Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “strain hardening”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 235 records · Page 13

A viscoplastic theory with thermodynamic considerations

A thermodynamic foundation using the concept of internal state variables is given for a general theory of viscoplasticity for initially isotropic materials. Three, fundamental, internal, state variables are admitted; they are: a tensorial back stress for kinematic effects, and scalar drag and yield strengths for isotropic effects. All three are considered to evolve phenomenologically according to competitive processes between strain hardening, deformation induced dynamic recovery, and thermally induced static recovery. Within this phenomenological framework, a thermodynamically admissible set of evolution equations is proposed. The theory allows each of the three internal variables to be composed as a sum of independently evolving constituents. The evolution of internal state can also include terms that vary linearly with the external variable rates, whose presence affects the energy dissipation properties of a material.

Freed, A. D.↗

Superplastic forming of ceramic insulation

Superplasticity has been demonstrated in many fine-grained structural ceramics and ceramic composites, including yttria-stabilized tetragonal zirconia polycrystal (YTZP), alumina, and Al2O3-reinforced zirconia (Al2O3/YTZ) duplex composites and SiC-reinforced Si3N4. These superplastic ceramics obviously offer the potential benefit of forming net shape or near net shape parts. This could be particularly useful for forming complicated shapes that are difficult to achieve using conventional forming techniques, or require elaborate, subsequent machining. In the present study, we successfully demonstrated the following: (1) superplastic 3Y-TXP and 20 percent Al2O3/YTZ composite have for the first time been successfully deformed into hemispherical caps via a biaxial gas-pressure forming technique; (2) no experimental difficulty was encountered in applying the required gas pressures and temperatures to achieve the results, thus, it is certain that higher rates of deformation than those presented in this study will be possible by using the current test apparatus at higher temperatures and pressures; and (3) an analytical model incorporating material parameters, such as variations during forming in the strain rate sensitivity exponent and grain growth-induced strain hardening, is needed to model accurately and therefore precisely control the biaxial gas-pressure forming of superplastic ceramics. Based on the results of this study, we propose to fabricate zirconia insulation tubes by superplastic extrusion of zirconia polycrystal. This would not only reduce the cost, but also improve the reliability of the tube products.

Nieh, T. G.↗

The stress criterion of a tension member with graded flexural stiffness : contribution to the problem of "clamping effect" outside of the elastic range

The approximate size of the stress criterion of a bar on two supports stressed beyond the elastic range is assessed by an approximation. The calculation proceeds from the premise of "substitute flexural stiffness" so defined that the part stressed beyond the elastic range may be considered as following Hooke's law when determining the flexural deformation quantities. For the determination of the substitute flexural stiffness, it is presumed that the material is already stressed so much beyond the yield point as to be strain-hardened. The data are directly applicable to materials having no definite yield point. For the rest, von Karman's method for compressed and subsequently deflected bars serves as basis for the calculation.

Kaul, Hans W↗

Forming Weld Lands On Metal Plates

Forming shoe pounds edge of newly inserted plate workpiece. After many passes of shoe and advances of plate, thick land builds up at edge. Workpiece heated to enable metal to flow without strain hardening. Proposed upset-forming process replaces relatively expensive, time-consuming, and wasteful process in which integral weld lands created by machining metal away from plates everywhere except at lands.

Weddendorf, Bruce↗

Use of photostress to characterize the mechanical behavior of weldments

Welded aluminum is an important part of many space structures. Knowledge of the properties and behavior of weld material and the material surrounding the weld is important for modeling and design of the structures. Photoelastic coatings (Photostress) and strain gages were used to determine behavior of heat treated and as welded joints made from 2219T87 parent material and 2319 weld material subjected to tensile loads. TIG welds of 1/8, 1/2, and 1.4 inches thickness were investigated. Discontinuous yielding was observed in all tests and highly non-uniform behavior through the weld thickness was observed in joints having welds 1.4 inches thick. Joints having welds 1/8 and 1/2 inches thick had only small differences in behavior through the thickness of the weld. Joints in the 1/2 inch thick material contained distinct zones of constant strain within the normal strain gradient extending outward from the weld centerline. These zones had different thickness and locations. Points at the weld centerline, and for a distance of nearly one inch from the centerline, exhibited very nonlinear behavior during the first loading but exhibited near perfect strain hardening during the second loading.

Gambrell, S. C., Jr.↗

The extensional rheology of non-Newtonian materials

It has been proposed to measure the extensional viscosity function of a non-Newtonian polymer solution in a reduced gravity environment as part of the Advanced Fluid Module. In ground-based extensional measurements, the no-sip boundary condition at solid-fluid interfaces always result in appreciable shear gradients in the test fluid; however the removal of gravitational body forces permits controlled extensional deformation of containerless test samples and the first unambiguous measurements of this kind. Imperative to successful implementation of this experiment is the generation and subsequent deformation of a stable cylindrical column of test fluid. A study of the generation and deformation of liquid bridges demonstrates that Newtonian liquid bridges undergo capillary breakup as anticipated when stretched beyond a critical aspect ratio; non-Newtonian liquid bridges, however, are stabilized by the strain-hardening phenomenon exhibited by these materials. Numerical simulations of Newtonian breakup are compared with experimental results, and show that previous ground-based attempts at measuring the extensional viscosity of Newtonian fluids are of limited accuracy.

Spiegelberg, Stephen H.↗

Sensitivity analysis for the dynamic response of thermoviscoplastic shells of revolution

A computational procedure is presented for evaluating the sensitivity coefficients of the dynamic axisymmetric, fully-coupled, thermoviscoplastic response of shells of revolution. The analytical formulation is based on Reissner's large deformation shell theory with the effects of large-strain, transverse shear deformation, rotatory inertia and moments turning around the normal to the middle surface included. The material model is chosen to be viscoplasticity with strain hardening and thermal hardening, and an associated flow rule is used with a von Mises effective stress. A mixed formulation is used for the shell equations with the fundamental unknowns consisting of six stress resultants, three generalized displacements and three velocity components. The energy-balance equation is solved using a Galerkin procedure, with the temperature as the fundamental unknown. Spatial discretization is performed in one dimension (meridional direction) for the momentum and constitutive equations of the shell, and in two dimensions (meridional and thickness directions) for the energy-balance equation. The temporal integration is performed by using an explicit central difference scheme (leap-frog method) for the momentum equation; a predictor-corrector version of the trapezoidal rule is used for the energy-balance equation; and an explicit scheme consistent with the central difference method is used to integrate the constitutive equations. The sensitivity coefficients are evaluated by using a direct differentiation approach. Numerical results are presented for a spherical cap subjected to step loading.

Kulkarni, Makarand↗

Aluminum U-groove weld enhancement based on experimental stress analyses

Though butt-welds are among the most preferred joining methods in aerostructures because of their sealing and assembly integrity and general elastic performance; their inelastic mechanics are generally the least understood. This study investigated experimental strain distributions across a thick aluminum U-grooved weld and identified two weld process considerations for improving the multipass weld strength. The extreme thermal expansion and contraction gradient of the fusion heat input across the tab thickness between the grooves produce severe peaking, which induces bending moment under uniaxial loading. The filler strain hardening decreased with increasing filler pass sequence. These combined effects reduce the weld strength, and a depeaking index model was developed to select filler pass thicknesses, pass numbers, and sequences to improve the welding process results over the current normal weld schedule.

Verderaime, V.↗

U-Groove aluminum weld strength improvement

Though butt-welds are among the most preferred joining methods in aerostructures, their strength dependence on inelastic mechanics is generally the least understood. This study investigated experimental strain distributions across a thick aluminum U-grooved weld and identified two weld process considerations for improving the multipass weld strength. The extreme thermal expansion and contraction gradient of the fusion heat input across the groove tab thickness produces severe peaking, which induces bending under uniaxial loading. The filler strain-hardening decreased with increasing filler pass sequence, producing the weakest welds on the last pass side. Current welding schedules unknowingly compound these effects which reduce the weld strength. A depeaking index model was developed to select filler pass thicknesses, pass numbers, and sequences to improve depeaking in the welding process. The intent is to combine the strongest weld pass side with the peaking induced bending tension to provide a more uniform stress and stronger weld under axial tensile loading.

Verderaime, V.↗

U-groove aluminum weld strength improvement

Though butt-welds are among the most preferred joining methods in aerostructures, their strength dependence on inelastic mechanics is generally the least understood. This study investigated experimental strain distributions across a thick aluminum U-grooved weld and identified two weld process considerations for improving the multipass weld strength. The extreme thermal expansion and contraction gradient of the fusion heat input across the groove tab thickness produces severe peaking which induces bending under uniaxial loading. The filler strain-hardening deceased with increasing filler pass sequence, producing the weakest welds on the last pass side. Current welding schedules unknowingly compound these effects which reduce the weld strength. A de-peaking index model was developed to select filler pass thicknesses, pass numbers, and sequences to improve de-peaking in the welding process. Intent is to combine the strongest weld pass side with the peaking induced bending tension to provide a more uniform stress and stronger weld under axial tensile loading.

Verderaime, V.↗

U-Groove Aluminum Weld Strength Improvement

Though butt-welds are among the most preferred joining methods in aerostructures, their strength dependence on inelastic mechanics is generally the least understood. This study investigated experimental strain distributions across a thick aluminum U-grooved weld and identified two weld process considerations for improving the multipass weld strength. One is the source of peaking in which the extreme thermal expansion and contraction gradient of the fusion heat input across the groove tab thickness produces severe angular distortion that induces bending under uniaxial loading. The other is the filler strain hardening decreasing with increasing filler pass sequences, producing the weakest welds on the last weld pass side. Both phenomena are governed by weld pass sequences. Many industrial welding schedules unknowingly compound these effects, which reduce the weld strength. A depeaking index model was developed to select filler pass thickness, pass numbers, and sequences to improve depeaking in the welding process. The result was to select the number and sequence of weld passes to reverse the peaking angle such as to combine the strongest weld pass side with the peaking induced bending tension component side to provide a more uniform stress and stronger weld under axial tensile loading.

Verderaime, V.↗

Effects of Heat Treatment on the Ballistic Impact Properties of Inconel 718 for Jet Engine Fan Containment Applications

The effects of heat treating Inconel 718 on the ballistic impact response and failure mechanisms were studied. Two different annealing conditions and an aged condition were considered. Large differences in the static properties were found between the annealed and the aged material, with the annealed condition having lower strength and hardness and greater elongation than the aged. Correspondingly large differences were found in the velocity required to penetrate material in the two conditions in impact tests involving 12.5 mm diameter, 25.4 mm long cylindrical Ti-6-4 projectiles impacting flat plates at velocities in the range of 150 to 300 m/sec. The annealed material was able to absorb over 25 percent more energy than the aged. This is contrary to results observed for ballistic impact response for higher velocity impacts typically encountered in military applications where it has been shown that there exists a correlation between target hardness and ballistic impact strength. Metallographic examination of impacted plates showed strong indication of failure due to adiabatic shear. In both materials localized bands of large shear deformation were apparent, and microhardness measurements indicated an increase in hardness in these bands compared to the surrounding material. These bands were more localized in the aged material than in the annealed material. In addition the annealed material underwent significantly greater overall deformation before failure. The results indicate that high elongation and better strain hardening capabilities reduce the tendency for shear to localize and result in an unstable adiabatic shear failure. This supports empirical containment design methods that relate containment thickness to the static toughness.

Pereira, J. Michael↗

Crack Turning and Arrest Mechanisms for Integral Structure

In the course of several years of research efforts to predict crack turning and flapping in aircraft fuselage structures and other problems related to crack turning, the 2nd order maximum tangential stress theory has been identified as the theory most capable of predicting the observed test results. This theory requires knowledge of a material specific characteristic length, and also a computation of the stress intensity factors and the T-stress, or second order term in the asymptotic stress field in the vicinity of the crack tip. A characteristic length, r(sub c), is proposed for ductile materials pertaining to the onset of plastic instability, as opposed to the void spacing theories espoused by previous investigators. For the plane stress case, an approximate estimate of r(sub c), is obtained from the asymptotic field for strain hardening materials given by Hutchinson, Rice and Rosengren (HRR). A previous study using of high order finite element methods to calculate T-stresses by contour integrals resulted in extremely high accuracy values obtained for selected test specimen geometries, and a theoretical error estimation parameter was defined. In the present study, it is shown that a large portion of the error in finite element computations of both K and T are systematic, and can be corrected after the initial solution if the finite element implementation utilizes a similar crack tip discretization scheme for all problems. This scheme is applied for two-dimensional problems to a both a p-version finite element code, showing that sufficiently accurate values of both K(sub I) and T can be obtained with fairly low order elements if correction is used. T-stress correction coefficients are also developed for the singular crack tip rosette utilized in the adaptive mesh finite element code FRANC2D, and shown to reduce the error in the computed T-stress significantly. Stress intensity factor correction was not attempted for FRANC2D because it employs a highly accurate quarter-point scheme to obtain stress intensity factors.

Pettit, Richard↗

Preliminary Thermal Stress Analysis of a High-Pressure Cryogenic Storage Tank

The thermal stresses on a cryogenic storage tank strongly affect the condition of the tank and its ability to withstand operational stresses. These thermal stresses also affect the growth of any surface damage that might occur in the tank walls. These stresses are particularly of concern during the initial cooldown period for a new tank placed into service, and during any subsequent thermal cycles. A preliminary thermal stress analysis of a high-pressure cryogenic storage tank was performed. Stresses during normal operation were determined, as well as the transient temperature distribution. An elastic analysis was used to determine the thermal stresses in the inner wall based on the temperature data. The results of this elastic analysis indicate that the inner wall of the storage tank will experience thermal stresses of approximately 145,000 psi (1000 MPa). This stress level is well above the room-temperature yield strength of 304L stainless steel, which is about 25,000 psi (170 MPa). For this preliminary analysis, several important factors have not yet been considered. These factors include increased strength of 304L stainless steel at cryogenic temperatures, plastic material behavior, and increased strength due to strain hardening. In order to more accurately determine the thermal stresses and their affect on the tank material, further investigation is required, particularly in the area of material properties and their relationship to stress.

Baker, J. Mark↗

Creep Strain and Strain Rate Response of 2219 Al Alloy at High Stress Levels

As a result of high localized plastic deformation experienced during proof testing in an International Space Station connecting module, a study was undertaken to determine the deformation response of a 2219-T851 roll forging. After prestraining 2219-T851 Al specimens to simulate strains observed during the proof testing, creep tests were conducted in the temperature range from ambient temperature to 107 C (225 F) at stress levels approaching the ultimate tensile strength of 2219-T851 Al. Strain-time histories and strain rate responses were examined. The strain rate response was extremely high initially, but decayed rapidly, spanning as much as five orders of magnitude during primary creep. Select specimens were subjected to incremental step loading and exhibited initial creep rates of similar magnitude for each load step. Although the creep rates decreased quickly at all loads, the creep rates dropped faster and reached lower strain rate levels for lower applied loads. The initial creep rate and creep rate decay associated with primary creep were similar for specimens with and without prestrain; however, prestraining (strain hardening) the specimens, as in the aforementioned proof test, resulted in significantly longer creep life.

Taminger, Karen M. B.↗

Test and Analysis of Sub-Components of Aluminum-Lithium Alloy Cylinders

Integrally machined blade-stiffened panels subjected to an axial compressive load were tested and analyzed to observe the buckling, crippling, and postcrippling response of the panels. The panels were fabricated from aluminum-lithium alloys 2195 and 2050, and both alloys have reduced material properties in the short transverse material direction. The tests were designed to capture a failure mode characterized by the stiffener separating from the panel in the postbuckling range. This failure mode is attributed to the reduced properties in the short transverse direction. Full-field measurements of displacements and strains using three-dimensional digital image correlation systems and local measurements using strain gages were used to capture the deformation of the panel leading up to the failure of the panel for specimens fabricated from 2195. High-speed cameras were used to capture the initiation of the failure. Finite element models were developed using an isotropic strain-hardening material model. Good agreement was observed between the measured and predicted responses for both alloys.

Haynie, Waddy T.↗

Low Temperature Creep of Hot-Extruded Near-Stoichiometric NiTi Shape Memory Alloy: Effect of Thermal Cycling - Part 2

This paper is the first report on the effect prior low temperature creep on the thermal cycling behavior of NiTi. The isothermal low temperature creep behavior of near-stoichiometric NiTi between 300 and 473 K was discussed in Part I. The effect of temperature cycling on its creep behavior is reported in the present paper (Part II). Temperature cycling tests were conducted between either 300 or 373 K and 473 K under a constant applied stress of either 250 or 350 MPa with hold times lasting at each temperature varying between 300 and 700 h. Each specimen was pre-crept either at 300 or at 473 K for several months under an identical applied stress as that used in the subsequent thermal cycling tests. Irrespective of the initial pre-crept microstructures, the specimens exhibited a considerable increase in strain with each thermal cycle so that the total strain continued to build-up to 15 to 20 percent after only 5 cycles. Creep strains were immeasurably small during the hold periods. It is demonstrated that the strains in the austenite and martensite are linearly correlated. Interestingly, the differential irrecoverable strain, in the material measured in either phase decreases with increasing number of cycles, similar to the well-known Manson-Coffin relation in low cycle fatigue. Both phases are shown to undergo strain hardening due to the development of residual stresses. Plots of true creep rate against absolute temperature showed distinct peaks and valleys during the cool-down and heat-up portions of the thermal cycles, respectively. Transformation temperatures determined from the creep data revealed that the austenitic start and finish temperatures were more sensitive to the pre-crept martensitic phase than to the pre-crept austenitic phase. The results are discussed in terms of a phenomenological model, where it is suggested that thermal cycling between the austenitic and martensitic phase temperatures or vice versa results in the deformation of the austenite and a corresponding development of a back stress due to a significant increase in the dislocation density during thermal cycling.

Raj, S. V.↗

Development of Aluminum-Lithium 2195 Gores by the Stretch Forming Process

Aluminum-Lithium alloy 2195 exhibits higher mechanical properties and lower density than aluminum alloy 2219, which is the current baseline material for Space Launch System (SLS) cryogenic tank components. Replacement of Al 2219 with Al-Li 2195 would result in substantial weight savings, as was the case when this replacement was made on the shuttle external tank. A key component of cryogenic tanks are the gores, which are welded together to make the rounded ends of the tanks. The required thicknesses of these gores depend on the specific SLS configuration and may exceed the current experience base in the manufacture of such gores by the stretch forming process. Here we describe the steps taken to enhance the formability of Al-Li 2195 by optimizing the heat treatment and stretch forming processes for gore thicknesses up to 0.75", which envelopes the maximum expected gore thicknesses for SLS tanks. An annealing treatment, developed at Marshall Space Flight Center, increased the forming range and strain hardening exponent of Al-Li 2195 plates. Using this annealing treatment, one 0.525" thick and two 0.75" thick gores were manufactured by the stretch forming process. The annealing treatment enabled the stretch forming of the largest ever cross sectional area (thickness x width) of an Al-Li 2195 plate achieved by the manufacturer. Mechanical testing of the gores showed greater than expected ultimate tensile strength, yield strength, modulus, and elongation values. The gores also exhibited acceptable fracture toughness at room and LN2 temperatures. All of the measured data indicate that the stretch formed gores have sufficient material properties to be used in flight domes.

Volz, M. P.↗