At least 253 records · Page 14

Corrosion of U233-Doped Uranium Oxide using Microfluidics Methods

The aim of work this year has been to investigate the role of alpha (α)-radiation and hydrogen (H 2 ) on the corrosion of uranium oxide (UO 2 ) using a microfluidic device. The microfluidic device, termed the Particle-Attached Microfluidic Electrochemical Cell, (PAMEC), enables monitoring of the UO 2 electrochemical corrosion potential (E corr ) under different environments, including de-aerated conditions and in the presence of dissolved H 2 . The Si 3 N 4 window allows us to study morphological and chemical changes under an electron microscope. We have previously demonstrated that the PAMEC matches the results from bulk electrochemical tests with UO 2 [1]. We used the high specific activity uranium (U) isotope, 233 U, (t 1/2 = 160,000 years) incorporated into UO 2 , to generate a localized a-field. The objective of the experiments were to mimic the radiation environment that would be experience at the surface of aged spent nuclear fuel (SNF) during long-term geologic disposal under anoxic conditions. Wittman et al. [2] predicted that in the presence of a pure a-radiation field and under H 2 conditions, the concentration of the radiolytic oxidant H 2 O 2 would be suppressed or even eliminated. In a UO 2 corrosion experiment this would be exhibited through a lowering of the measured UO 2 corrosion potential compared to identical conditions in the absence of dissolved H 2 . We found that the predictions of Wittman and co-workers were supported and that the corrosion potential of the 233 U-doped UO 2 in solution lowered with presence of H 2 gas and increased in the absence of H 2 , when under anoxic conditions. The PAMEC experiments indicate that H 2 O 2 has been eliminated in a solution sparged with H 2 while exposed to an a-radiation field. The corrosion potential of the a-doped 233 U(10%)- 238 UO 2 in a solution sparged with Ar/H 2 matched the corrosion potential of 238 UO 2 in solution sparged with air. This clearly demonstrated that the H 2 O 2 had been eliminated and that the only oxidant present was O 2 in this system in complete agreement with the modeling results of Wittman et al. These results point to the need to improve the Fuel Matrix Degradation (FMD) Process Model training data set that is being used in the FMD surrogate model that is being developed for the repository program. The incorporation of realistic radiation chemistry will improve the scientific basis for the FMD Model.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Multiscale Development and Validation of the Stainless Steel Alloy Corrosion (SStAC) Tool for High Temperature Engine Materials

The goal of this project was to create a simulation tool to assist in part design, reducing costs by eliminating the need for conservative material selection, and enabling alloy optimization to improve corrosion resistance. Thus, it helps decrease costs for existing engines and assists in the material and engine design for the engines of the future. To meet our stated goal, we developed the Stainless-Steel Alloy Corrosion (SStAC) tool, which: (1) Models corrosion of engine valves fabricated from 21-2N valve steel in an engine environment at temperatures up to 800 °C. (2) Runs in 1D for a fast estimate of the corrosion rate, and in 2D or 3D for more detailed simulations that represent any part geometry and predict the precise location and rate of corrosion and its impact on the mechanical and thermal behavior. (3) Was implemented using the open-source Multiphysics Object Oriented Simulation Environment (MOOSE). (4) Couples the corrosion model with mechanics and thermal transport models. The SStAC tool can predict the corrosion rate of 21-2N engine valves with less than 10% error.

36 MATERIALS SCIENCE↗

Property Measurements of LiF-NaF-KF Molten Salts Doped with Corrosion Products and Oxygen

Measurements of thermophysical properties of molten salts are needed for modeling and simulation activities that support the development of molten salt reactor (MSR) technologies. Properties of interest including transition temperatures, phase behavior, heat capacity, density, volumetric thermal expansion, surface tension, viscosity, thermal diffusivity, thermal conductivity, and vapor pressure are being performed at Argonne. Results of these property measurements are suitable for use in evaluating reactor performance during startup and the early operating life of the reactor. Ingressions of oxygen and moisture into the fuel salt are expected to occur at different times during the operating life of the reactor due to system leaks, maintenance, and refueling activities. The presence of these environmental contaminants induces corrosion of structural materials. The introduction of corrosion-derived species, oxygen and moisture is expected to affect the physical and chemical properties of the salt and operation of the reactor. Previous work performed at Argonne evaluated the effects of fission product dopants on the thermal properties of eutectic LiF-NaF-KF (FLiNaK). Properties of FLiNaK are commonly used to represent those of fluoride-bearing fuel salts. Metallic corrosion products such as chromium and nickel ions together with dissolved oxygen are expected to affect system redox differently than the accumulation of fission products. Work summarized in this report was performed to measure the effects of corrosion products and dissolved oxygen on the phase transitions, and specific heat capacity of FLiNaK. Thermophysical property measurements were made using four salts that were prepared by doping aliquots of a eutectic mixture of FLiNaK with surrogate corrosion products. Controlled additions of CrF 3 and NiF 2 were used as surrogates for corrosion product contamination anticipated during extended reactor operations in which fuel salt is in contact with steel reactor components. Controlled additions of UF 4 from two sources containing known amounts of UO 2 at different concentrations were used to represent oxygen contamination. The phase transitions and specific heat capacities of the four salts were measured by using differential scanning calorimetry. Measurements were made at temperatures spanning the range of 500−900 °C, which is the expected operating range of MSRs. Measured property values were compared to values measured previously with eutectic FLiNaK without dopants. Differences between property values measured for the doped and non-doped salts were compared with the uncertainties of the measurements to determine the significance of the effect of corrosion products and oxygen on salt properties.

22 GENERAL STUDIES OF NUCLEAR REACTORS↗

Accelerated corrosion testing of cold spray coatings on 304L in chloride environments

Cold spray is an advanced metal manufacturing technique applied across many fields for a wide range of functions. Low heat input and compressive stresses induced into the substrate by the cold spray process makes it a promising choice for protective corrosion resistant coatings. One potential application for cold spray is as a protective coating against corrosion for spent nuclear fuel (SNF) interim dry storage canisters. As these canisters are currently stored at interim storage locations longer than originally intended, chloride induced stress corrosion cracking has been identified as a high priority knowledge gap, specifically with respect to prolonging or extending canister lifetimes ( Teague et al., 2019 ). The high deployability of cold spray, for which nozzles have been developed for application in constrained spaces, in conjunction with beneficial properties inherent to cold spray makes this a good candidate for a corrosion protection coating on SNF canisters. This work explores a pathway to rapidly down-select cold spray coatings for canisters by focusing on the corrosion properties. Specifically, this study examines the corrosion protection abilities of nickel and nickel-based alloy cold spray coatings on 304 L stainless steel in chloride rich environments through electrochemical scans and ferric chloride pitting tests (ASTM G48 Method A). It was shown that the porosity of the coating, the processing gas, material selection, and deformation in the substrate all impact the corrosion behavior of cold spray coatings and are areas where optimization could reduce potential materials degradation, enabling enhanced coatings development.

Karasz, Erin K.↗

Evaluation of Corrosion and Its Impact on the Mechanical Performance of Al–Steel Joints

Aluminum–steel joints are increasingly used in the automotive industry to meet the requirements for energy saving and emission reduction. Among various joining technologies, self-pierce riveting (SPR) and resistance spot welding (RSW) are two well-established technologies for fabricating dissimilar joints with stable and high mechanical performance. However, corrosion will occur in these joints inevitably due to different electrochemical properties, which can degrade the surface quality and the mechanical performance, such as strength. This paper presents a method of understanding the corrosion mechanisms in joining aluminum and steel. For this understanding, a hybrid method combining experimental observations, mechanical properties identification, and analytical approaches was used to assess the evolution of the impact of corrosion on the joining performance, such as traction separation curves. The study was conducted on common combinations used in the vehicles, e.g., a 1.2 mm thickness aluminum alloy (AA 6022) and 2.0 mm thickness hot deep galvanized steel (HDG HSLA 340) joined by SPR and RSW. After the fabrication of these joints, accelerated cyclic corrosion tests of up to 104 cycles were performed, which reproduced the environmental conditions to which a vehicle was exposed. By investigating the microstructural evolution within the joints, the corrosion mechanisms of SPR and RSW joints were revealed, including the initiation and propagation. Moreover, the intrinsic impact of the corrosion on the mechanical performance, including the strength, axial stiffness, and crashworthiness, was analyzed by performing a lap-shear test. It showed that as corrosion proceeds, the fracture modes and mechanical performance are affected significantly.

Chemistry↗

Modeling the Impact of Grain Size on Corrosion Behavior of Ni-Based Alloys in Molten Chloride Salt via Cellular Automata

Molten chloride salts hold significant promise as both thermal transfer and storage media for next-generation concentrated solar power (CSP) systems. However, molten chlorides pose a considerable corrosion risk to structural materials, particularly Ni-based alloys. One approach to enhancing corrosion resistance is through the optimization of grain structure; however, it remains uncertain whether increasing or decreasing grain size enhances corrosion resistance. A cellular automata (CA) program was developed to evaluate the interplay between grain size and corrosion in Ni-based alloy. Our CA program tracks alloy composition, surface roughness, and thickness loss via a graphical user interface, displaying corrosion and diffusion status, and multiple user input cards for tuning the simulation. CA simulations of Inconel 625 indicate enhanced corrosion resistance with increased grain size, with passivating oxides offering limited protection. Additionally, the temporal evolution of alloy surface roughness demonstrates notable fluctuations, with abrupt increases attributed to corrosion along vertical grain boundaries and sudden decreases to grain detachment from the protective film.

Materials Science↗

Susceptibility to hot corrosion of four nickel-base superalloys, NASA-TRW VIA, B-1900, 713C and IN-738

The susceptibility to hot corrosion of four nickel-base, cast superalloys has been studied at 900 and 1000 C. The test consisted of coating alloy samples with known amounts of Na2SO4 and oxidizing the coated samples isothermally in 1 atmosphere of slowly flowing oxygen, the weight-gain being monitored on a sensitive recording microbalance. Susceptibility to hot corrosion decreased in the order of decreasing molybdenum content of the alloys. Preoxidation of samples before hot-corrosion testing markedly increased the induction period observed prior to the inception of hot corrosion for all alloys tested. X-ray diffraction analyses of the oxide scales were made. All samples that underwent hot corrosion showed the presence of a (Ni,Co)MoO4 layer near the alloy-oxide interface. Several specimens displayed resistance to hot corrosion and these showed NaTaO3 as a prominent feature in their oxide scale. Our results may be interpreted as indicating that molybdenum in an alloy is detrimental, with respect to hot corrosion, while tantalum is beneficial.

Stearns, C. A.↗

Effect of sodium, potassium, magnesium, calcium, and chlorine on the high temperature corrosion of IN-100, U-700, IN-792, and Mar M-509

The effects of potential impurities such as Na, K, Mg, Ca, and Cl, in coal-derived liquid fuels on accelerated corrosion of IN-100, U-700, IN-792, and Mar M-509 were investigated using a Mach 0.3 burner rig for times to 200 hours in one hour cycles. These impurities were injected in combination as aqueous solutions into the combustor. Other variables were time, temperature, and fuel-to-air ratio. The experimental matrix was a central composite fractional fractorial design divided into blocks to allow modification of the design as data was gathered. The extent of corrosion was determined by metal consumption. The time exponent was near 1.0 for the least corrosion resistant alloys, U-700 and IN-100; near 0.8 for the moderately resistant IN-792; and close to Mar M-509, the most corrosion resistant alloy. As anticipated, corrosion rapidly increased with increasing temperature as well as Na and K concentrations, while corrosion decreased somewhat as the Ca concentration increased for all alloys. Mg was beneficial for the Ni-base alloys but had little effect on the Co-base alloy. Surprisingly, the effect of increasing Cl was to decrease the corrosion of all alloys. Little interaction among the dopants was noted.

Lowell, C. E.↗

Atmospheric corrosion model and monitor for low cost solar arrays

An atmospheric corrosion model and corrosion monitoring system has been developed for low cost solar arrays (LSA). The corrosion model predicts that corrosion rate is the product of the surface condensation probability of water vapor and the diffusion controlled corrosion current. This corrosion model is verified by simultaneous monitoring of weather conditions and corrosion rates at the solar array test site at Mead, Nebraska.

Kaelble, D. H.↗

Interaction of sulfuric acid corrosion and mechanical wear of iron

Friction and wear experiments were conducted with elemental iron sliding on aluminum oxide in aerated sulfuric acid at concentrations ranging from very dilute (0.00007 N; i.e., 4 ppm) to very concentrated (96 percent acid). Load and reciprocating sliding speed were kept constant. With the most dilute acid concentration of 0.00007 to 0.0002 N, a complex corrosion product formed that was friable and often increased friction and wear. At slightly higher concentrations of 0.001 N, metal losses were essentially by wear alone. Because no buildup of corrosion products occurred, this acid concentration became the standard from which to separate metal loss from direct corrosion and mechanical wear losses. When the acid concentration was increased to 5 percent (1 N), the well-established high corrosion rate of iron in sulfuric acid strongly dominated the total wear loss. This strong corrosion increased to 30 percent acid and decreased somewhat to 50 percent acid in accordance with expectations. However, the low corrosion of iron expected at acid concentrations of 65 to 96 percent was not observed in the wear area. It was apparent that the normal passivating film was being worn away and a galvanic cell established that rapidly attacked the wear area. Under the conditions where direct corrosion losses were highest, the coefficient of friction was the lowest.

Rengstorff, G. W. P.↗

Interaction of sulfuric acid corrosion and mechanical wear of iron

Friction and wear experiment were conducted with elemental iron sliding on aluminum oxide in aerated sulfuric acid at concentrations ranging from very dilute (0.00007 N; i.e., 4 ppm) to very concentrated (96 percent acid). Load and reciprocating sliding speed were kept constant. With the most dilute acid concentration of 0.00007 to 0.0002 N, a complex corrosion product formed that was friable and often increased friction and wear. At slightly higher concentrations of 0.001 N, metal losses were essentially by wear alone. Because no buildup of corrosion products occurred, this acid concentration became the standard from which to separate metal loss from direct corrosion and mechanical wear losses. When the acid concentration was increased to 5 percent (1 N), the well-established high corrosion rate of iron in sulfuric acid strongly dominated the total wear loss. This strong corrosion increased to 30 percent acid and decreased somewhat to 50 percent acid in accordance with expectations. However, the low corrosion of iron expected at acid concentrations of 65 to 96 percent was not observed in the wear area. It was apparent that the normal passivating film was being worn away and a galvanic cell established that rapidly attacked the wear area. Under the conditions where direct corrosion losses were highest, the coefficient of friction was the lowest.

Rengstorff, G. W. P.↗

Na2SO4 induced corrosion of nickel at high temperature

Sodium sulfate-induced corrosion of nickel was studied at 900 C as a function of oxygen partial pressure. For high O2 partial pressures, accelerated corrosion during the first few minutes occurred by rapid penetration of the melt along the metal grain boundaries. A mechanism is proposed to explain this phenomenon. Repetitive scale metal detachment was observed for corrosion in lower O2 partial pressures and during the later period of corrosion in higher O2 partial pressures. The effect of preoxidation on the hot corrosion has also been studied. An induction period is observed before the onset of rapid corrosion for the preoxidized samples; the onset of rapid corrosion is associated with sudden cracking of the scale. The length of the induction period for the preoxidized samples is a function of the length of preoxidation, and appears to be related to the structure of the oxide scale after the preoxidation treatment.

Misra, A. K.↗

Sodium sulfate-induced corrosion of pure nickel and superalloy Udimet 700 in a high velocity burner rig at 900 C

Sodium sulfate-induced corrosion of pure nickel and a commercial nickel-base superalloy, Udimet 700 (U-700), were studied at 900 C in a Mach 0.3 burner rig with different Na levels in the combustor. The corrosion rate of Ni was independent of the Na level in the combustor and considerably lower than that measured in laboratory salt spray tests. The lower rates are associated with the deposition of only a small amount of Na2SO4 on the surface of the NiO scale. Corrosion of U-700 was observed to occur in two stages. During the first stage, the corrosion proceeds by reaction of Cr2O3 scale with the Na2SO4 and evaporation of the Na2CrO4 reaction product from the surface of the corroding sample. Cr depletion in the alloy occurs and small sulfide particles are formed in the Cr depletion zone. Extensive sulfidation occurs during the second state of corrosion, and a thick scale forms. The relationship between the corrosion rate of U-700 and the Na level in the combustor gives a good correlation in the range of 0.3 to 1.5 ppm by weight Na. Very low levels of Na in the combustor cause accelerated oxidation of U-700 without producing the typical hot corrosion morphology.

Misra, A. K.↗

Localized corrosion of high performance metal alloys in an acid/salt environment

Various vacuum jacketed cryogenic supply lines at the Space Shuttle launch site at Kennedy Space Center use convoluted flexible expansion joints. The atmosphere at the launch site has a very high salt content, and during a launch, fuel combustion products include hydrochloric acid. This extremely corrosive environment has caused pitting corrosion failure in the thin walled 304L stainless steel flex hoses. A search was done to find a more corrosion resistant replacement material. The study focussed on 19 metal alloys. Tests which were performed include electrochemical corrosion testing, accelerated corrosion testing in a salt fog chamber, and long term exposure at a beach corrosion testing site. Based on the results of these tests, several nickel based alloys were found to have very high resistance to this corrosive environment. Also, there was excellent agreement between the electrochemical tests and the actual beach exposure tests. This suggests that electrochemical testing may be useful for narrowing the field of potential candidate alloys before subjecting samples to long term beach exposure.

Macdowell, L. G.↗

Development of an Accelerated Test Method for the Determination of Susceptibility to Atmospheric Corrosion

The theoretical rationale is presented for use of a repetitive cyclic current reversal voltammetric technique for characterization of localized corrosion processes, including atmospheric corrosion. Applicability of this proposed experimental protocol is applied to characterization of susceptibility to crevice and pitting corrosion, atmospheric corrosion and stress corrosion cracking. Criteria upon which relative susceptibility is based were determined and tested using two iron based alloys commonly in use at NASA-Kennedy; A36 (a low carbon steel) and 4130 (a low alloy steel). Practicality of the procedure was demonstrated by measuring changes in anodic polarization behavior during high frequency current reversal cycles of 25 cycles per second with 1 mA/sq cm current density amplitude in solutions containing Cl anions. The results demonstrated that, due to excessive polarization which affects conductivity of barrier corrosion product layers, A36 was less resistant to atmospheric corrosion than its 4130 counterpart; behavior which was also demonstrated during exposure tests.

Ambrose, John R.↗

Experimental Design for the Evaluation of Detection Techniques of Hidden Corrosion Beneath the Thermal Protective System of the Space Shuttle Orbiter

The detection of corrosion beneath Space Shuttle Orbiter thermal protective system is traditionally accomplished by removing the Reusable Surface Insulation tiles and performing a visual inspection of the aluminum substrate and corrosion protection system. This process is time consuming and has the potential to damage high cost tiles. To evaluate non-intrusive NDE methods, a Proof of Concept (PoC) experiment was designed and test panels were manufactured. The objective of the test plan was three-fold: establish the ability to detect corrosion hidden from view by tiles; determine the key factor affecting detectability; roughly quantify the detection threshold. The plan consisted of artificially inducing dimensionally controlled corrosion spots in two panels and rebonding tile over the spots to model the thermal protective system of the orbiter. The corrosion spot diameter ranged from 0.100" to 0.600" inches and the depth ranged from 0.003" to 0.020". One panel consisted of a complete factorial array of corrosion spots with and without tile coverage. The second panel consisted of randomized factorial points replicated and hidden by tile. Conventional methods such as ultrasonics, infrared, eddy current and microwave methods have shortcomings. Ultrasonics and IR cannot sufficiently penetrate the tiles, while eddy current and microwaves have inadequate resolution. As such, the panels were interrogated using Backscatter Radiography and Terahertz Imaging. The terahertz system successfully detected artificially induced corrosion spots under orbiter tile and functional testing is in-work in preparation for implementation.

Kemmerer, Catherine C.↗

Electrochemical, Polarization, and Crevice Corrosion Testing of Inconel X750: A Supplement to the Environmental Control and Life Support System Sustaining Metal Materials Compatibility Study

In previous studies, electrochemical test results were experimentally acquired and then presented for several noble alloys in two specific solutions representative of waste liquids generated or present within the Environmental Control and Life Support System (ECLSS) aboard the International Space Station (ISS). Subsequently, another metal candidate, Inconel X750, has been submitted and was subjected to the same test routines in the same solutions and evaluated with the same statistical/analytical methodologies as those utilized in the earlier studies. Previous studies included three titanium grades, (Commercially Pure, 6Al-4V alloy, and 6Al-4V Low Interstitial alloy), two nickel-chromium alloys (Inconel® 625 and Hastelloy® C276), one high tier stainless steel (Cronidur® 30), and a nickel-titanium alloy (Nitinol 60). Thus far, all candidate alloys have exhibited excellent corrosion protection and galvanic compatibility attributes and have been deemed qualified materials for application within the ECLSS facility. Inconel X750 now joins that group. The titanium alloys gave the best results of all the metal candidates by demonstrating superior nobility and galvanic protection properties. It is worth noting that the corrosion performance properties for the three titanium alloys were essentially indistinguishable. As such and for expediency, this study and all future evaluations will refer only to the comparative properties already documented for Titanium 6Al-4V as this alloy is representative of all three alloys and considered to be more mainstream. Now the measured corrosion properties for Inconel X750 were very similar to those determined previously for Inconel 625 and Hastelloy C276 which were also determined to be very high performers. For the current effort, the results have clearly shown that Inconel X750 possesses exceptional anti-corrosion attributes comparable to metals in the highest tier of the galvanic series. Overall, one can conclude that Inconel X750 is quite noble, highly corrosion resistant and galvanically compatible with the other metal groups from both an electrochemical perspective and a long-term exposure scenario. This was clearly demonstrated after utilizing the same techniques as those applied in previous studies which included linear, Tafel and cyclic polarization, galvanic coupling with each of the other metal candidates, and pitting/crevicing assessments after one full year of immersion in the subject test solutions. Attributes defining the nobility and anti-corrosion capabilities for X750 appear to be on par with all the other candidates thus far and this alloy can now be classified as ‘excellent’ exhibiting very high resistance toward general, localized, and galvanic corrosion in the subject test media.

Lee, R. E.↗

Corrosion Behavior of Alloy Structural Steels in Catechol and Biomass-Derived Pyrolysis Oils

Electrochemical impedance spectroscopy (EIS) was used to assess the corrosion behavior of three steels, 2.25Cr-1Mo, 5Cr-1Mo and 9Cr-1Mo (UNS K21590, S50200 and K90941) in bio-oils and catechol, an organic constituent commonly found in bio-oils. Two types of biomass pyrolysis oils produced from selected forest residue feedstocks, classified as high-ash and high-moisture (HAHM) and low-ash and low-moisture (LALM) types and 10 wt.% catechol, were used to test the alloys. According to previous results, 10 wt.% catechol in a water and methanol mixture was corrosive to 2.25Cr-1Mo but not to 9Cr-1Mo, highlighting that increasing Cr content in the steels resulted in improved corrosion resistance. 5Cr-1Mo, a steel with an intermediate Cr content, was tested in catechol solutions to better estimate the critical value of Cr for corrosion resistance under these conditions. Also, the three alloys were tested in both HAHM and LALM bio-oils to assess corrosion susceptibility. For EIS measurements, a customized electrochemical setup was employed to minimize the ohmic path through the bio-oils. The corrosion susceptibility was evaluated by determining the resistance at the alloy-corrosive medium interface.

Jun, Jiheon↗