-irradiated and safety tested particles. These results have provided key information on the fission product transport behavior through irradiated SiC at varying temperatures. Knowledge of these reaction pathways will allow for better simulation of the long-term behavior of TRISO fuels. They may also suggest ways to modify the SiC layer to improve fuel performance and mitigate fission product release, which is critical for safety strategies required to commercialize these nuclear fuel technologies. (authors)

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Development of Ti 3 SiC 2 MAX phase tubular structures for solar receiver applications

Solar receiver tubes are key components of concentrating solar-thermal power (CSP) systems that harvest solar energy. For better efficiency, the Gen3 CSP receivers, which collect heat into a heat transfer fluid, require a temperature exceeding 700 °C during operation and need to perform under extreme conditions of high temperature and high thermal stress. Operators are seeking CSP designs using new high-temperature structural materials with high thermal conductivity and high creep resistance to achieve a design life of 30 years and thus help recover the plant capital cost sooner. MAX phase materials, which consist of an early transition metal element, an A-group element, and carbon or nitrogen, are expected to exhibit high creep resistance as well as high fracture toughness. Here, in this paper, we describe fabricating both (1) dense Ti 3 SiC 2 MAX phase disks and (2) short-length tubes using field-assisted sintering technology (FAST). First, the disk samples that we fabricated are fully dense and contain ≈90 % Ti 3 SiC 2 MAX phase materials and ≈10 % TiC phase materials. We determined a flexure strength of 519 ± 32 MPa by conducting a four-point bending test at room temperature with rectangular bar samples of ≈100 % density. The thermal conductivity of the Ti 3 SiC 2 MAX phase samples, measured by light flashing analysis, decreases linearly from a value of 41 W . m -1 . K -1 at room temperature to a value of 36 W . m -1 . K -1 at 650 °C. A solar reflectance measurement of the Ti 3 SiC 2 MAX phase revealed that, temperature increases from 400 to 1400 °C, thermal emittance increases from 0.39 to 0.49, while selectivity decreases from 1.8 to 1.4, respectively. Whereas the surface oxidized MAX phase samples after 100 h exposure to air at 1000 °C exhibit that of SiC. Next, we discuss fabrication of the crack-free Ti 3 SiC 2 MAX phase tubular structures accomplished by using FAST processing in graphite bedding. A Ti 3 SiC 2 MAX phase content of > 95 % with traceable ≈3% remaining TiC phase and ≈15 % porosity were demonstrated after high-temperature annealing. An average fracture strength of ≈250 MPa was determined with Ti 3 SiC 2 MAX phase tubes of ≈85 % density by diametral compression testing at room temperature. Our work demonstrated that using FAST processing to produce Ti 3 SiC 2 MAX phase tubular structures for CSP receiver applications is a viable approach.

14 SOLAR ENERGY↗

Electric Drive Technologies Consortium (EDTC)/ Cost competitive, high-Performance, highly Reliable (CPR) Power Devices on 4H-SiC (Final Report)

4H-Silicon carbide (4H-SiC) is a wide bandgap semiconductor that offers superior material properties over silicon, including higher critical electric field, thermal conductivity, and electron saturation velocity. These advantages make 4H-SiC highly attractive for high-voltage, high-efficiency power electronics. However, realizing the full potential of SiC requires device technologies that are not only high-performing but also manufacturable and reliable under real-world operating conditions. This report summarizes the outcomes of a five-year R&D effort funded by the U.S. Department of Energy (DOE) under the Electric Drive Technologies Consortium (EDTC), focused on developing cost-competitive, high-performance, and highly reliable (CPR) power devices on 4H-SiC substrates. The program targeted scalable and manufacturable 1.2 kV-class SiC MOSFETs optimized for next-generation electric vehicles, renewable energy systems, and industrial power conversion. The project delivered transformative advancements in SiC power device performance and ruggedness. Particularly, Specific on-resistance (R on,sp ) was reduced by up to 37%, from ~4.0 m$\Omega \cdot$cm 2 in earlier designs to an industry-leading 2.40 m$\Omega \cdot$cm 2 , driven by optimized doping, refined JFET widths, and layout engineering. Breakdown voltages (BV) exceeded 1600 V, marking improvement over legacy baselines, and demonstrating the robustness of newly implemented junction profiles and edge terminations. Short-circuit withstand time (SCWT) saw a remarkable 4$\times$ increase, from ~2 $\mu$s to over 8 $\mu$s, achieved through the successful deployment of deep P-well structures (~1.8–2.0 $\mu$m) via channeling implantation. This innovative process breakthrough enabled precise junction formation without MeV-class implantation tools, reduced leakage under high field stress, and allowed even the shortest-channel devices (down to 0.3 $\mu$m) to achieve both high BV and excellent ruggedness—breaking the traditional trade-off between conduction efficiency and blocking capability. Several novel architectures pushed the performance envelope further. JBSFETs—featuring embedded Schottky portions—eliminated bipolar degradation and drastically reduced third-quadrant leakage, while Ladder MOSFETs introduced a clever orthogonal conduction path that achieved a 15.4% reduction in R on,sp over standard linear designs. Switching performance reached new benchmarks: short-channel devices showed a 31% reduction in total switching energy compared to 0.5 $\mu$m counterparts, while maintaining manageable gate drive requirements. Layout-optimized structures not only improved transconductance but also accelerated switching transitions, pointing to real-world benefits in converter-level efficiency. The devices also passed rigorous reliability validation. Stress-tested across TDDB, HTGB, HTRB, HVP, and burn-in, the devices screened under 30 V/10 hr and 43 V/1 s protocols consistently exhibited tighter lifetime distributions and long-term oxide robustness. These screening techniques proved effective in identifying latent defects and ensuring deployment-grade reliability. Meanwhile, advanced 3D TCAD simulations revealed and resolved electric field hotspots—particularly in HEXFET corners—where fields exceeding 4.8 MV/cm were mitigated through geometry-aware layout corrections. Overall, the results of this project demonstrate a manufacturable and scalable SiC power device platform that addresses key DOE performance targets for efficient, robust, and reliable 1.2kV 4H-SiC Power Devices. The developed technologies represent a meaningful step forward in the commercial readiness of high-voltage SiC solutions and provide a strong foundation for continued advancement in wide bandgap power electronics.

42 ENGINEERING↗

Assessment of SiC-CMC compatibility with components of actinide fuel systems

Silicon carbide (SiC) fiber reinforced SiC ceramic matrix composites (CMC) represent an alternative cladding material for accident tolerant fuel light water reactor (LWR) applications, however, data and technology gaps exist that need to be understood before SiC-CMCs can be considered. One technology gap is the understanding of fuel-clad chemical interactions (FCCI) in SiC-CMC clad LWR systems. A review of SiC interactions with relevant elements to the LWR fuel system is discussed. Insights are drawn from research focusing on the use of SiC for high temperature electronics applications and high temperature structural materials applications as well as insights from tristructural-isotropic (TRISO) coated particle fuel development, where SiC is a critical component of the TRISO design. The interactions discussed in this review are framed relative to the expected conditions for SiC-CMC cladding application. Furthermore, the general observation is that limited risk of FCCI exists under normal operating conditions for SiC-CMC cladding systems in LWR applications.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Influence of SiC microstructure on its corrosion behavior in molten FLiNaK salt

The influence of the microstructure on the corrosion rate of three monolithic SiC samples in FLiNaK salt at 900 °C for 250 h was studied. The SiC samples, labeled as SiC-1, SiC-2, and SiC-3, had corrosion rates of 0.137, 0.020, and 0.043 mg/cm 2 h, respectively. Compared with grain size and the presence of special grain boundaries (i.e., Σ3), the content of high-angle grain boundaries (HAGBs) appeared to have the strongest influence on the corrosion rate of SiC in FLiNaK salt, since the corrosion rate increased six times as the concentration of high-angle grain boundaries increased from 19 to 32% for SiC-2 and SiC-1, respectively. The results here stress the importance of controlling the content of HAGBs during the production process of SiC.

36 MATERIALS SCIENCE↗

Morphology and mechanism study for the synthesis of ZrB{sub 2}–SiC powders by different methods

ZrB{sub 2}–SiC ceramics, whose SiC is generally incorporated into the system by mechanical mixing, are known to have better performance than monolithic ZrB{sub 2}. Therefore, synthesis of duplex ZrB{sub 2}–SiC powders is beneficial for improving sinterability and mechanical properties of ZrB{sub 2}–SiC composites. In the present work, ZrB{sub 2}–SiC duplex powders with different morphologies were synthesized at 1550 °C for 2 h using as-synthesized amorphous hydrous ZrO{sub 2}–SiO{sub 2}. Both precipitation and sol–gel methods were used to prepare ZrO{sub 2}–SiO{sub 2} precursors. ZrB{sub 2}–SiC powder derived from precipitation method presented a rod-like morphology with smaller irregular particles adhering to them. And the morphology from sol–gel method was equiaxed shape with a very uniform distribution for principal components of Zr and Si. - Graphical abstract: SEM images of the ZrB2-SiC powders obtained by different methods. Display Omitted - Highlights: • ZrB{sub 2}–SiC powders with different morphologies were synthesized. • Precipitation and sol–gel methods were used to prepare ZrO{sub 2}–SiO{sub 2} precursors. • Possible mechanisms of morphology formation were investigated. • This work provided a potential way of morphology control for raw powders. • The synthesized duplex powders achieved a uniform distribution of SiC in ZrB{sub 2}.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Bamboo-like 3C-SiC nanowires with periodical fluctuating diameter: Homogeneous synthesis, synergistic growth mechanism, and their luminescence properties

Herein, bamboo-like 3C-SiC nanowires have been successfully fabricated on homogeneous 6H-SiC substrate by a simple chemical vapor reaction (CVR) approach. The obtained 3C-SiC nanostructure with periodical fluctuating diameter, is composed of two alternating structure units, the typical normal-sized stem segment with perfect crystallinity and obvious projecting nodes segment having high-density stacking faults. The formation of the interesting morphology is significantly subjected to the peculiar growth condition provided by the homogeneous substrate as well as the varying growth elastic energy. Furthermore, the photoluminescence (PL) performance measured on the bamboo-like SiC nanowire shows an intensive emission peaks centered at 451 nm and 467 nm, which has been expected to make a positive progress toward the optical application of the SiC-based one-dimensional (1D) nanostructures, such as light emission diode (LED). - Graphical abstract: Based on the synergistic growth mechanism from homogeneous substrate and elastic energy, bamboo-like 3C-SiC nanowires with periodically fluctuating diameter have been synthesized on 6H-SiC. The blue-violet light emission properties of the bamboo-like nanowires have also been investigated for exploring their peculiar optical application. - Highlights: • Bamboo-like 3C-SiC nanowires with periodically fluctuating diameter have been synthesized on 6H-SiC. • A synergistic growth mechanism from homogeneous substrate and elastic energy has been proposed firstly. • The blue-violet light emission properties of the products displayed peculiar optical application.

36 MATERIALS SCIENCE↗

Influence of surface morphology and UFG on damping and mechanical properties of composite reinforced with spinel MgAl{sub 2}O{sub 4}-SiC core-shell microcomposites

Interface between ceramic particulate and matrix is known to control the response of the materials and functionality of the composite. Among numerous physical properties, grain structure of the materials has also played a significant role in defining the behaviour of metal matrix composites. Usually, silicon carbide (SiC) particles show poor interfacial wettability in aluminium melt. Herein, we were successfully synthesized magnesium oxide (MgO) and nanocrystalline magnesium aluminate (MgAl{sub 2}O{sub 4}) spinel coated silicon carbide (SiC) core-shell micro-composites through sol-gel technique to improve the wettability of dispersoids. Core-shell structures of submicron size were thoroughly investigated by various characterization techniques. Further, aluminium matrix composites incorporated with pristine SiC, MgO grafted SiC and MgAl{sub 2}O{sub 4} grafted SiC particles were fabricated by stir casting technique, respectively. Additionally, as-cast composites were processed via friction stir processing (FSP) technique to observe the influence of grain refinement on mechanical and damping properties. Electron back scattered diffraction (EBSD), Field emission scanning electron microscopy (FE-SEM) and X-ray energy dispersion spectroscopy (EDX) analysis were conducted for investigating grain size refinement, adequate dispersion, stability and de-agglomeration of encapsulated SiC particles in aluminium matrix. The mechanical as well as thermal cyclic (from − 100 to 400 °C) damping performance of the as-cast and friction stir processed composites were studied, respectively. Finally, the enhanced properties were attributable to reduced agglomeration, stabilization and proper dispersion of the tailored SiC particles Al matrix. - Highlights: •Synthesizing a novel coating layer of MgO and MgAl{sub 2}O{sub 4} spinel onto SiC particles •Significant improvement in UTS and hardness by reinforcing tailored SiC in Al •Significant grain refinements were obtained through FSP •SiC/MgAl{sub 2}O{sub 4}/Al exhibits ~ 61% higher storage modulus as compare to pure Al after FSP.

36 MATERIALS SCIENCE↗

Microstructure and nanoindentation analysis of Mg-SiC nanocomposite powders synthesized by mechanical milling

Highlights: • Mechanical milling as an effective solution to reach a homogeneous distribution of SiC nanoparticles up to 10 vol% in Mg matrix • No deformation twinning in the nanostructured Mg matrix even after the severe plastic deformation and hard SiC nanoparticles up to 10 vol%. • Significant enhancement of nanohardness and reduced elastic modulus in the milled nanocomposite powders - Abstract: Mixtures of magnesium powder and SiC nanoparticles at various volume fractions were mechanically milled to produce nanocrystalline Mg-SiC nanocomposites. X-ray diffraction (XRD), scanning electron microscopy (SEM) and transmission electron microscopy (TEM) were utilized to characterize the microstructure of the milled powders. The microstructural evidences revealed that mechanical milling is a proper method to achieve a uniform distribution of the SiC nanoparticles, even up to 10% in the Mg matrix. Based on the results, higher volume fraction of the SiC nanoparticles raise the value of measured microstrain and reduce the crystallite size of the Mg matrix. The TEM results pointed to the fact that no deformation twinning takes place in the nanostructured Mg matrix even after severe plastic deformation through mechanical milling and the presence of hard SiC nanoparticles up to 10 vol%. The effects of nanoparticle volume fraction on mechanical properties of the milled Mg-SiC nanocomposites were evaluated using nanoindentation tests. The results clearly showed a significant enhancement of nanohardness and reduced elastic modulus in the milled powders compared to that of the reference material namely as-received pure magnesium. It was found that the SiC nanoparticles (even up to 10 vol%), well distributed in the magnesium matrix, remarkably improve the reduced elastic modulus and nanohardness of the nanocomposite powders.

77 NANOSCIENCE AND NANOTECHNOLOGY↗

Phase evolution during spark plasma sintering of novel Si3N4-doped TiB2–SiC composite

Highlights: • The effect of Si{sub 3}N{sub 4} addition on microstructure of TiB{sub 2}–SiC composite was studied. • Fully dense TiB{sub 2}-based composite was obtained by addition of SiC and Si{sub 3}N{sub 4}. • TiC, B{sub 4}C and SiO{sub 2} were formed in Si{sub 3}N{sub 4}-free and Si{sub 3}N{sub 4}-doped TiB{sub 2}–SiC ceramics. • TiN and BN were in-situ formed only in Si{sub 3}N{sub 4}-doped TiB{sub 2}–SiC sample. - Abstract: Spark plasma sintering process was employed to fabricate TiB{sub 2}–SiC and novel Si{sub 3}N{sub 4}-doped TiB{sub 2}–SiC ceramic composites at 1900 °C for 7 min under 40 MPa. The microstructural development of TiB{sub 2}-based composites was significantly influenced by the addition of SiC as a reinforcement phase and Si{sub 3}N{sub 4} as a sintering aid. Thermodynamic assessment, X-ray diffractometry, scanning electron microscopy and energy dispersive spectroscopy disclosed the in-situ formation of TiC, B{sub 4}C and SiO{sub 2} in both samples as well as TiN and BN in the Si{sub 3}N{sub 4}-doped TiB{sub 2}–SiC sample through the chemical reactions of SiC and Si{sub 3}N{sub 4} additives with the surface oxide impurities of TiB{sub 2} particles (TiO{sub 2} and B{sub 2}O{sub 3}). The elimination of harmful oxide layers and the in-situ formation various secondary phases had remarkable influences on the sinterability and final microstructure of TiB{sub 2}.

36 MATERIALS SCIENCE↗

The epitaxial growth of (1 1 1) oriented monocrystalline Si film based on a 4:5 Si-to-SiC atomic lattice matching interface

Highlights: ► A monocrystalline Si film was demonstrated by XRD to epitaxially grow on the 6H-SiC substrate. ► A 4:5 Si-to-SiC lattice matching structure was observed at the Si/SiC interface. ► The calculated value of the actual lattice mismatch is only 0.26%. ► Defects can be effectively reduced at the 4:5 Si-to-SiC lattice matching Si/SiC interface. -- Abstract: Due to a huge lattice mismatch of about 20% theoretically existing between SiC and Si, it is difficult for growing monocrystalline Si/SiC heterojunction to realize the light control of SiC devices. However, based on a 4:5 Si-to-SiC atomic lattice matching interface structure, the monocrystalline Si films were epitaxially prepared on the 6H-SiC (0 0 0 1) substrate by hot-wall chemical vapor deposition in our work. The film was characterized by X-ray diffraction analysis with only (1 1 1) orientation occurring. The X-ray rocking curves illustrated good symmetry with a full width at half maximum of 0.4339° omega. A 4:5 Si-to-SiC atomic matching structure of the Si/6H-SiC interface clearly observed by the transmission electron microscope revealed the essence of growing the monocrystalline Si film on the SiC substrate.