At least 235 records · Page 13

Flexibilized copolyimide adhesives

Two copolyimides, LARC-STPI and STPI-LARC-2, with flexible backbones were processed and characterized as adhesives. The processability and adhesive properties were compared to those of a commercially available form of LARC-TPI. Lap shear specimens were fabricated using adhesive tape prepared from each of the three polymers. Lap shear tests were performed at room temperature, 177 C, and 204 C before and after exposure to water-boil and to thermal aging at 204 C for up to 1000 hours. The three adhesive systems possess exceptional lap shear strengths at room temperature and elevated temperatures both before and after thermal exposure. LARC-STPI, because of its high glass transition temperature provided high lap shear strengths up to 260 C. After water-boil, LARC-TPI exhibited the highest lap shear strengths at room temperature and 177 C, whereas the LARC-STPI retained a higher percentage of its original strength when tested at 204 C. These flexible thermoplastic copolyimides show considerable potential as adhesives based on this study and because of the ease of preparation with low cost, commercially available materials.

Progar, Donald J.↗

Evaluation of Surlyn 8920 as PHE Visor Material and Evaluations of New Adhesives for Improving Bonding Between Teflon and Stainless Steel at Cryogenic Temperature

Two studies are presented, and in the first study, Surlyn 8920 (an ionic and amorphous low density polyethylene made by Dupont) was evaluated as a possible replacement of Plexyglass G as PHE visor material. Four formulations of the polymer were made by adding different amounts of UV stabilizer, energy quencher, and antioxident in a Brabender Plasticorder. The formulated polymers were molded in the form of sheets in a compression molder. Cut samples from the molded sheets were exposed in a weatherometer and tested on Instron Tensile Tester for strength and elongation. Specially molded samples of the formulated polymers were subjected to Charpy Impact Tests. In the second study, preliminary evaluations of adhesives for improvement of bonding between Teflon and stainless steel (SS) were performed. Kapton, a high temperature polyimide made by Dupont, and a rubber based adhesive made by Potter Paint Co., were evaluated against industrial quality epoxy, the current material used to bond Teflon and SS. The degreased surfaces of the SS discs were etched mechanically, with a few of these etched chemically. The surfaces of the SS discs were etched mechanically, with a few of these etched chemically. Bonding strengths were evaluated using lap shear tests on the Instron Tensile Tester for the samples bonded by Kapton and industrial quality epoxy. Bond strengths were also evaluated using a pull test on the Instron for the samples bonded by Potter adhesive (CWL-152) and industrial quality epoxy. Based on limited lap shear data, Kapton gave bond strength favorable compared to that of industrial epoxy. Based on limited pull test data, Kapton bonded and CWL-152 bonded samples showed poor strength compared to epoxy bonded sample.

Ray, Asit K.↗

Compact forced simple-shear sample for studying shear localization in materials

In this paper, a new specimen geometry, the compact forced-simple-shear specimen (CFSS), has been developed as a means to achieve simple shear testing of materials over a range of temperatures and strain rates. The stress and strain state in the gage section is designed to produce essentially “pure” simple shear, mode II in-plane shear, in a compact-sample geometry. The 2-D plane of shear can be directly aligned along specified directional aspects of a material's microstructure of interest; i.e., systematic shear loading parallel, at 45°, and orthogonal to anisotropic microstructural features in a material such as the pancake-shaped grains typical in many rolled structural metals, or to specified directions in fiber-reinforced composites. Finally, the shear-stress shear-strain response and the damage evolution parallel and orthogonal to the pancake grain morphology in 7039-Al are shown to vary significantly as a function of orientation to the microstructure.

36 MATERIALS SCIENCE↗

Numerical analysis of the Iosipescu specimen for composite materials

A finite element analysis of the Iosipescu shear tests for unidirectional and cross-ply composites is presented. It is shown that an iterative analysis procedure must be used to model the fixture-specimen kinematics. The correction factors which are needed to compensate for the nonuniformity of stress distribution in calculating shear modulus are shown to be dependent on the material orthotropic ratio and the finite element loading models. Test section strain distributions representative of typical graphite-epoxy specimens are also presented.

Ho, H.↗

Numerical analysis of the Iosipescu specimen for composite materials

A finite element analysis of the Iosipescu shear tests for unidirectional and cross-ply composites is presented. It is shown that an iterative analysis procedure must be used to model the fixture-specimen kinematics. The correction factors which are needed to compensate for the nonuniformity of stress distribution in calculating shear modulus are shown to be dependent on the material orthotropic ratio and the finite element loading models. Test section strain distributions representative of typical graphite-epoxy specimens are also presented.

Ho, H.↗

Low Temperature Mechanical Testing of Carbon-Fiber/Epoxy-Resin Composite Materials

The use of cryogenic fuels (liquid oxygen and liquid hydrogen) in current space transportation vehicles, in combination with the proposed use of composite materials in such applications, requires an understanding of how such materials behave at cryogenic temperatures. In this investigation, tensile intralaminar shear tests were performed at room, dry ice, and liquid nitrogen temperatures to evaluate the effect of temperature on the mechanical response of the IM7/8551-7 carbon-fiber/epoxy-resin system. Quasi-isotropic lay-ups were also tested to represent a more realistic lay-up. It was found that the matrix became both increasingly resistant to microcracking and stiffer with decreasing temperature. A marginal increase in matrix shear strength with decreasing temperature was also observed. Temperature did not appear to affect the integrity of the fiber-matrix bond.

Nettles, Alan T.↗

Influence of the resin on interlaminar mixed-mode fracture

Both literature review data and new data on toughness behavior of seven matrix and adhesive systems in four types of tests were studied in order to assess the influence of the resin on interlaminar fracture. Mixed mode (i.e., various combinations of opening mode 1, G sub 1, and shearing mode 2; G sub 2) fracture toughness data showed that the mixed mode relationship for failure appears to be linear in terms of G sub 1 and G sub 2. The study further indicates that fracture of brittle resins is controlled by the G sub 1 component, and that fracture of many tough resins is controlled by total strain-energy release rate, G sub T. Regarding the relation of polymer structure and the mixed mode fracture: high mode 1 toughness requires resin dilatation; dilatation is low in unmodified epoxies at room temperature/dry conditions; dilatation is higher in plasticized epoxies, heated epoxies, and in modified epoxies; modification improves mode 2 toughness only slightly compared with mode 1 improvements. Analytical aspects of the cracked lap shear test specimen were explored.

Johnson, W. S.↗

Influence of the resin on interlaminar mixed-mode fracture

Both literature review data and new data on toughness behavior of seven matrix and adhesive systems in four types of tests were studied in order to assess the influence of the resin on interlaminar fracture. Mixed mode (i.e., various combinations of opening mode 1, G sub 1, and shearing mode 2; G sub 2) fracture toughness data showed that the mixed mode relationship for failure appears to be linear in terms of G sub 1 and G sub 2. The study further indicates that fracture of brittle resins is controlled by the G sub 1 component, and that fracture of many tough resins is controlled by total strain-energy release rate, G sub T. Regarding the relation of polymer structure and the mixed mode fracture: high mode 1 toughness requires resin dilatation; dilatation is low in unmodified epoxies at room temperature/dry conditions; dilatation is higher in plasticized epoxies, heated epoxies, and in modified epoxies; modification improves mode 2 toughness only slightly compared with mode 1 improvements. Analytical aspects of the cracked lap shear test specimen were explored.

Johnson, W. S.↗

Plasma treatment on both adhesive tape and adherends for significantly enhanced CFRTP-related adhesive joints

Unlike existing literature that primarily concentrates on either the plasma treatment of adherends alone or solely on adhesive surfaces, this work leverages plasma modification of both adhesive in tape form and adherend surfaces to largely enhance the interfacial bonding between a thermoset-based adhesive tape and carbon-fiber-reinforced thermoplastic polymer (CFRTP) for structural bonding applications. Here, by conducting single lap shear tests on adhesively-bonded AA6061-CFRPPA (carbon-fiber-reinforced polyphthalamide) dissimilar joints, it is shown that the plasma treatment of adherends alone can increase the lap shear strength (LSS) of the joints by approximately 200% compared to non-treated counterparts. An additional plasma treatment of adhesive tape surfaces leads to even higher LSS improvement, reaching up to 315%, due to the formation of a denser crosslinked network of covalent bonds and a reduced area fraction of interfacial voids at the CFRPPA/adhesive interface. The highest plasma-enhanced LSS of the metal-CFRTP dissimilar joints rivals that of metal-metal joints, which is typically stronger than the joints associated with fiber-reinforced polymers. This study is important for achieving strong CFRTP-related structural components bonded using adhesive tape, providing better compatibility with plasma treatment and other joining methods like riveting compared to adhesive paste or liquid.

36 MATERIALS SCIENCE↗

Brazing ZrO{sub 2} ceramic to Ti–6Al–4V alloy using NiCrSiB amorphous filler foil: Interfacial microstructure and joint properties

Reliable brazing of ZrO{sub 2} ceramic and Ti–6Al–4V alloy was achieved using NiCrSiB amorphous filler foil. The interfacial microstructure of ZrO{sub 2}/Ti–6Al–4V joints was characterized by scanning electron microscope, energy dispersive spectrometer and micro-focused X-ray diffractometer. The effects of brazing temperature on the interfacial microstructure and joining properties of brazed joints were investigated in detail. Active Ti of Ti–6Al–4V alloy dissolved into molten filler metal and reacted with ZrO{sub 2} ceramic to form a continuous TiO reaction layer, which played an important role in brazing. Various reaction phases including Ti{sub 2}Ni, Ti{sub 5}Si{sub 3} and β-Ti were formed in brazed joints. With an increasing of brazing temperature, the TiO layer thickened gradually while the Ti{sub 2}Ni amount reduced. Shear test indicated that brazed joints tend to fracture at the interface between ZrO{sub 2} ceramic and brazing seam or Ti{sub 2}Ni intermetallic layer. The maximum average shear strength reached 284.6 MPa when brazed at 1025 °C for 10 min. - Graphical Abstract: Interfacial microstructure of ZrO{sub 2}/TC4 joint brazed using NiCrSiB amorphous filler foil was: ZrO{sub 2}/TiO/Ti{sub 2}Ni + β-Ti + Ti{sub 5}Si{sub 3}/β-Ti/Widmanstätten structure/TC4. - Highlights: • Brazing of ZrO{sub 2} ceramic and Ti-6Al-4V alloy was achieved. • Interfacial microstructure was TiO/Ti{sub 2}Ni + β + Ti{sub 5}Si{sub 3}/β/Widmanstätten structure. • The formation of TiO produced the darkening effect of ZrO{sub 2} ceramic. • The highest joining strength of 284.6MPa was obtained.

36 MATERIALS SCIENCE↗

Composite transport wing technology development: Design development tests and advanced structural concepts

Numerous design concepts, materials, and manufacturing methods were investigated for the covers and spars of a transport box wing. Cover panels and spar segments were fabricated and tested to verify the structural integrity of design concepts and fabrication techniques. Compression tests on stiffened panels demonstrated the ability of graphite/epoxy wing upper cover designs to achieve a 35 percent weight savings compared to the aluminum baseline. The impact damage tolerance of the designs and materials used for these panels limits the allowable compression strain and therefore the maximum achievable weight savings. Bending and shear tests on various spar designs verified an average weight savings of 37 percent compared to the aluminum baseline. Impact damage to spar webs did not significantly degrade structural performance. Predictions of spar web shear instability correlated well with measured performance. The structural integrity of spars manufactured by filament winding equalled or exceeded those fabricated by hand lay-up. The information obtained will be applied to the design, fabrication, and test of a full-scale section of a wing box. When completed, the tests on the technology integration box beam will demonstrate the structural integrity of an advanced composite wing design which is 25 percent lighter than the metal baseline.

Griffin, Charles F.↗

Strength and compressibility of returned lunar soil.

Two oedometer and three direct shear tests have been performed in vacuum on a 200 g sample of lunar soil from Apollo 12 (12001, 119). The compressibility data have been used to calculate bulk density and shear wave velocity versus depth on the lunar surface. The shear wave velocity was found to increase approximately with the one-fourth power of the depth, and the results suggest that the Apollo 14 Active Seismic Experiment may not have detected the Fra Mauro formation at a depth of 8.5 m, but only naturally consolidated lunar soil. The shear data indicate that the strength of the lunar soil sample is about 65% that of a ground basalt simulant at the same void ratio.

Carrier, W. D., III↗

Laser Ablation Surface Preparation of Ti-6A1-4V for Adhesive Bonding

Adhesive bonding offers many advantages over mechanical fastening, but requires certification before it can be incorporated in primary structures for commercial aviation without disbond-arrestment features or redundant load paths. Surface preparation is widely recognized as the key step to producing robust and predictable bonds. Laser ablation imparts both topographical and chemical changes to a surface which can lead to increased bond durability. A laser based process provides an alternative to chemical-dip, manual abrasion and grit blast treatments which are expensive, hazardous, polluting, and less precise. This report documents preliminary testing of a surface preparation technique using laser ablation as a replacement for the chemical etch and abrasive processes currently applied to Ti-6Al-4V alloy adherends. Failure mode, surface roughness, and chemical makeup were analyzed using fluorescence enhanced visualization, microscopy, and X-ray photoelectron spectroscopy, respectively. Single lap shear tests were conducted on bonded and aged specimens to observe bond strength retention and failure mode. Some promising results showed increasing strength and durability of lap shear specimens as laser ablation coverage area and beam intensity increased. Chemical analyses showed trends for surface chemical species which correlated with improved bond strength and durability. Combined, these results suggest that laser ablation is a viable process for inclusion with or/and replacement of one or more currently used titanium surface treatments. On-going work will focus on additional mechanical tests to further demonstrate improved bond durability.

Palmieri, Frank L.↗

A Statistical Analysis of Impact Ice Adhesion Strength Data Acquired with a Modified Lap Joint Test

Numerous methodologies have been utilized to measure the adhesion strength of impact ice, and the data reported in the literature varies significantly from method to method. In order to initiate an investigation to determine the cause of this disparity, a lap-joint shear test methodology that was recently developed was utilized in the Icing Research Tunnel at the NASA Glenn Research Center. Data was obtained while varying the temperature, test section velocity, liquid water content, and cloud droplet median volumetric diameter, among other parameters, over five campaigns. A new data set acquired using this new test method is presented. The results are analyzed with standard statistical methodologies and demonstrate a strong correlation between the apparent adhesion strength of ice and temperature, annealing time, and heating time. Observations during the test and analysis of the results suggest the presence of large residual stresses in the samples, which is in agreement with prior work. Due to the nature of the test methodology, and all known ice adhesion test methodologies, the measured, or apparent, adhesion strength is geometry dependent, a fact emphasized by the results presented here. The data was organized both cumulatively and independently by result code. Trends in the data are discussed in the context of causal physical mechanisms. The data shows the apparent adhesion strength was not linear with temperature, liquid water content, annealing time, and other variables. Short-term heating of the samples was shown to have negligible effect, and the apparent adhesion strength had a flat trend with velocity.

Ice Adhesion↗

Structural characterization of high temperature composites

Glass, ceramic, and carbon matrix composite materials have emerged in recent years with potential properties and temperature resistance which make them attractive for high temperature applications such as gas turbine engines. At the outset of this study, only flexural tests were available to evaluate brittle matrix composites at temperatures in the 600 to 1000 C range. The results are described of an ongoing effort to develop appropriate tensile, compression, and shear test methods for high temperature use. A tensile test for unidirectional composites was developed and used to evaluate the properties and behavior of ceramic fiber reinforced glass and glass-ceramic matrix composites in air at temperatures up to 1000 C. The results indicate generally efficient fiber reinforcement and tolerance to matrix cracking similar to polymer matrix composites. Limiting properties in these materials may be an inherently very low transverse strain to failure, and high temperature embrittlement due to fiber/matrix interface oxidation.

Mandell, J. F.↗

Strength Tests on Paper Cylinder in Compression, Bending and Shear

Static tests on paper cylinders were conducted at the Langley Memorial Aeronautical Laboratory at Langley Field, Virginia, to obtain qualitative information in connection with a study of the strength of stressed-skin fuselages. The effects of radius-thickness ratio and bulkhead spacing were investigated with the cylinders in compression, bending, combined bending and shear, and torsion.

STRESSED SKIN - CYLINDER, PAPER - STRENGTH↗

Ultrasonic Spectroscopy of Stainless Steel Sandwich Panels

Enhanced, lightweight material systems, such as 17-4PH stainless steel sandwich panels are being developed for use as fan blades and fan containment material systems for next generation engines. In order to improve the production for these systems, nondestructive evaluation (NDE) techniques, such as ultrasonic spectroscopy, are being utilized to evaluate the brazing quality between the 17-4PH stainless steel face plates and the 17-4PH stainless steel foam core. Based on NDE data, shear tests are performed on sections representing various levels of brazing quality from an initial batch of these sandwich structures. Metallographic characterization of brazing is done to corroborate NDE findings and the observed shear failure mechanisms.

Cosgriff, Laura M.↗