At least 235 records · Page 13

Preparation and crystal structure of a new tin titanate containing Sn{sup 2+}; Sn{sub 2}TiO{sub 4}

Single crystals of a new tin titanate containing Sn{sup 2+}, Sn{sub 2}TiO{sub 4} was prepared by high temperature reaction in an evacuated quartz tube and its crystal structure was determined by single crystal X-ray diffraction data. The tin titanate crystallizes in the tetragonal space group P4{sub 2}/mbc with a = 8.490(2) and c = 5.923(3) A, Z = 4 and the final R factors are R = 0.0497 and R{sub w} = 0.0676 for 354 unique reflections. This tin titanate is isostructural with the low temperature form of Pb{sub 3}O{sub 4}(Pb{sub 2}{sup 2+}Pb{sup 4+}O{sub 4}). This compound was oxidized above 600 deg. C accompanying the mass gain and finally changed to rutile-type solid solution (Sn,Ti)O{sub 2}.

36 MATERIALS SCIENCE↗

Alkaline earth metal doped tin oxide as a novel oxygen storage material

Alkaline earth metal doped tin oxide (SnO{sub 2}) hollow nanospheres with a diameter of 50 nm have been synthesized successfully via a facial solvothermal route in a very simple system composed of only ethanol, acetic acid, SnCl{sub 4}·5H{sub 2}O and A(NO{sub 3}){sub 2}·xH{sub 2}O (A = Mg, Ca, Sr, Ba). The synthesized undoped SnO{sub 2} and A-doped SnO{sub 2} hollow nanospheres were characterized by the oxygen storage capacity (OSC), X-ray diffraction, transmission electron microscopy and the Brunauer–Emmet–Teller (BET) technique. The OSC values of all samples were measured using thermogravimetric-differential thermal analysis. The incorporation of alkaline earth metal ion into tin oxide greatly enhanced the thermal stability and OSC. Especially, Ba-doped SnO{sub 2} hollow nanospheres calcined at 1000 °C for 20 h with a BET surface area of 61 m{sup 2} g{sup −1} exhibited the considerably high OSC of 457 μmol-O g{sup −1} and good thermal stability. Alkaline earth metal doped tin oxide has the potential to be a novel oxygen storage material.

36 MATERIALS SCIENCE↗

The formation of tin oxides in thin-film Sn/C/KCl(100) structures

The formation of oxides upon the thermal annealing (both in air and vacuum) of island tin films grown on a KCl(100) substrate, which was coated by a thin layer of amorphous carbon, has been investigated by transmission electron microscopy. It is established that thermal annealing at temperatures below the tin melting point (T{sub m}) does not lead to phase transitions with the formation of new crystalline oxide phases. At the same time, the films undergo structural changes: the average size of blocks in the substrate plane decreases compared to those in an as-deposited film. Thermal annealing in air at temperatures above the tin melting point leads to the formation of multiphase oxide structures and increases the average size of blocks and islands in the substrate plane. It is shown that preliminary thermal annealing in air at temperatures below T{sub m} hinders oxidation upon subsequent heat treatment.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

States of antimony and tin atoms in lead chalcogenides

It is shown by Moessbauer spectroscopy of the {sup 119}Sb({sup 119m}Sn) isotope that impurity antimony atoms in PbS, PbSe, and PbTe lattices are distributed between cation and anion sublattices. In n-type samples, the greatest part of antimony is located in the anion sublattice; in hole ones, in the cation sublattice. The tin atoms formed as a result of radioactive decay of {sup 119}Sb (antisite state) are electrically inactive in the anion sub-lattice of PbS and PbSe, while, in the cation sublattice, they form donor U{sup -} centers. Electron exchange between the neutral and doubly ionized tin U{sup -} centers via the allowed band states is observed. The tin atoms formed after radioactive decay of {sup 119}Sb are electrically inactive in the anion and cation sublattices of PbTe.

36 MATERIALS SCIENCE↗

Electron exchange between tin impurity U{sup –} centers in PbS{sub z}Se{sub 1–z} alloys

Using emission {sup 119mm}Sn({sup 119m}Sn) and {sup 119}Sb({sup 119m}Sn) Mössbauer spectroscopy, it is shown that impurity tin atoms in PbS{sub z}Se{sub 1–z} alloys substitute lead atoms and are two-electron donors with negative correlation energy (U{sup –} centers). It is found that the energy levels related to impurity tin atoms are in the lower half of the band gap at z ≥ 0.5 against the background of allowed valence-band states at z ≤ 0.4. The electron exchange between neutral and doubly ionized tin U{sup –} centers in partially compensated Pb{sub 0.99}Sn{sub 0.005}Na{sub 0.005}S{sub z}Se{sub 1–z} alloys is studied. The activation energy of this process decreases from 0.111(5) eV for a composition with z = 1 to 0.049(5) eV for compositions with c ≤ 0. For all z, the exchange is implemented via the simultaneous transfer of two electrons using delocalized valence-band states.

36 MATERIALS SCIENCE↗

Observations of Shock-Loaded Tin and Zirconium Surfaces with Single-Pulse X-ray Diffraction

A single-pulse X-ray diffraction (XRD) diagnostic has been developed for the investigation of shocked material properties on a very short time scale. The diagnostic, which consists of a 37-stage Marx bank high-voltage pulse generator coupled to a needle-and-washer electron beam diode via coaxial cable, produces line-and-bremsstrahlung X-ray emission in a 40 ns pulse. The molybdenum anode produces 0.71 Å characteristic K lines used for diffraction. The X-ray beam passes through a pinhole collimator and is incident on the sample with an approximately 2 mm×5 mm spot and 1° full width at half maximum angular divergence. Coherent scattering from the sample produces a Debye-Scherrer diffraction pattern on an image plate located at 75 mm from the polycrystalline sample surface. An experimental study of the polycrystalline structures of zirconium and tin under high-pressure shock loading has been conducted with single-pulse XRD. The experimental targets were 0.1-mm-thick foils of zirconium and tin using 0.4-mm-thick vitreous carbon back windows for shock loading, and the shocks were produced by either Detasheet or PBX-9501 high explosives buffered by 1-mm-thick 6061-T6 aluminum. The diffraction patterns from both shocked zirconium and tin indicated a phase transition into a polymorphic mix of amorphous and new solid phases.

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗

Influence of current density on microstructure of pulse electrodeposited tin coatings

Pulse electrodeposited tin coatings on copper substrate have been synthesized from an aqueous solution containing sodium stannate (Na{sub 2}SnO{sub 3}.3H{sub 2}O) and sodium hydroxide (NaOH). The effect of current density on surface morphology of the deposits has been investigated. As deposited coatings are characterized by X-ray diffraction, scanning electron microscopy, electron backscatter diffraction, and line profile analysis. The X-ray diffraction analysis shows that the deposits consist of tetragonal ({beta}-Sn) structure with microcrystalline grains. The deposits plated at lower current density exhibit (110) texture which decreases with increasing current densities. The effects of current density on Cu-Sn diffusion and whisker growth of the electrodeposited tin coatings are also reported here. - Highlights: Black-Right-Pointing-Pointer Pulse electrodeposition of Sn from aqueous alkaline solution without adding any organic additive. Black-Right-Pointing-Pointer Effect of current density on morphology and whisker growth in tin coatings aged for 1 year. Black-Right-Pointing-Pointer Solution bath is stable and can be operated over a wide range of current density.

36 MATERIALS SCIENCE↗

Evolution of microstructure and grain boundary character distribution of a tin bronze annealed at different temperatures

Specimens cut from a rolled tin bronze sheet were annealed at 400–800 °C for 1 h and evolution of their microstructures was then characterized in details by electron channeling contrast imaging and electron backscatter diffraction techniques. Particularly, statistics on special boundaries (SBs) with Σ ≤ 29 and network connectivity of random high angle boundaries (HABs) in the annealed specimens were examined to probe optimization potentials of grain boundary character distribution (GBCD) for this material. Results show that the deformed microstructure in the as-received material begins to be recrystallized when the annealing temperature increase to 500 °C and average grain sizes surge with further increasing temperatures. As a result of the recrystallization, a large number of annealing twins (with Σ3 misorientation) are produced, leading to remarkably increased fractions of SBs (f{sub SBs}). Thanks to preexisting dense low angle boundaries, the majority of SBs in the 500 °C specimen with only partial recrystallization are Σ3{sub ic} (incoherent) boundaries, which effectively disrupt connectivity of random HABs network. Although the f{sub SBs} can be further increased (up to 72.5%) in specimens with full recrystallization (at higher temperatures), the Σ3{sub ic} boundaries would be replaced to some extent by Σ3{sub c} (coherent) boundaries which do not contribute directly to optimizing the GBCD. This work should be able to provide clear suggestions on applying the concept of grain boundary engineering to tin bronze alloys. - Highlights: • The rolled tin bronze begins to be recrystallized as temperature increases to 500 °C. • A lot of SBs are produced after recrystallization and the highest f{sub SBs} is 72.5%. • Partially recrystallized specimen has the optimum GBCD due to more Σ3{sub ic} boundaries. • The Σ3{sub ic} boundaries are replaced by Σ3{sub c} boundaries after full recrystallization.

36 MATERIALS SCIENCE↗

Solvothermal synthesis of carbon-coated tin nanorods for superior reversible lithium ion storage

Highlights: Black-Right-Pointing-Pointer Large-scale synthesis of Sn-C core-shell nanorods. Black-Right-Pointing-Pointer Facile template-engaged solvothermal approach. Black-Right-Pointing-Pointer The combination of tin with high specific capacity and carbon with good cycle life. Black-Right-Pointing-Pointer Relatively higher initial Coulombic efficiency and lithium storage capacities. -- Abstract: This paper reports the large-scale synthesis of carbon-coated tin (Sn-C) nanorods through a facile solvothermal carbonization approach by using Sn nanorods as templates and ethanol as a solvent. The as-synthesized Sn-C nanorods have been applied as anode materials for lithium-ion batteries. The Sn-C anode, which exhibits relatively higher initial Coulombic efficiency and lithium storage capacities, is more attractive than the previously reported tin oxide or sulfide anodes. The superior performance of the Sn-C nanorods makes it a promising anode material in high-energy density batteries.

36 MATERIALS SCIENCE↗

Synthesis of silicon nanowires using tin catalyst by hot wire chemical vapor processing

Highlights: ► Silicon nanowires are grown by hot wire chemical vapor processing at 400 °C using Sn as catalyst material via VLS. ► For nanowire synthesis Sn nanotemplates are formed with hot wire generated atomic hydrogen. ► The TEM image reveals the crystalline nature of nanowire. - Abstract: Silicon nanowires (SiNWs) have been synthesized at temperatures in the range 300–400 °C by the hot wire chemical vapor processing (HWCVP) using tin nanotemplate. The tin nano-template is formed by hot wire atomic hydrogen treatment of thermally evaporated Sn films (∼300 nm thick) on glass substrates. Silicon nanowires are then grown using hot wire induced dissociation of SiH{sub 4} gas over the nanotemplate. Growth conditions like growth time and temperature were varied to study their effect on the tin nanoparticle size and on the silicon nanowire dimensions thereafter. From the observations, it is clear that the nanowire diameters and lengths depend on the size of nanoparticles and the growth time respectively. Though SiNWs were observed to grow at temperatures as low as 300 °C, nanowires with a narrow diameter distribution were achieved at 400 °C. Raman spectra and transmission electron microscope (TEM) reveal the crystalline nature of the silicon nanowires.

36 MATERIALS SCIENCE↗

Influence of Fluorine incorporation on the photocatalytic activity of Tin Oxide thin films

Highlights: • Fluorine doped SnO{sub 2} thin films prepared by a facile homemade jet nebulizer spray pyrolysis technique. • XRD, XPS, PL, FESEM, AFM studies support the discussions. • The photocatalytic activities of the prepared tin oxide (TO) and FTO thin films for the degradation of MB aqueous solution were tested. . - Abstract: This work reports the photocatalytic activity of undoped tin oxide (TO) and F doped tin oxide (FTO) thin films for MB dye degradation under visible light irradiation. A facile homemade jet nebulizer spray pyrolysis technique was employed to prepare these samples. The results indicate that FTO film exhibits superior photocatalytic activity compared to TO film. Dye degradation of nearly 95% is achieved using FTO film at 90 min whereas TO film degrades only 78% of dye molecules in the same time interval. This enhancement for FTO films might be due to the generation of large number of free electrons caused by the fluorine incorporation. The mechanism behind the enhancement of photocatalytic activity of FTO films is discussed elaborately with the aid of optical and PL studies. The structure, composition and morphology of the samples were analyzed using XRD, XPS, FTIR, FESEM and AFM. The incorporation of F into SnO{sub 2} lattice is confirmed through FTIR analysis.

36 MATERIALS SCIENCE↗

Leaching studies for tin recovery from waste e-scrap

Printed circuit boards (PCBs) are the most essential components of all electrical and electronic equipments, which contain noteworthy quantity of metals, some of which are toxic to life and all of which are valuable resources. Therefore, recycling of PCBs is necessary for the safe disposal/utilization of these metals. Present paper is a part of developing Indo-Korean recycling technique consists of organic swelling pre-treatment technique for the liberation of thin layer of metallic sheet and the treatment of epoxy resin to remove/recover toxic soldering material. To optimize the parameters required for recovery of tin from waste PCBs, initially the bench scale studies were carried out using fresh solder (containing 52.6% Sn and 47.3% Pb) varying the acid concentration, temperature, mixing time and pulp density. The experimental data indicate that 95.79% of tin was leached out from solder material using 5.5 M HCl at fixed pulp density 50 g/L and temperature 90 Degree-Sign C in mixing time 165 min. Kinetic studies followed the chemical reaction controlled dense constant size cylindrical particles with activation energy of 117.68 kJ/mol. However, 97.79% of tin was found to be leached out from solder materials of liberated swelled epoxy resin using 4.5 M HCl at 90 Degree-Sign C, mixing time 60 min and pulp density 50 g/L. From the leach liquor of solder materials of epoxy resin, the precipitate of sodium stannate as value added product was obtained at pH 1.9. The Pb from the leach residue was removed by using 0.1 M nitric acid at 90 Degree-Sign C in mixing time 45 min and pulp density 10 g/L. The metal free epoxy resin could be disposed-of safely/used as filling material without affecting the environment.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Shifting Defect Self-Regulation via Disordered Vacancies in Hollow Tin Perovskites

Tin(II)-based hybrid halide perovskites typically suffer from severe self-doping behavior as a result of facile oxidation of Sn(II) to Sn(IV), leading to high carrier densities (holes) and metallic-like conductivities that limit their applications. In this contribution, we describe how substituting the large ethylenediammonium cation for methylammonium in the intentionally defective “hollow” perovskite family, MA 1−x en x Sn 1−0.7x I 3−0.4x (MA = methylammonium, en = ethylenediammonium), where 0 ≤ x ≤ 0.38, effectively minimizes the intrinsic self-doping behavior. The use of a solvent-free, mechanochemical synthesis route further circumvents oxidative side reactions typical in solution processing, enabling more precise control and understanding of both composition and defect chemistry. Dark and time-resolved microwave conductivity measurements of these materials as a function of “x” reveal two regimes of conductivity suppression: at low x incorporation (x ≤ 0.15), the carrier density decreases by an order of magnitude via defect-mediated charge compensation, while higher substitution (0.15 < x ≤ 0.38) greatly reduces the carrier mobility. At these lower substitution levels, the observations suggest that intrinsic equilibrium tin vacancies are compensated instead by ionic defects in lieu of mobile holes. For the higher substitution levels, the less mobile carriers exhibit long recombination lifetimes, consistent with polaron-mediated transport. These findings establish a strategy for relatively low iodine chemical potential synthesis and defect-driven control of the carrier concentration in tin halide perovskites, advancing the rational discovery of dopable hybrid semiconductors.

36 MATERIALS SCIENCE↗

Electrochemical Corrosion and Catalysis Dynamics of Tin Oxide during Water Oxidation

Metal oxide corrosion severely limits anodic electrocatalysis, particularly at high potentials in acidic environments, where degradation pathways remain poorly defined. This study establishes explicit connections between corrosion and electrocatalysis on tin oxide during water oxidation by examining the roles of lattice defects, reactive oxygen species, interfacial pH variations, and speciation of corroded tin in acid. We first demonstrate the presence of structural defects such as oxygen vacancies and substoichiometric Sn(II) species by integrating electron paramagnetic resonance spectroscopy, ultraviolet photoelectron spectroscopy, and Mott–Schottky analysis. Kohn–Sham density functional theory calculations reveal that explicit water structures thermodynamically stabilize reaction intermediates and lower reaction overpotentials. Moreover, we propose that water dissociation leads to hydrogen-bonding networks formed by H* and OH* intermediates, which may span the entire catalyst surface and decrease the interfacial pH to drive corrosion. In contrast, the electrochemical generation of reactive oxygen species is shown to play a minor role in catalyst corrosion during water oxidation using inductively coupled plasma mass spectrometry coupled with selective chemical scavengers. Square-wave voltammetry combined with rotating ring-disk electrodes is used to reveal that under open-circuit conditions, only Sn(IV) cations chemically dissolve from tin oxide, while both Sn(IV) and Sn(II) species electrochemically corrode during water oxidation. Our results unveil a dynamic and complicated interplay between corrosive and catalytic pathways on metal oxide electrocatalysts: a decrease in interfacial pH due to water oxidation exacerbates Sn(II)/Sn(IV) corrosion. Subsequently, the electrochemical corrosion of Sn(II)/Sn(IV) facilitates product formation from lattice oxygen, while the redeposition of corroded Sn(II) as Sn(IV) can enable oxygen exchange with water. By elucidating the roles of defects and interfacial chemistry, this work provides a roadmap for engineering improved electrocatalysts that balance activity and stability, a critical step toward scalable and durable energy technologies.

36 MATERIALS SCIENCE↗

Real-time X-ray Diffraction Measurements of Shocked Polycrystalline Tin and Aluminum

A new, fast, single-pulse x-ray diffraction (XRD) diagnostic for determining phase transitions in shocked polycrystalline materials has been developed. The diagnostic consists of a 37-stage Marx bank high-voltage pulse generator coupled to a needle-and-washer electron beam diode via coaxial cable, producing line and bremsstrahlung x-ray emission in a 35-ns pulse. The characteristic Kα lines from the selected anodes of silver and molybdenum are used to produce the diffraction patterns, with thin foil filters employed to remove the characteristic Kβ line emission. The x-ray beam passes through a pinhole collimator and is incident on the sample with an approximately 3-mm by 6-mm spot and 1° full-width-half-maximum (FWHM) angular divergence in a Bragg-reflecting geometry. For the experiments described in this report, the angle between the incident beam and the sample surface was 8.5°. A Debye-Scherrer diffraction image was produced on a phosphor located 76 mm from the polycrystalline sample surface. The phosphor image was coupled to a charge-coupled device (CCD) camera through a coherent fiberoptic bundle. Dynamic single-pulse XRD experiments were conducted with thin foil samples of tin, shock loaded with a 1-mm vitreous carbon back window. Detasheet high explosive with a 2-mm-thick aluminum buffer was used to shock the sample. Analysis of the dynamic shock-loaded tin XRD images revealed a phase transformation of the tin beta phase into an amorphous or liquid state. Identical experiments with shock-loaded aluminum indicated compression of the face-centered-cubic (fcc) aluminum lattice with no phase transformation.

46 INSTRUMENTATION RELATED TO NUCLEAR SCIENCE AND ↗

Picosecond time scale dynamics of short pulse laser-driven shocks in tin

The dynamics of high strain rate shock waves driven by a subnanosecond laser pulse in thin tin slabs have been investigated. These shocks, with pressure up to 1 Mbar, have been diagnosed with an 800 nm wavelength ultrafast laser pulse in a pump-probe configuration, which measured reflectivity and two-dimensional interferometry of the expanding rear surface. Time-resolved rear surface expansion data suggest that we reached pressures necessary to shock melt tin upon compression. Reflectivity measurements, however, show an anomalously high drop in the tin reflectivity for free standing foils, which can be attributed to microparticle formation at the back surface when the laser-driven shock releases.

71 CLASSICAL AND QUANTUM MECHANICS, GENERAL PHYSIC↗

Disordered surface structure of an ultra-thin tin oxide film on Rh(100)

The composition and structure of an ultra-thin tin oxide film on Rh(100), prepared by the deposition of a submonolayer of tin followed by annealing in an O{sub 2} atmosphere, were examined by a combination of low-energy electron diffraction (LEED), Auger electron spectroscopy, X-ray photoemission spectroscopy (XPS), scanning tunneling microscopy (STM), and ab initio calculations based on density functional theory (DFT). Although the LEED pattern exhibited c(2 x 8) spots clearly, a uniform periodicity of the c(2 x 8) unit cell was not observed in the STM images. The bright dots that were observed periodically in the STM image were similar to those of the ultra-thin Sn{sub 2}O{sub 3} film on Rh(111) and formed a zigzag arrangement with the numerous point and line defects. The XPS study revealed that the Sn 3d{sub 5/2} peak of the tin oxide film on Rh(100) showed a metallic state as well as an oxide state that was between the SnO{sub 2} and SnO states. The structural models, which were based on the Sn{sub 2}O{sub 3} structure on Rh(111), were determined using DFT total energy calculations. The simulated STM images of the two slightly different honeycomb-chain models well reproduced the zigzag arrangement in the STM image. The STM image and XPS spectrum were interpreted using a combination of the two models.

36 MATERIALS SCIENCE↗

Electrochemical fabrication and optical properties of porous tin oxide films with structural colors

Photonic crystals with porous features not only provide the capability to control light but also enable structural colors that are environmentally sensitive. Here, we report a novel kind of tin oxide-based photonic crystal featuring periodically arranged air pores fabricated by the periodic anodization of tin foil. The existence of a photonic band gap in the fabricated structure is verified by its vivid color, and its reflective spectra which are responsive to environmental stimuli. Furthermore, the sample colors (i.e., the photonic band gap positions) can be easily adjusted by manipulating the anodization parameters. The theoretical modeling results of these tin oxide photonic crystals agree well with the reported experimental ones.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗