Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “LiF”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 253 records · Page 14

Thermophysical properties of FLiBe using moment tensor potentials

Fluoride salts are prospective materials for applications in some next-generation nuclear reactors and their thermophysical properties at various conditions are of interest. Experimental measurement of the properties of these salts is often difficult and, in some cases, unfeasible due to challenges from high temperatures, impurity control, and corrosivity. Therefore, accurate theoretical methods are needed for fluoride salt property prediction. In this work, we used moment tensor potentials (MTP) to approximate the potential energy surface of eutectic FLiBe (66.6% LiF – 33.3% BeF2) predicted by the ab initio (DFT-D3) method. Here, we then used the developed potential and molecular dynamics to obtain several thermophysical properties of FLiBe, including radial distribution functions, density, self-diffusion coefficients, thermal expansion, specific heat capacity, bulk modulus, viscosity, and thermal conductivity. Our results show that the MTP potential approximates the potential energy surface accurately and the overall approach yields very good agreement with experimental values. The converged fitting can be obtained with less than 600 configurations generated from DFT calculations, which data can be generated in just 1200 core hours on today's typical processors. The MTP potential is faster than many machine learning potentials and about one order of magnitude slower than widely used empirical molten salt potentials such as Tosi/Fumi.

36 MATERIALS SCIENCE↗

Modeling athermal phonons in novel materials using the G4CMP simulation toolkit

Understanding phonon and charge propagation in superconducting devices plays an important role in both performing low-threshold dark matter searches and limiting correlated errors in superconducting qubits. The Geant4 Condensed Matter Physics (G4CMP) package, originally developed for the Cryogenic Dark Matter Search (CDMS) experiment, models charge and phonon transport within silicon and germanium detectors and has been validated by experimental measurements of phonon caustics, mean charge-carrier drift velocities, and heat pulse propagation times. Here, in this work, we present a concise framework for expanding the capabilities for phonon transport to a number of other novel substrate materials of interest to the dark matter and quantum computing communities, including sapphire (Al 2 O 3 ), gallium arsenide (GaAs), lithium fluoride (LiF), calcium tungstate (CaWO 4 ), and calcium fluoride (CaF 2 ). We demonstrate the use of this framework in generating phonon transport properties of these materials and compare these properties with experimentally-determined values where available.

46 INSTRUMENTATION RELATED TO NUCLEAR SCIENCE AND ↗

Experimental study of vorticity-strain interactions in turbulent premixed counterflow flames

Here, the effects of heat release on interactions between vorticity (ω) and strain rate (s) in turbulent premixed CH 4 /O 2 /N 2 counterflow flames are investigated using simultaneous OH laser-induced fluorescence (LIF) and tomographic particle image velocimetry (TPIV) measurements. A comparison between the flames and a corresponding turbulent non-reacting variable density N 2 -vs-products counterflow reveals the impact of heat release on vorticity-strain rate alignment statistics. Vorticity and strain rate statistics in the flames and non-reacting flow are conditioned on distance from the local flame front and gas mixing layer interface (GMLI) contours, respectively. The magnitude, alignment, and spatial distribution of the vorticity and principal strain rates (s 1 , s 2 , s 3 ) are rather different when heat release is present. Density variations without heat release enhance the ω-s 2 alignment while significantly reducing the ω-s 3 alignment and modestly reducing the ω-s 1 alignment. In contrast, heat release at the flame front further reduces the ω-s 1 alignment but increases the ω-s 3 alignment and suppresses the preferential ω-s 2 alignment. Furthermore, increasing turbulence diminishes the effect of heat release on this preferential alignment. In regions with the largest vorticities, both the reacting and non-reacting counterflows show an increase in the probability of ω-s 2 alignment. All counterflow cases have a net positive vortex-stretching contribution to the enstrophy production with a peak production rate at the flame front or GMLI, but the peak values depend on the density variation, heat release, and turbulence level. Elucidation of the complex interplay between these factors contributes to the understanding of the dynamics of turbulence-flame interactions.

42 ENGINEERING↗

Convective heat transfer and friction factor characteristics of molten salts in spirally fluted tubes

Spirally fluted tubes have been widely used for heat exchangers due to their superior heat transfer enhancement. However, most of the previous studies focused on the effects of a limited number of geometric parameters, i.e., the flute pitch and flute depth, on convective heat transfer and friction factor characteristics of low-Prandtl-number fluids, i.e., air and water. The correlations developed in these studies may not be accurate or applicable for medium-Prandtl-number fluids, such as molten salts. A numerical analysis using a Computational Fluid Dynamics (CFD) tool, STAR–CCM+, is therefore carried out in this study to systematically investigate the effects of four geometric parameters, including the flute pitch ρ, flute depth e, flute start number N s (or flute helix angle θ), and trough length L tr on convective heat transfer and friction factor characteristics of a medium-Prandtl-number fluid, FLiNaK (46.5LiF-11.5NaF-42KF mol %), in spirally fluted tubes. Additionally, the convective heat transfer and Darcy friction factor correlations are proposed and validated, with ± 20% uncertainties, for medium-Prandtl-number fluids under the following conditions: Re = 88–1600, Pr = 2.5–40, ρ/D c = 0.44–3.51, e/D c = 0.10–0.40, θ/90= 0.20–0.81, and L tr /D c = 0.71–2.16. The correlations proposed help improve the design of spirally fluted-tube heat exchangers.

42 ENGINEERING↗

Tribocorrosion of stainless steel sliding against graphite in FLiNaK molten salt

The molten salt reactor (MSR) concept recently gained renewed interest in developing Generation IV nuclear reactors. One MSR design uses fluoride molten salts to cool tri-structural isotropic particle fuel encapsulated by a carbon matrix into spherical pebbles, which would inevitably contact the reactor's stainless steel container wall during salt circulation. Characterizing this interaction is crucial for reactor safety. Here, in this work, we report the tribocorrosion behavior of graphite sliding against Type 316H stainless steel lubricated by a FLiNaK (LiF:NaF:KF; 46.5:11.5:42 mol %) molten salt in an argon environment. Accelerated wear loss was observed at a higher temperature because of a lower molten salt viscosity and a higher corrosion rate. The graphite had a more rapid material loss at a higher sliding speed than stainless steel because of its higher vulnerability to vibration-induced microfracture. The salt-starved condition caused more material loss than either the no-salt or the salt-flooded condition because neither a graphite transfer film nor stable boundary lubrication could be established at salt starvation. An interesting dual-layer surface film was discovered on the stainless steel worn surface: a chromium-rich top film and a nickel-accumulated but chromium-depleted interlayer. The film composition and structure provide fundamental insights to the mechanochemical interactions between stainless steel and graphite in a molten salt environment.

22 GENERAL STUDIES OF NUCLEAR REACTORS↗

Resolving Chemical and Spatial Heterogeneities at Complex Electrochemical Interfaces in Li-Ion Batteries

The high specific capacities of Ni-rich transition metal oxides have garnered immense interest for improving the energy density of Li-ion batteries (LIBs). Despite the potential of these materials, Ni-rich cathodes suffer from interfacial instabilities that lead to crystallographic rearrangement of the active material surface as well as the formation of a cathode electrolyte interphase (CEI) layer on the composite during electrochemical cycling. While changes in crystallographic structure can be detected with diffraction-based methods, probing the chemistry of the disordered, heterogeneous CEI layer is challenging. In this work, we use a combination of ex situ solid-state nuclear magnetic resonance (SSNMR) spectroscopy and X-ray photoemission electron microscopy (XPEEM) to provide chemical and spatial information, on the nanometer length scale, on the CEI deposited on LiNi 0.8 Mn 0.1 Co 0.1 O 2 (NMC811) composite cathode films. XPEEM elemental maps offer insight into the lateral arrangement of the electrolyte decomposition products that comprise the CEI and paramagnetic interactions (assessed with electron paramagnetic resonance (EPR) and relaxation measurements) in 13 C SSNMR provide information on the radial arrangement of the CEI from the NMC811 particles outward. Using this approach, here we find that LiF, Li 2 CO 3 , and carboxy-containing structures are directly appended to NMC811 active particles, whereas soluble species detected during in situ 1 H and 19 F solution NMR experiments (e.g., alkyl carbonates, HF, and vinyl compounds) are randomly deposited on the composite surface. We show that the combined approach of ex situ SSNMR and XPEEM, in conjunction with in situ solution NMR, allows spatially-resolved, molecular-level characterization of paramagnetic surfaces and new insights into electrolyte oxidation mechanisms in porous electrode films.

36 MATERIALS SCIENCE↗

Comparative Studies of the Structural and Transport Properties of Molten Salt FLiNaK Using the Machine-Learned Neural Network and Reparametrized Classical Forcefields

Despite surging interest in molten salt reactors and thermal storage systems, knowledge of the physicochemical properties of molten salts are still inadequate due to demanding experiments that require high temperature, impurity control, and corrosion mitigation. Therefore, the ability to predict these properties for molten salts from first-principles computations is urgently needed. Herein, we developed and compared a machine-learned neural network force field (NNFF) and a reparametrized rigid ion model (RIM) for a prototypical molten salt LiF–NaF–KF (FLiNaK). We found that NNFF was able to reproduce both the structural and transport properties of the molten salt with first-principles accuracy and classical-MD computational efficiency. Furthermore, the correlation between the local atomic structures and the dynamics was identified by comparing with RIMs, suggesting the significance of polarization of anions implicitly embedded in the NNFF. Furthermore, this work demonstrated a computational framework that can facilitate the screening of molten salts with different chemical compositions, impurities, and additives, and at different thermodynamic conditions suitable for the next-generation nuclear reactors and thermal energy storage facilities.

36 MATERIALS SCIENCE↗

Insight into SEI Growth in Li-Ion Batteries using Molecular Dynamics and Accelerated Chemical Reactions

The performance of lithium-ion batteries (LIB) using organic electrolytes strongly depends on the formation of a stable solid electrolyte interphase (SEI) film. Elucidating the dynamic evolution and spatial composition of the SEI can be very useful to study the stability of SEI components and help optimize the formation cycles of LIB. We propose a classical molecular dynamics simulation protocol for predicting the first stages of SEI formation using a reaction method involving the decomposition of EC and LiPF 6 molecules in the electrolyte. We accelerate the formation of SEI components near the anode surface by increasing the probability of reactions, implemented through a geometry matching scheme, followed by a force-field reconfiguration. We observe the formation of gases (C 2 H 4 ), inorganic (Li 2 CO 3 and LiF) and organic (LEDC) components. Finally, this protocol shows promise to be able to evaluate the effects of varying electrolyte compositions and additives on SEI layer structure and composition.

25 ENERGY STORAGE↗

Degradation in Ni-Rich LiNi 1– x – y Mn x Co y O 2 /Graphite Batteries: Impact of Charge Voltage and Ni Content

Ni-rich LiNi 1– x–y Mn x CoyO 2 (NMC) materials are attractive as cathodes for Li-ion batteries due to their high energy density and low Co content. However, these materials may display poor electrochemical reversibility relating to structural and interfacial instabilities. The influence of Ni content and level of delithiation during charge on degradation mechanisms and relevance to electrochemical cycling behavior are probed for LiNi 0.6 Mn 0.2 Co 0.2 O 2 (NMC622) and LiNi 0.8 Mn 0.1 Co 0.1 O 2 (NMC811) cathode materials in a full cell configuration under two upper voltage limits (4.1 and 4.3 V). The combined use of dQ/dV analysis of electrochemical voltage profiles, operando XRD, and postcycling scanning electron microscopy (SEM) measurements indicates that a major contributor to capacity fade is the large anisotropic volume change from an H2 $\leftrightarrows$ H3 phase transition and associated mechanical degradation particularly for NMC811. Notably, transition metal dissolution and deposition on the negative electrode are found to correlate with the structural changes occurring in the cathode under high voltage charge. X-ray photoelectron spectroscopy (XPS) analyses of the cycled cathodes reveal a more organic-rich cathode–electrolyte interphase (CEI) when cycling to 4.3 V with lower relative amounts of LiF. Surface reconstruction is not a significant factor under these cycling conditions as determined by soft X-ray absorption spectroscopy (sXAS) analysis. The results emphasize the opportunity to match the electrochemical test parameters with the specific NMC active material to mitigate degradation and extend cycle life.

36 MATERIALS SCIENCE↗

Electrolyte Design for Silicon-Based Li-Ion Battery Guided by Chemical Reactivity of Solvents with a Model Silicon Anode

Here, the use of a model compound trimethylsilyllithium was demonstrated to study the chemical reactions of electrolyte with as a principal guide to design electrolyte for silicon-based Li-ion battery. Me 3 Si - anion initiates ring-opening polymerization of EC leading to the formation of poly(ethylene ether carbonate), which subsequently defragments into oligomers and dissolves in electrolyte. FEC was found to react differently, generating LiF and vinylene carbonate (VC). Further reaction of VC with Me 3 SiLi generated poly(hydroxymethylene), which is a nonsoluble polymer and the critical SEI component. The insights from this study have guided the new electrolyte design for the Si-based battery.

25 ENERGY STORAGE↗

Self-Diffusivity Measurement of Eutectic F 7 LiNaK with and without Additives Using Quasi-Elastic Neutron Scattering

The atomic scale relaxation dynamics of eutectic F 7 LiNaK (46.5 LiF–11.5 NaF–42 KF mol %, Li-7 enriched) were measured using quasi-elastic neutron scattering (QENS) over a temperature range of 500–750 °C. Here, the effect of adding 0.988 mol % cerium, 0.499 mol % cesium, and 1.21 mol % zirconium individually to the dynamics of F 7 LiNaK was also investigated. The relaxation process in both pure and doped F 7 LiNaK molten salts was fit with a stretched exponential function and the temperature dependence follows an Arrhenius behavior over a wavevector transfer range of 0.4 Å –1 < Q < 0.9 Å –1 . The measured activation energy for self-diffusion is E a = 0.77 ± 0.02 eV/atom for pure molten F 7 LiNaK. The QENS response with additives added to F 7 LiNaK was also fit with a stretched exponential and the associated Arrhenius behavior was characterized with activation energies of E a = 0.88 ± 0.01 eV/atom for zirconium (1.21 mol %), E a = 1.02 ± 0.02 eV/atom for cerium (0.988 mol %), and E a = 0.71 ± 0.03 eV/atom for cesium (0.499 mol %). The measured diffusivities are compared to those simulated with a neural network force field model by Lee et al. [Lee, S.-C. Comparative Studies of the Structural and Transport Properties of Molten Salt FLiNaK Using the Machine-Learned Neural Network and Reparametrized Classical Forcefields. J. Phys. Chem. B 2021, 125(37), 10562–10570].

FLiNaK↗

Enhanced Performance of Silicon Anodes through Hybrid Surface Engineering

Silicon (Si) is a promising anode material for nextgeneration lithium-ion batteries (LIBs) due to its high theoretical capacity. However, Si-containing anodes typically suffer from unacceptably short lives because of the unrestricted growth of the solid electrolyte interphase (SEI). Here, in this study, hybrid surface coatings are developed to stabilize the SEI in high loading pure Si anodes using atomic and molecular layer deposition. The coatings, consisting of LiF paired with lithicone, create an ionically conductive surface that enhances the capacity retention, rate performance, and longevity. Careful binder selection helps demonstrate the full utility of the coatings by enabling high loading electrodes to cycle continuously at current densities of 1200 mA/g Si . Uncoated controls, in comparison, fail within just 10 cycles at lower loadings. X-ray photoelectron spectroscopy and electrochemical impedance spectroscopy are used to provide supporting evidence of the coating composition and efficacy. The data indicate that our lithicone coating is converted to Li 2 CO 3 upon cycling contributing to favorable LiF/Li 2 CO 3 interfaces that enhance the space-charge effect at the active material’s surface. When applied to electrodes made with thermally stable binders and increasingly higher loadings (approaching 5 mAh/cm 2 ), ion transport through the bulk electrode, rather than SEI growth, is shown to be the limiting factor. Furthermore, data suggests a favorable interaction between lithicone precursors and poly(acrylic acid) binders mitigates thermal decomposition at higher temperatures. The work presented here represents the successful realization of composite coatings containing LiF/Li 2 CO 3 components to stabilize high-loading Si anodes. This work helps inform advanced surface engineering strategies to achieve highly reversible, high-capacity Si anodes capable of fast charging for high-performance LIBs.

atomic layer deposition↗

Probing the Formation of Cathode-Electrolyte Interphase on Lithium Iron Phosphate Cathodes via Operando Mechanical Measurements

Interfacial instabilities in electrodes control the performance and lifetime of Li-ion batteries. While the formation of solid-electrolyte interface (SEI) on anodes has received much attention, there is still lack of understanding about the formation of cathode-electrolyte interface (CEI) on the cathodes. To fill this gap, we report on dynamic deformations on lithium iron phosphate, LiFePO 4 cathodes during charge / discharge by utilizing in-operando digital image correlation, impedance spectroscopy and Cryo X-ray photoelectron spectroscopy. LiFePO4 cathodes were cycled in either LiPF 6 , LiClO 4 or LiTFSI- containing organic liquid electrolytes. Beyond the first cycle, Li-ion intercalation results in a nearly linear correlation between electrochemical strains and the state of (dis)-charge, regardless of the electrolyte chemistry. However, during the first charge in LiPF 6 - containing electrolyte, there is a distinct irreversible positive strain evolution at the onset of anodic current rise as well as current decay at around 4.0V. Impedance studies show the increase in surface resistance in the same potential window, suggesting the formation of CEI layers on the cathode. The chemistry of the CEI layer was characterized by X-ray photoelectron spectroscopy. LiF is detected in CEI layer starting as early as 3.4 V and Li $x$ PO $y$ F $z$ appeared at voltages higher than 4.0 V during the first charge. In conclusion, our approach offers new insights into the formation mechanism of CEI layers on the cathode electrodes, which is crucial for the development of robust cathode and electrolyte chemistries for higher performance batteries.

25 ENERGY STORAGE↗

Insights into the Chemistry of the Cathodic Electrolyte Interphase for PTFE-Based Dry-Processed Cathodes

Dry processing is a promising method for high-performance and low-cost lithium-ion battery manufacturing which uses polytetrafluoroethylene (PTFE) as a binder. However, the electrochemical stability of the PTFE binder in the cathodes and the generated chemistry of the cathode electrolyte interphase (CEI) layers are rarely reported. In this work, the CEI properties and PTFE electrochemical stability are studied via cycling the high-loading dry-processed electrodes in electrolytes with LiPF 6 or LiClO 4 salt. Using LiClO 4 salt can eliminate other possible F sources, allowing the decomposition of PTFE to be studied. The detection of LiF in cells with the LiClO 4 salt confirms that PTFE undergoes side reaction(s) in the cathodes. When compared with LiClO 4 , the CEI layer is much thicker when LiPF 6 is used as the electrolyte salt. These results provide insights into the CEI layer and may potentially enlighten the development of binders and electrolytes for the high efficiency and long durability of DP-based LIBs.

25 ENERGY STORAGE↗

Comparative Study of Vinylene Carbonate and Lithium Difluoro(oxalate)borate Additives in a SiO x /Graphite Anode Lithium-Ion Battery in the Presence of Fluoroethylene Carbonate

The SiO x /graphite composite is recognized as a promising anode material for lithium-ion batteries (LIBs), owing to the high theoretical capacity of SiO x combined with the excellent stability of graphite. However, the inherent disadvantage of volume expansion in silicon-based anodes places significant challenges on the solid electrolyte interphase (SEI) and severely degrades the electrochemical performance. Rational formulation of electrolyte, including its additives, is crucial in accommodating and optimizing the composition of the SEI and enhancing the cell performance. In this work, we present a comparative study of vinylene carbonate (VC) and lithium difluoro(oxalate)borate (LiDFOB) additives combined with fluoroethylene carbonate (FEC) in the electrolyte for SiO x /graphite∥LiNi 1–x–y–z Co x Mn y Al z O 2 full cells. VC outperformed LiDFOB as an additive, delivering higher capacity cycling, higher Coulombic efficiency, and better cycle stability up to 400 cycles. XPS and impedance analyses reveal that LiDFOB contributed to SEI/CEI with both a lower proportion of LiF and a higher proportion of poly(VC), which tended to produce higher cell impedance. XRD and XANES further indicated that using the LiDFOB additive, the NCMA cycled to a shallower degree than that of the VC additive. Although the VC additive maintained a higher capacity up to 400 cycles, microstrain and SEM analyses show a higher strained NCMA along with clear evidence of cracking over the surface of the NCMA particle in VC-based electrolyte but not in LiDFOB. In conclusion, this suggests that the negative influence of LiDFOB at the anode (inferior SEI) supersedes the negative impact of both a cracked NCMA and a deeper cycled NCMA and SiO x -based anode.

36 MATERIALS SCIENCE↗

Delineating the Factors Impacting the Electrochemical Behavior of Single-Crystal High-Nickel Layered Oxide Cathodes

High-nickel (Ni) (≥80%) single-crystal LiNi 1-x-y Mn x Co y O 2 (NMCs) have garnered recent interest as cathodes in lithium (Li)-ion batteries (LIBs). However, capacity fade at high voltages, particularly after the onset of the H2–H3 phase transition, hampers their viability. In this study, single-crystal LiNi 0.8 Mn x Co 0.2-x O 2 (x = 0.2, 0.1, 0) are synthesized and tested in LiPF 6 in ethyl methyl carbonate-based electrolytes, with and without monofluoroethylene carbonate and LiF 2 PO 2 additives, to clarify the effects of Co/Mn ratio and surface stabilization on high-voltage cycling degradation. By imposing a kinetic barrier to the accessible H2–H3 capacity, surface reconstruction is identified as the primary driver of high-voltage capacity loss, being greater in the Co-free cathode and in the absence of fluorinated electrolyte components. This is attributed to a synergy between increased mechanical stress due to worsened bulk and interfacial H2–H3 kinetics and decreased interfacial stability due to the poor passivating capability of the electrolyte. Here, the findings highlight the importance of limiting cathode impedance growth during high-voltage cycling, which can be achieved by tuning bulk dopants and electrolyte chemistry.

25 ENERGY STORAGE↗

Lithium Cyano Tris(2,2,2-trifluoroethyl) Borate as a Multifunctional Electrolyte Additive for High-Performance Lithium Metal Batteries

Lithium cyano tris(2,2,2-trifluoroethyl) borate (LCTFEB) has been synthesized and investigated as a new electrolyte additive for high performance of lithium metal batteries. LCTFEB is prepared by the reaction of tris(2,2,2-trifluoroethyl) borate with lithium cyanide. Incorporation of LCTFEB into carbonate-based electrolyte has been investigated. The electrochemical performance of NCM523/Li cells as well as symmetric Li/Li cells are significantly improved upon incorporation of LCTFEB (5 wt.%) into the electrolyte. Various characterizations of lithium metal morphology and the solid electrolyte interphase (SEI) on the lithium metal anode have been conducted using by FE-SEM, cryo-TEM and XPS suggesting the generation of a thin (≈ 10 nm) LiF rich SEI with low concentrations of B and N-compounds. The different SEI structure is formed by the preferential reductive decomposition of LCTFEB resulting in improved electrochemical performance. As a result, the new electrolyte additive provides insight into innovative approaches for multi-functional electrolyte additive design.

25 ENERGY STORAGE↗

Quantifying Graphite Solid-Electrolyte Interphase Chemistry and its Impact on Fast Charging

The solid-electrolyte interphase (SEI) enables the remarkable capacity retention of lithium-ion batteries, yet a comprehensive quantitative description of the SEI composition remains elusive. Using a combination of differential electrochemical mass spectrometry and mass spectrometry titration, we quantify graphite SEI components formed under electrolytes of varying salt concentrations. We find that, regardless of salt concentration, a conversion of initially deposited lithium ethylene dicarbonate to monocarbonates (likely lithium ethylene monocarbonate) and noncarbonate species occurs, and the extent of this conversion increases with electrolyte aging. Here, we additionally demonstrate that as the concentration increases (up to 2.0 M LiPF6), the SEI becomes progressively thinner with more LiF and less solid carbonates deposited. Finally, we reveal that less dead lithium formation and less solid carbonate deposition occur during prolonged fast charging for higher-concentration electrolytes. Because of the advantages imparted by a thinner SEI, the onset state of charge for lithium plating for the 2.0 M electrolyte is later than that predicted by a standard electrochemical model, underscoring the importance of explicit SEI effects in future electrochemical models.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗