Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “FERRITE”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 253 records · Page 14

Effect of Ce{sup 3+} Ion on Structural and Hyperfine Interaction Studies of Co{sub 0.5}Ni{sub 0.5}Fe{sub 2−x}Ce{sub x}O{sub 4} Ferrites: Useful for Permanent Magnet Applications

Nanoparticles of Co{sub 0.5}Ni{sub 0.5}Fe{sub 2−x}Ce{sub x}O{sub 4} (where x = 0.0, 0.01, 0.015 and 0.02) ferrites are prepared by the modified solution combustion method using a mixture of fuels and are characterized to understand their structural, microstructural and magnetic properties. The X-ray diffraction is used to confirm the formation of a single-phase cubic spinel structure. The average crystallite sizes are calculated using the Scherrer formula and are found to be less than 50 nm. The microstructural features are obtained by the scanning electron microscopy, and the compositional analysis is done by using the energy-dispersive spectroscopy. The transmission electron microscopy (TEM) investigations show that the synthesized ferrites are made up of very fine spherical nanoparticles. The influence of a rare-earth element (Ce{sup 3+}) on the magnetic properties of the samples was studied using the Mössbauer spectroscopy. The Mössbauer spectroscopy reveals the formation of broadened Zeeman lines and quadrupole-split lines and the presence of the Fe{sup 3+} charge state at B sites in the samples. The quadrupole splitting shows that the orientation of the magnetic hyperfine field with respect to the principle axes of the electric field gradient was random. The magnetic hyperfine field values indicate that the A sites have more A-O-B superexchange interactions than the B sites. The coexistence of magnetic sextet and a doublet component on the room-temperature spectra suggests superparamagnetic properties of the nanoparticles. The low-temperature (15 K) Mössbauer spectroscopy explores the paramagnetic relaxation in the nanoparticles. The area under the sextet refers to Fe{sup 3+} concentrations in the tetrahedral and octahedral sites of the ferrite. This study confirms that the Ce{sup 3+} substitution of Fe{sup 3+} only for octahedron sites causes the decrease in Fe-O-Fe arrangement. The effect of Ce{sup 3+} doping on the magnetic properties of Co{sub 0.5}Ni{sub 0.5}Fe{sub 2}O{sub 4} is examined from the vibrating sample magnetometry (VSM) spectra. Saturation magnetization values are decreased initially and then increased, as result of Ce{sup 3+} doping. This can be explained by Neel’s two-sub-lattice model. Further, the value of coercivity is found to be increasing with increasing Ce{sup 3+} concentration. The obtained results of M-H loop with improved coercivity (from 851 to 1039 Oe) by Ce{sup 3+} doping of Co{sub 0.5}Ni{sub 0.5}Fe{sub 2}O{sub 4} demonstrate the usefulness for permanent magnet applications.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Law of Approach to Saturation in Mn–Zn Ferrite Nanoparticles

In this paper, the law of approach to saturation (LAS) was applied to a series of Mn–Zn ferrite nanoparticles with compositional formula Mn{sub 1−x}Zn{sub x}Fe{sub 2}O{sub 4} where x = 0, 0.1, 0.2, 0.3, 0.4 and 0.5 to study the dependence of magnetization, M, on the applied magnetic field, H. Using the statistical parameters, the field range was chosen. The dependence of magnetization on the applied field was studied based upon the output of the statistical parameters for the curve fitted using different forms of LAS, namely, M=M{sub s}[1−(a/H)−(b/(H{sup 2}))]+kH, M=M{sub s}[1−(a/H)−(b/(H{sup 2}))],M=M{sub s}[1−(b/(H{sup 2}))] and M=M{sub s}(1−(1/15)((H{sub A}{sup 2})/(H{sup (1/2)}(H{sup (3/2)}+H{sub R}{sup (3/2)}))))+kH. A critical examination on the output parameters resulted from fitting into different equations, indicates the dependency of magnetization on the applied field as a characteristic of the composition of Mn–Zn ferrites. The statistical parameters, along with physically meaningful fitted parameters, provide knowledge on dependency of magnetization of different compositions of Mn–Zn ferrites over different regions of applied field.

77 NANOSCIENCE AND NANOTECHNOLOGY↗

Structural, Infrared, Magnetic, and Electrical Properties of Ni{sub 0.6}Cd{sub 0.2}Cu{sub 0.2}Fe{sub 2}O{sub 4} Ferrites Synthesized Using Sol-Gel Method Under Different Sintering Temperatures

Ni{sub 0.6}Cd{sub 0.2}Cu{sub 0.2}Fe{sub 2}O{sub 4} ferrites were synthesized using sol-gel method under different sintering temperatures. XRD patterns with the Rietveld refinement indicate that samples crystallize in the cubic spinel structure. The increase of sintering temperature leads successively to the increase of lattice constant, average crystallite size, intensities of absorption bands, magnetization, and electrical conductivity of the prepared ferrites. Dielectric constants decrease with frequency and their behaviors have been investigated using the interfacial polarization theory predicted by Maxwell. The modulus analysis shows the presence of electrical relaxation phenomenon and non-Debye nature for the samples. An appropriate electrical equivalent circuit was used to analyze the Nyquist plots, and the results show that the conduction mechanism of the synthesized ferrites is mainly due to the grain boundary contribution.

36 MATERIALS SCIENCE↗

Co{sup 2+} Substituted ZnCuFe{sub 2}O{sub 4} (0.0 ≤ x ≤ 0.5) Ferrites: Synthesis, Magneto-structural and Optical Properties for Their Photocatalytic Performance

The cobalt (Co{sup 2+}) has been successively substituted in ZnCuFe{sub 2}O{sub 4} to obtain Zn{sub 0.5−x}Co{sub x}Cu{sub 0.5}Fe{sub 2}O{sub 4} (0.0 ≤ x ≤ 0.5) ferrites by auto-combustion technique. Prior to photocatalytic degradation, all as-synthesized ferrites were characterized to study their structure, composition, morphology, magnetic and optical behavior. The shifting of tetrahedral as well as octahedral stretching peaks towards higher frequencies observed in the Fourier transform infrared spectroscopy indicates that Co{sup 2+} ion is substituted in ZnCuFe{sub 2}O{sub 4}. X-ray diffraction pattern confirms the formation of single-phase cubic spinel with decrease in average lattice constant from 8.3915 to 8.3224 Å with increase in Co{sup 2+} substitution. The photocatalytic performance of obtained ferrite catalyst was determined using methylene blue (MB) as model dye under visible light and direct sunlight. The degradation of MB with as-obtained photocatalyst under sunlight improves (91%) which proves the effective utilization of visible light active magnetic photocatalyst.

36 MATERIALS SCIENCE↗

Structural and Electrical Dependence in Zn-Doped Li-Ferrite Nanostructures

Zinc-doped lithium ferrite nanoparticles with general formula Li{sub 0.46}Zn{sub 0.04}Fe{sub 2.5}O{sub 4} were prepared by Co-precipitation method and their thin films were grown by spin coating method. X-ray diffraction (XRD) confirmed the spinel structure of the synthesized samples. Fine morphology of the films was obtained by controlling the parameters. AC electrical properties including dielectric constant (έ), dielectric loss tangent (tanδ), AC electrical conductivity (σ{sub ac}), and impedance (Z) were studied as a function of frequency at different temperatures and at 1 MHz frequency in a temperature range of 40–500 °C. Dielectric constant, dielectric loss tangent, and ac electrical conductivity showed the decreasing trend with increase in temperature while opposite trend was observed for impedance. Zinc-doped Li-ferrite has better absorption properties in the studied frequency and temperature range as compared to that of Li-ferrites.

77 NANOSCIENCE AND NANOTECHNOLOGY↗

Solubility of Zinc Silicate and Zinc Ferrite in Aqueous Solution to High Temperatures

Crystalline zinc silicate, Zn{sub 2}SiO{sub 4}, and zinc ferrite, ZnFe{sub 2}O{sub 4}, were prepared and characterized. The solubilities of these phases were measured using flow-through apparatus from 50 to 350 C in 100 C intervals over a wide range of pH. Both solid phases dissolve incongruently, presumably to form ZnO(s) and Fe{sub 2}O{sub 3}(s) (or the corresponding hydroxide phases at low temperature), respectively. The respective concentrations of zinc(II) and iron(III) matched those of ZnO(cr) and Fe{sub 2}O{sub 3}(s) ({ge}150 C) reported in the literature, whereas the corresponding Si(IV) and Zn(II) concentrations were at least an order of magnitude below the solubility limits for their pure oxide phases. Therefore, the solubility constants for zinc silicate and ferrite were determined with respect to the known solubility constants for ZnO(cr) and Fe{sub 2}O{sub 3}(s) ({ge}150 C), respectively, and the corresponding concentrations of Si(IV) and Zn(II) measured in this study. The results of independent experiments, as well as those reported in the literature provide insights into the mechanism(s) of formation of zinc silicate and ferrite in the primary circuits of nuclear reactors.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Study of Ferrite During Refinement of Prior Austenite Grains in Microalloyed Steel Continuous Casting

The formation of coarse prior austenite grain is a key factor to promote transverse crack, and the susceptibility to the transverse crack can be reduced by refining the austenite grain size. In the present study, the high-temperature confocal laser scanning microscope (CLSM) was used to simulate two types of double phase-transformation technologies. The distribution and morphology of ferrites under different cooling conditions were analyzed, and the effects of ferrite distribution and morphology on the double phase-transformation technologies were explored to obtain the suitable double phase-change technology for the continuous casting process. The results indicate that, under the thermal cycle TH0 [the specimens were cooled down to 913 K (640 °C) at a cooling rate of 5.0 K/s (5.0 °C/s)], the width of prior austenite grain boundaries was thick, and the dislocation density at grain boundaries was high. It had strong inhibition effect on crack propagation; under the thermal cycle TH1 [the specimens were cooled down to 1073 K (800 °C) at a cooling rate of 5.0 K/s (5.0 °C/s) and then to 913 K (640 °C) at a cooling rate of 1.0 K/s (1.0 °C/s)], the width of prior austenite grain boundary was thin, and the dislocation density at grain boundaries was low. It was beneficial to crack propagation. After the first phase change, the developed film-like ferrite along the austenite grain boundaries improved the nucleation conditions of new austenitic grains and removed the inhibition effect of the prior austenite grain boundaries on the austenite grain size.

36 MATERIALS SCIENCE↗

Effect of Aluminum Dissolved in Hematite on Formation of Calcium Ferrites at 1473 K

Silico-ferrite of calcium and aluminum (SFCA) is a primary bonding phase, which determines the quality of high basicity sinter used widely as raw materials in blast furnace ironmaking. Calcium ferrite containing aluminum (CFA) is a key precursor during the formation process of SFCA and is influenced by Al{sub 2}O{sub 3} content in iron ore fines. In this work, the experiment was conducted to investigate the effect of the aluminum occurrence state on the formation of calcium ferrite by the simulating sintering process of different types of aluminum-bearing hematite at 1473 K. X-ray diffraction, optical microscope, scanning electron microscopy, and energy-dispersive spectroscopy were used to characterize the mineral change in sintered samples. The result shows that the formation of CFA was promoted by both granular Al{sub 2}O{sub 3} wrapped in Fe{sub 2}O{sub 3} and aluminum dissolved in Fe{sub 2}O{sub 3} solid solution, especially for the latter, due to the formation of the CFA directly from the reaction between Fe{sub 2}O{sub 3}-Al{sub 2}O{sub 3} solid solution and CaO, and the aluminum content in CFA formed was influenced obviously by the solid solution amount of alumina into Fe{sub 2}O{sub 3} as raw materials.

36 MATERIALS SCIENCE↗

Effect of Mg-Bearing Oxide(+TiN) Inclusion on Microstructure of Fe-16 Mass Pct Cr Ferritic Alloy and Its Evolution During Heating at 1573 K (1300 °C)

Both the effects of Mg-bearing oxide and Mg-bearing oxide +TiN inclusions on the microstructures of Fe-16 mass pct Cr alloy should be clarified. In this paper, the effects of Mg-bearing oxide(+TiN) inclusions on the microstructures of Fe-16 mass pct Cr ferritic alloy and changes due to the inclusions during heating at 1573 K (1300 °C) were studied by manual and automatic SEM-EDS analyses. Three alloys were used as specimens. The inclusions were Al{sub 2}TiO{sub 4} +TiN with a small amount of TiN in alloy #1, Al{sub 2}(Mg, Ti)O{sub 4} in alloy #2 and Al{sub 2}(Mg, Ti)O{sub 4} +TiN in alloy #3. The average grain size was smaller, and the ratio of columnar grains was lower in the as-cast alloy #2 and as-cast alloy #3 than that in the as-cast alloy #1. This is attributed to the heterogeneous nucleation of delta ferrite on Al{sub 2}(Mg, Ti)O{sub 4} during solidification. Refinement of the microstructures of ferritic steel by Mg-bearing oxide + multi-TiN inclusions is proposed. Changes in composition, aspect ratio, and size distribution of inclusions in each alloy during heating were investigated systematically. Mg-bearing oxide(+TiN) was dispersed in both the as-cast alloys and heated alloys, which contributed to microstructural refinement of the heated alloys through the pinning effect.

36 MATERIALS SCIENCE↗

Control of Carbon Content in Steel by Introducing Proeutectoid Ferrite Transformation into Hot-Rolled Q&P Process

A processing strategy involving primary and secondary carbon partitioning is proposed for the hot-rolled quenching and partitioning process through the introduction of proeutectoid ferrite transformation after rolling. The microstructures of the steels were characterized using scanning electron microscopy, transmission electron microscopy, electron probe microanalysis, and x-ray diffraction, and the mechanical properties were evaluated using a universal tensile machine. The blocky retained austenite that distributed along the ferrite grain boundaries was promoted based on the coupling action of the primary and secondary carbon partitioning, which enhanced the transformation-induced plasticity effect during deformation despite the high carbon concentration. A ferrite formation temperature range of ~ 760 to 800 °C was proposed. In addition, from the perspective of industrialization, the observed ‘plateau trends’ for the retained austenite fraction and product of strength and elongation suggest the availability of a wide processing window of 215-362 °C for controlling the coiling temperature.

36 MATERIALS SCIENCE↗

Carbon supersaturation of ferrite in a nanocrystalline bainitic steel

The extremely slow transformation kinetics of a nanocrystalline bainitic steel allows the carbon content of the bainitic ferrite away from any carbon-enriched regions such as dislocations and boundaries to be determined by atom probe tomography as the bainite transformation progresses at 200 C. A high level of carbon, well above that expected from para-equilibrium with austenite, has been detected in solid solution in bainitic ferrite at the early stage of transformation. Results provide strong evidence that bainite transformation is essentially displacive in nature so that the newly formed bainitic ferrite retains much of the carbon content of the parent austenite.

36 MATERIALS SCIENCE↗

Low temperature bainitic ferrite: Evidence of carbon super-saturation and tetragonality

Experimental evidence indicates that bainitic ferrite formed by transformation at low temperatures (200-350 °C) includes quantities of carbon in solid solution far beyond those expected from para-equilibrium. A change in the conventional symmetry of the bainitic ferrite lattice from cubic to tetragonal explains the abnormal solid solubility detected. This carbon supersaturation was measured by atom probe tomography, and the tetragonality of the bainitic ferrite, was characterized by means of X-ray diffraction analysis and high resolution transmission electron microscopy.

54 ENVIRONMENTAL SCIENCES↗

The crystal structure, orientation relationships and interfaces of the nanoscale oxides in nanostructured ferritic alloys

The capability of nanostructured ferritic alloys (NFAs) to manage high levels of transmutation product helium will help resolve one of the grand challenges to transforming the promise of C-free fusion energy into a reality. NFAs are dispersion strengthened by an ultrahigh density of Y-Ti-O nano-oxides (NOs), which result in both high strength and temperature limits, as well as unique irradiation tolerance. We used aberration-corrected high-resolution transmission electron microscopy to characterize the NOs in four NFA conditions, including following severe deformation and extreme neutron radiation exposure. Fast Fourier Transform analysis of focal series images revealed the NO crystal structure, including the smallest at < 2 nm in diameter, to be Y 2 Ti 2 O 7 pyrochlore in all cases, consistent with both exit wave analysis and scanning transmission Z-contrast imaging of the atomic columns in a larger feature. The faceted NOs exhibit a quasi-epitaxial orientation relationship with the ferrite matrix: [110] YTO ||[100] Fe and [001] YTO ||[010] Fe , forming a 5 × 7 near coincidence site interface. Also, the NOs exhibit size-dependent strains in both the oxide and matrix ferrite phases.

36 MATERIALS SCIENCE↗

(Mn,Co)(3)O-4 Spinel Coatings on Ferritic Stainless Steels for SOFC Interconnect Applications

(Mn,Co)3O4 spinel with a nominal composition of Mn1.5Co1.5O4 demonstrates excellent electrical conductivity, satisfactory thermal and structural stability, as well as good thermal expansion match to ferritic stainless steel interconnects. A slurry-coating technique was developed for fabricating the spinel coatings onto the steel interconnects. Thermally grown layers of Mn1.5Co1.5O4 not only significantly decreased the contact resistance between a LSF cathode and stainless steel interconnect, but also acted as a mass barrier to inhibit scale growth on the stainless steel and to prevent Cr outward migration through the coating. The level of improvement in electrical performance and oxidation resistance (i.e. the scale growth rate) was dependent on the ferritic substrate composition. For E-brite and Crofer22 APU, with a relatively high Cr concentration (27wt% and 23%, respectively) and negligible Si, the reduction of contact ASR and scale growth on the ferritic substrates was significant. In comparison, limited improvement was achieved by application of the Mn1.5Co1.5O4 spinel coating on AISI430, which contains only 17% Cr and a higher amount of residual Si.

30 DIRECT ENERGY CONVERSION↗

Type IV failure in weldment of creep resistant ferritic alloys: II. Creep fracture and lifetime prediction

The creep rupture behavior (Type IV failure) for weldments of creep strength enhanced ferritic steel is numerically analyzed, using an integrated microstructure- and micromechanics-based finite element model. To account for the large microstructure gradients across weldments, a two-dimensional digital microstructure is constructed based on the actual observed microstructure of ferritic steel weldment by using the Voronoi-tessellation method. According to the fracture mechanism studies and literature experimental observations, the Type IV failure is identified as an intergranular creep fracture in the fine-grained or intercritical heated affected zone (FGHAZ or ICHAZ). In the present study, the following micromechanics model is employed to determine the micromechanical and microstructural origins for the failure process above, accounting for the underlying physical fracture mechanisms at different length scales, including nucleation of grain boundary cavities, their growth by competition of grain boundary diffusion and grain interior creep, viscous grain boundary sliding, and the emergence of microcracks by coalescence and their evolution to the ultimate failure. The methodology demonstrates the capabilities in modeling the Type IV failure and providing quantitative creep rupture lifetime prediction which shows an excellent agreement with long-term creep experimental data for creep strength enhanced ferritic steels and their weldments. In particular, the drop-off in time to rupture at high temperatures and low stress levels in the creep rupture curves is quantitatively predicted, and the transition of failure mechanisms from creep-controlled to diffusion-controlled creep fracture mechanism is illustrated.

36 MATERIALS SCIENCE↗

Suppression of irradiation hardening in tungsten-coated ferritic steel for fusion reactor blanket applications

W-coated reduced activation ferritic steels have been developed for use as plasma facing components in fusion reactor blankets, offering excellent sputtering resistance and structural strength. Previous high-temperature coating methods, such as diffusion bonding and brazing, caused interfacial deterioration due to thermal stress from mismatched thermal expansion between W and reduced activation ferritic steel. To address this, underwater explosive welding was introduced as a high-velocity cold process that joins dissimilar materials while maintaining a strong, thin interface without the thermal issues associated with traditional methods. In this study, the effects of neutron irradiation on the hardness and microstructure in W-coated F82H reduced activation ferritic steel (W/F82H) joined by underwater explosive welding are investigated. Following neutron irradiation at 290 °C, irradiation hardening is suppressed in W, F82H, and their interface within the W/F82H material. Furthermore, microstructural observations indicate that the recovery of work hardening and relaxation of elastic strain introduced during coating significantly contribute to the suppression of irradiation hardening in W/F82H. In conclusion, W/F82H exhibits significantly suppressed irradiation hardening compared with those in stand-alone materials. This suppression is explained by residual stress from thermal expansion mismatch and the unique microstructure at the interface. These results provide valuable insights for the development of more durable materials in nuclear fusion applications.

36 MATERIALS SCIENCE↗

Studies on the magnetism of cobalt ferrite nanocrystals synthesized by hydrothermal method

Fe-Co/CoFe{sub 2}O{sub 4} nanocomposite and CoFe{sub 2}O{sub 4} nanopowders were prepared by the hydrothermal method. The structure of magnetic powders were characterized by X-ray diffraction diffractometer (XRD), field emission scanning electron microscopy (FE-SEM), transmission electron microscopy (TEM), thermal gravity analysis (TGA) and differential thermal analysis (DTA) analysis, X-ray photoelectron spectrometry (XPS), and Fourier transform infrared spectra (FTIR) techniques, while magnetic properties were determined by using a vibrating sample magnetometer (VSM) at room temperature. The effects of hydrothermal reaction conditions on magnetic properties were also discussed in details. The values of saturation magnetization (M{sub s}) and coercive fore (H{sub c}) for Fe-Co/CoFe{sub 2}O{sub 4} nanocomposite are 113 emu/g and 1.4 kOe, respectively. Furthermore, CoFe{sub 2}O{sub 4} ferrite with a single-domain critical size of 70 nm was fabricated by controlling the hydrothermal reaction conditions carefully, which presents high coercive force (ca. 4.6 kOe) and high squareness ratio (ca. 0.65). One interesting thing is M{sub s} value of CoFe{sub 2}O{sub 4} ferrite with a diameter of 40 nm is 86 emu/g which is comparable to that of the bulk counterpart. - Graphical abstract: CoFe{sub 2}O{sub 4} ferrite with a single-domain critical size of 70 nm was fabricated by controlling the hydrothermal reaction conditions carefully, which presents high coercive force (ca. 4.6 kOe) and high squareness ratio (ca. 0.65)

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Chemical equilibria involved in the oxygen-releasing step of manganese ferrite water-splitting thermochemical cycle

Sodium ferrimanganite carbonatation reaction was investigated at different temperatures/carbon dioxide partial pressures to evaluate the feasibility of the thermochemical water-splitting cycle based on the MnFe{sub 2}O{sub 4}/Na{sub 2}CO{sub 3}/Na(Mn{sub 1/3}Fe{sub 2/3})O{sub 2} system. After thermal treatments in selected experimental conditions, the obtained powder samples were investigated by using the X-ray diffraction (XRD) technique and Rietveld analysis. Two different lamellar Na{sub 1-x}Mn{sub 1/3}Fe{sub 2/3}O{sub 2-{delta}} phases were observed together with the expected MnFe{sub 2}O{sub 4}/Na{sub 2}CO{sub 3} mixture. Different equilibrium regions among sodium-depleted lamellar phases, manganese ferrite and sodium carbonate were found as a function of the different reaction conditions. A hypothesis concerning the regeneration mechanism of the initial compounds is proposed. Chemical equilibrium between stoichiometric and sub-stoichiometric forms of sodium ferrimanganite and sodium carbonate formation/dissociation appears to be essential factors governing the oxygen-releasing step of the manganese ferrite thermochemical cycle. - Graphical abstract: Na(Mn{sub 1/3}Fe{sub 2/3})O{sub 2} disproportion reaction in the presence of CO{sub 2} was studied. Chemical equilibria among Na{sub 1-x}(Mn{sub 1/3}Fe{sub 2/3})O{sub 2}, MnFe{sub 2}O{sub 4} and Na{sub 2}CO{sub 3} compounds were evidenced and studied by means of Rietveld analysis performed on XRD patterns. Two different sodium-depleted lamellar structures were identified. The role of sodium carbonate formation/dissociation equilibrium in the oxygen-releasing step of the manganese ferrite thermochemical cycle has been highlighted.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗