Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “WEAR”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 235 records · Page 13

Completion of the Long Duration Wear Test of the NASA HERMeS Hall Thruster

The NASA Hall Effect Rocket with Magnetic Shielding (HERMeS) 12.5-kW Hall thruster has been the subject of extensive technology maturation by NASA GRC and JPL in preparation for development into a flight propulsion system. As part of this effort, a series of wear tests have been conducted to identify erosion phenomena and the accompanying failure modes as well as to validate service-life models for magnetically-shielded thrusters. This work presents a summary of the results obtained during the Long Duration Wear Test (LDWT), which was the third in this wear test series. The LDWT accumulated approximately 3,570 hours of operation and had the overall goal to identify and correct design or facility issues prior to the flight qualification campaign. Thruster performance, stability, and plume properties were invariant throughout the duration of the LDWT and consistent with measurements acquired during previous HERMeS performance and wear characterizations. Average erosion rates of a carbon-carbon composite pole cover were found to match those measured with graphite to within the empirical uncertainty while the previously observed time-dependence of pole cover erosion rates was linked to changes in pole cover roughness. Azimuthal variations in keeper wear rate were observed including deposition on one of the azimuthal-facing sides of the keeper mask. This strongly suggests the presence of an azimuthal component in the process driving keeper erosion.

Frieman, Jason D.↗

Completion of the Long Duration Wear Test of the NASA HERMeS Hall Thruster

The NASA Hall Effect Rocket with Magnetic Shielding (HERMeS) 12.5-kW Hall thruster has been the subject of extensive technology maturation by NASA GRC and JPL in preparation for development into a flight propulsion system. As part of this effort, a series of wear tests have been conducted to identify erosion phenomena and the accompanying failure modes as well as to validate service-life models for magnetically-shielded thrusters. This work presents a summary of the results obtained during the Long Duration Wear Test (LDWT), which was the third in this wear test series. The LDWT accumulated approximately 3,570 hours of operation and had the overall goal to identify and correct design or facility issues prior to the flight qualification campaign. Thruster performance, stability, and plume properties were invariant throughout the duration of the LDWT and consistent with measurements acquired during previous HERMeS performance and wear characterizations. Average erosion rates of a carbon-carbon composite pole cover were found to match those measured with graphite to within the empirical uncertainty while the previously observed time-dependence of pole cover erosion rates was linked to changes in pole cover roughness. Azimuthal variations in keeper wear rate were observed including deposition on one of the azimuthal-facing sides of the keeper mask. This strongly suggests the presence of an azimuthal component in the process driving keeper erosion.

Frieman, Jason D.↗

Completion of the Long Duration Wear Test of the NASA HERMeS Hall Thruster

The NASA Hall Effect Rocket with Magnetic Shielding (HERMeS) 12.5-kW Hall thruster has been the subject of extensive technology maturation by NASA GRC and JPL in preparation for development into a flight propulsion system. As part of this effort, a series of wear tests have been conducted to identify erosion phenomena and the accompanying failure modes as well as to validate service-life models for magnetically-shielded thrusters. This work presents a summary of the results obtained during the Long Duration Wear Test (LDWT), which was the third in this wear test series. The LDWT accumulated approximately 3,570 hours of operation and had the overall goal to identify and correct design or facility issues prior to the flight qualification campaign. Thruster performance, stability, and plume properties were invariant throughout the duration of the LDWT and consistent with measurements acquired during previous HERMeS performance and wear characterizations. Average erosion rates of a carbon-carbon composite pole cover were found to match those measured with graphite to within the empirical uncertainty while the previously observed time-dependence of pole cover erosion rates was linked to changes in pole cover roughness. Azimuthal variations in keeper wear rate were observed including deposition on one of the azimuthal-facing sides of the keeper mask. This strongly suggests the presence of an azimuthal component in the process driving keeper erosion.

Jason David Frieman↗

Experimental Investigation of Friction and Wear Behavior of 304L Stainless Steel Sliding Against Different Counterface in Dry Contact

In this study, friction and wear behavior of 304L stainless steel sliding against different ball counterface under dry contact was investigated. Tests were conducted using a ball-on-flat contact configuration in reciprocating sliding with 440C stainless steel, Al alloy (2017) and bronze ball counterfaces under different loads. Detailed surface analysis was also done using 3-D profilometry technique and optical microscopy in order to determine wear mechanism and dimension. All the pairs exhibited initial rapid increase in coefficient of friction after which a variety of friction behavior, depending on the ball counterface, was observed. The flat and the ball counterface in 304L stainless steel-440C stainless steel pair showed wear that was proportional to applied load. In both 304L stainless steel-Al alloy (2017) and 304L stainless steel-bronze pairs, ball samples showed severe wear that was proportional to the applied load while material transfer from the different balls occurred in the flat. The study concluded that friction and wear were not material properties but a kind of responses that characterize a pair of surfaces in contact undergoing relative motion.

Olofinjana, Bolutife↗

Method and apparatus for providing thermal wear leveling

Exemplary embodiments provide thermal wear spreading among a plurality of thermal die regions in an integrated circuit or among dies by using die region wear-out data that represents a cumulative amount of time each of a number of thermal die regions in one or more dies has spent at a particular temperature level. In one example, die region wear-out data is stored in persistent memory and is accrued over a life of each respective thermal region so that a long term monitoring of temperature levels in the various die regions is used to spread thermal wear among the thermal die regions. In one example, spreading thermal wear is done by controlling task execution such as thread execution among one or more processing cores, dies and/or data access operations for a memory.

Roberts, David A.↗

Method and apparatus for providing thermal wear leveling

Exemplary embodiments provide thermal wear spreading among a plurality of thermal die regions in an integrated circuit or among dies by using die region wear-out data that represents a cumulative amount of time each of a number of thermal die regions in one or more dies has spent at a particular temperature level. In one example, die region wear-out data is stored in persistent memory and is accrued over a life of each respective thermal region so that a long term monitoring of temperature levels in the various die regions is used to spread thermal wear among the thermal die regions. In one example, spreading thermal wear is done by controlling task execution such as thread execution among one or more processing cores, dies and/or data access operations for a memory.

Roberts, David A.↗

Mechanical, corrosion, and wear properties of biomedical Ti–Zr–Nb–Ta–Mo high entropy alloys

The microstructures, mechanical, corrosion, and wear behaviors of the Ti x ZrNbTaMo (x = 0.5, 1, 1.5, and 2, molar ratio) high entropy alloys (HEAs) were studied in this work. It was found that the Ti–Zr–Nb–Ta–Mo HEAs showed a dendrite structure with two body-centered-cubic (BCC) solid solution phases. The Ti 0.5 ZrNbTaMo HEA exhibited a high hardness of about 500 HV, high compressive strength approaching 2,600 MPa, and large plastic strain of over 30%. Furthermore, the highly-protective oxide films formed on the surface of Ti–Zr–Nb–Ta–Mo HEAs in the phosphate buffer saline (PBS) solution, which resulted in the high corrosion resistance of the HEAs. The Ti–Zr–Nb–Ta–Mo HEAs exhibited the greater dry- and wet-wear resistance than that of the traditional biomedical Ti6Al4V alloy. The results also indicated that with the decrease in the Ti content, the wear resistance of the Ti–Zr–Nb–Ta–Mo HEAs in the PBS solution improved. Finally, the Ti 0.5 ZrNbTaMo alloy presented the highest corrosive wear resistance among the four HEAs owing to its combination of good mechanical properties and high chemical stability.

36 MATERIALS SCIENCE↗

Microstructure and wear properties of Fe-VC-Cr{sub 7}C{sub 3} composite coating on surface of cast steel

An Fe-VC-Cr{sub 7}C{sub 3} composite coating on the surface of cast steel was produced by a novel metal-coated casting technique. The microstructure and wear properties of the product were studied by means of X-ray diffraction, electron beam probe, scanning electron microscopy, and wear testing. The results show that the composite coating consisted of VC and Cr{sub 7}C{sub 3} as the reinforcing phases and {alpha}-Fe as the matrix. The composite coating was metallurgically bonded to the cast steel substrate. The quantity of VC and Cr{sub 7}C{sub 3} carbides decreased gradually from the top surface of the composite coating to the cast steel substrate. The Fe-VC-Cr{sub 7}C{sub 3} composite coating displayed excellent wear-resistance under dry sliding wear test conditions.

36 MATERIALS SCIENCE↗

On the role of processing parameters in producing Cu/SiC metal matrix composites via friction stir processing: Investigating microstructure, microhardness, wear and tensile behavior

The main aim of this study is to produce copper reinforced metal matrix composite (MMC) layers using micron sized SiC particles via friction stir processing (FSP) in order to enhance surface mechanical properties. Microstructural evaluation using optical microscopy (OM) and scanning electron microscopy (SEM) indicated that an increase in traverse speed and a decrease in rotational speed cause a reduction in the grain size of stir zone (SZ) for the specimens friction stir processed (FSPed) without SiC particles. With the aim of determining the optimum processing parameters, the effect of traverse speed as the main processing variable on microstructure and microhardness of MMC layers was investigated. Higher traverse speeds resulted in poor dispersion of SiC particles and consequently reduced the microhardness values of MMC layers. It was found that upon addition of SiC particles, wear properties were improved. This behavior was further supported by SEM images of wear surfaces. Results demonstrated that the microcomposite produced by FSP exhibited enhanced wear resistance and higher average friction coefficient in comparison with pure copper. Tensile properties and fracture characteristics of the specimens FSPed with and without SiC particles and pure copper were also evaluated. According to the results, the MMC layer produced by FSP showed lower strength and elongation than pure copper while a remarkable elongation was observed for FSPed specimen without SiC particles. Research Highlights: {yields} Decrease in traverse speed leads to good dispersion of SiC particles in composites. {yields} No distinct TMAZ in side regions of SZ of FSPed specimens with SiC particles. {yields} Microhardness of FSPed specimens with SiC particles shows a remarkable increase. {yields} Reinforcement of Cu with SiC particles improves wear and friction behavior of surface. {yields} A weak bonding in tensile due to probable agglomeration for SiC containing samples.

36 MATERIALS SCIENCE↗

Effect of vanadium carbide on dry sliding wear behavior of powder metallurgy AISI M2 high speed steel processed by concentrated solar energy

Mixtures of AISI M2 high speed steel and vanadium carbide (3, 6 or 10 wt.%) were prepared by powder metallurgy and sintered by concentrated solar energy (CSE). Two different powerful solar furnaces were employed to sinter the parts and the results were compared with those obtained by conventional powder metallurgy using a tubular electric furnace. CSE allowed significant reduction of processing times and high heating rates. The wear resistance of compacts was studied by using rotating pin-on-disk and linearly reciprocating ball-on-flat methods. Wear mechanisms were investigated by means of scanning electron microscopy (SEM) observations and chemical inspections of the microstructures of the samples. Better wear properties than those obtained by conventional powder metallurgy were achieved. The refinement of the microstructure and the formation of carbonitrides were the reasons for this. - Highlights: •Powder metallurgy of mixtures of M2 high speed steel and VC are studied. •Some sintering is done by concentrated solar energy. •Rotating pin-on-disk and linearly reciprocating ball-on-flat methods are used. •The tribological properties and wear mechanisms, under dry sliding, are studied.

36 MATERIALS SCIENCE↗

Material Characterization-Based Wear Mechanism Investigation for Biomass Hammer Mills

Biomass, as harvested, is composed of inorganic compounds both intrinsically and extrinsically and can be abrasive. The present study investigates the wear modes and mechanisms of two types of blades of hammer mills used in biomass size reduction (impacting the particle size and distribution) and densification (impacting the size, shape, and density). The dominant wear modes for the stage 1 steel blades are determined to be erosive and polishing wear. For the stage 2 blades with a carbide weld overlay, the main wear mechanisms are erosion and fracture. Partial replacement of Co by Fe in the outer layer of the carbide grits, likely induced by diffusion during high-temperature welding, has been correlated to the observed microcracking. Finally, the microcracking is believed to weaken the grit strength and fracture toughness to make the overlay prone to fracture and erosion due to repetitive contact with the inorganic contents in chopping biomass.

42 ENGINEERING↗

The Effect of Li Additions on Wear Properties of Al-Mg{sub 2}Si Cast In-situ Composites

Wear rate of a modified Al-Mg{sub 2}Si composite was studied by the use of a conventional pin-on-disc technique. In-situ Al-Mg{sub 2}Si composites (15, 20, 25 wt.%) were cast in a simple cylindrical mold. 0.3 wt.% Li was added into the molten composite to modify its microstructure. It has been found that Li addition decreases the mean size of primary Mg{sub 2}Si particles. The wear behavior of different composites at different rates revealed that Li addition increases the wear properties of Al-15%Mg{sub 2}Si to some extent but it did not have any significant influence on wear properties of two other composites.

36 MATERIALS SCIENCE↗

Impact of tool wear on joint strength in friction stir spot welding of DP 980 steel

Friction stir spot welding has been shown to be a viable method of joining ultra high strength steel (UHSS), both in terms of joint strength and process cycle time. However, the cost of tooling must be reasonable in order for this method to be adopted as an industrial process. Recently a new tool alloy has been developed, using a blend of PCBN and tungsten rhenium (W-Re) in order to improve the toughness of the tool. Wear testing results are presented for two of these alloys: one with a composition of 60% PCBN and 40% W-Re, and one with 70% PCBN and 30% W-Re. The sheet material used for all wear testing was 1.4 mm DP 980. Lap shear testing was used to show the relationship between tool wear and joint strength. The Q70 tool provided the best combination of wear resistance and joint strength.

36 MATERIALS SCIENCE↗

Effects of self-assembled monolayer and PFPE lubricant on wear characteristics of flat silicon tips.

The effects of self-assembled monolayer (SAM) and perfluoropolyether (PFPE) lubricant on the wear characteristics of flat silicon tips were investigated. The wear test consisted of sliding the silicon tips fabricated on a flat silicon specimen against SAM and PFPE (Z-tetraol) coated silicon (100) wafer. The tips were slid at a low speed for about 15 km under an applied load of 39.2 {micro}N. The wear volume of the tip was obtained by measuring the tip profile using an Atomic Force Microscope (AFM). It was found that the coatings were effective in reducing the wear of the tips by an order of magnitude from 10{sup -6} to 10{sup -7}.

36 MATERIALS SCIENCE↗

Effects of Laser Energies on Wear and Tensile Properties of Biomimetic 7075 Aluminum Alloy

Inspired by the non-smooth surface of certain animals, a biomimetic coupling unit with various sizes, microstructure, and hardness was prepared on the surface of 7075 aluminum alloy. Following experimental studies were conducted to investigate the wear and tensile properties with various laser energy inputs. The results demonstrated that the non-smooth surface with biomimetic coupling units had a positive effect on both the wear resistance and tensile property of 7075 aluminum alloy. In addition, the sample with the unit fabricated by the laser energy of 420.1 J/cm{sup 2} exhibited the most significant improvement on the wear and tensile properties owing to the minimum grain size and the highest microhardness. Also, the weight loss of the sample was one-third of the untreated one’s, and the yield strength, the ultimate tensile strength, and the elongation improved by 20, 20, and 34% respectively. Moreover, the mechanisms of wear and tensile properties improvement were also analyzed.

36 MATERIALS SCIENCE↗

Effect of Reduced Graphene Oxide Reinforcement on the Wear Characteristics of Electroless Ni-P Coatings

Electroless composite coatings with various concentrations of reduced graphene oxide (rGO) particles were deposited onto mild steel substrate. The effects of adding rGO particles by varying their concentration from 0 to 100 mg/L on morphology, composition, microhardness, adhesion, wear and friction of the electroless composite coatings were investigated. Among the various parameters that influence the tribological behavior, sliding velocity was varied within a specific range for definite concentrations of rGO to obtain enhanced wear resistance in this study. The micrographs of the worn surfaces and indented spots were examined for the nature of wear mechanism and interfacial adhesion. The wear rate increased with increasing sliding velocity but was relatively stable for coatings with lower concentrations of rGO.

77 NANOSCIENCE AND NANOTECHNOLOGY↗

Parametric Optimization of Erosive Wear Response of TiAlN-Coated Aluminium Alloy Using Taguchi Method

In this research work, high-velocity oxy-fuel thermal spraying is used to develop TiAlN coatings on AA1050 and AA5083 aluminium alloy substrates. Slurry wear behavior of coatings is evaluated using jet-type test rig. Surface studies were carried out to investigate the potential erosion mechanism. The influence of key parameters identified using the Taguchi analysis is also corroborated with a wear model. The potential mechanism identified by wear model is in excellent convergence with that observed experimentally. Mixed ploughing and cutting, formation of platelets, abrasion grooves and cracks are witnessed as primary mechanisms causing loss of coating. Results indicate that impact velocity is recognized as a highly contributing parameter with contribution ratio of 79.24 and 83.75% followed by impingement angle with contribution ratio of 15.81 and 11.58% for AA1050 and AA5083, respectively. The important sequences of the control parameters are recognized to be impact velocity > impingement angle > erodent feed rate > erodent size for AA1050 and impact velocity > impingement angle > erodent size > erodent feed rate for AA5083. The best possible combination of control parameters for AA1050 and AA5083 to achieve minimal wear rate with respect to impact velocity, erodent size, impingement angle and erodent feed rate is 30 m/s, 225 µm, 30°, 160 g/min and 25 m/s, 150 µm, 30°, 160 g/min, respectively.

36 MATERIALS SCIENCE↗

Processing, As-Cast Microstructure and Wear Characteristics of a Monotectic Al-Bi-Cu Alloy

Ternary Al-based monotectic alloys have a good combination of wear resistance and mechanical strength. While self-lubricating soft elements guarantee an adequate wear resistance, the modification with third elements can increase the ability to support load. In the present investigation, a collection of microstructures is generated through transient directional solidification of the Al-3.2wt.%Bi-3.0wt.%Cu alloy. Samples with different Bi spacing have been subjected to micro-adhesive wear ball tests. A relationship linking the wear volume, V, the microstructural spacing and the test time is proposed for Bi spacing higher than 16 μm, according to which V decreases with the decrease in Bi spacing. It is observed that wider and deeper grooves emerged on the surface of the samples related to more refined Bi and Al{sub 2}Cu phases, that is, associated with Bi spacing and Bi diameter lower than 16 and 2.4 μm, respectively. A reverse trend is noted for these finer microstructures, for which V increases with further decrease in Bi spacing. This can be caused by the detachment of the very fine and less cohesive Al{sub 2}Cu lamellas as the Al{sub 2}O{sub 3} oxide breaks up forming debris, with the presence of these lamellas as loose debris at the interface acting as third-body abrasives.

36 MATERIALS SCIENCE↗