Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “RUPTURES”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 253 records · Page 14

Effect of heating method on stress-rupture life

The effect of radiant(furnace), resistance(electric current), burner(hot gas stream), and a combination of resistance and burner heating on intermediate time (100 to 300 hr) stress-rupture life and reduction of area was evaluated. All heating methods were studied using the nickel-based alloy Udimet 700 while all but burner heating were evaluated with the cobalt-based alloy Mar-M 509. Limited test results of eight other superalloys were also included in this study. Resistance heated specimens had about 20 to 30 percent of the stress-rupture life of radiant heated specimens. The limited burner heating data showed about a 50 percent life reduction as compared to the radiant heated tests. A metallurgical examination gave no explanation for these reductions.

Bizon, P. T.↗

Creep-rupture behavior of seven iron-base alloys after long term aging at 760 deg in low pressure hydrogen

Seven candidate iron-base alloys for heater tube application in the Stirling automotive engine were aged for 3500 hours at 760 C in argon and hydrogen. Aging degraded the tensile and creep-rupture properties. The presence of hydrogen during aging caused additional degradiation of the rupture strength in fine grain alloys. Based on current design criteria for the Mod 1 Stirling engine, N-155 and 19-9DL are considered the only alloys in this study with strengths adequate for heater tube service at 760 C.

Witzke, W. R.↗

Creep and creep rupture of laminated graphite/epoxy composites

An incremental numerical procedure based on lamination theory is developed to predict creep and creep rupture of general laminates. Existing unidirectional creep compliance and delayed failure data is used to develop analytical models for lamina response. The compliance model is based on a procedure proposed by Findley which incorporates the power law for creep into a nonlinear constitutive relationship. The matrix octahedral shear stress is assumed to control the stress interaction effect. A modified superposition principle is used to account for the varying stress level effect on the creep strain. The lamina failure model is based on a modification of the Tsai-Hill theory which includes the time dependent creep rupture strength. A linear cumulative damage law is used to monitor the remaining lifetime in each ply.

Dillard, D. A.↗

Creep rupture of polymer-matrix composites

The time-dependent creep-rupture process in graphite-epoxy laminates is examined as a function of temperature and stress level. Moisture effects are not considered. An accelerated characterization method of composite-laminate viscoelastic modulus and strength properties is reviewed. It is shown that lamina-modulus master curves can be obtained using a minimum of normally performed quality-control-type testing. Lamina-strength master curves, obtained by assuming a constant-strain-failure criterion, are presented along with experimental data, and reasonably good agreement is shown to exist between the two. Various phenomenological delayed failure models are reviewed and two (the modified rate equation and the Larson-Miller parameter method) are compared to creep-rupture data with poor results.

Brinson, H. F.↗

Structure and creep rupture properties of directionally solidified eutectic gamma/gamma-prime-alpha alloy

A simple ternary gamma/gamma-prime-alpha alloy of nominal composition (wt-%) Ni-32Mo-6Al has been directionally solidified at 17 mm/h and tested in creep rupture at 1073, 1173, and 1273 K. A uniform microstructure consisting of square-shaped Mo fibers in a gamma + gamma-prime matrix was found despite some variation in the molybdenum and aluminum concentrations along the growth direction. Although the steady-state creep rate is well described by the normal stress temperature equation, the stress exponent (12) and the activation energy (580 kJ/mol) are high. The rupture behavior is best characterized by the Larson-Miller parameter where the constant equals 20.

Whittenberger, J. D.↗

Effects on stress rupture life and tensile strength of tin additions to Inconel 718

Because Inconel 718 represents a major use of columbium and a large potential source of columbium for aerospace alloys could be that of columbium derived from tin slags, the effects of tin additions to Inconel 718 at levels which might be typical of or exceed those anticipated if tin slag derived columbium were used as a melting stock were investigated. Tin was added to 15 pound Inconel 718 heats at levels varying from none added to approximately 10,000 ppm (1 wt%). Limited 1200 F stress rupture testing was performed at stresses from 68,000 to 115,000 psi and a few tensile tests were performed at room temperature, 800 and 1200 F. Additions of tin in excess of 800 ppm were detrimental to ductility and stress rupture life.

Dreshfield, R. L.↗

Correlation of Rupture Life, Creep Rate, and Microstructure for Type 304 Stainless Steel

The stress and temperature sensitivites of the rupture life and secondary creep rate were examined in detail for a single heat of type 304 stainless steel (9T2796). Assuming that the rupture life has a power law stress dependency, relatively small differences in the stress exponent were observed over a broad range of stress and temperature. In contrast, large changes were observed for equivalent parameter for secondary creep rate. As a result of these differences, the Monkman-Grant correlation was sensitive to stress and temperature below 650 C. Metallurgical studies based on light and transmission electron microscopy suggested that the temperature and stress sensitivities of secondary creep rate at temperatures below 650 C were related to features of the substructure not present at higher temperature. Specifically, the presence of a fine dislocation network stabilized by precipitates altered the stress and temperature sensitivities relative to what might be expected from high temperature studies.

Swindeman, R. W.↗

A continuous damage model based on stepwise-stress creep rupture tests

A creep damage accumulation model is presented that makes use of the Kachanov damage rate concept with a provision accounting for damage that results from a variable stress history. This is accomplished through the introduction of an additional term in the Kachanov rate equation that is linear in the stress rate. Specification of the material functions and parameters in the model requires two types of constituting a data base: (1) standard constant-stress creep rupture tests, and (2) a sequence of two-step creep rupture tests.

Robinson, D. N.↗

Creep rupture behavior of Stirling engine materials

The automotive Stirling engine, being investigated jointly by the Department of Energy and NASA Lewis as an alternate to the internal combustion engine, uses high-pressure hydrogen as the working fluid. The long-term effects of hydrogen on the high temperature strength properties of materials is relatively unknown. This is especially true for the newly developed low-cost iron base alloy NASAUT 4G-A1. This iron-base alloy when tested in air has creep-rupture strengths in the directionally solidified condition comparable to the cobalt base alloy HS-31. The equiaxed (investment cast) NASAUT 4G-A1 has superior creep-rupture to the equiaxed iron-base alloy XF-818 both in air and 15 MPa hydrogen.

Titran, R. H.↗

Elevated temperature tension, compression and creep-rupture behavior of (001)-oriented single crystal superalloy PWA 1480

Tensile and compressive flow behavior at various temperatures and strain rates, and tensile creep rupture behavior at 850 and 1050 C and various stresses were studied for (001)-oriented single crystals of the Ni-base superalloy PWA 1480. At temperatures up to 760 C, the flow stress is insensitive to strain rate and of greater magnitude in tension than in compression. At temperatures of 800 C and above, the flow stress decreases continuously with decreasing strain rate and the tension/compression anisotropy diminishes. The second stage creep rate and rupture time exhibited power law relationships with the applied stress for both 850 and 1050 C, however with different stress dependencies. The stress exponent for the steady state creep rate was about 7 at 1050 C, but much higher at 850 C, about 12. Directional coarsening of the gamma' phase occurred during creep at 1050 C, but not at 850 C.

Hebsur, Mohan G.↗

Rupture testing for the quality control of electrodeposited copper interconnections in high-speed, high-density circuits

Printed Wiring Multilayer Board (PWMLB) structures for high speed, high density circuits are prone to failure due to the microcracking of electrolytic copper interconnections. The failure can occur in the foil that makes up the inner layer traces or in the plated through holes (PTH) deposit that forms the layer to layer interconnections. It is shown that there are some distinctive differences in the quality of Type E copper and that these differences can be detected before its use in a PWMLB. It is suggested that the strength of some Type E copper can be very low when the material is hot and that it is the use of this poor quality material in a PWMLB that results in PTH and inner layer microcracking. Since the PWMLB failure in question are induced by a thermal stress, and since the poorer grades of Type E materials used in these structures are susceptible to premature failure under thermal stress, the use of elevated temperature rupture and creep rupture testing is proposed as a means for screening copper foil, or its PTH equivalent, in order to eliminate the problem of Type E copper microcracking in advanced PWMLBs.

Zakraysek, Louis↗

Preliminary evaluation of tensile and stress-rupture behavior of W + 24 at. pct Re + 0.4 at. pct HfC wire

Results are presented of an evaluation of tensile properties and stress-rupture bahavior of a small-diameter W24ReHfC (W-24Re-0.4(HfC)) wire, which is considered to be an excellent reinforcing fiber candidate for a variety of metal-matrix composites. The results were compared to data of Petrasek (1972) on W4ReHfC (W-4Re-0.4(HfC)) wire. It was found that the room-temperature (RT) tensile strength of the W24ReHfC wire was about 3250 MPa, higher than that of the W4ReHfC (3160 MPa) and WHfC (2250 MPa) wires. Above 1366 K, the W4ReHfC wire had both a greater tensile strength and the stress rupture strength than the W24ReHfC wire.

Yun, H. M.↗

Behavior of Forged S-816 Turbine Blades in Steady-state Operation of J33-9 Turbojet Engine with Stress-rupture and Metallographic Evaluations / by F. B.garrett, C. A. Gyorgak, and J. W. Weeton

An investigation was conducted to determine the behavior of recently produced, forged S-816 turbine blades in a full-scale turbojet engine, and in particular, the scatter in performance of the alloy. The turbine blades were operated as continuously as possible at a temperature of 1500 degrees F and a centrifugal stress of 21,500 pounds per square inch. The operating lives of the turbine blades varied from 181 to 539 hours, a range of 358 hours. Stress-rupture properties of specimens cut from blade airfoils also varied considerably, as much as 1257 hours at 20,000 pounds per square inch and 1500 degrees F. Since the variability of scatter of stress-rupture data is greater than that of blade performance, the scatter is probably caused by variations in the properties of the forged blades rather than by variations caused by engine operation or installation of the blades. Metallographic examinations were made to determine possible causes of the scatter and although numerous differences in microstructures of blades were found, no consistent tendencies were observed and the findings did not permit an explanation of the scatter of blade performance. The results of the metallographic examinations and of the physical tests indirectly indicated variables in the fabricating method caused the scatter in properties.

Garrett, Floyd B↗

Statistical scaling relationships and size effects in the strength and creep rupture of fibrous composites

In this presentation we discuss a new theoretical model and supporting experimental results for the strength and lifetime in creep rupture of unidirectional, carbon fiber/epoxy matrix composites at ambient conditions. First we review the 'standard' Weibull/power-law methodology that has been standard practice. Then we discuss features of a recent model which build on the statistical aspects of fiber strength, micromechanical aspects of stress transfer around fiber breaks, and time-dependent creep of the matrix. The model is applied to 'microcomposites' consisting of seven fibers in a matrix for which strength and creep-rupture data are available. The model yields Weibull distributions in an envelope format for both strength and lifetime. The respective shape, scale and power-law parameters depend on such parameters as the Weibull shape parameter for fiber strength, the exponent for matrix creep, the effective load transfer length (which grows in time due to matrix creep) and the critical cluster size for failed fibers. The experimental results are consistent with the theory, though time-dependent debonding appears to be part of the failure process.

Phoenix, S. Leigh↗

Comparison of the Tensile, Creep, and Rupture Strength Properties of Stoichiometric SiC Fibers

Tensile strength, creep strength, and rupture strength properties were measured for the following types of polymer-derived stoichiometric SiC fibers: Hi-Nicalon Type S from Nippon Carbon, Tyranno SA from Ube, and Sylramic from Dow Corning. Also included in this study were an earlier version of the SA fiber plus two recent developmental versions of the Sylramic fiber. The tensile strength measurements were made at room temperature on as-received fibers and on fibers after high-temperature inert exposure. The creep-rupture property data were obtained at 1400 deg C in air as well as, argon. Some fiber types showed strong effects of environment on their strength properties. These results are compared and discussed in terms of underlying mechanisms and implications for ceramic composites.

Yun, H. M.↗

Long-Term Creep and Creep Rupture Behavior of Woven Ceramic Matrix Composites

Tensile creep behavior of SiC/SiNC ceramic matrix composites at elevated temperatures and at various stress levels have been investigated for turbine engine applications. The objective of this research is to present creep behavior of SiC/SiCN composites at stress levels above and below the monotonic proportional limit strength and predict the life at creep rupture conditions. Tensile creep-rupture tests were performed on an Instron 8502 servohydraulic testing machine at constant load conditions up to a temperature limit of 1000 C. Individual creep curves indicate three stages such as primary, secondary, and tertiary. The creep rate increased linearly at an early stage and then gradually became exponential at higher strains. The stress exponent and activation energy were also obtained at 700 and 1000 C. The specimen lifetime was observed to be 55 hrs at 121 MPa and at 700 C. The life span reduced to 35 hrs at 143 MPa and at 1000 C. Scanning electron microscopy observations revealed significant changes in the crystalline phases and creep damage development. Creep failures were accompanied by extensive fiber pullout, matrix cracking, and debonding along with fiber fracture. The creep data was applied to Time-Temperature-Stress superposition model and the Manson-Haferd parametric model for long-time life prediction.

Haque, A.↗

Temperature Dependence on the Strength and Stress Rupture Behavior of a Carbon-Fiber Reinforced Silicon Carbide (C/SiC) Composite

Tensile strengths and stress rupture lives of carbon-fiber reinforced silicon carbide (C/SiC) specimens were measured at 800 C and are compared to previously reported 1200 C data. All tests were conducted in an environmental chamber containing 1000 ppm of oxygen in argon. The average 800 C tensile strength of 610 MPa is 10% greater than at 1200 C. Average stress rupture lives at 800 C were 2.5 times longer than those obtained at 1200 C. The difference in the 800 and 1200 C lives is related to the oxidation rate of the reinforcing carbon fibers, which is the primary damage mode of C/SiC composites in oxygen-containing environments.

Verrilli, Michael J.↗