Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “oxide”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 235 records · Page 13

Controlling structure distortions in 3-layer ferroelectric Aurivillius oxides

Combined Rietveld refinements of x-ray and neutron powder diffraction data were used to understand the subtle structure distortions in 3-layer Aurivillius oxides that yield off-centering displacements in ferroelectric and multiferroic compositions. Ferroelectric phases including Bi{sub 2}A{sub 2}Ti{sub 3}O{sub 12} (A=La, Pr, Nd, La/Pr, La/Nd, Pr/Nd), Bi{sub 2}A{sub 2}TiNb{sub 2}O{sub 12} (A=Ca/Sr, Sr, and Sr/Ba) and Bi{sub 2}A{sub 2}TiTa{sub 2}O{sub 12} (A=Ca/Sr, and Sr/Ba) were studied to separate the effects of cation size and charge on the structure distortions and properties. A new approach to describing the local coordination around the Ti, Nb, and/or Ta ions is presented, where the oxygen octahedra are characterized as containing kinks in three dimensions. The kink angles follow trends with the A-site ionic radius and the ferroelectric polarization. The driving force for extensive cation site mixing between the Bi and A-site cations has been clearly established, with site mixing required to maintain interlayer bonding. - Graphical abstract: Distortion of the oxygen octahedra from planar geometries can be controlled via choice of the perovskite A-site cation, and the kink angle correlates with cation off-centering and ferroelectric polarization. Highlights: Black-Right-Pointing-Pointer A-site cations define the tilt and distortion of the octahedral. Black-Right-Pointing-Pointer Distortions of oxygen octahedra, ignoring the central cation, link to ferroelectric polarization. Black-Right-Pointing-Pointer Bi ion occupancy in the perovskite causes distortion of the oxygen sublattice. Black-Right-Pointing-Pointer We predict multiferroic behavior from off-centering caused by the Bi ion lone pair.

36 MATERIALS SCIENCE↗

Compositional Tuning of Ultrathin Surface Oxides on Metal and Alloy Substrates Using Photons: Dynamic Simulations and Experiments

Oxide synthesis with controlled functional properties is desirable for a plethora of applications but is elusive due to oxide growth kinetics. Here, we report on the ability to modify the structure and composition of ultra-thin oxides grown on Ni-Al alloy surfaces at room temperature utilizing photon illumination. Atomistic simulations that take into account dynamic charge transfer predict that the electric field produced across an oxide film in photon-assisted synthesis overcomes the activation energy barrier for ionic migration, leading to enhanced oxidation kinetics and oxygen incorporation into the oxide, enabling us to control the oxide composition at atomic length scales. Experiments (near-edge x-ray absorption fine structure (NEXAFS) and X-ray photoelectron spectroscopy) indicate that the native oxide on 5%Ni-Al alloy is primarily composed of aluminum oxide with no nickel oxide whereas the photon-assisted oxide comprises of both aluminum oxide and nickel oxide. The ability to tune the composition at the atomic scale of the ultra-thin oxide films leads to excellent passivity as verified from polarization experiments.

36 MATERIALS SCIENCE↗

Comparison of the sputter rates of oxide films relative to the sputter rate of SiO{sub 2}

There is a growing interest in knowing the sputter rates for a wide variety of oxides because of their increasing technological importance in many different applications. To support the needs of users of the Environmental Molecular Sciences Laboratory, a national scientific user facility, as well as our research programs, the authors made a series of measurements of the sputter rates from oxide films that have been grown by oxygen plasma-assisted molecular beam epitaxy, pulsed laser deposition, atomic layer deposition, electrochemical oxidation, or sputter deposition. The sputter rates for these oxide films were determined in comparison with those from thermally grown SiO{sub 2}, a common reference material for sputter rate determination. The film thicknesses and densities for most of these oxide films were measured using x-ray reflectivity. These oxide films were mounted in an x-ray photoelectron or Auger electron spectrometer for sputter rate measurements using argon ion sputtering. Although the primary objective of this work was to determine relative sputter rates at a fixed angle, the measurements also examined (i) the angle dependence of the relative sputter rates, (ii) the energy dependence of the relative sputter rates, and (iii) the extent of ion beam induced reduction for some oxides. Oxide films examined include SiO{sub 2}, Al{sub 2}O{sub 3}, CeO{sub 2}, Cr{sub 2}O{sub 3}, Fe{sub 2}O{sub 3}, HfO{sub 2}, In-Sn oxide, Ta{sub 2}O{sub 5}, TiO{sub 2} (anatase, rutile, and amorphous), and ZnO. The authors found that the sputter rates for the oxides can vary up to a factor of 2 (usually lower) from that observed for SiO{sub 2}. The ratios of sputter rates relative to those of SiO{sub 2} appear to be relatively independent of ion beam energy in the range of 1-4 kV and for incident angles <50 deg. As expected, the extent of ion beam induced reduction of the oxides varies with the sputter angle.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Potential-pH diagrams considering complex oxide solution phases for understanding aqueous corrosion of multi-principal element alloys

The potential-pH diagram, a graphical representation of the thermodynamically predominant reaction products in aqueous corrosion, is originally proposed for the corrosion of pure metals. The original approach only leads to stoichiometric oxides and hydroxides as the oxidation products. However, numerous experiments show that non-stoichiometric oxide scales are prevalent in the aqueous corrosion of alloys. In the present study, a room temperature potential-pH diagram considering oxide solid solutions, as a generalization of the traditional potential-pH diagram with stoichiometric oxides, is constructed for an FCC single-phase multi-principal element alloy (MPEA) based on the CALculation of PHAse Diagram method. The predominant reaction products, the ions in aqueous solution, and the cation distribution in oxides are predicted. The oxide solid solution is stabilized by the mixing free energy (or mixing entropy) and the stabilizing effect becomes more significant as the temperature increases. Consequently, solid solution oxides are stable in large regions of the potential-pH diagram and the mixing free energy mostly affects the equilibrium composition of the stable oxides, while the shape of stable regions for oxides is mostly determined by the structure of the stable oxides. Agreements are found for Ni 2+ , Fe 2+ , and Mn 2+ between the atomic emission spectroelectrochemistry measurements and thermodynamic calculations, while deviations exist for Cr 3+ and Co 2+ possibly due to surface complexation with species such as Cl - and the oxide dissolution. By incorporating the solution models of oxides, the current work presents a general and more accurate way to analyze the reaction products during aqueous corrosion of MPEAs.

Materials Science↗

Electrochemical Oxidation of Organic Molecules at Lower Overpotential: Accessing Broader Functional Group Compatibility with Electron-Proton Transfer Mediators

CONSPECTUS: Electrochemical organic oxidation reactions are highly appealing because protons are often effective terminal electron acceptors, thereby avoiding undesirable stoichiometric oxidants. These reactions are often plagued by high overpotentials, however, that greatly limit their utility. Single-electron transfer (SET) from organic molecules generates high energy radical-cations. Formation of such intermediates often requires electrode potentials far above the thermodynamic potentials of the reaction and frequently causes decomposition and/or side reactions of ancillary functional groups. In this Account, we show how electrocatalytic electron-proton transfer mediators (EPTMs) address this challenge. EPTMs bypass the formation of radical-cation intermediates by supporting mechanisms that operate at electrode potentials much lower (=1 V) than analogous direct electrolysis reactions. The stable aminoxyl radical TEMPO (2,2,6,6-tetramethylpiperidine N-oxyl) is an effective mediator for electrochemical alcohol oxidation, and we have employed such processes for applications ranging from pharmaceutical synthesis to biomass conversion. A complementary electrochemical alcohol oxidation method employs a cooperative Cu/TEMPO mediator system that operates at 0.5 V lower electrode potential than the TEMPO-only mediated process. This difference, which arises from a different catalytic mechanism, rationalizes the broad functional group tolerance of Cu/TEMPO-based aerobic alcohol oxidation catalysts. Aminoxyl mediators address long-standing challenges in the "Shono oxidation", an important method for a-C–H oxidation of tertiary amides and carbamates. Shono oxidations are initiated by a high-potential SET step that limits their utility. Aminoxyl-mediated Shono-type oxidations have been developed that operate at much lower potentials and tolerate diverse functional groups. Analogous reactivity underlies a-C–H cyanation of secondary cyclic amines, a new method that enables efficient diversification of piperidine-based pharmaceutical building blocks and preparation of non-natural amino acids. Electrochemical oxidations of benzylic C–H bonds are commonly initiated by SET to generate radical cations, but such methods are again plagued by large overpotentials. Mediated electrolysis methods that promote hydrogen-atom-transfer (HAT) from benzylic C–H bonds to Fe-oxo species and phthalimide N-oxyl (PINO) support C–H oxygenation, iodination, and oxidative-coupling reactions. A complementary method merges photochemistry with electrochemistry to achieve amidation of C(sp3)–H bonds. This unique process operates at much lower overpotentials compatible with diverse functional groups. These results have broad implications for organic electrochemistry, highlighting the importance of "overpotential" considerations and the prospects for expanding synthetic utility by using mediators to bypass high-energy outer-sphere electron-transfer mechanisms. Principles demonstrated here for oxidation are equally relevant to electrochemical reductions.

Wang, Fei↗

Assembly and Succession of Iron Oxide Microbial Mat Communities in Acidic Geothermal Springs

Biomineralized ferric oxide microbial mats are ubiquitous features on Earth, are common in hot springs of Yellowstone National Park (YNP, WY, USA), and form due to direct interaction between microbial and physicochemical processes. The overall goal of this study was to determine the contribution of different community members to the assembly and succession of acidic high-temperature Fe(III)-oxide mat ecosystems. Spatial and temporal changes in Fe(III)-oxide accretion and the abundance of relevant community members were monitored over 70 days using sterile glass microscope slides incubated in the outflow channels of two acidic geothermal springs (pH = 3-3.5; temperature = 68-75°C) in YNP. Hydrogenobaculum spp. were the most abundant taxon identified during early successional stages (4-40 days), and have been shown to oxidize arsenite, sulfide, and hydrogen coupled to oxygen reduction. Iron-oxidizing populations of Metallosphaera yellowstonensis were detected within 4 days, and reached steady-state levels within 14-30 days, corresponding to visible Fe(III)-oxide accretion. Heterotrophic archaea colonized near 30 days, and emerged as the dominant functional guild after 70 days and in mature Fe(III)-oxide mats (1-2 cm thick). First-order rate constants of Fe(III)-oxide accretion ranged from 0.046 to 0.05 day -1 , and in situ microelectrode measurements showed that the oxidation of Fe(II) is limited by the diffusion of O2 into the Fe(III)-oxide mat. The formation of microterracettes also implicated O2 as a major variable controlling microbial growth and subsequent mat morphology. The assembly and succession of Fe(III)-oxide mat communities follows a repeatable pattern of colonization by lithoautotrophic organisms, and the subsequent growth of diverse organoheterotrophs. The unique geochemical signatures and micromorphology of extant biomineralized Fe(III)-oxide mats are also useful for understanding other Fe(II)-oxidizing systems.

58 GEOSCIENCES↗

The role of proton coupled electron transfer in water oxidation

Water oxidation is a key half reaction in energy conversion schemes based on solar fuels and targets such as light driven water splitting or carbon dioxide reduction into CO, other oxygenates, or hydrocarbons. Carrying out these reactions at rates that exceed the rate of solar insolation for the extended periods of time required for useful applications presents a major challenge. Water oxidation is the key “other” half reaction in these schemes and it is dominated by PCET given its multi-electron, multi-proton character, 2H2O → O2 + 4e- + 4H+. Identification of PCET was an offshoot of experiments designed to investigate energy conversion by electron transfer quenching of molecular excited states. The concepts “redox potential leveling” and concerted electron–proton transfer came from measurements on stepwise oxidation of cis-RuII(bpy)2(py)(OH2)2+ to RuIV(bpy)2(py)(O)2+. The Ru “blue dimer”, cis,cis-(bpy)2(H2O)RuORu(OH2)(bpy)24+, was the first designed catalyst for water oxidation. It undergoes oxidative activation by PCET to give the transient (bpy)2(O)RuVORuV(O)(bpy)24+, O-atom attack on water to give a peroxidic intermediate, and further oxidation and O2 release. More recently, a class of single site water oxidation catalysts has been identified, e.g., Ru(tpy)(bpm)(OH2)2+ (tpy is 2,2':6',2''-terpyridine; bpm is 2,2'-bipyrimidine). They undergo stepwise PCET oxidation to RuIV=O2+ or RuV(O)3+ followed by O-atom transfer with formation of peroxidic intermediates which undergo further oxidation and O2 release. PCET plays a key role in the three zones of water oxidation reactivity: oxidative activation, O•••O bond formation, oxidation and O2 release from peroxidic intermediates. Similar schemes have been identified for electrocatalytic water oxidation on oxide electrode surfaces based on phosphonated derivatives such as [Ru(Mebimpy)(4,4'-(PO3H2CH2)2bpy)(OH2)]2+. A PCET barrier to RuIII–OH2+ → RuIV=O2+ oxidation arises from the large difference in pKa values between RuIII–OH2+ and RuIV(OH)3+. On oxide surfaces this oxidation occurs by multiple pathways. Kinetic, mechanistic, and DFT results on single site catalysts reveal a new pathway for the O•••O bond forming step (Atom-Proton Transfer, APT), significant rate enhancements by added proton acceptor bases, and accelerated water oxidation in propylene carbonate as solvent with water added as a stoichiometric reagent. Lessons learned about water oxidation and the role of PCET and concerted pathways appear to have direct relevance for water oxidation in Photosystem II (PSII) with PSII a spectacular example of PCET in action. This includes a key role for Multiple Site-Electron Proton Transfer in oxidative activation of the Oxygen Evolving Complex (OEC) in the S0 → S1 transition in the Kok cycle.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Influence of support hydroxides on the catalytic activity of oxidized gold clusters

Gold oxide nanoparticles were prepared on the native surface and a hydroxylated surface of a non-porous TiO2 support (Degussa P25). Scanning transmission electron microscopy results show the formation of similarly sized clusters on both support materials (1.86 and 1.61 nm clusters on the native oxide and the hydroxylated oxide respectively). X-ray absorption near edge spectroscopy and X-ray photoelectron spectroscopy clearly indicate the formation of Au3+ rich oxide nanoparticles. Despite the similar cluster sizes and oxidation states the gold oxide clusters grown on the hydroxylated surface were at least 180 times more catalytically active for the oxidation of carbon monoxide then those grown on the native oxide surface. These hydroxides are conveniently introduced during the solution phase synthesis of gold catalysts and play a dominate, but previously unrecognized, role in the catalytic properties of both oxidized and metallic gold particles.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Mineral surface-catalyzed oxidation of Mn(II) by bromate: Implications for the occurrence of Mn oxides on Mars

The occurrence of manganese (Mn) oxides on Mars is believed to be an indicator of an O 2 -rich paleoenvironment of Mars because Mn oxides often form through the oxidation of Mn(II) by O 2 on the surface of Earth. An alternative formation pathway was recently proposed, in which Mn(II) is oxidized by bromate (BrO 3 - ), a common oxidant in contemporary Martian regolith. However, the oxidation of Mn(II) by bromate in solution is kinetically controlled and slow unless using very high concentrations (100 mM) of reactants that may be irrelevant to the conditions of Mars. We conducted laboratory simulations to determine whether iron (Fe) oxides (hematite and goethite) and a phyllosilicate (montmorillonite), abundant minerals on the surface of Mars, could catalyze the oxidation of Mn(II) by bromate. Hematite and goethite, but not montmorillonite, dramatically accelerated the oxidation with a low concentration (1 mM) of Mn(II) and bromate under various solution conditions. Further, the reaction system was autocatalytic with Fe oxides initiating the oxidation of Mn(II) at the early stage and the subsequent catalysis mainly provided by the Mn oxide products. In contrast to producing Mn(IV)O 2 only during the homogeneous oxidation of Mn(II) by bromate in solutions, the heterogeneous mineral-surface catalyzed oxidation resulted in a mixture of Mn(III)OOH and Mn(IV)O 2 phases. Mn(III)OOH was an intermediate product and can be further oxidized by bromate to Mn(IV)O 2 . The occurrence and accumulation of the intermediate product MnOOH can be attributed to its rapid formation due to surface-enhanced nucleation and growth on Fe oxide surfaces and to its higher resistance to oxidation by bromate than Mn(III) ions or clusters. Overall, mineralsurface catalyzed oxidation of Mn(II) by bromate is favorable from both thermodynamic and kinetic perspectives, and can be a major pathway for the occurrence of Mn oxides on Mars where microorganisms are lacking to catalyze the reaction. Our study further improves our understanding of the thermodynamic and kinetic controls on Mn(II) oxidation.

54 ENVIRONMENTAL SCIENCES↗

Atomistic modeling of ultra-thin surface oxide growth on a ternary alloy : oxidation of Al-Ni-Fe.

By employing variable-charge molecular dynamics, surface oxide film growth on aluminum-nickel-iron alloys has been studied at 300 and 600 K. The dynamics of oxidation and oxide growth is strongly dependent on the composition of the initial alloy and the ambient temperature. Higher content of Ni and Fe in Al alloys is found to reduce the oxide growth kinetics; 15% Ni + 15% Fe Al alloy yielded 30-40% less growth at 400 ps oxygen exposure compared to pure Al. We observe dopant segregation, which disrupts the interaction between O atoms and Al atoms in the alloy, leading to a nonlinear oxide growth profile in the case of ternary Al-Ni-Fe alloy. Compared to oxidation at 300 K, 30% more oxide layer was yielded at 600 K, due to the elevated temperature. The simulated oxide kinetics indicates that the growth rate of anion surpasses the cation rate with higher sensitivity to the stoichiometry of the base metal substrate. Charge state analysis provides insights into the evolution of cation and anion species as the oxide layer grows. In particular, due to higher correlation, Fe shows a high rate of oxidation when the content is high, whereas the rate of Ni oxidation is consistently low. Density profile analysis suggests the segregation of dopant atoms below the growing ultrathin oxide layer, showing the presence of a layer-by-layer mode of oxide layer even with disordered structure. Coordination number (Z, the number of oxygen atoms around an aluminum atom) of aluminum oxide has been used to identify how the initial oxidation transitions into equilibrated states. Z = 3 is dominant in the early stages of oxidation and at the interface between oxide and bulk substrate, but it transitions quickly to Z = 4 (45%) and 5 (35%) as the oxide equilibrates and approaches its self-limiting thickness. Even though growth kinetics is dependent on the base metal stoichiometry, the composition of the oxide microstructure is not significantly affected, primarily segregating dopant elements, i.e., Ni and Fe outside of the oxide layer.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Passivation of a Corrosion Resistant High Entropy Alloy in Non-oxidizing Sulfate Solutions

The passivation behavior of a novel high entropy alloy (HEA) of composition 38Ni-21Cr-20Fe-13Ru-6Mo-2W at.% (33Ni-16Cr-17Fe-19Ru-9Mo-6W wt.%) was investigated in sulfate solutions of various pH levels. The HEA was compared to a commercially available Ni-Cr-Mo-W-Fe alloy, C-22. Experiments were conducted using in-situ electrochemical and ex-situ surface-sensitive methods to probe the growth and dissolution of the passive layer. The HEA exhibited excellent corrosion resistance in highly acidic and highly alkaline solutions, maintaining passivity through a broad range of potentials below the Cr transpassivity range. Extremely rapid and efficient oxide formation and lower quasi-steady passive current densities were observed during oxide growth in the passive range compared to commercial alloy C-22. Ex-situ characterization of the passive film by atom probe tomography and X-ray photoelectron spectroscopy provided insight into the oxide composition, thickness, and elemental valence states of potentiostatically-grown and air-formed oxides. All elements in the alloy were oxidized following potentiostatic oxide growth. Instead of distinct stoichiometric and phase-distinct oxides, a disordered solid solution oxide was observed with significant enrichment in Cr and Ru with the latter depending sensitively on potential, as well as depletion of Fe and Ni. Enrichment of Cr was modeled with a modified surface enrichment model. The oxide thickness was estimated to be 3-4 nm thick. The connection between the enrichment of Cr in the passive layer, Mo and W presence, and excellent passivity is discussed.

corrosion, High entropy alloys, XPS, atom probe to↗

Inhibition of Chromium(III) Oxidation through Manganese(IV) Oxide Passivation and Iron(II) Abiotic Reduction

Manganese (Mn) oxides are strong oxidants that are ubiquitous in soils and can oxidize redox-active metals, including chromium (Cr). In soil environments, trivalent chromium (Cr(III)) is a benign, immobile micronutrient, whereas the hexavalent Cr(VI) form is present as a highly mobile, toxic chromate oxyanion. Although many studies have characterized the capacity of Mn(III/IV) oxides to oxidize Cr(III) to toxic Cr(VI), the oxidative capacity of Mn oxides in the presence of potentially passivating soil constituents, specifically reduced soluble iron (Fe(II) aq ), remains unresolved. We hypothesized that chemical processes at redox interfaces, such as diffusion-limited environments within soil aggregates, can lead to decreased Cr(VI) production from Mn oxide-driven oxidation due to passivation by Fe(II) aq . A multichamber diffusion-limited reactor was used to simulate transport at soil redox interfaces and investigate the capacity of poorly crystalline and crystalline Mn oxides to oxidize solid Cr(III) minerals to Cr(VI) in the presence of Fe(II) aq . As predicted, Cr(VI) was produced through the Mn oxide-catalyzed oxidation of Cr(III) at a rate controlled by the solubility of Cr(OH) 3 . However, in the presence of Fe(II) aq , the concentration of aqueous Cr(VI) decreased as a function of the Fe(II) aq concentration, where high concentrations of Fe(II) aq completely inhibited Cr(VI) production, likely through both the passivation of the Mn oxide and the direct reduction of Cr(VI) by Fe(II). At both low (14 μM) and high (100 μM) Fe(II) aq concentrations, the iron oxide minerals hematite (Fe 2 O 3 ) and goethite (α-FeOOH) were associated with the Mn oxides, which can cause surface passivation, a likely role that decreases Cr(III) oxidation. Additionally, the Cr(III) oxidation rate decreased with increasing crystallinity of the Mn oxides whether or not Fe(II) was present.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Accelerated Cu2O Reduction by Single Pt Atoms at the Metal-Oxide Interface§

The reducibility of metal oxides, when serving as the catalyst support or the active sites themselves, plays an important role in heterogeneous catalytic reactions. Here we present an integrated experimental and theoretical study that reveals how the addition of small amounts of atomically dispersed Pt at the metal/oxide interface dramatically enhances the reducibility of a Cu2O thin film by H2. X-ray photoelectron spectroscopy (XPS) and temperature-programmed desorption (TPD) results reveal that upon oxidation, a PtCu single-atom alloy (SAA) surface is covered by a thin Cu2O film and is therefore unable to dissociate H2. Despite this, in situ studies using ambient pressure (AP) XPS reveal that the presence of a small amount of Pt under the oxide layer can, at the single-atom limit, promote the reduction of Cu2O by H2 at room temperature. We build two density functional theory based surface models to better understand these experimental findings: A Cu2O/Cu(111)-like surface oxide layer, known as the ‘29’ oxide, in which Pt is alloyed into the Cu(111) surface as well as a PtCu SAA. Our calculations suggest that the increased activity is due to the presence of atomically dispersed Pt under the surface oxide layer, which weakens the Cu-O bonds in its immediate vicinity, thus making the interface between subsurface Pt and the surface oxide a nucleation site for the formation of metallic Cu. This initial step in the reduction process results in the presence of surface Pt atoms surrounded by metallic Cu patches, and the Pt atoms become active in H2 dissociation, which consequently accelerates the reduction of the oxide layer. This work demonstrates how isolated Pt atoms at the metal/oxide interface of a Cu-based catalyst accelerate the reduction of the oxide and, therefore, helps maintain the active, reduced state of the catalyst under reaction conditions, as is required for the synthesis of methanol from CO2 hydrogenation.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Microstructure Evolution in Ion-Irradiated Oxidized Zircaloy-4 Studied with Synchrotron Radiation Microdiffraction and Transmission Electron Microscopy

The corrosion process (oxidation and hydriding) of zirconium alloy fuel cladding is one of the limiting factors on fuel rod lifetime, particularly for Zircaloy-4. The corrosion rate of this alloy shows indeed a great acceleration at high burnup in light water reactors (LWRs). Understanding the corrosion behavior under irradiation for this alloy is an important technological issue for the safety and efficiency of LWRs. In particular, understanding the effect of irradiation on the metal and oxide layers is a key parameter in the study of corrosion behavior of zirconium alloys. In this study, Zircaloy-4 samples underwent helium and proton ion irradiation up to 0.3 dpa, forming a uniform defect distribution up to 1 pm deep. Both as-received and precorroded samples were irradiated to compare the effect of metal irradiation to that of oxide layer irradiation. After irradiation, samples were corroded to study the impact of irradiation defects in the metal and in preexisting oxide layers on the formation of new oxide layers. Synchrotron X-ray microdiffraction and microfluorescence were used to follow the evolution of oxide crystallographic phases, texture, and stoichiometry both in the metal and in the oxide. In particular, the tetragonal oxide phase fraction, which has been known to play an important role in corrosion behavior, was mapped in both unirradiated and irradiated metals at the submicron scale and appeared to be significantly affected by irradiation. These observations, complemented with electron microscopy analyses on samples in carefully chosen areas of interest, were combined to fully characterize changes caused by irradiation in metal and oxide phases of both alloys.

ion-irradiation↗

Interfacial engineering of solution-processed Ni nanochain-SiO{sub x} (x < 2) cermets towards thermodynamically stable, anti-oxidation solar selective absorbers

Cermet solar thermal selective absorber coatings are an important component of high-efficiency concentrated solar power (CSP) receivers. The oxidation of the metal nanoparticles in cermet solar absorbers is a great challenge for vacuum-free operation. Recently, we have demonstrated that oxidation is kinetically retarded in solution processed, high-optical-performance Ni nanochain-SiO{sub x} cermet system compared to conventional Ni-Al{sub 2}O{sub 3} system when annealed in air at 450–600 °C for several hours. However, for long-term, high-temperature applications in CSP systems, thermodynamically stable antioxidation behavior is highly desirable, which requires new mechanisms beyond kinetically reducing the oxidation rate. Towards this goal, in this paper, we demonstrate that pre-operation annealing of Ni nanochain-SiO{sub x} cermets at 900 °C in N{sub 2} forms the thermodynamically stable orthorhombic phase of NiSi at the Ni/SiO{sub x} interfaces, leading to self-terminated oxidation at 550 °C in air due to this interfacial engineering. In contrast, pre-operation annealing at a lower temperature of 750 °C in N{sub 2} (as conducted in our previous work) cannot achieve interfacial NiSi formation directly, and further annealing in air at 450–600 °C for >4 h only leads to the formation of the less stable (metastable) hexagonal phase of NiSi. Therefore, the high-temperature pre-operation annealing is critical to form the desirable orthorhombic phase of NiSi at Ni/SiO{sub x} interfaces towards thermodynamically stable antioxidation behavior. Remarkably, with this improved interfacial engineering, the oxidation of 80-nm-diameter Ni nanochain-SiO{sub x} saturates after annealing at 550 °C in air for 12 h. Additional annealing at 550 °C in air for as long as 20 h (i.e., 32 h air annealing at >550 °C in total) has almost no further impact on the structural or optical properties of the coatings, the latter being very sensitive to any interfacial changes due to the localized surface plasmon resonances of the metal nanostructures. This phenomenon holds true for Ni nanoparticle diameter down to 40 nm in Ni-SiO{sub x} system, where the optical response remains stable for 53 h at 550 °C in air. The oxidation vs. time curve also shows saturation behavior deviating from the kinetic Deal-Grove oxidation model. These results strongly suggest a promising approach to thermodynamically stable, anti-oxidation Ni/SiO{sub x} cermet absorbers via interfacial engineering.

71 CLASSICAL AND QUANTUM MECHANICS, GENERAL PHYSIC↗

Oxidative Dissolution Potential of Biogenic and Abiogenic TcO2 in Subsurface Sediments

Technetium-99 (Tc) is an important fission product contaminant associated with sites of nuclear fuels reprocessing and geologic nuclear waste disposal. Exhibiting an intermediate redox potential, Tc is highly mobile in its anionic, oxidized state [Tc(VII)O4-]; and less mobile as a poorly soluble oxyhydroxide precipitate [Tc(IV)O2•nH2O] in its reduced state. Here we investigate the potential for oxidation of Tc(IV) that was heterogeneously reduced by reaction with biogenic Fe(II) in two sediments differing in mineralogy and aggregation state (FRC, RG). Both sediments contained Fe(III) and Mn(III/IV) as redox active phases, but FRC also contained mass-dominant Fe-phyllosilicates of different types. Biogenic Tc(IV)O2•nH2O was oxidized in anoxic, but unreduced RG and FRC sediments through redox interaction with Mn(III/IV) oxides. Bioreduction by Shewanella putrefaciens CN32 dissolved Mn(III/IV) oxides and generated biogenic Fe(II) that was reactive with Tc(VII) in heat-killed, bioreduced sediment. Biogenic Fe(II) in the FRC exceeded that in RG by a factor of two. More rapid reduction rates were observed in the RG that had lower biogenic Fe(II), and less particle aggregation. EXAFS measurements indicated that the primary reduction product was a TcO2-like phase in both sediments. Redox product Tc(IV) oxidized rapidly and completely in RG when contacted with air. Oxidation, in contrast, was slow and incomplete in the FRC, in spite of similar molecular speciation to RG. X-ray microprobe, electron microprobe, x-ray absorption spectroscopy, and micro x-ray diffraction were applied to the whole sediment and isolated Tc-contained particles. These analyses revealed that non-oxidizable Tc(IV) in the FRC existed as complexes with octahedral Fe(III) within intra-grain domains of 50-100 µm-sized, Fe-containing micas presumptively identified as celadonite. The markedly slower oxidation rates in FRC as compared to RG were attributed to mass-transfer-limited migration of O2 into intra-aggregate and intraparticle domains where Tc(IV) existed; and the formation of unique, oxidation-resistant, intragrain Tc(IV)-Fe(III) molecular species.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Effects of Lytic Polysaccharide Monooxygenase Oxidation on Cellulose Structure and Binding of Oxidized Cellulose Oligomers to Cellulases

In nature, polysaccharide glycosidic bonds are cleaved by hydrolytic enzymes for a vast array of biological functions. Recently, a new class of enzymes that utilize an oxidative mechanism to cleave glycosidic linkages was discovered; these enzymes are called lytic polysaccharide monooxygenases (LPMO). These oxidative enzymes are synergistic with cocktails of hydrolytic enzymes and are thought to act primarily on crystalline regions, in turn providing new sites of productive attachment and detachment for processive hydrolytic enzymes. In the case of cellulose, the homopolymer of ..beta..-1,4-d-glucose, enzymatic oxidation occurs at either the reducing end or the nonreducing end of glucose, depending on enzymatic specificity, and results in the generation of oxidized chemical substituents at polymer chain ends. LPMO oxidation of cellulose is thought to produce either a lactone at the reducing end of glucose that can spontaneously or enzymatically convert to aldonic acid or 4-keto-aldose at the nonreducing end that may further oxidize to a geminal diol. Here, we use molecular simulation to examine the effect of oxidation on the structure of crystalline cellulose. The simulations highlight variations in behaviors depending on the chemical identity of the oxidized species and its location within the cellulose fibril, as different oxidized species introduce steric effects that disrupt local crystallinity and in some cases reduce the work needed for polymer decrystallization. Reducing-end oxidations are easiest to decrystallize when located at the end of the fibril, whereas nonreducing end oxidations readily decrystallize from internal cleavage sites despite their lower solvent accessibility. The differential in decrystallization free energy suggests a molecular mechanism consistent with experimentally observed LPMO/cellobiohydrolase synergy. Additionally, the soluble oxidized cellobiose products released by hydrolytic cellulases may bind to the active sites of cellulases with different affinities relative to cellobiose itself, which potentially affects hydrolytic turnover through product inhibition. To examine the effect of oxidation on cello-oligomer binding, we use thermodynamic integration to compute the relative change in binding free energy between the hydrolyzed and oxidized products in the active site of Family 7 and Family 6 processive glycoside hydrolases, Trichoderma reesei Cel7A and Cel6A, which are key industrial cellulases and commonly used model systems for fungal cellulases. Our results suggest that the equilibrium between the two reducing end oxidized products, favoring the linear aldonic acid, may increase product inhibition, which would in turn reduce processive substrate turnover. In the case of LMPO action at the nonreducing end, oxidation appears to lower affinity with the nonreducing end specific cellulase, reducing product inhibition and potentially promoting processive cellulose turnover. Overall, this suggests that oxidation of recalcitrant polysaccharides by LPMOs accelerates degradation not only by increasing the concentration of chain termini but also by reducing decrystallization work, and that product inhibition may be somewhat reduced as a result.

09 BIOMASS FUELS↗