What Happens to Material Strength at High Strain Rates and Pressures: An Experimental Study
Explore the source record for details and available documents.
SEARCH · Engineering Papers
Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.
Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.
Explore the source record for details and available documents.
Abstract not provided.
Explore the source record for details and available documents.
Methods for making metastable lead-free piezoelectric materials are presented herein.
Explore the source record for details and available documents.
The addition of a tempering or austempering step to the double soaking of a 0.14C–7.17Mn (wt pct) steel was investigated in the present contribution. The double soaking heat treatment is a two-step intercritical annealing heat treatment, which generates microstructures of athermal martensite, retained austenite and ferrite when applied to medium manganese steels. Microstructures following double soaking and (aus)tempering contained a combination of retained austenite, athermal or tempered martensite, and blocky or bainitic ferrite. X-ray diffraction, dilatometry and transmission Kikuchi diffraction were utilized to investigate microstructural changes which occurred during tempering or austempering. The resulting mechanical properties were measured using uniaxial tensile testing. The double soaking plus tempering heat treatment was shown to generate an ultimate tensile strength of 1,340 MPa in combination with 28 pct total elongation while the double soaking plus austempering heat treatment resulted in an ultimate tensile strength of 1,675 MPa and total elongation of 22 pct. Overall, both novel heat treatments produced a combination of strength and ductility desired for the third generation of advanced high strength steels.
Current Ni-based alloys used in turbine blade applications are operating at 1100°C which is approximately 90% of the solidus of Ni-based alloys. Further increases in temperature can be achieved only through the use of alloys with higher solidus temperatures such as refractory alloys which include Mo, Nb, W, Ta alloys. Niobium has a unique combination of physical properties that include a high melting point (2468°C), lowest density (8.57 g/cc), and the lowest modulus amongst refractory alloys, a good thermal conductivity that increases from 45 W/mK at room temperature to 62 W/mK at 1093°C, good ductility with fabricability using traditional techniques, high strength, good creep resistance, and general chemical inactivity. Hence niobium alloys offer many advantages for use at the desired temperature of 1300°C. One of the major deterrents to the use of niobium and its alloys at high temperatures is achieving good oxidation resistance. In addition, achieving balanced properties of room temperature strength, ductility, fracture toughness, high temperature strength, and creep resistance required for 1300°C operation at a density of 9 g/cm 3 is extremely challenging since the addition of W which is a potent strengthener increases the density of the alloy. This project seeks to enable the development of a tri-layered turbine blade that can operate continuously at 1300°C with the core of the turbine blade providing good creep resistance, the second layer providing improved oxidation resistance over the core layer, and the third layer being an environmental barrier providing oxidation resistance. The objective of this Phase 1 project was to use computational modeling and advanced characterization tools to develop two classes of Nb alloys which could be used as the core layer and the transition layer. The first class of alloys developed in this project was a Nb-alloy designed to serve as the turbine blade core with excellent room temperature strength, ductility, and high temperature strength and creep resistance required for 1300°C operation. These alloys were designed to contain sufficient solute solution strengthening elements (W, Mo) but constrained by the density of alloy, along with the addition of elements such as Zr, Hf, Ta, C, and N to achieve a combination of primary and secondary carbide precipitation. A total of 38 “creep-resistant” alloys were designed and cast during the duration of the project. Processing techniques were developed to keep the oxygen contents as low as possible with typical oxygen contents less than 250 ppm. One alloy with a density of < 9.5 g/cc was successful in meeting the Phase 2 intermediate project mechanical property milestone requirements of room temperature ductility greater than 1.0%, 1200°C creep strain of less than 3% at 150 MPa and 100 hours in vacuum, and with solidus temperature greater than 1500ᵒC. The second class of alloys was designed to be a Nb-rich alloy with improved oxidation resistance when compared to the core layer and was designed specifically to be compatible with the core layer and the outer environmental barrier coating. This Nb- alloy will be specifically designed to be microstructurally stable at these temperatures when in contact with the core alloy and provide protection against catastrophic failure of the barrier coating. Two alloys were cast and processed but further development was discontinued to focus on the development of the creep resistant alloy.
The mechanical performance of an Fe-Co intermetallic alloy processed by laser powder bed fusion (L-PBF) and laser directed energy deposition (L-DED) additive manufacturing is compared. L-PBF material was characterized by high strength (500–550 MPa) and high ductility (35%) in tension, corresponding to a ~250% increase in strength and an order-of-magnitude improvement in ductility relative to conventional material. Conversely, L-DED material exhibited similarly poor tensile properties to the conventional wrought alloy, with low strength (200–300 MPa) and low ductility (0–2.7%). Finally, the disparity in properties between L-PBF and L-DED material is discussed in the context of the fundamental differences between manufacturing methods.
Electrodeposition is a commonly used method for depositing a metal layer on a metallic substrate, to provide a decorative finish or for functional purposes including wear and corrosion resistance. The interfacial bonding strength is a critical factor in determining the quality of electrodeposition, as it ensures the adhesion of the deposited layer to the substrate. Despite its importance, there has not previously been a suitable mechanical testing method to quantitatively characterize the bonding strength between the electrodeposited layers and the substrate, due to the high strength of the materials and to restrictions imposed by the geometry (due to the small thickness of the plating layer) to manufacture tensile bars. In this study, we introduce a novel mesoscale mechanical testing method to overcome these limitations. This technique was applied to assess the bonding strength between a 304 stainless steel (SS) substrate and electrodeposited nickel with three different plating formulae (nickel sulfamate, Watts bath, and hard nickel). The thickness of the pure nickel coatings achieved for each of the three electrolyte solutions was approximately 1 mm on each side of the substrate. Mesoscale tensile bars of 1 mm length were manufactured by a femtosecond laser, with the material interface at the center of the gauge section, and then tensile-tested with digital image correlation. Further, the results proved that the electrodeposition technique is able to produce a very high bonding strength that is close to the yield strength of both the substrate material and the electrodeposited nickel layer. Additionally, in the case of the Watts bath formula, the interfacial bonding strength between the SS 304 and electrodeposited nickel can exceed that of the nickel layer. This method is expected to be useful for quantifying the interfacial bonding strength in numerous applications.
Third-generation silicon carbide (SiC) composites reinforced by SiC fibers (Hi-Nicalon S [HNS] and Tyranno SA3 [SA3]) are attractive for use in next generation reactors owing to their high strength and chemical inertness at high temperatures, as well as enhanced radiation tolerance under neutron irradiation environments. To optimize composite performance, the interfacial mechanical properties of chemical vapor–infiltrated (CVI) SiC f /SiC composites are investigated in this effort by using a slant interface micropillar compression testing procedure. The micropillar test specimens, containing an inclined pyrolytic carbon (PyC) interphase, are prepared using a focused ion beam. The novel microcompression testing successfully quantifies the debond shear strength and internal friction coefficient of micropillar test samples by using the Mohr-Coulomb formulation. Furthermore, according to four types of SiCf/SiC composite microcompression test results, interfacial properties and debond mechanisms are significantly affected by the PyC layer thickness, the local bonding mechanism of the PyC interphase on the SiC fiber surface, and the surface roughness of fibers. Regardless of PyC thicknesses, SA3-reinforced CVI SiC f /SiC composites are found to have much higher debond shear strengths than HNS-reinforced SiC f /SiC CVI composites. By using this micropillar compression technique alongside analytical methods, we uncover new understandings of PyC interface properties. Additionally, the micropillar test results obtained are correlated with macroscopic mechanical properties of neutron-irradiated CVI SiCf/SiC composites.
High carbon levels have been found to improve the fabricability of high-strength cast and wrought Ni-based superalloys, enabling the development of superior cast/wrought materials. However, carbon also strongly influences the microstructure and mechanical properties of the alloys. Nimonic 105 variants with three different carbon concentrations were manufactured. A bimodal grain size was found in the intermediate carbon content variant, while the high (low) carbon resulted in fine (coarse) grains thereby significantly affecting creep performance. The variations in grain structure were attributed to the primary carbides. An intermediate carbon level showed the best combination of strength and ductility in tension at high-temperature but little improvement in, or even inferior, creep performance. Discussion of the results will establish an understanding of the influence of carbon on the microstructure and mechanical properties of high strength cast and wrought superalloys, providing insights into obtaining high-quality alloys for future high-temperature applications.
In the present study, a unique friction self-piercing riveting (F-SPR) was applied to join high-strength, low-ductility aluminum alloy (AA) 7055-T76 and AA7055-T76 to mitigate a cracking issue. Also, the effect of die design on both joint formation and the mechanical joint performance were investigated. A crack-free joint was achieved when joining AA7055-T76 and AA7055-T76 by F-SPR. As the bottom diameter of the die increased, the mechanical interlocking distance initially increased then became almost saturated. At the same time, the solid-state bonding gradually disappeared, and the lap-shear fracture changed from bottom aluminum fracture to rivet pull-out with partial bottom aluminum fracture. The average maximum lap-shear joint strength of 11.57 kN and cross tension of 5.65 kN were achieved from the D2 die design owing to the combined contributions from high mechanical interlocking distance and good solid-state bonding at the joint interface. Ultrafine grain refinement was observed at the region next to the rivet shank outer surface and along the materials flow line between the top and bottom aluminum sheet in the rivet cavity. Further, because of the same joint-process parameters, the hardness profile at the joints made by different dies did not show obvious differences. As the distance from the base metal to the rivet outer surface decreased, frictional heat caused the hardness to initially decrease from 190 to 150 HV in the heat-affected zone. Hardness increased up to 175 HV in the thermomechanical affected zone (TMAZ-I) owing to large plastic deformation.
Nanotwinned metals have demonstrated the capacity for concomitant high strength and ductility. However, metals with high stacking fault energies, such as aluminum (Al), have a low propensity for twin formation. Here, we show the fabrication of supersaturated solid-solution Al–Zr alloys with a high density of growth twins. Incoherent twin boundaries (ITBs) are strong barriers to dislocation motion, while mobile partial dislocations promote plasticity. These deformable nanotwinned Al–Zr alloys reach a flow stress of ∼1 GPa, as demonstrated using in situ micropillar compression tests. Density functional theory calculations uncover the role Zr solute plays in the formation and deformation of the nanotwinned microstructure. This study features a strategy for incorporating ITBs and 9R phase into Al alloys for simultaneous benefits to strength and deformability.
Precipitate strengthened high-temperature alloys are currently used in safety-critical applications. Understanding precipitate stability and solute segregation mechanisms at high temperatures is key to designing high-strength alloys. Rapid in-situ approaches, therefore, are pivotal in accelerating the alloy design process. Hereby using the test case of a promising high-temperature Al-Cu-Mn-Zr alloy, we demonstrate the value of in-situ atom probe tomography coupled with in-situ transmission electron microscopy to reveal atomic-scale mechanisms that lead to the emergence of non-equilibrium solute segregation. Mn and Zr segregation at strengthening precipitate(θ’)-matrix interface increases the kinetic barrier for phase transformation thus retaining high-temperature strength.
Low-density steels constitute a broad and complex alloy space (Fe–Mn–Al–C) suitable for a variety of applications. In particular, there has been growing interest in duplex (ferrite + austenite) or multiphase (+ martensite, carbides) low-density steels as a lightweight, advanced high-strength steel (AHSS) for vehicle applications, spurred by extensive decarbonization efforts. Medium-Mn (med-Mn) (3 to 12 wt pct) steels with 3.5 to 10 wt pct Al additions have decreased densities, presenting an interesting opportunity for high-specific strength, intrusion-resistant, and energy-absorbing sheet components with reduced alloying contents compared to high-Mn grades like austenitic Fe–Mn–Al–C or twinning-induced plasticity steels. Compared to leaner med-Mn steels, the physical metallurgy of med-Mn, low-density steels (MMLS) is complex and distinguished by increased δ-ferrite fractions and austenite stacking fault energies, decreased martensite start temperatures, and modified phase transformation windows. Mechanical properties of MMLS are comparable to 3rd generation AHSS, attributable to the unique, multiphase microstructures, and the array of strengthening mechanisms that can be accessed. Despite this, challenges and unknowns remain with respect to their industrial implementation, and new processing routes may need to be developed. Here, this review aims to highlight the composition effects, processing methods, microstructural evolution, deformation behavior, and application properties geared toward manufacturing and performance, altogether assessing the potential of MMLS for transportation applications.
Current Ni-based alloys used in turbine blade applications are operating at 1100°C which is approximately 90% of the solidus of Ni-based alloys. Further increases in temperature can be achieved only through the use of alloys with higher solidus temperatures such as refractory alloys which include Mo, Nb, W, Ta alloys. Niobium has a unique combination of physical properties that include a high melting point (2468°C), lowest density (8.57 g/cc), and the lowest modulus amongst refractory alloys, a good thermal conductivity that increases from 45 W/mK at room temperature to 62 W/mK at 1093°C, good ductility with fabricability using traditional techniques, high strength, good creep resistance, and general chemical inactivity. Hence niobium alloys offer many advantages for use at the desired temperature of 1300°C. One of the major deterrents to the use of niobium and its alloys at high temperatures is achieving good oxidation resistance. In addition, achieving balanced properties of room temperature strength, ductility, fracture toughness, high temperature strength, and creep resistance required for 1300°C operation at a density of 9 g/cm 3 is extremely challenging since the addition of W which is a potent strengthener increases the density of the alloy. This project seeks to enable the development of a tri-layered turbine blade that can operate continuously at 1300°C with the core of the turbine blade providing good creep resistance, the second layer providing improved oxidation resistance over the core layer, and the third layer being an environmental barrier providing oxidation resistance. The objective of this Phase 1 project was to use computational modeling and advanced characterization tools to develop two classes of Nb alloys which could be used as the core layer and the transition layer.
The high-entropy transition metal borides containing a random distribution of five or more constituent metallic elements offer novel opportunities in designing materials that show crystalline phase stability, high strength, and thermal oxidation resistance under extreme conditions. We present a comprehensive theoretical and experimental investigation of prototypical high-entropy boride (HEB) materials such as (Hf, Mo, Nb, Ta, Ti)B2 and (Hf, Mo, Nb, Ta, Zr)B2 under extreme environments of pressures and temperatures. The theoretical tools include modeling elastic properties by special quasi-random structures that predict a bulk modulus of 288 GPa and a shear modulus of 215 GPa at ambient conditions. HEB samples were synthesized under high pressures and high temperatures and studied to 9.5 GPa and 2273 K in a large-volume pressure cell. The thermal equation of state measurement yielded a bulk modulus of 276 GPa, in excellent agreement with theory. The measured compressive yield strength by radial X-ray diffraction technique in a diamond anvil cell was 28 GPa at a pressure of 65 GPa, which is a significant fraction of the shear modulus at high pressures. The high compressive strength and phase stability of this material under high pressures and high temperatures make it an ideal candidate for application as a structural material in nuclear and aerospace fields.
Recent research efforts to develop advanced–/ultrahigh–strength medium-Mn steels have led to the development of a variety of alloying concepts, thermo-mechanical processing routes, and microstructural variants for these steel grades. However, certain grades of advanced–/ultrahigh–strength steels (A/UHSS) are known to be highly susceptible to hydrogen embrittlement, due to their high strength levels. Hydrogen embrittlement characteristics of medium–Mn steels are less understood compared to other classes of A/UHSS, such as high Mn twinning–induced plasticity steel, because of the relatively short history of the development of this steel class and the complex nature of multiphase, fine-grained microstructures that are present in medium–Mn steels. The motivation of this paper is to review the current understanding of the hydrogen embrittlement characteristics of medium or intermediate Mn (4 to 15 wt pct) multiphase steels and to address various alloying and processing strategies that are available to enhance the hydrogen-resistance of these steel grades.