Surface radicals in silane/hydrogen discharges
Using threshold ionization mass spectrometry, radical densities have been measured at the substrate surface of a radio frequency discharge in silane plus hydrogen vapor. The conditions are 100-300 Pa pressure and a ratio (R) of hydrogen flow/silane flow typical of discharges used to produce large area amorphous (R=20) and microcrystalline (R=40) silicon. For comparison, we include measurements in pure-silane vapor. The neutral radicals observed in the mixed gases are H, SiH{sub 3}, Si{sub 2}H{sub 2}, and Si{sub 2}H{sub 5}, with decreasing flux in that order. (Si{sub 2}H{sub 4} is also seen in pure silane and SiH{sub 2} for R=20.) The H flux is sufficient for major film etching and restructuring, particularly for R=40. The ion-bombardment species were also measured, establishing that Si{sub y}H{sub n}{sup +} (y=1-3) ion flux is much larger than the H{sub n}{sup +} (n=1-3) flux. The ion flux provides 15{+-}4% of the total Si flux to the film for R=20 and 37{+-}10% for R=40. This is larger than in pure-silane discharges, and it may be very important to film properties due to the impact energy.