Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “STEELS, STAINLESS - WELDING”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 235 records · Page 13

Irradiation Accelerated Corrosion of Stainless Steel and Ferritic-Martensitic Steel in Simulated Primary Water

Austenitic stainless steel, and ferritic-martensitic steel were irradiated with a proton beam while simultaneously exposed to simulated PWR primary water. Samples were exposed for 4-72 hr in 320°C water with 3 wppm hydrogen while simultaneously irradiated at surface dose rates from 400-4000 kGy/s (4x10-7 to 7x10-6 dpa/s). After exposure, samples were characterized with TEM, EDS, and Raman spectroscopy to determine the effects of radiation on the growth and stability of the oxide films. Samples which were irradiated during exposure had thinner inner oxides compared to unirradiated samples. Irradiated samples also had hematite on their surfaces, while unirradiated samples did not, indicating an increase in corrosion potential due to irradiation. Sample regions which were not irradiated but were exposed to the flow of irradiated water were similar to directly irradiated regions, suggesting that water radiolysis is the mechanism primarily responsible for the observed effects.

Stainless Steel, ferritic-martensitic steel, radia↗

Dislocation channel broadening–A new mechanism to improve irradiation-assisted stress corrosion cracking resistance of additively manufactured 316 L stainless steel

Additively manufactured (AM) 316 L stainless steel (SS) after hot isostatic pressing (HIP) was found to exhibit superior resistance to irradiation-assisted stress corrosion cracking (IASCC) in high-temperature water, as compared to wrought 316 L SS. The well-accepted IASCC factors of radiation-induced segregation (RIS) and radiation hardening are not accurate descriptions of IASCC susceptibility in this case. A decreased strain localization along grain boundaries, caused by dislocation channel broadening, was confirmed to suppress crack initiation. A unique distribution of irradiation-induced defects in HIP AM 316 L SS eased dislocation cross-slip compared to those in the wrought counterpart, thus increasing the channel width near the grain boundaries. Here for the first time, this study highlights the importance of dislocation channel broadening as a potential mechanism to further improve the IASCC resistance of 316 L SS and provides direct experimental evidence based on commercial-grade materials.

316L stainless steel↗

Aluminum to Stainless-Steel Joints for Cryogenic Applications

Aluminum to stainless-steel joints are necessary for cryogenic applications such as cryogenic fluid management and combustion devices. Supplemental development in this area was required for a test program at NASA Marshall Space Flight Center (MSFC) of an Al6061-RAM2 additively manufacturing liquid rocket nozzle. The test program identified a risk for installing stainless-steel fluid fittings to aluminum manifolds. To address this, a literature search was completed for various joint designs, and three designs were down selected to be cryogenic pressure cycle tested at MSFC. The test pieces were subsequently burst tested with ambient temperature water. This paper provides an overview of the literature review, down selected designs, test setup, test results, and fractography. The test results informed design decisions for the Al6061-RAM2 nozzle, and the recommended design proved to be a robust option with no notable issues identified during hot-fire testing.

Tessa M. Fedotowsky↗

A Kinetic Study Investigating the Carbothermic Recovery of Chromium from a Stainless-Steel Slag

In 2018, the stainless-steel industry produced > 10 million tons of slag, which for the most part was landfilled because of chromium oxide contamination. Long-term studies indicate a possible formation of soluble hexavalent chromium, which is classified as carcinogenic. Recent research focuses on the development of a treatment technology to recover chromium from the slag into a ferroalloy, producing an oxidic material that can be utilized in the construction industry. To date, there has been no literature dealing with the kinetics of a carbothermic treatment process to result in a model to predict the necessary treatment time. The present article fills this gap by investigating the reduction kinetics of chromium oxide of a process close to practical applications. Based on experimental measurements, a model has been developed to predict the necessary treatment time to reach a specific final chromium concentration as a function of the starting concentration and required process temperature in the range between 1600 °C and 1700 °C. Finally, presented findings can serve as a guideline to develop kinetic models in similar pyrometallurgical recovery processes.

36 MATERIALS SCIENCE↗

Development and testing of coarse-grained models for ultrasonic simulations of cast austenitic stainless steel

Ultrasonic inspection of cast austenitic stainless steel (CASS) in the nuclear industry is particularly challenging because of sound field scatter and attenuation caused by the coarse-grained microstructure. Modeling and simulation are important tools in ultrasonic testing, as they can be used to help address key aspects of inspections, such as developing new probe designs, predicting inspection reliability, and testing phased-array focal laws. However, developing a useful and reliable CASS model is challenging due to the many grain interfaces and crystalline orientations that must be captured. We demonstrate a method of creating a realistic CASS model that is usable in CIVA, a commercially available modeling and simulation software platform. Using polished and chemically etched sections, we generate models of a coarse-grained equiaxed specimen and a columnar specimen. We also test an alternative method of generating a coarse-grained model using Voronoi regions. We qualitatively compare sound field scatter and quantitatively compare sound field attenuation and beam partitioning in simulated sound fields to those of laboratory-measured sound fields. Results show that the Voronoi models perform as well as or better than the models based on actual grain morphology. Here we also show that model-to-model randomness in Voronoi grain structure can impact the magnitude of a simulated echo response by a factor of two or more. Although CASS models are potentially a good depiction of reality for a given scenario, they should not be considered representative since CASS morphology can change significantly from specimen to specimen or within the same specimen.

36 MATERIALS SCIENCE↗

Effect of thermal treatments on electrochemical behavior of binder jetted 17-4 PH stainless steel

Binder jetted 17–4 PH stainless steel was post-processed to relate heat treatment, microstructure, and corrosion in 3.5 wt% NaCl. Specimens were sintered at 1380 or 1400 °C, solution-annealed at 1055 °C for 1 h, and aged at 482 °C for 1 h. Here, as-sintered parts showed α′-martensitic matrix with a δ-ferrite network and Cu-rich precipitates in ferrite; inclusions (MnS, NbC) promoted localized attack. solutionizing redistributed elements and reduced ferrite, while aging generated coherent Cu nano-precipitates. Corrosion resistance was highly sensitive to post-processing in which aged specimens exhibited the lowest corrosion current density and formed a thicker, stable Cr 2 O 3 -rich passive film, whereas sintered specimens degraded most. Pitting potential depended on sintering temperature and microstructure, with 1400 °C sintering yielding more positive pitting potentials and the best overall performance after aging. Although the 1400-solutionized condition showed a relatively noble pitting response versus 1380-solutionized, it displayed unstable corrosion kinetics attributed to an imperfect passive film linked to higher NbC density. XPS depth profiles corroborated these trends, showing thicker, more continuous Cr 2 O 3 in aged states and discontinuous/thinning oxides in less resistant conditions. Practically, high-temperature sintering (∼1400 °C) followed by solutionizing and aging is recommended, with further gains expected from reducing NbC/MnS populations and porosity via powder and process control.

36 MATERIALS SCIENCE↗

Hydrogen-Assisted Fracture of Stainless Steel

Symmetric four-point bending (S4PB) and anti-symmetric four-point bending (AS4PB) were applied to assess the effect of hydrogen on crack initiation and propagation in a stable, nitrogen-strengthened austenitic stainless steel (21Cr-6Ni-9Mn). Specimens of a high strength aluminum alloy (AA2219-T851), which has also been identified as hydrogen-compatible, were used for test method development prior to completing the stainless steel test matrix. Single edge notched bend (SEN(B)) specimens were extracted from forged 21Cr-6Ni-9Mn bar and AA2219 plate. The 21Cr-6Ni-9Mn specimens were then hydrogen charged with ~200 wt. ppm hydrogen; AA2219 specimens were not charged. Aluminum specimens were tested in S4PB to induced mode I (pure bending), and AS4PB to attain varying levels of mode I/II mixity and mode II (pure shear), where the ratio of mode I to mode II varies with the position of the crack plane relative to the load line. After test method troubleshooting and validation, hydrogen charged stainless steel specimens were then subjected to mode I and two ratios of mixed mode I/II. Mode II loading was not achieved due to high load limitations. Analyses of fracture profiles for both materials reveal a marked effect of loading mode mixity on initial crack propagation orientation, however a specific contribution of hydrogen was not readily identifiable. Fracture initiation toughness in the presence of hydrogen, J IH , was calculated following the J-integral approach; the mode I J IH calculated for stainless steel samples fractured in S4PB were consistent with published values determined from compact tension specimens. The peak loads required to initiate fracture during AS4PB far exceeded those required during S4PB. This is attributed to the increasing shear force applied to the specimens as the degree of mode mixity increases. Ultimately, understanding the fracture response of hydrogen exposed stainless steels subjected to mixed mode I/II loading is critical for designing hydrogen containment vessels or gas transfer systems (GTS).

36 MATERIALS SCIENCE↗

Partitioning of tritium between surface and bulk of 316 stainless steel at room temperature

The distribution of tritium between the near surface and the bulk of 316 stainless steel has been measured using two independent techniques: pulsed-plasma exposures and a zinc-chloride wash. Between 17% and 20% of the total inventory absorbed into a stainless-steel sample during a 24-h exposure to DT gas at room temperature resides in the water layers present on the metal surface. Redistribution of tritium between the surface and the bulk of stainless steel, if it occurs, is very slow. Finally, tritium does not appear to enter into the bulk at a rate defined solely by lattice diffusivity.

316 stainless steel↗

Corrosion Compatibility of Stainless Steels and Nickel in Pyrolysis Biomass-Derived Oil at Elevated Storage Temperatures

Corrosion compatibility of stainless steels and nickel (Ni200) was assessed in fast pyrolysis bio-oil produced from pyrolysis of high ash and high moisture forest residue biomass. Sample mass change, ICP-MS and post-exposure electron microscopy characterization was used to investigate the extent of corrosion. Among the tested samples, type 430F and type 316 stainless steels (SS430F and SS316) and Ni200 (~98.5% Ni) showed minimal mass changes (less than 2 mg∙cm−2) after the bio-oil exposures at 50 and 80 °C for up to 168 h. SS304 was also considered to be compatible in the bio-oil due to its relatively low mass change (1.6 mg∙cm−2 or lower). SS410 samples showed greater mass loss values even after exposures at a relatively low temperature of 35 °C. Fe/Cr values from ICP-MS data implied that Cr enrichment in stainless steels would result in a protective oxide layer associated with corrosion resistance against the bio-oil. Post exposure characterization showed continuous and uniform Cr distribution in the surface oxide layer of SS430F, which showed a minimal mass change, but no oxide layer on a SS430 sample, which exhibited a significant mass loss.

09 BIOMASS FUELS↗

Development of cast alumina-forming austenitic stainless steels

Cast Fe-Ni-Cr chromia-forming austenitic stainless steels with Ni levels up to 45 wt. % are used at high temperatures in a wide range of industrial applications that demand microstructural stability, corrosion resistance, and creep strength. Although alumina scales offer better corrosion protection at these temperatures, designing cast austenitic alloys that form a stable alumina scale and achieve creep strength comparable to existing cast chromia-forming alloys is challenging. This work outlines the development of cast Fe-Ni-Cr-Al austenitic stainless steels containing about 25 wt. % Ni with good creep strength and the ability to form a protective alumina scale for use at temperatures up to 800 C - 850 C in H 2 O-, S-, and C- containing environments. Creep properties of the best alloy were comparable to that of HK-type cast chromia-forming alloy along with improved oxidation resistance typical of alumina-forming alloys. Lastly, challenges in the design of cast alloys and a potential path to increasing the temperature capability are discussed.

36 MATERIALS SCIENCE↗

Formation of Nitrogen Bubbles During Solidification of Duplex Stainless Steels

The nucleation and growth of nitrogen bubbles for duplex stainless steels are of great significance for the formation mechanism of bubbles during solidification. In the current study, numerical method and theoretical analysis of formula derivation were used to study the formation of nitrogen bubbles during solidification. The critical sizes of the bubble for homogeneous nucleation and heterogeneous nucleation at the solid–liquid interface during solidification were derived theoretically by the classical nucleation theory. The results show that the calculated values for the solubility of nitrogen in duplex stainless steel are in good agreement with the experimental values which are quoted by references: for example, when the temperature T = 1823 K and the nitrogen partial pressure P{sub N 2 =40P Θ , the calculated value (0.8042 wt pct) for the solubility of Fe-12Cr alloy nitrogen in molten steel is close to the experimental value (0.780 wt pct). Moreover, the critical radii for homogeneous nucleation and heterogeneous nucleation are identical during solidification. On the one hand, with the increasing temperature or the melt depth, the critical nucleation radius of bubbles at the solid–liquid interface increases, but the bubble growth rate decreases. On the other hand, with the decreasing initial content of nitrogen or the cooling rate, the critical nucleation radius of bubbles at the solid–liquid interface increases, but the bubble growth rate decreases. Furthermore, when the melt depth is greater than the critical depth, which is determined by the technological conditions, the change in the Gibbs free energy for the nucleation is not conducive enough to form new bubbles.

36 MATERIALS SCIENCE↗

Distribution of Tritium in the Near Surface of Type 316 Stainless Steel

The distribution of tritium in the near surface of stainless steel, type 316, has been measured using a combination of a ZnCl 2 wash and acid etching with diluted aqua regia. This method improves upon etching measurements reported in the literature: results show depth resolutions of ~10 nm using the diluted aqua regia. The ZnCl 2 wash results show very high surface concentrations (~1.5 x10 13 Bq/cm 3 ), which decreases by a factor of 10 6 after etching to a depth of ~10 um. Further, the tritium concentrations in the near surface (<10 um) of unmodified stainless-steel samples do not change significantly over the course of 233 days, which indicates a quasi-equilibrium state has been reached. Tritium migration to the surface from the subsurface region was measured by etching a sample, then storing it in air for 2 to 4 days. After storing in air, the surface concentrations increased a thousandfold and rapidly decreased to base levels after etching an additional ~2 um. Finally, these measurements indicate that perturbing the quasi-equilibrium concentration profile results in tritium migration to the surface in order to reestablish the prior equilibrium state.

36 MATERIALS SCIENCE↗

Deuterium permeation and retention in 316L Stainless Steel Manufactured by Laser Powder Bed Fusion

Deployment of additively manufactured materials into nuclear energy systems requires investigation of the full range of the unique environmental effects on these materials. Hydrogen isotopes are common gaseous species in nuclear reactors and exhibit ample high mobility in most materials. While hydrogen isotopes mobility in wrought stainless steel is well understood, this property is not thoroughly studied for its additively manufactured variants. In this study, we investigated the deuterium permeation and retention in 316L stainless steel manufactured by laser powder bed fusion. The results showed that the deuterium permeability in the as-built additively manufactured 316L stainless steel (AM SS316L) is greater than that of the reference wrought 316L stainless steel by a factor of 2.8. However, the stress-relieved and solution-annealed AM SS316L samples exhibit lower deuterium permeability in comparison with the as-built condition. Following the solution annealing, the deuterium permeability of AM SS316L is comparable with that of the reference wrought SS316L. Deuterium retention in the as-built AM SS316L is 45% higher than that of the wrought 316L stainless steel and slightly higher than that of the two thermally annealed AM SS316L materials. Finally, transmission electron microscopy and positron annihilation lifetime spectroscopy were used to obtain microstructural information used to determine deuterium permeation and retention behavior in the studied materials.

36 MATERIALS SCIENCE↗

On the measurement of austenite in supermartensitic stainless steel by X-ray diffraction

Sections of a 13Cr supermartensitic stainless steel were investigated to determine the optimum sample preparation for measurement of the austenite content by X-ray diffraction. The surface of several samples was mechanically ground or polished using media of grit sizes in the range 1–120 μm. The strained surface layer was afterwards removed stepwise by electropolishing, and the austenite content measured at each step. It was found that any level of mechanical grinding or polishing results in a reduction of the measured austenite fraction relative to the true bulk value, and that coarser grinding media impart greater damage and greater reduction in the measured austenite content. The results thus highlight the importance of the electropolishing step in preparation of such samples, but suggest that the American Society for Testing and Materials standard E975-03 substantially overestimates the amount of material which needs to be removed to recover the true “bulk” content. - Highlights: • Quantitative Rietveld analysis of austenite/martensite ratio in supermartensitic stainless steels • Critical evaluation of sample preparation for residual austenite measurements by X-ray diffraction • Highlighting of the importance of electropolishing as a final preparation step.

36 MATERIALS SCIENCE↗

High-Temperature Chemical Compatibility of As-Fabricated TRIGA Fuel and Type 304 Stainless Steel Cladding

Chemical interaction between TRIGA fuel and Type-304 stainless steel cladding at relatively high temperatures is of interest from the point of view of understanding fuel behavior during different TRIGA reactor transient scenarios. Since TRIGA fuel comes into close contact with the cladding during irradiation, there is an opportunity for interdiffusion between the U in the fuel and the Fe in the cladding to form an interaction zone that contains U-Fe phases. Based on the equilibrium U-Fe phase diagram, a eutectic can develop at a composition between the U 6 Fe and UFe 2 phases. This eutectic composition can become a liquid at around 725°C. From the standpoint of safe operation of TRIGA fuel, it is of interest to develop better understanding of how a phase with this composition may develop in irradiated TRIGA fuel at relatively high temperatures. One technique for investigating the development of a eutectic phase at the fuel/cladding interface is to perform out-of-pile diffusion-couple experiments at relatively high temperatures. This information is most relevant for lightly irradiated fuel that just starts to touch the cladding due to fuel swelling. Similar testing using fuel irradiated to different fission densities should be tested in a similar fashion to generate data more relevant to more heavily irradiated fuel. This report describes the results for TRIGA fuel/Type-304 stainless steel diffusion couples that were annealed for one hour at 730 and 800°C. Scanning electron microscopy with energy- and wavelength-dispersive spectroscopy was employed to characterize the fuel/cladding interface for each diffusion couple to look for evidence of any chemical interaction. Overall, negligible fuel/cladding interaction was observed for each diffusion couple.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Microstructure and corrosion resistance of nanocrystalline TiZrN films on AISI 304 stainless steel substrate

This study investigated the microstructure and properties of nanocrystalline TiZrN films on AISI 304 stainless steel substrate. TiZrN films were prepared by reactive magnetron sputtering based on the previous optimum coating conditions (substrate temperature, system pressure, nitrogen flow, etc.) for TiN and ZrN thin films. The composition ratio of TiZrN coatings were adjusted by changing the Zr target power, while keeping the Ti target power constant. Experiments were conduced to find the optimum composition with desired properties. The ratio of TiZrN composition was analyzed by x-ray photoelectron spectroscopy and Rutherford backscattering spectrometer. In terms of phase formation, there were two types of coatings that were considered: single-phase solid solutions of TiZrN and interlacing nuclei of TiZr in the matrix of TiZrN. The thickness of all TiZrN films as measured by the secondary ion mass spectroscopy was about 500 nm, and the composition depth profiles indicated that the compositions in the TiZrN films were uniform from the film surface to the 304 stainless steel substrate. The crystal structure of the TiZrN films was determined by x-ray diffraction using a M18XHF-SRA diffractometer with Cu K{sub {alpha}} radiation. A diffraction peak of TiZrN (002) was observed between that of TiN (002) and ZrN (002); similarly, a diffraction peak of TiZrN (111) was observed between that of TiN(111) and ZrN(111), respectively. The corrosion resistance of the TiZrN film deposited on the 304 stainless steel has been investigated by electrochemical measurement. The electrolyte, 0.5M H{sub 2}SO{sub 4} containing 0.05M KSCN, was used for the potentiodynamic polarization. The potentiodynamic scan was conducted from -800 to 800 mV standard calomel electrode (SCE).

36 MATERIALS SCIENCE↗

Spreading of lithium on a stainless steel surface at room temperature

Lithium conditioned plasma facing surfaces have lowered recycling and enhanced plasma performance on many fusion devices and liquid lithium plasma facing components are under consideration for future machines. A key factor in the performance of liquid lithium components is the wetting by lithium of its container. We have observed the surface spreading of lithium from a mm-scale particle to adjacent stainless steel surfaces using a scanning Auger microprobe that has elemental discrimination. Here, the spreading of lithium occurred at room temperature (when lithium is a solid) from one location at a speed of 0.62 μm/day under ultrahigh vacuum conditions. Separate experiments using temperature programmed desorption (TPD) investigated bonding energetics between monolayer-scale films of lithium and stainless steel. While multilayer lithium desorption from stainless steel begins to occur just above 500 K (E des = 1.54 eV), sub-monolayer Li desorption occurred in a TPD peak at 942 K (E des = 2.52 eV) indicating more energetically favorable lithium-stainless steel bonding (in the absence of an oxidation layer) than lithium lithium bonding.

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗