Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “interfacial resistance”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 235 records · Page 13

Development of thermal joints for conduction-cooling applications

Abstract In support of the development of conduction-cooled superconducting radiofrequency (SRF) niobium cavities for use in continuous-wave linear accelerators, an experimental study of thermal contact resistance was performed on bolted joints using high-purity niobium, aluminium, and copper along with Apiezon N grease and indium foil as interfacial materials. The geometry of each joint investigated aims at replicating the design adopted in conduction-cooled SRF cavities currently under development at Jefferson Lab. The materials’ thermal conductivity and the joints’ thermal resistance were measured in the temperature range of 3.5 - 10 K. The results showed that the low thermal contact resistance of 2-4 K·cm 2 /W at 4.3 K achieved with Al-In-Nb and Al-Apiezon N-Cu joints should allow the operation of conduction-cooled SRF cavities at a targeted accelerating gradient of ∼10 MV/m.

Lewis, J. [Old Dominion University]↗

Mechanical Properties and Interfacial Bonding of Overmolded Polymer Composite Lattice Structures

This study investigates the mechanical properties and interfacial bonding of Polyamide 12 filled with Glass Fiber (PA12/GF) lattice structures overmolded with Nylon 66 (PA66) and Thermoplastic Polyurethane (TPU). The PA12/GF lattices, designed in Gyroid, Isotruss, and Octahedral geometries, were produced using the Selective Laser Sintering (SLS) technique. The thermal characteristics of both the lattice and overmolding materials were analyzed using Differential Scanning Calorimetry (DSC) and Thermogravimetric Analysis (TGA). The mechanical performance and interfacial bonding were evaluated through mechanical testing and microstructural analysis. The results indicate that overmolding improved flexural strength and impact resistance of the PA12/GF lattices. For instance, the plain PA12/GF Isotruss lattice exhibited a flexural strength of 15.5 MPa. By overmolding it with TPU the flexural strength increased by up to 137%, while PA66-overmolding resulted in an increase of 371%, achieving a flexural strength of 73 MPa. In terms of impact resistance, TPU-overmolding improved performance significantly, with an increase of 1800% (Gyroid) compared to the plain lattice. Microstructural analysis revealed good adhesion at the interface, especially when both the lattice and overmolding materials were thoroughly dried prior to the overmolding process to minimize interfacial porosity. This study highlights the potential of using overmolding to enhance lattice structures performance, offering lightweight and cost-efficient solutions for automotive applications.

Talabi, Isaac [ORNL] (ORCID:0000000340215594)↗

Structural effects of composition tuning in A-site disordered perovskite La0.5Li0.5−xMxTiO3 (M = Na, K) nanorods for fast interfacial transport for solid composite electrolyte design

Polymer-ceramic composite electrolytes (CPE) have emerged as promising replacements for currently used liquid organic electrolytes, which pose as safety hazards, in Li-ion batteries. Limits in conductivity enhancement in CPEs is often attributed to a high resistance for Li-ion transport along the interface due to the incompatibility of the polymer and ceramic phases. A clear understanding of the interfacial structure and how this impacts interfacial Li-ion transport is needed in order to efficiently design a CPE with optimal ionic conductivity. In this study, density functional theory (DFT) calculations, in conjunction with scanning transmission electron microscopy (STEM) and electron energy loss spectroscopy (EELS), are used to unveil the bulk and surface structure of La0.5Li0.5−xMxTiO3 (M = Na, K) (LMTO) nanorods, a newly-reported ceramic system with promising applications in CPEs, and the LMTO interactions with the poly(lithium sulfonyl (trifluoromethane sulfonyl)imide methacrylate) (p(MTFSILi)) polymerized ionic liquid. Substitution of lithium for sodium and potassium onto the A-site perovskite lattice is shown to increase the stability of the preferred pseudocubic perovskite phase because of their increased cation size which allows them to reduce the TiO6 octahedral rotations in the bulk and at the surface. STEM and EELS results show that LMTO nanorods with differing compositions have Ti-enriched (110)-oriented surfaces. Increased sodium and potassium compositions in LMTO is also shown using the DFT calculations to weaken the binding of the lithium atom to the MTFSI unit when LiMTFSI is adsorbed to the LMTO surface. This weakening of lithium binding to the polymer at the LMTO interface indicates that the lithium mobility is increased, correlating to an increase in interfacial Li-ion transport. Overall, this work provides insights into how to tune the interfacial interactions between the polymer (p(MTFSI)) and ceramic (LMTO) for optimal CPE design.

Shepard, Lauren B [Pennsylvania State University, ↗

Constitutional under-potential plating (CUP) – New insights for predicting the morphological stability of deposited lithium anodes in lithium metal batteries

Lithium (Li) cycling in lithium metal batteries (LMBs) inevitably witnesses a non-planar Li/electrolyte interface (cellular/dendritic microstructure) affecting the performance, safety and reliability of LMBs. Herein, the “constitutional under-potential plating” (CUP) concept is presented for the first time to understand the evolution, formation and predict the morphological stability/instability of the Li/electrolyte interface. Here, the CUP condition, a measure of the driving force for interface perturbation, occurs when the true potential gradient at the interface is smaller than the equilibrium electrodeposition potential gradient at the Li/electrolyte interface resulting in the electrolyte ahead of the Li-electrolyte interface to be in an under-potential state. Detailed CUP criterion calculations conducted herein establishes the relationship of battery operating conditions (e.g. current density, potential gradient) with the electrolyte properties (e.g. Li-ion transference number and diffusion coefficient) predicting the morphological stability condition at the interface. In addition to the driving force for interface perturbation, the capillarity effect or the Gibbs Thomson effect, a measure of the resistance to perturbation of the perturbed interface is discussed for understanding the influence of interfacial energy/adhesion energy between the current collector and the deposited Li on the overall morphological stability of the Li/electrolyte interface, a critical criterion for the unwanted dendritic morphology.

25 ENERGY STORAGE↗

Performance degradation due to anodic failure mechanisms in lithium-ion batteries

Here, we report a mechano-chemical model for anodic degradation during fast-charging of nickel-manganese-cobalt (NMC)/graphite (C) cell due to SEI growth, lithium plating/stripping, dead lithium storage, and film fracture of composite SEI and plated lithium film. Degradation of the battery is analyzed for a range of charging rates from 1 to 6 C-rates, and the influence of plating mechanisms – lithium plating and dead lithium deposition and recovery during stripping – on the film resistance of the anode are accounted for in the model. Dynamic evolution of the interfacial properties is modeled using rule-of-mixture approach. Model predictions of plating associated stress fields are used to compute critical energy release rate for film cracking. The results indicate an increased tendency of fracture for thinner SEI film with lithium plating at higher charging rates. The process of reforming the cracked film absorbs a significant portion of the electrode current thereby reducing the cell capacity and plating efficiency. The mechano-chemical model provides an extensive analytical framework for understanding the synergistic coupling of anodic degradation mechanisms, prognosticating conditions of SEI failure, and evaluating the capacity fade and efficiency of lithium-ion battery.

25 ENERGY STORAGE↗

Changes in Hydrogen Concentration and Defect State Density at the Poly-Si/SiOx/c-Si Interface Due to Firing

We determined the density of defect states of poly-Si/SiOx/c-Si junctions featuring a wet chemical interfacial oxide from lifetime measurements using the MarcoPOLO model to calculate recombination and contact resistance in poly-Si/SiOx/c-Si-junctions. In samples that did not receive any hydrogen treatment, the Dit,cSi is about 2 × 1012 cm-2 eV1 before firing and rises to 3–7 × 1012 cm2 eV1 during firing at measured peak temperatures between 620 °C and 863 °C. To address the question of why AlOx/SiNy stacks in contrast to pure SiNy layers for hydrogenation during firing provides better passivation quality, we have measured the hydrogen concentrations at the poly-Si/SiOx/c-Si interface as a function of AlOx layer thickness and compared these to J0 and calculated Dit,c-Si values. We observe an increase of the hydrogen concentration at the SiOx/c-Si interface upon firing as a function of the firing temperature that exceeds the defect concentrations at the interface several times. However, the AlOx layer thickness appears to cause an increase in hydrogen concentration at the SiOx/c-Si interface in these samples rather than exhibiting a hydrogen blocking property.

41 EE - Solar Energy Technologies Office (EE-4S)↗

Free convection in the Martian atmosphere

Researchers investigated the free convective regime for the Martian atmospheric boundary layer (ABL). Researchers generalized Schumann's model describing horizontal fluctuations and mean vertical gradients occurring during free convection to include convection driven by water vapor gradients and to include the effects of circulation above both aerodynamically smooth and rough surfaces. Applying the model to Mars, researchers found that nearly all the resistance to sensible and latent heat transfer in the ABL occurs within the thin interfacial sublayer at the surface. Free convection is found to readily occur at low pressures and high temperatures when surface ice is present. At 7 mb, the ABL should freely convect whenever the mean windspeed at the top of the surface layer drops below about 2.5 m s(-1) and surface temperatures exceed 250 K. Mean horizontal fluctuations within the surface layer are found to be as high as 3 m (-1) for windspeed, 0.5 K for temperature, and 10 (-4) kg m (-3) for water vapor density. Airflow over surfaces similar to the Antarctic Polar Plateau was found to be aerodynamically smooth on Mars during free convection for all pressures between 6 and 1000 mb, while surfaces with z sub o approx. equals 1 cm are aerodynamically rough over this pressure range.

Clow, G. D.↗

Effects of Hydrogen Annealing, Sulfur Segregation and Diffusion on the Cyclic Oxidation Resistance of Superalloys: a Review

This review is based on the phenomenon of improved oxide scale adhesion for desulfurized superalloys. The proposed adhesion mechanism involves sulfur interfacial segregation and scale-metal bond weakening. Sulfur surface segregation on superalloys is examined as a function of temperature and sulfur content and related to classical behavior predicted by the McLean isotherm. Effective desulfurization to less than 1 ppmw can be accomplished by hydrogen annealing and is governed by sulfur diffusion kinetics in nickel. Hydrogen annealing results in excellent cyclic oxidation resistance for a number of advanced superalloys. The concept of a critical sulfur content is discussed in terms of practical annealing conditions and section thicknesses.

Smialek, J. L.↗

Effects of hydrogen annealing, sulfur segregation and diffusion on the cyclic oxidation resistance of superalloys: A review

This review is based on the phenomenon of improved oxide scale adhesion for desulfurized superalloys. The proposed adhesion mechanism involves sulfur interfacial segregation and scale-metal bond weakening. Sulfur surface segregation on superalloys is examined as a function of temperature and sulfur content, and is related to the classical behavior predicted by the McLean isotherm. Effective desulfurization to less than 1 ppmw can be accomplished by hydrogen annealing and is described by sulfur diffusion kinetics in nickel. Hydrogen annealing results in excellent cyclic oxidation resistance for a number of advanced superalloys. The concept of a critical sulfur content is discussed in terms of practical annealing conditions and section thicknesses.

Smialek, J. L.↗

Thermal conductance in a bolted joint.

The thermal contact resistance of a bolted joint is composed of two components: large scale constriction which is influenced by the extent of the interfacial pressure distribution and small scale constriction which is influenced by the magnitude of the local pressure. It is analytically shown how the roughness asperities at the contact surfaces of the joint affect these two constrictions but in opposite senses. The sum of the two effects, the total resistance, may increase or decrease with changing resistance and examples are given where an optimum roughness will minimize total joint resistance.

Roca, R. T.↗

An Interface–Type Memristive Device for Artificial Synapse and Neuromorphic Computing

Interface-type (IT) metal/oxide Schottky memristive devices have attracted considerable attention over filament-type (FT) devices for neuromorphic computing because of their uniform, filament-free, and analog resistive switching (RS) characteristics. The most recent IT devices are based on oxygen ions and vacancies movement to alter interfacial Schottky barrier parameters and thereby control RS properties. However, the reliability and stability of these devices have been significantly affected by the undesired diffusion of ionic species. Herein, a reliable interface-dominated memristive device is demonstrated using a simple Au/Nb-doped SrTiO 3 (Nb:STO) Schottky structure. The Au/Nb:STO Schottky barrier modulation by charge trapping and detrapping is responsible for the analog resistive switching characteristics. Because of its interface-controlled RS, the proposed device shows low device-to-device, cell-to-cell, and cycle-to-cycle variability while maintaining high repeatability and stability during endurance and retention tests. Furthermore, the Au/Nb:STO IT memristive device exhibits versatile synaptic functions with an excellent uniformity, programmability, and reliability. A simulated artificial neural network with Au/Nb:STO synapses achieves a high recognition accuracy of 94.72% for large digit recognition from MNIST database. These results suggest that IT resistive switching can be potentially used for artificial synapses to build next-generation neuromorphic computing.

36 MATERIALS SCIENCE↗

Simulated Start-Stop and the Impact of Catalyst Layer Redox on Degradation and Performance Loss in Low-Temperature Electrolysis

Stress tests are developed that focus on anode catalyst layer degradation in proton exchange membrane electrolysis due to simulated start-stop operation. Ex situ testing indicates that repeated redox cycling accelerates catalyst dissolution, due to near-surface reduction and the higher dissolution kinetics of metals when cycling to high potentials. Similar results occur in situ, where a large decrease in cell kinetics (>70%) is found along with iridium migrating from the anode catalyst layer into the membrane. Additional processes are observed, however, including changes in iridium oxidation, the formation of thinner and denser catalyst layers, and platinum migration from the transport layer. Increased interfacial weakening is also found, adding to both ohmic and kinetic loss by adding contact resistances and isolating portions of the catalyst layer. Repeated shutoffs of the water flow further accelerate performance loss and increase the frequency of tearing and delamination at interfaces and within catalyst layers. These tests were applied to several commercial catalysts, where higher loss rates were observed for catalysts that contained ruthenium or high metal content. These results demonstrate the need to understand how operational stops occur, to identify how loss mechanisms are accelerated, and to develop strategies to limit performance loss.

08 HYDROGEN↗

The platinum microelectrode/Nafion interface - An electrochemical impedance spectroscopic analysis of oxygen reduction kinetics and Nafion characteristics

The objectives of this study were to use electrochemical impedance spectroscopy (EIS) to study the oxygen-reduction reaction under lower humidification conditions than previously studied. The EIS technique permits the discrimination of electrode kinetics of oxygen reduction, mass transport of O2 in the membrane, and the electrical characteristics of the membrane. Electrode-kinetic parameters for the oxygen-reduction reaction, corrosion current densities for Pt, and double-layer capacitances were calculated. The production of water due to electrochemical reduction of oxygen greatly influenced the EIS response and the electrode kinetics at the Pt/Nafion interface. From the finite-length Warburg behavior, a measure of the diffusion coefficient of oxygen in Nafion and diffusion-layer thickness was obtained. An analysis of the EIS data in the high-frequency domain yielded membrane and interfacial characteristics such as ionic conductivity of the membrane, membrane grain-boundary capacitance and resistance, and uncompensated resistance.

Parthasarathy, Arvind↗

Ultrathin epitaxial MgB 2 on SiC: Substrate surface-polarity-dependent properties

High-quality, ultrathin superconducting films are required for advanced devices such as hot-electron bolometers, superconducting nanowire single-photon detectors, and quantum applications. Using hybrid physical-chemical vapor deposition, we show that MgB 2 films as thin as 4 nm can be fabricated on the carbon-terminated 6⁢H-SiC (0001) surface with a superconducting transition temperature above 33 K and a rms roughness of 0.7 nm. Remarkably, the film quality is a function of the SiC surface termination, with the C-terminated surface preferred to the Si-terminated surface. To understand the MgB 2 thin film/SiC substrate interactions giving rise to this difference, we characterized the interfacial structures using Rutherford backscattering spectroscopy/channeling, electron-energy-loss spectroscopy, and x-ray photoemission spectroscopy. The MgB 2 /SiC interface structure is complex and different for the two terminations. Both terminations incorporate substantial unintentional oxide layers influencing MgB 2 growth and morphology, but with a different extent, intermixing, and interface chemistry. In this paper, we report measurements of transport, resistivity, and the critical superconducting temperature of MgB 2 /SiC that are different for the two terminations, and they link interfacial structure variations to observed differences. The result shows that the C face of SiC is a preferred substrate for the deposition of ultrathin superconducting MgB 2 films.

36 MATERIALS SCIENCE↗

An Analysis of the Impact of Particle Growth on Transport Losses in Polymer-Electrolyte Fuel Cells

Voltage cycling causes catalyst nanoparticles in polymer-electrolyte fuel cells to grow. The concomitant loss of interfacial area results in larger kinetic, transport, and possibly ohmic overpotentials. This paper uses recently published experimental data and mathematical models to investigate the evolutions of transport and ohmic resistances to platinum nanoparticles located on the surface and inside the micropores of carbon black supports. Resistance to oxygen transport rises as surface area declines primarily because the flux to each remaining larger platinum particle increases. The path lengths governing oxygen diffusion to surface and buried platinum sites also increase as nanoparticles grow. Platinum nanoparticles on the surface become relatively less favorable as voltage cycling proceeds because they grow faster than platinum in micropores. Because voltage cycling causes total interfacial area to decline, and the fraction located inside micropores to increase, nanoscale ohmic losses increase as a catalyst layer decays. The practical importance of this effect is difficult to discern because proton conductivity in carbon micropores is not well characterized.

07 ISOTOPE AND RADIATION SOURCES↗

Mechanistic mass transfer in hollow fiber membrane solvent extraction for bio-based isobutanol

Membrane solvent extraction (MSE) has emerged as a promising method for selectively recovering bioproducts from complex aqueous streams. Bio-isobutanol, a next-generation feedstock for biofuel, remains challenging to recover because of its low concentration and the presence of inhibitory substances. This study explores the potential of hollow fiber (HF) MSE for bio-isobutanol recovery and systematically examines the coupled effects of fiber packing, shell-side flow dynamics, and aqueous chemistry on performance. A resistance-in-series model is applied to understand mass transfer in the HF MSE modules, quantify local resistances, and validate overall performance. The results show that increasing the fiber packing provides a larger interfacial area but induces poor flow distribution and channeling, hindering effective isobutanol transport. Meanwhile, increasing the shell-side velocity improves isobutanol recovery due to reductions in the boundary layer thickness. The presence of salts, added to mimic fermentation broth, increases the partition coefficient through salting-out effects, further improving isobutanol flux. A modified correlation for the shell-side mass transfer coefficient (k s,ϕ+v ), integrating geometric and hydrodynamic effects, was developed and validated. The proposed model achieves highly predictive accuracy (r 2 = 0.9808) across a wide range of conditions, outperforming previous models. The findings provide mechanistic insight into the interaction of geometric packing, hydrodynamics, and chemistry in governing mass transfer in HF MSE. Overall, this work demonstrates the potential of HF MSE for efficient bio-isobutanol recovery and also provides practical guidelines on critical factors (packing fraction, partition coefficient, and shell-side velocity), aiding in the design and scaling of MSE systems for resource recovery.

Aqueous chemistry↗

Key Durability Issues with Mullite-Based Environmental Barrier Coatings for Si-Based Ceramics

Plasma-sprayed mullite (3Al2O3 central dot 2SiO2) and mullite/yttria-stabilized-zirconia (YSZ) dual layer coatings have been developed to protect silicon-based ceramics from environmental attack. Mullite-based coating systems show excellent durability in air. However, in combustion environments, corrosive species such as molten salt or water vapor penetrate through cracks in the coating and attack the Si-based ceramics along the interface, Thus modification of the coating system for enhanced crack-resistance is necessary for long-term durability in combustion environments. Other key durability issues include interfacial contamination and coating/substrate bonding. Interfacial contamination leads to enhanced oxidation and interfacial pore formation, while weak coating/substrate bonding leads to rapid attack of the interface by corrosive species, both of which can cause premature failure of the coating. Interfacial contamination can be minimized by limiting impurities in coating and substrate materials. The interface may be modified to improve the coating/substrate bond.

Lee, Kang N.↗

Key Durability Issues with Mullite-Based Environmental Barrier Coatings for Si-Based Ceramics

Plasma-sprayed mullite (3Al2O3.2SiO2) and mullite/yttria-stabilized-zirconia (YSZ) dual layer coatings have been developed to protect silicon -based ceramics from environmental attack. Mullite-based coating systems show excellent durability in air. However, in combustion environments, corrosive species such as molten salt or water vapor penetrate through cracks in the coating and attack the Si-based ceramics along the interface. Thus the modification of the coating system for enhanced crack-resistance is necessary for long-term durability in combustion environments. Other key durability issues include interfacial contamination and coating/substrate bonding. Interfacial contamination leads to enhanced oxidation and interfacial pore formation, while a weak coating/substrate bonding leads to rapid attack of the interface by corrosive species, both of which can cause a premature failure of the coating. Interfacial contamination can be minimized by limiting impurities in coating and substrate materials. The interface may be modified to improve the coating/substrate bond.

Lee, Kang N.↗