Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “Alloy”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 253 records · Page 14

Estimation of grain boundary segregation enthalpy and its role in stable nanocrystalline alloy design

Grain boundary segregation provides a method for stabilization of nanocrystalline metals—an alloying element that will segregate to the boundaries can lower the grain boundary energy, attenuating the driving force for grain growth. The segregation strength relative to the mixing enthalpy of a binary system determines the propensity for segregation stabilization. This relationship has been codified for the design space of positive enthalpy alloys; unfortunately, quantitative values for the grain boundary segregation enthalpy exist in only very few material systems, hampering the prospect of nanocrystalline alloy design. We present a Miedema-type model for estimation of grain boundary segregation enthalpy, with which potential nanocrystalline phase-forming alloys can be rapidly screened. Calculations of the necessary enthalpies are made for ~2500 alloys and used to make predictions about nanocrystalline stability.

36 MATERIALS SCIENCE↗

Evaluation of the effect of alloy chemistry on the susceptibility of weld solidification cracking of Alloy 709 weldment and development of mitigation strategy

Alloy 709 is an attractive candidate construction material for Sodium Fast Reactor. As part of the Alloy 709 Intermediate Term Test Program, this work covers the development of the technical basis for welding fabrication and weld qualification of Alloy 709. The phase of research reported herein focused on the issue of weld solidification cracking recently experienced in some experimental heats of Alloy 709 with relatively high P levels. To this end, computational thermodynamics simulations were used to investigate the solidification behavior of Alloy 709.

36 MATERIALS SCIENCE↗

Manufacturing Dissolvable Alloy Components using ShAPE: A Study on Solid Phase Processing of Mg-W Composites and WJ11 Alloys

Dissolvable alloys and composites are an emerging class of materials that demonstrate tailored sorptivity in corrosive environments. This work explored the viability of solid phase processing (SPP) techniques, namely the shear assisted processing and extrusion (ShAPETM) method, to manufacture dissolvable magnesium composites and alloys components such as rods and tubes. The study also determined the effects of material composition and manufacturing process conditions on material microstructures developed during SPP and the resulting performance of the components. Explicit properties of interest included ultimate tensile strength, ultimate compressive strength, and yield strength. The application fields of interest for dissolvable alloys were identified as oil-and-gas operations and biomedical implants. Accordingly, PNNL collaborated with industrial and academia partners, Fortek Industries, Houston and University of Pittsburgh, during the course of this project for material and ShAPE process development. PNNL determined the viability of the using ShAPE to process the custom-designed materials provided by the project partners. This was done by identifying process parameters such as tool rotation rate, tool plunge rate, and process cooling optimal for manufacturing components with consolidated microstructures. Subsequently, PNNL also performed microstructural characterization on unprocessed and processed samples and mechanical property testing. One of the major findings from this work is that ShAPE was able to manufacture dissolvable magnesium composite and alloy rods and tubes with consolidated homogeneous microstructures and minimal macroscale defects on component surfaces. It was observed that samples processed via ShAPE demonstrated an average grain size < 2 - 5 µm, which was markedly lower than that of the precursors with 8 – 13 µm grains. Results showed that the ShAPE synthesized dissolvable magnesium composite and alloy strength was on par with or better than those components that were manufactured using traditional manufacturing processes such as forging and extrusion. It is noteworthy that the ShAPE samples were made with considerably lower number of process steps.

36 MATERIALS SCIENCE↗

Alloy and structural optimization of a directionally solidified lamellar eutectic alloy

Mechanical property characterization tests of a directionally solidified Ni-20 percent Cb-2.5 percent Al-6 percent Cr cellular eutectic turbine blade alloy demonstrated excellent long time creep stability and indicated intermediate temperature transverse tensile ductility and shear strength to be somewhat low for turbine blade applications. Alloy and structural optimization significantly improves these off-axis properties with no loss of longitudinal creep strength or stability. The optimized alloy-structure combination is a carbon modified Ni-20.1 percent Cb-2.5 percent Al-6.0 percent Cr-0.06 percent C composition processed under conditions producing plane front solidification and a fully-lamellar microstructure. With current processing technology, this alloy exhibits a creep-rupture advantage of 39 C over the best available nickel base superalloy, directionally solidified MAR M200+ Hf. While improved by about 20 percent, shear strength of the optimized alloy remains well below typical superalloy values.

Sheffler, K. D.↗

Friction and wear with a single-crystal abrasive grit of silicon carbide in contact with iron base binary alloys in oil: Effects of alloying element and its content

Sliding friction experiments were conducted with various iron-base binary alloys (alloying elements were Ti, Cr, Mn, Ni, Rh, and W) in contact with a rider of 0.025-millimeter-radius, single-crystal silicon carbide in mineral oil. Results indicate that atomic size and content of alloying element play a dominant role in controlling the abrasive-wear and -friction properties of iron-base binary alloys. The coefficient of friction and groove height (wear volume) general alloy decrease, and the contact pressure increases in solute content. There appears to be very good correlation of the solute to iron atomic radius ratio with the decreasing rate of coefficient of friction, the decreasing rate of groove height (wear volume), and the increasing rate of contact pressure with increasing solute content C. Those rates increase as the solute to iron atomic radius ratio increases from unity.

Miyoshi, K.↗

Stability of several oxide dispersion strengthened alloys and a directionally solidified gamma/gamma prime-alpha eutectic alloy in a thermal gradient

Thermal gradient testing of three oxide dispersion strengthened alloys (two Ni-base alloys, MA 754 and MA 6000 E, and the Fe-base MA 956) and the directionally solidified eutectic alloy, gamma/gamma prime-alpha, have been conducted. Experiments were carried out with maximum temperatures up to 1200 C and thermal gradients on the order of 100 C/mm. The oxide dispersion strengthened alloys were difficult to test because the thermal stresses promoted crack nucleation and growth; thus the ability of these alloys to maintain a thermal gradient may be limited. The stability of individual fibers in gamma/gamma prime-alpha was excellent; however, microstructural changes were observed in the vicinity of grain boundaries. Similar structures were also observed in isothermally annealed material; therefore thermal gradients do not affect the microstructure of gamma/gamma prime-alpha in any significant manner.

Staniek, G.↗

On improving the fracture toughness of a NiAl-based alloy by mechanical alloying

Mechanical alloying (MA) has been used to process the NiAl-based alloy Ni-35Al-20Fe, such that a fine-grain (about 2 microns) microstructure is obtained through the addition of 2 vol pct Y2O3 particles. When compared to a conventionally processed, coarse-grained (about 28 microns) Ni-35-20 alloy without the Y2O3 particles, the MA alloy exhibits two to three times higher fracture toughness values, despite a 50-percent increase in yield strength. Room-temperature K(O) values as high as 34 MPa sq rt m are observed, accompanied by a yield strength in excess of 1100 MPa. Fractography confirms a change in fracture characteristics of the fine-grained MA alloy.

Kostrubanic, J.↗

Method for producing La/Ce/MM/Y base alloys, resulting alloys and battery electrodes

A carbothermic reduction method is provided for reducing a La-, Ce-, MM-, and/or Y-containing oxide in the presence of carbon and a source of a reactant element comprising Si, Ge, Sn, Pb, As, Sb, Bi, and/or P to form an intermediate alloy material including a majority of La, Ce, MM, and/or Y and a minor amount of the reactant element. The intermediate material is useful as a master alloy for in making negative electrode materials for a metal hydride battery, as hydrogen storage alloys, as master alloy additive for addition to a melt of commercial Mg and Al alloys, steels, cast irons, and superalloys; or in reducing Sm.sub.2O.sub.3 to Sm metal for use in Sm--Co permanent magnets.

25 ENERGY STORAGE↗

Alloys for shaped charge liners method for making alloys for shaped charge liners

One embodiment of the invention provides an alloy with a density greater than 10 g/cm3, the alloy comprising a single phase solution of tungsten, nickel, and iron. Also provided is a cone liner for use in shaped charges, the liner comprised of a tungsten, nickel, iron alloy having a single phase microstructure. Substantially no precipitates or second phases exist in the alloy. One embodiment of the invention further provides a method for producing a single phase alloy, the method comprising establishing a melt of iron and nickel; dissolving tungsten in the melt to form a solution; wherein the atomic percents of the nickel, tungsten and iron range from between approximately Ni-7%W-0%Fe, Ni-18%W-0%Fe, and Ni-8%W-24%Fe, wherein Ni is the remainder, maintaining the solution at a first temperature sufficient to create a homogeneous mixture; allowing the homogeneous mixture to solidify; and thermochemically treating the solidified mixture for a time to dissolve any second phases or microstructure within the mixture.

36 MATERIALS SCIENCE↗

Method for producing La/Ce/MM/Y base alloys, resulting alloys, and battery electrodes

A carbothermic reduction method is provided for reducing a La-, Ce-, MM-, and/or Y-containing oxide in the presence of carbon and a source of a reactant element comprising Si, Ge, Sn, Pb, As, Sb, Bi, and/or P to form an intermediate alloy material including a majority of La, Ce, MM, and/or Y and a minor amount of the reactant element. The intermediate material is useful as a master alloy for in making negative electrode materials for a metal hydride battery, as hydrogen storage alloys, as master alloy additive for addition to a melt of commercial Mg and Al alloys, steels, cast irons, and superalloys; or in reducing Sm2O3 to Sm metal for use in Sm—Co permanent magnets.

25 ENERGY STORAGE↗

Effect of mechanical milling on Ni-TiH{sub 2} powder alloy filler metal for brazing TiAl intermetallic alloy: The microstructure and joint's properties

A TiH{sub 2}-50 wt.% Ni powder alloy was mechanically milled in an argon gas atmosphere using milling times up to 480 min. A TiAl intermetallic alloy was joined by vacuum furnace brazing using the TiH{sub 2}-50 wt.% Ni powder alloy as the filler metal. The effect of mechanical milling on the microstructure and shear strength of the brazed joints was investigated. The results showed that the grains of TiH{sub 2}-50 wt.% Ni powder alloy were refined and the fusion temperature decreased after milling. A sound brazing seam was obtained when the sample was brazed at 1140 deg. C for 15 min using filler metal powder milled for 120 min. The interfacial zones of the specimens brazed with the milled filler powder were thinner and the shear strength of the joint was increased compared to specimens brazed with non-milled filler powder. A sample brazed at 1180 deg. C for 15 min using TiH{sub 2}-50 wt.% Ni powder alloy milled for 120 min exhibited the highest shear strength at both room and elevated temperatures.

36 MATERIALS SCIENCE↗

Coupling Thermomechanical Processing and Alloy Design to Improve Textures in Mg-Zn-Ca Sheet Alloys

Abstract The effect of Ca and Zn additions on the microstructure and texture evolution during thermomechanical processing of Mg-Zn-Ca sheet alloys was systematically investigated and quantified. Plane strain compression testing in a Gleeble thermomechanical simulator was used to physically simulate a 10-pass rolling schedule, while allowing for careful control and monitoring of the processing parameters. Textures in the as-deformed ternary alloy samples demonstrate a weak maximum basal intensity and spreading in the transverse direction. Increasing the Zn content to 3.2 wt.% in the ternary alloys resulted in samples that exhibited weak textures in the as-deformed state. Importantly, static recrystallization (SRX) during post-deformation annealing of these alloys promoted a desirable annular texture, with the c -axis tipped from the normal direction and a lower basal texture intensity. The evolution in texture during SRX is associated with as-deformed microstructures with broad grain orientation spreads and a low degree of recrystallization.

36 MATERIALS SCIENCE↗

The effect of interstitial carbon on the mechanical properties and dislocation substructure evolution in Fe 40.4 Ni 11.3 Mn 34.8 Al 7.5 Cr 6 high entropy alloys

A systematic study of the effects of up to 1.1 at. % carbon on the mechanical properties and evolution of the dislocation substructure in a series of a high entropy alloys (HEA) based on Fe40.4Ni11.3Mn34.8Al7.5Cr6 is presented. Transmission electron microscopy (TEM), synchrotron X-ray diffraction (XRD) and atom probe tomography (APT) were used to show that all the alloys are single-phase f.c.c. random solid solutions. The lattice constant, determined from synchrotron XRD measurements, increases linearly with increasing carbon concentration, which leads to a linear relationship between the yield strength and the carbon concentration. The dislocation substructures, as determined by a TEM, show a transition from wavy slip to planar slip and, at higher strains, and from cell-forming structure (dislocations cells, cell blocks and dense dislocation walls) to non-cell forming structure (Taylor lattice, microbands and domain boundaries) with the addition of carbon, features related to the increase in lattice friction stress. The stacking fault energy (measured via weak-beam imaging of the separation of dislocation partials) decreases with increasing carbon content, which also contributes to the transition from wavy slip to planar slip. The formation of non-cell forming structure induced by carbon leads to a high degree of strain hardening and a substantial increase in the ultimate tensile strength. The consequent postponement of necking due to the high strain hardening, along with the plasticity accommodation arising from the formation of microbands and domain boundaries, result in an increase of ductility due to the carbon addition. (C) 2016 Acta Materialia Inc. Published by Elsevier Ltd. All rights reserved.

Dislocation structures↗

Stress corrosion crack initiation of alloy 600 in PWR primary water

Stress corrosion crack (SCC) initiation of three mill-annealed (MA) alloy 600 heats in simulated pressurized water reactor primary water has been investigated using constant load tests equipped with in-situ direct current potential drop (DCPD) measurement capabilities. SCC initiation times were greatly reduced by a small amount of cold work. Shallow intergranular (IG) attack and/or cracks were found on most high-energy grain boundaries intersecting the surface with only a small fraction evolving into larger cracks and IGSCC growth. Crack depth profiles were measured and related to DCPD-detected initiation response. Processes controlling the SCC initiation in MA alloy 600 are discussed. IN PRESS, CORRECTED PROOF, 05/02/2017 - mfl

alloy↗

Dynamic shear localization of a titanium alloy under high-rate tension characterized by x-ray digital image correlation

Highlights: • First systematic error analyses for XDIC • First XDIC study of Ti-6Al-4V under dynamic tension • Deformation mode transition induces dynamic ductility decrease. • Dynamic shear localization due to rate-dependent microvoid coalescence process. - Abstract: Dynamic and quasi-static tension experiments are conducted on Ti-6Al-4V alloys, with in situ, synchrotron-based, high-speed, x-ray phase contrast imaging implemented to characterize the dynamic deformation and fracture process of Ti alloys at the Advanced Photon Source. X-ray digital imaging correlation (XDIC) is applied for strain field mapping. The size distribution of x-ray speckles are quantified via a morphological analysis, with a mean of ∼20 μm. Systematic error analyses of displacement and strain field measurements are firstly conducted for XDIC, and demonstrate that the displacement and strain errors can be controlled below 0.01 pixel and 0.1%, respectively. Mesoscale strain characteristics measured via XDIC are consistent with and reveal mechanisms for the bulk-scale stress–strain responses. Under dynamic tension, a sharp transition to strain softening occurs when the bulk strain exceeds about 0.04, which leads to a lower dynamic fracture strain (0.08) than the quasi-static one (0.1). The corresponding strain filed mapping demonstrates that shear deformation localizations grow and coalesce rapidly into a narrow shear deformation band under dynamic loading, while tensile deformation and necking progresses gradually under quasi-static loading. Scanning electron microscopy shows that void nucleation occurs mainly at the interface of α and β phases for both quasi-static and dynamic tension. However, microvoids coalesce preferentially along colony boundaries or the boundary α phase under quasi-static tension, but along the maximum shear stress direction (across colonies) under dynamic tension. Fractography of recovered samples also shows consistent features.

36 MATERIALS SCIENCE↗