Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “compositional properties”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 235 records · Page 13

Computer aided derivation of equations for composite mechanics problems and finite element analyses

Explicit equations are derived for analysis of multilayered fiber composites and for finite element analyses. The equations are obtained using a symbolic program and tested for various composite properties as well as for different fiber orientations. In order to analyze multilayered fiber composite structures, a variable thickness finite element is formulated. Examples of an airfoil geometry, simulated in a form of a cantilevered beam with various fiber orientations are studied.

Sarigul, N.↗

Testing of High S Matrix Glasses to Expand DFHLW Glass Compositional Ranges (Rev.1)

Gaps in glass composition-property data for direct-feed high-level waste (DFHLW) have recently been identified. One such gap is the region of high sulfur solubility since previous, pretreated, high-level wastes contained very little sulfur. Filling this data gap will significantly broaden the range of process flowsheet options including minimal washing and will allow for optimized waste loading in DFHLW glasses. This report summarizes the data collected during the characterization of the DFHLW High S Glass Matrix (HS24). A glass matrix of 50 glass compositions was developed to evenly cover the DFHLW composition region for high sulfur glass. Matrix glasses were designed to expand the composition region outside the current component concentration and property limits so as to reduce uncertainties at the limits. The 50 matrix glasses were fabricated and tested for properties important to the success of DFHLW vitrification including: compositions, canister centerline cooling (CCC) crystallinity and isothermal crystallinity, density, viscosity, electrical conductivity (EC), product consistency test (PCT) response, toxicity, and sulfate solubility. Melter materials corrosion testing is reported elsewhere. These glasses were intentionally designed to have high SO 3 solubilities (0.7 to 2.2 SO 3 wt%) in compositional regions that had not been previously explored. Forty-eight glasses showed the measured SO 3 content retained >80% of the target SO 3 and the densities of all the glasses ranged from 2.49 g·cm -3 to 2.74 g·cm -3 . While the model predicted nepheline formation in 5 glasses, one of the tested 50 CCC glasses formed nepheline, and 35 glasses formed Cr-containing phases such as spinels and eskolaite. Only five glasses were amorphous after CCC treatment where 44 glasses with detectable crystals contained =10 wt% crystals and only one glass had > 10 wt% crystals. None of the glasses exceeded the allowable T 2% for spinel crystal formation at 950 ºC (i.e., no glasses had >2 wt% spinel at 950 ºC) during isothermal crystal fraction tests where 10 glasses showed no crystalline phases at or below 950 ºC. All the glasses (except one which failed being slightly lower than the target) satisfied the SO 3 constraint while 98 glasses did not meet the viscosity constraints and 4 failed the EC constraints. Six quenched (Q) and six CCC glasses failed the Defense Waste Processing Facility (DWPF) Environmental Assessment (EA) glass PCT threshold and 3 Q and 4 CCC failed the PCT design constraint. One glass exceeded the WTP delisting limits for Cr via EPA Method 1311 (i.e., Toxicity Characteristic Leaching Procedure, TCLP). It should be emphasized that some of these glasses were specifically designed to approach or even exceed certain property constraints, as filling data gaps in these regions will provide the greatest benefit for future model development by improving accuracy and reducing uncertainties. These insights will ultimately support the development of more robust glass formulation strategies, enabling higher waste loading, reducing operational risks, and expanding the processing envelope.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Characterization of elastic-plastic properties of AS4/APC-2 thermoplastic composite

Elastic and inelastic properties of AS4/APC-2 composites were characterized with respect to temperature variation by using a one-parameter orthotropic plasticity model and a one parameter failure criterion. Simple uniaxial off-axis tension tests were performed on coupon specimens of unidirectional AS4/APC-2 thermoplastic composite at various temperatures. To avoid the complication caused by the extension-shear coupling effect in off-axis testing, new tabs were designed and used on the test specimens. The experimental results showed that the nonlinear behavior of constitutive relations and the failure strengths can be characterized quite well using the one parameter plasticity model and the failure criterion, respectively.

Sun, C. T.↗

The effect of thermal exposure on the mechanical properties of aluminum-graphite composites

To promote the development of aluminum-graphite composites with improved properties for aerospace applications, composite samples were fabricated by solid-state diffusion bonding of liquid-phase Al-infiltrated Thornel 50 fibers, and their mechanical properties were measured at room temperature in the as-received condition, after temperature exposure and after thermal cycling. The interface structure in aluminum-graphite composites and its effect on the composite properties, the effect of thermal cycling on the tensile properties of the composites, and the characteristics of failures of the composites in tension is discussed. The studied composites exhibited tensile properties corresponding well with those predicted by the rule of mixtures. Thermal cycling between 20 C and 500 C, as well as the formation of the Al4C3 at the Al-graphite interfaces at temperatures above 500 C resulted in degradation of the composite strength. Scanning electron microscopy of fractured surfaces indicated that the relatively weak interface governs the mode of failure in tension.

Khan, I. H.↗

Tension, Compression, and Bend Properties for Sic/RBSN Composites

The room-temperature tension, compression, and bend properties of unidirectional SiC fiber-reinforced reaction-bonded silicon nitride composites (SiC/RBSN) have been investigated. The effects of fiber content on the modulus, first matrix cracking strength, and ultimate strength properties were determined. In tension, composites with greater than 8-percent fiber content showed strain capability beyond matrix fracture and fiber-dominated ultimate strength. In compression, the composites displayed essentially elastic behavior, and matrix-dominated ultimate strength. For both deformation modes, most mechanical properties increased with fiber content. In bend, the modulus, strength properties, and failure modes of the composites were influenced by span-to-thickness ratio.

Bhatt, Ramakrishna T.↗

Fibrous refractory composite insulation

Family of high-temperature, low-density refractory composite insulations made from aluminoborosilicate and silica fibers has insulating material with improved mechanical and thermal properties. Composition is useful for reusable heat-shield materials.

Goldstein, H. E.↗

Fiber reinforced glasses and glass-ceramics for high performance applications

The development of fiber reinforced glass and glass-ceramic matrix composites is described. The general concepts involved in composite fabrication and resultant composite properties are given for a broad range of fiber and matrix combinations. It is shown that composite materials can be tailored to achieve high levels of toughness, strength, and elastic stiffness, as well as wear resistance and dimensional stability.

Prewo, K. M.↗

Continuous fiber ceramic matrix composites for heat engine components

High strength at elevated temperatures, low density, resistance to wear, and abundance of nonstrategic raw materials make structural ceramics attractive for advanced heat engine applications. Unfortunately, ceramics have a low fracture toughness and fail catastrophically because of overload, impact, and contact stresses. Ceramic matrix composites provide the means to achieve improved fracture toughness while retaining desirable characteristics, such as high strength and low density. Materials scientists and engineers are trying to develop the ideal fibers and matrices to achieve the optimum ceramic matrix composite properties. A need exists for the development of failure models for the design of ceramic matrix composite heat engine components. Phenomenological failure models are currently the most frequently used in industry, but they are deterministic and do not adequately describe ceramic matrix composite behavior. Semi-empirical models were proposed, which relate the failure of notched composite laminates to the stress a characteristic distance away from the notch. Shear lag models describe composite failure modes at the micromechanics level. The enhanced matrix cracking stress occurs at the same applied stress level predicted by the two models of steady state cracking. Finally, statistical models take into consideration the distribution in composite failure strength. The intent is to develop these models into computer algorithms for the failure analysis of ceramic matrix composites under monotonically increasing loads. The algorithms will be included in a postprocessor to general purpose finite element programs.

Tripp, David E.↗

Microfracture in high temperature metal matrix laminates

Computational simulation procedures are described to evaluate the composite microfracture behavior, establish the hierarchy/sequence of fracture modes, and the influence of compliant layers and partial debonding on composite properties and microfracture initiation. These procedures are based upon three-dimensional finite element analysis and composite micromechanics equations. Typical results for the effects of compliant layers and partial debonding, microfracture initiation, and propagation and the thermomechanical cyclic loading on a SiC/Ti15 composite system are presented and discussed. The results show that interfacial debonding follows fiber or matrix fracture, and the thermomechanical cyclic loading severely degrades the composite integrity.

Mital, Subodh K.↗

Basic failure mechanisms in advanced composites

The fundamental failure mechanisms which result from the interaction of thermal cycling and mechanical loading of carbon-epoxy composites were studied. This work was confined to epoxy resin uniderictionally reinforced with HTS carbon fibers, and consists of first identifying local fiber, matrix and interface failure mechanisms using the model composite specimen containing a small number of fibers so that optical techniques can be used for characterization. After the local fracture process has been established for both mechanical loading and thermal cycling, engineering composite properties and gross fracture modes are then examined to determine how the local events contribute to real composite performance. Flexural strength in high fiber content specimens shows an increase in strength with increased thermal cycling. Similar behavior is noted for 25 v/o material up to 200 cycles; however, there is a drastic reduction after 200 cycles indicating a major loss of integrity probably through the accumulation of local cleavage cracks in the tensile region.

Mazzio, V. F.↗

Development of a heterogeneous laminating resin system

The factors which effect the impact resistance of laminating resin systems and yet retain equivalent performance with the conventional 450 K curing epoxy matrix systems in other areas were studied. Formulation work was conducted on two systems, an all-epoxy and an epoxy/bismaleimide, to gain fundamental information on the effect formulation changes have upon neat resin and composite properties. The all-epoxy work involved formulations with various amounts and combinations of eight different epoxy resins, four different hardeners, fifteen different toughening agents, a filler, and a catalyst. The epoxy/bismaleimide effort improved formulations with various amounts and combinations of nine different resins, four different hardeners, eight different toughening agents, four different catalysts, and a filler. When a formulation appeared to offer the proper combination of properties required for a laminating resin Celion 3K-70P fabric was prepregged. Initial screening tests on composites primarily involved Gardner type impact and measurement of short beam shear strengths under dry and hot/wet conditions.

Biermann, T. F.↗

Expansion of the Direct Feed High-Level Waste Glass Composition in the High Al Range

Baseline glass compositions have been developed and demonstrated for successful immobilization of Hanford high-level waste (HLW) prepared through a pretreatment process. Recent enhanced waste glass formulations have shown promise to increase the waste loading of pretreated sludge compositions from a broader range of HLW feeds. This project proposes to increase the loading of minimally pretreated Hanford HLW in glass by expanding the existing database and glass property-composition models. Estimated direct-feed high level waste (DFHLW) compositions were generated by the Hanford Tank Operations Contractor and used by Pacific Northwest National Laboratory to determine target glass compositions. Gaps in existing data were identified including one high-priority gap in the high Al compositional region. This report summarizes the data collected during the characterization of the DFHLW High Al Glass Matrix. These glasses were intentionally designed with high aluminum concentrations (15 to 30 wt%) and a high likelihood of nepheline formation, which is known to negatively affect glass durability. Some glasses were expected to either fail or approach property constraints to fill data gaps in poorly understood regions of the compositional space due to lack of data. Out of the 50 glasses tested, 14 glasses formed nepheline, while the model predicted nepheline formation in 20 glasses. All quenched glasses met the product consistency test durability constraint; however, 8 glasses failed this constraint after undergoing the canister centerline cooling treatment. Additionally, 17 glasses did not meet the viscosity constraints, 4 failed the EC constraints, and 2 exceeded the allowable T2% for spinel crystal formation. All glasses satisfied the SO 3 solubility limit. The resulting dataset provides valuable information to improve model accuracy and reduce prediction uncertainty. These insights will ultimately support the development of more robust glass formulation strategies, enabling higher waste loadings, reducing operational risks, and expanding the processing envelope.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Waste Glass Property Database and Data Qualification Plan

The U.S. Department of Energy vitrification facilities currently employ glass property-composition models to ensure processability of waste streams and acceptability of the final glass products. The efficiency (e.g., process flexibility, reduced down time, and reduced cost) of waste vitrification is directly tied to the size of the waste processing envelope. To increase the size of the processing envelope, a larger database was developed. The database will improve the prediction accuracy of glass properties, leading to higher waste loadings, higher waste throughput, broader process flexibility, and reduced mission life. Some of the data in this expanded database has insufficient quality assurance (QA) rigor for use in nuclear facility operation and glass qualification. A plan was developed to qualify high-value data under the appropriate QA rigor for use at the Hanford Waste Treatment and Immobilization Plant’s High-Level Waste (HLW) Facility. This qualification plan first compares the data coverage over the composition region of interest to Hanford HLW by property. Those studies that significantly improve the data coverage in the Hanford HLW glass composition region were prioritized for qualification activities. Qualification methods including QA equivalence, peer review, data corroboration, and confirmatory testing have been assigned to each high-priority study.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

High Solids Loading Aqueous Slurry Formation of Corn Stover Before Pretreatment in a Fed-batch Bioreactor

With the increase on population the world will depend on renewable sources to meet the increasingly energy needs. Use of lignocellulosic biomass as a renewable source has been proven efficient for conversion to cellulosic ethanol and capable of contributing to achieve the threshold on energy demand while reducing greenhouse gases in 90% when compared with fossil fuels (Wang et al., 2007, 2012). However, the processing of biomass encounters limitations in feeding and flow within biorefineries due to the system plugging by compaction and slurry high yield stress, preventing transport of biomass materials and in some cases unexpected plant shutdowns that results in high operational costs (dos Santos et al., 2021; Ximenes et al., 2021). Different solutions for biomass handling and slurry formation from densified materials like pellets have been studied. Cellulosic biomass residues are typically processed in pretreatment reactors to which acid or base is added (Humbird et al., 2002). Other pretreatments such as liquid hot water (LHW) and steam explosion that act without the addition of chemicals use pressures above the saturation vapor of water, to disrupt biomass structure (Ruiz et al., 2021). Although these methods are widely known, the use of pretreatments like acid digestion and LHW present challenges like waste disposal and could be energy inefficient (Mosier et al., 2005). Alternatively other approaches like enzymatic liquefaction have been applied for biomass transformation into slurries with promising results and without the use of pretreatments (dos Santos et al., 2021). Nevertheless, enzymatic liquefaction implementation faces difficulties due to the recalcitrant properties of biomass, its variability, and the release of enzyme inhibitors. While it has been proven that chemical composition properties in biomass have effects on enzyme inhibition (Huang et al., 2022; Kim et al., 2011; Zhai et al., 2018), hindering the efficiency of the liquefaction, not ample research has been conducted in understanding the physical properties as particle size, porosity, water adsorption retention and their effect in the ability to form a slurry at high solids concentration (Yan et al., 2020). In order to improve lignocellulosic biomass handling and formation of biomass slurries, enzyme assisted liquefaction for slurry creation from corn stover at solids loadings up to 30% is reported in this work. Two different kinds of biomass (pelleted corn stover and cobs) were liquefied in a fed-batch process using commercial enzymes Celluclast 1.5L or Ctec-2 at 1FPU or 3 FPU per gram of dry solids in 10 mM sodium citrate buffer solution (pH 4.8). Pellets were fed into a 1 L stirred bioreactor according to a predefined fed-batch protocol over the first 5 hours until reaching 30% of solids loading. After 6, 24 and 96 hours, samples were taken and characterized with respect to their sugar composition, rheology and water absorption. Successful slurry creation with dramatically reduced yield stress was achieved for corn stover for both assessed enzymes. Yield stresses of 178±7 Pa (3 FPU, Celluclast 1.5L) and 79±6 Pa (3 FPU, Ctec-2) were measured for corn stover at 24 hours, compared to 6,000 Pa for samples without enzyme. Yield stress was 155± 29 Pa (3FPU, Ctec-2) and 257 ± 72 Pa (1 FPU, Celluclast 1.5L) for corn cobs at 24 hours. Yield stress decreased when residence time increased with an enhanced fluidity noted for higher enzyme concentrations. A profile for 6, 24 and 96h of yield stress measurements is presented.

Gutierrez, Diana↗

Chemistry and adhesive properties of poly(arylene ether)s containing heterocyclic units

Novel poly(arylene ether)s containing heterocyclic units were prepared, characterized, and evaluated as adhesives and composite matrices. The polymers were prepared by reacting a heterocyclic bisphenol with an activated aromatic dihalide in a polar aprotic solvent, using potassium carbonate. The polymerizations were generally carried out in N,N-dimethylacetamide at 155 C. In some cases, where the polymers were semicrystalline, higher temperatures and thus higher boiling solvents were necessary to keep the polymers in solution. Heterocyclic rings incorporated into the poly(arylene ether) backbone include phenylquinoxaline, phenylimidazole, benzimidazole, benzoxazole, 1,3,4-oxadiazole, and 1,2,4-triazole. The polymers were characterized by differential scanning calorimetry, solution viscosity, X-ray diffraction, thin film, and adhesive and (in some cases) composite properties. The glass transition temperatures, crystalline melt temperature, solubility, and mechanical properties varied depending upon the heterocyclic ring. The chemistry and properties of these materials are discussed.

Connell, John W.↗

Influence of Chemical Composition on Rupture Properties at 1200 Degrees F. of Forged Chromium-Cobalt-Nickel-Iron Base Alloys in Solution-Treated and Aged Condition

The influence of systematic variations of chemical composition on rupture properties at 1200 degrees F. was determined for 62 modifications of a basic alloy containing 20 percent chromium, 20 percent nickel, 20 percent cobalt, 3 percent molybdenum, 2 percent tungsten, 1 percent columbium, 0.15 percent carbon, 1.7 percent manganese, 0.5 percent silicon, 0.12 percent nitrogen and the balance iron. These modifications included individual variations of each of 10 elements present and simultaneous variations of molybdenum, tungsten, and columbium. Laboratory induction furnace heats were hot-forged to round bar stock, solution-treated at 2200 degrees F., and aged at 1400 degrees F. The melting and fabrication conditions were carefully controlled in order to minimize all variable effects on properties except chemical composition. Information is presented which indicates that melting and hot-working conditions play an important role in high-temperature properties of alloys of the type investigated.

Reynolds, E E↗

Impact of Material and Architecture Model Parameters on the Failure of Woven Ceramic Matrix Composites (CMCs) via the Multiscale Generalized Method of Cells

It is well known that failure of a material is a locally driven event. In the case of ceramic matrix composites (CMCs), significant variations in the microstructure of the composite exist and their significance on both deformation and life response need to be assessed. Examples of these variations include changes in the fiber tow shape, tow shifting/nesting and voids within and between tows. In the present work, the effects of many of these architectural parameters and material scatter of woven ceramic composite properties at the macroscale (woven RUC) will be studied to assess their sensitivity. The recently developed Multiscale Generalized Method of Cells methodology is used to determine the overall deformation response, proportional elastic limit (first matrix cracking), and failure under tensile loading conditions. The macroscale responses investigated illustrate the effect of architectural and material parameters on a single RUC representing a five harness satin weave fabric. Results shows that the most critical architectural parameter is weave void shape and content with other parameters being less in severity. Variation of the matrix material properties was also studied to illustrate the influence of the material variability on the overall features of the composite stress-strain response.

Liu, Kuang C.↗