Microstructure and electrical properties of LaNiO{sub 3} thin films by RF sputtering for the growth of (Pb,La)(Zr,Ti)O{sub 3} films on silicon and nickel substrates
Conductive LaNiO{sub 3} (LNO) thin films were deposited on Si substrates by RF sputtering at room temperature to 600 Degree-Sign C. X-ray diffraction of the LNO films showed that preferred orientation varied from (100) below 500 Degree-Sign C to (110) at 600 Degree-Sign C at deposition temperature of 200-600 Degree-Sign C. The room temperature resistivity was 2250-3400 {mu}{Omega}-cm at the range of 200 Degree-Sign C {approx}500 Degree-Sign C. The LNO films, deposited at room temperature, were postannealed in air from 500 to 800 Degree-Sign C, and the resistivity value was 280 {mu}{Omega}-cm at a postannealing temperature of 600 Degree-Sign C. Subsequently, sol-gel derived (Pb,La)(Zr,Ti)O{sub 3} thin films were deposited on LNO-buffered nickel substrates and characterized, the results were compared to those of the same films on silicon substrates. The comparison demonstrated that the performance characteristics of the LNO-buffered nickel foils are similar to those of LNO-buffered silicon substrates. Thus, LNO films prepared by the sputtering method can act as an effective barrier layer on nickel substrates for embedded microelectronic devices.