Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “SHEAR PROPERTIES”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 235 records · Page 13

Microstructure and Mechanical Properties of a SiO{sub 2} Ceramic and TC4 Alloy Joint Brazed with a Nanocomposite Filler

Vacuum brazing of TC4 alloy and SiO{sub 2} ceramic was achieved using a nano-AgCuNi braze alloy. The melting temperature of nano-AgCu powders was analyzed by differential scanning calorimeter. Furthermore, the effects of the Ni content on the microstructure and mechanical properties of the joints were studied. The results showed that the melting temperature of the nano-AgCu filler was 774 °C. A decrease in the melting temperature of 6 °C was observed, compared with the general AgCu filler, and this decrease enabled the interfacial reaction of the joint to begin earlier. The typical interfacial microstructure of the TC4/nano-AgCuNi/SiO{sub 2} ceramic joint brazed at 950 °C for 10 min was TC4/α-Ti + Ti{sub 2}(Cu,Ni) + Ti{sub 2}(Ni,Cu) hypereutectoid structure/Ti{sub 2}(Cu,Ni) compound with α-Ti + Ti{sub 2}(Cu,Ni) + Ti{sub 2}(Ni,Cu) hypereutectic structure/Ti{sub 4}O{sub 7} + TiSi{sub 2}/SiO{sub 2} ceramics. The homogeneous microstructure of α-Ti + Ti{sub 2}(Cu,Ni) + Ti{sub 2}(Ni,Cu) hypereutectoid structure primarily existed in the diffusion layer. Additionally, the refined α-Ti + Ti{sub 2}(Cu,Ni) + Ti{sub 2}(Ni,Cu) hypereutectic structure created via a eutectic reaction and Ti{sub 2}(Cu,Ni) compound was distributed in the brazing seam. The Ni content could influence the formation of Ti-Cu-Ni ternary intermetallic compounds (IMCs). An increase in Ni led to an increase in the α-Ti + Ti{sub 2}(Cu,Ni) + Ti{sub 2}(Ni,Cu) hypereutectic structure in the brazing seam. The shear strength of the brazed joints first increased and then decreased with the increase in the nano-Ni content, and the optimal shear strength of 30.1 MPa was achieved at 10 wt.% Ni. The increase in the α-Ti + Ti{sub 2}(Cu,Ni) + Ti{sub 2}(Ni,Cu) hypereutectic structure and the decrease in brittle compounds enhanced the shear strength of the joint. Fracture analysis of the joints brazed at 950 °C for 10 min indicated that the cracks mainly occurred in SiO{sub 2} ceramic.

36 MATERIALS SCIENCE↗

Topology-Dependent Polymer Stretching and Scission in Solution at Extreme Shear Rates

There has been significant interest in the engineering of polymer topology to control rheology and mechanical stability in dilute solutions for applications involving extreme shear rate flows. However, methods to experimentally probe properties at relevant shear rates (≈ 10 4 –10 6 s –1 ) have remained ex situ, obscuring access to measures of polymer deformation and rheology that would otherwise provide mechanistic insight into the topology-dependent properties that control their behavior in extreme shear flows. In this study, we used novel in situ small angle neutron scattering measurements in a capillary rheometer (capillary rheo-SANS) to simultaneously measure solution viscosities and polymer deformations in high shear on a series of chemically homologous topology-defined polymers including linear, randomly branched, and star-shaped molecules. We demonstrate that differences in the onset of chain stretching and shear thinning of these polymers in dilute solution are controlled primarily by differences in their molecular relaxation time. These differences correlate with differences in chain scission inferred from ex situ measurements at more extreme shear rates. Together, the results demonstrate a direct coupling between chain deformation and scission, and suggest that the dominant effect of branching as a means to impart resilience against mechanical degradation is through differences in relaxation dynamics due to branching. We anticipate that these results will provide key insights to engineer topology-controlled polymers for rheological modification, mechanical stability, and controlled mechano-chemistry.

32 ENERGY CONSERVATION, CONSUMPTION, AND UTILIZATI↗

EFFECT OF TOOL FEATURE ON THE JOINT STRENGTH OF DISSIMILAR FRICTION STIR LAP WELDS

Several variations of friction stir tools were used to investigate the effects on the joint strengths of dissimilar friction stir lap welds. In the present lap weld configuration the top sheet was a 2.32 mm thick Mg (AZ 31) alloy. The bottom sheet consisted of two different steels, a (i) 0.8 mm thick electro-galvanized (EG) mild steel, or a (ii) 1.5 mm thick hot dip galvanized (HDG) high strength low alloy (HSLA) steel. Initially the tool shape was modified to accommodate the material, at which point the tool geometry was fixed. With a fixed tool geometry an additional feature was added to the pin bottom on one of the tools by incorporating a short hard insert, which would act as a stronger bottom sheet cutter. The effects of such modification on the unguided lap shear strength, and associated microstructural changes are discussed in this study.

36 MATERIALS SCIENCE↗

The Contributions of Polar Nanoregions to the Dielectric and Piezoelectric Responses in Domain-Engineered Relaxor-PbTiO 3 Crystals

The existence of polar nanoregions is the most important characteristic of relaxor-based ferroelectric materials. Recently, the contributions of polar nanoregions to the shear piezoelectric property of relaxor-PbTiO 3 (PT) crystals are confirmed in a single domain state, accounting for 50%–80% of room temperature values. For electromechanical applications, however, the outstanding longitudinal piezoelectricity in domain-engineered relaxor-PT crystals is of the most significance. In this paper, the contributions of polar nanoregions to the longitudinal properties in [001]-poled Pb(Mg 1/3 Nb 2/3 )O 3 -0.30PbTiO 3 and [110]-poled Pb(Zn 1/3 Nb 2/3 )O3-0.15PbTiO 3 (PZN-0.15PT) domain-engineered crystals are studied. Taking the [110]-poled tetragonal PZN-0.15PT crystal as an example, phase-field simulations of the domain structures and the longitudinal dielectric/piezoelectric responses are performed. According to the experimental results and phase-field simulations, the contributions of polar nanoregions (PNRs) to the longitudinal properties of relaxor-PT crystals are successfully explained on the mesoscale, where the PNRs behave as “seeds” to facilitate macroscopic polarization rotation and enhance electric-field-induced strain. The results reveal the importance of local structures to the macroscopic properties, where a modest structural variation on the nanoscale greatly impacts the macroscopic properties.

36 MATERIALS SCIENCE↗

Interfacial Shear Strength of Oxide Scale and SS 441 Substrate

Recent developments on decreasing the operating temperature for Solid Oxide Fuel Cells (SOFCs) have enabled the use of high temperature ferritic alloys as interconnect materials. Oxide scale will inevitably grow on the ferritic interconnects in a high temperature oxidation environment of SOFCs. The growth of the oxide scale induces growth stresses in the scale layer and on the scale/substrate interface. These growth stresses combined with the thermal stresses induced upon stacking cooling by the thermal expansion coefficient mismatch between the oxide scale and the substrate may lead to scale delamination/buckling and eventual spallation, which may lead to serious cell performance degradation. Hence the interfacial adhesion strength between the oxide scale and the substrate is crucial to the reliability and durability of the metallic interconnect in SOFC operating environments. In this paper, we applied an integrated experimental/modeling methodology to quantify the interfacial adhesion strength between the oxide scale and the SS 441 metallic interconnect. The predicted interfacial strength is discussed in details.

30 DIRECT ENERGY CONVERSION↗

Effect of Joining Atmosphere in Transient Liquid Phase Bonding of Inconel 617 Superalloy

In the present paper, transient liquid phase (TLP) bonding of Inconel 617 alloy under the different furnace atmospheres of vacuum, argon gas, and air was investigated. The experiments were carried out at 1408 K (1135 °C) for 300 minutes by using BNi-1 filler metals with different thicknesses of 50 and 100 µm. The microstructure, chemical analysis, shear strength, and microhardness of the resultant joints were studied. After 300 minutes, complete isothermal solidification was obtained for both the interlayers having 50 and 100 µm thicknesses under all the furnace atmospheres. The specimens bonded under vacuum condition showed the highest shear strength, failure energy, and ductility. Also, the joint produced under argon gas atmosphere using 100-µm-thick filler metal showed a good strength and may be acceptable in many applications. However, the specimens bonded under air atmosphere were weak, due to their further cavities and non-dissolved carbides. The presence of non-dissolved carbides in the diffusion-affected zone resulted in increasing the hardness of the base metal near the interface. The carbides were dissolved and the hardness of the diffusion-affected zone was reduced under vacuum condition compared to argon and air atmospheres. The best result was obtained for the specimen joined using the 50-µm-thick interlayer under vacuum atmosphere, with about 95.8 pct joint efficiency.

36 MATERIALS SCIENCE↗

Wetting and Brazing of Chromium Film-Deposited Alumina Using AgCu Filler Metal

Wetting behavior of AgCu filler on chromium film-deposited Al{sub 2}O{sub 3} ceramics was studied by sessile drop method under vacuum, and brazing of chromium-deposited alumina using AgCu was carried out. Cr film can improve the wettability of AgCu filler on alumina ceramics, and the contact angle decreased dramatically. However, with further increase in temperature and extension of wetting time, Cr atom might diffuse excessively to molten alloy or substrate leading to thinned or disappeared Cr film on alumina; thus, the contact angle of AgCu on alumina increased. The reliable alumina joint was obtained via chromium deposition using AgCu filler brazed at 900 °C for 10 min, and no hard or brittle intermetallic compounds formed in the brazed joint. The maximum shear strength of 16.8 MPa was achieved when the thickness of deposited chromium film was 2 μm.

36 MATERIALS SCIENCE↗

Effect of Surface Self-Nanocrystallization on Diffusion Bonding Between a Titanium Alloy and a TiAl-Based Alloy

A self-nanocrystallization layer was prepared on the surface of a Ti alloy sample via shot peening to investigate its influence on the follow-up diffusion bonding between a titanium alloy and a TiAl-based alloy. The experiment results show that surface self-nanocrystallization treatment can accelerate the interface reaction between a Ti alloy and a TiAl alloy, lowering the bonding temperature of the sound joints by more than 50 K. Moreover, the thickness of the interface reaction layer plays an important role in the interfacial bonding strength. In this work, the maximum shear strength of the joint appears to have a thickness of about 1.8 μm. As a consequence, it is found that surface self-nanocrystallization treatment is helpful for optimizing the diffusion bonding process.

77 NANOSCIENCE AND NANOTECHNOLOGY↗

Effects of Laser Fluence on Microstructure and Bonding Characteristics of Wideband Laser-Deposited Nickel Composite Coatings

The wideband laser has shown great potential in metal–ceramic coatings deposition due to the high efficiency and low dilution rate. However, the effects of wideband laser process on microstructure evolution and bonding mechanism at the coatings/substrate interface are still a critical problem and need further investigation. In this work, nickel composite coatings are fabricated on the surface high-strength low-alloy steel. The effects of laser fluence on microstructure evolution, shear strength and fracture mechanism are studied. Results indicated the added WC particles were partly dissolved due to the high-power laser irradiation. Many block precipitates and dense eutectic were synthesized in composite coatings. Reinforced phases mainly consist of Cr{sub 5}B{sub 3}, Cr{sub 23}C{sub 6}, W{sub 2}C and Cr{sub 3}Ni{sub 2}. The dilution of Q550 steel contributed to the formation of nickel dendrites and facilitated a dense metallurgical bonding at coating/substrate interface when laser fluence was high. Shear strength tests indicated the laser fluence and shear strength had a positive correlation. For Ni60/WC composite coatings designed in these experiments, the recommend laser fluence should be higher than 55 J/mm{sup 2}, above which the shear strength could be greater than 200 MPa. Fracture surfaces indicated the failure mechanism of composite coatings was quasi-cleavage fracture.

36 MATERIALS SCIENCE↗

A Weighting Grade-Based Optimization Method for Determining Refill Friction Stir Spot Welding Process Parameters

The welding process used in fabricating thin-walled structures by refill friction stir spot welding (RFSSW) should be characterized by a high strength of welds and high process repeatability which is demonstrated by a small dispersion of the load capacity of the joints. The present work is designed to optimize RFSSW process parameters for 7075-T6 Alclad aluminum alloy sheets used to fabricate aircraft structures. The optimization was performed by scalarization of the objective function using the weighting grades method. The study considers the effect of process parameters, i.e., tool plunge depth, duration of welding, tool rotational speed, on the tensile/shear strength of the joints, and dispersion of the load capacity. It was found that it was possible to choose the optimal welding parameters taking into account maximization of the load capacity and minimization of the dispersion of the joint strength via a best compromise between the tool rotational speed ensuring adequate plasticization of the base material and the duration of welding ensuring that a fine-grained joint microstructure is obtained.

36 MATERIALS SCIENCE↗

Fabrication of a High Chromium Cast Iron/Low Carbon Steel Bimetal: Diffusion Behavior and Bonding Strength

In the present study, a high chromium cast iron (HCCI) alloyed with Mo (16 wt.% Cr-6 wt.% Mo-2.4 wt.% C) with excellent wear resistance was bonded to a low carbon steel (LCS) by surface liquid-phase sintering. The bimetal was also subjected to a quenching + tempering treatment. The diffusion behavior of the atoms between the HCCI and LCS was analyzed. The bonding strength of the bimetal was investigated before and after heat treatment. The results show that the bimetal had a good bonding quality due to the uphill diffusion of C atoms. A diffusion zone with a width of approximately 37 μm and a troostite structure formed on the HCCI side by the interface. With different bonding times, there was no obvious change in the width of the diffusion zone. The shear strength of the bimetal at all holding times was reduced from a high level after heat treatment and decreased with increasing tempering temperature. The impact toughness of the bimetal substantially increased compared with that of the HCCI. After a quenching treatment, the impact toughness of the bimetal decreased, and the microhardness of the diffusion zone improved. As the tempering temperature increased, the microhardness and impact toughness decreased and increased, respectively.

36 MATERIALS SCIENCE↗

Effect of Cu Interlayer on the Microstructure and Strength for Brazing of Tungsten/316L Steel

Brazing is an effective technique for joining tungsten and steel. However, the high residual stresses are produced due to the different coefficients of thermal expansions between tungsten and steel. Compared with the direct brazing with BNi-2 foil filler, BNi-2/Cu/ BNi-2 multiple interlayer was used as filler to minimize the residual stresses between tungsten and 316L steel. The brazing experiments were conducted at 1050 °C for 25 min using Cu foils with different thickness. The results show that tungsten and 316L steel have been successfully joined by brazing. The intermetallic compound of NiW formed at the W/BNi-2 interface, which was detrimental to the strength of the joint. The microhardness of different diffusion zones is higher than that of the substrates owing to the formation of intermetallic compound and solid solution. All specimens of shear testing fractured at the W/BNi-2 interface close to W substrate, and the average strength of joints was 197, 275 and 268 MPa with multiple interlayer thickness of 0.2 , 0.1 and 0.05 mm copper foil, respectively, while the average strength of joints was 143 MPa with BNi-2 foil filler. The significant increase in the joint shear strength can be ascribed to the Cu foil in the multiple interlayer because of with excellent plasticity and toughness.

36 MATERIALS SCIENCE↗

Revealing meso-structure dynamics in additive manufacturing of energy storage via operando coherent X-ray scattering

3D printing is an emerging technology for the fabrication of energy storage devices, offering advantages over traditional manufacturing methods. However, optimization and design of such devices requires an understanding of the meso-structure formation during the 3D printing process. This study utilizes operando coherent X-ray scattering, X-ray Photon Correlation Spectroscopy (XPCS), to study the spatiotemporally-resolved far-from-equilibrium dynamics during direct ink writing 3D printing. Here, Lithium Titanate (LTO) based ink is prepared and rheologically tested for its shear-thinning properties. Two-time intensity-intensity functions are calculated to be used in subsequent quantitative analysis, which allows for an overall characterization of the dynamics, description of an initial fast decorrelation and identification of sudden rearrangements of subdomains of the sample. The results show the dynamics to be anisotropic, spatiotemporally heterogenous and marked by distinct rearrangement events, all of which impact the electrochemical performance of energy storage devices. The studied 3D printing ink is used to fabricate electrodes which are then electrochemically tested, showing good performance in cycling and retaining structural integrity. This work furthers the understanding of the far-from-equilibrium material dynamics during 3D printing, giving quantitative characterization of this process, and highlights aspects of structure formation relevant to the electrochemical performance of the resultant energy storage device.

36 MATERIALS SCIENCE↗

Micromechanical properties of spherical and facetted He bubble loaded copper

Exploring new irradiation resistant materials requires understanding their mechanical responses to irradiation. Resistance to helium bubble formation and understanding bubble effects on the mechanical response of candidate materials are crucial factors to qualify materials as irradiation resistant. Here, in this paper, we explore the effect of spherical and facetted helium bubbles on the mechanical response of copper via in-situ micromechanical tensile testing at room temperature. Bubble formation and shape effects on strength and ductility, and their behavior on grain boundaries are discussed and compared to literature. Loading Cu with helium bubbles is shown here to increase strength but decrease ductility.

42 ENGINEERING↗

Delivery of Vegetable Oil Suspensions in a Shear Thinning Fluid for Enhanced Bioremediation

In situ anaerobic biological processes are widely applied for dechlorination of chlorinated solvents in groundwater. A wide range of organic substrates have been tested and applied to support the dechlorination processes. Vegetable oils are a promising substrate and have been shown to induce effective dechlorination, have limited geochemical impacts, and good longevity. Distribution of vegetable oil in the subsurface, because it is a non-aqueous phase material, has typically been addressed by creating emulsified oil solutions. In this study, inexpensive waste vegetable oils were suspended in a xanthan gum solution, a shear-thinning fluid, as an alternative oil delivery mechanism. The stability, oil droplet size and distribution, and rheological behavior of the oil suspensions that are created in the xanthan solutions were studied in batch experiments. The injectability of the suspensions and oil distribution in porous medium were evaluated in column tests. Numerical modeling of the oil droplet transport and distribution in porous media was conducted to help interpret the column-test data. Batch studies showed that simple mixing of vegetable oil and xanthan solution produced stable suspensions of the oil as micron-size droplets. The mixture rheology retains shear-thinning properties that facilitate improved uniformity of substrate distribution in heterogeneous aquifers. Column tests demonstrated successful injection of the vegetable oil suspension into porous medium. This study provided evidence that vegetable oil suspensions in xanthan are a potential substrate to support in situ anaerobic bioremediation with favorable injection properties.

Zhong, Lirong↗

Enhanced delivery of engineered Fe-Mn binary oxides in heterogeneous porous media for efficient arsenic stabilization

Heterogeneity in sediment and aquifer is universal, resulting in preferential flows of injected materials in the high permeability regions and forming flow by-passed zones in the low permeability regions during in-situ subsurface remediation. This adverse effect can considerably delay the completion of remedial operations and significantly increase the cost. Column experiments were designed and conducted to study the transport of starch- and starch-xanthan gum modified Fe-Mn binary oxide particles (SFM and SXFM) in saturated heterogeneous porous media and to reveal the particles’ arsenic (As) stabilization performance. Fine-in-Coarse (FIC) and Coarse-in-Fine (CIF) patterns of heterogeneous packings were set up in the columns. Testing results demonstrated that starch-xanthan gum dual treatment on Fe-Mn binary oxides successfully improved the particles’ migration capability in heterogeneous porous media and their distribution uniformity attributed to the profound shear thinning behavior of xanthan gum solution. The addition of xanthan gum to the system increased the viscosity and shear thinning property of SXFM suspension, making it a better candidate for delivery. Both SFM and SXFM stabilized As in heterogeneously packed sediment collected from a contaminated site, with SXFM showing better stabilization performance than SFM. The stabilization effects of SXFM were 90.7-97.0%, compared to 82.0-95.2% of SFM.

Yan, Xiulan↗

Characterization of diffusion bonded joint between titanium and 304 stainless steel using a Ni interlayer

Solid-state diffusion bonded joints were prepared between commercially pure titanium and 304 stainless steel with nickel as an intermediate material in the temperature range of 800-950 deg. C for 10.8 ks under a 3 MPa uniaxial pressure in vacuum. The interface microstructures and reaction products of the transition joints were investigated by optical and scanning electron microscopy. Up to 850 deg. C processing temperature, a 300-{mu}m nickel interlayer completely restricts the diffusion of titanium to stainless steel. However, the nickel interlayer cannot block the diffusion of Ti to the stainless side and {lambda} + {chi} + {alpha}-Fe, {lambda} + FeTi and {lambda} + FeTi + {beta}-Ti phase mixtures are formed at the SS-Ni interface, when bonding was processed at 900 deg. C and above. These reaction products were confirmed by X-ray diffraction. A maximum tensile strength of {approx} 270 MPa and shear strength of {approx} 194 MPa, along with 6.2% ductility, were obtained for the diffusion bonded joint processed at 850 deg. C. Fracture surface observation in SEM using EDS demonstrates that failure occurred through the Ni-Ti interface of the joints when processed up to 850 deg. C and through the SS-Ni interface when processed at and above 900 deg. C.

36 MATERIALS SCIENCE↗

Diffusion bonding of iron aluminide Fe{sub 72}Al{sub 28} using a copper interlayer

An Fe{sub 72}Al{sub 28} alloy was diffusion-bonded using a copper interlayer under vacuum at 1075 deg. C for 1 h, 2 h, 4 h and 6 h durations at 3.2 MPa applied pressure. The bond microstructure was found to be composed of the copper rich interlayer, copper rich precipitates and the base metal. SEM-EDS studies indicated major diffusion of aluminium and iron atoms from Fe{sub 72}Al{sub 28} into the copper interlayer and copper atoms from the copper interlayer into the Fe{sub 72}Al{sub 28} matrix. SEM observations of fractured surfaces of the diffusion-bonded samples showed some plastic deformation and signs of good bonding. Cu{sub 3}Al and B{sub 2}-FeAl-based phases were identified by SEM-EDS and X-ray diffraction studies at the bond and on the fracture surfaces of all samples investigated. Good bonding was achieved with a maximum shear strength of 298 MPa which is 65% of the parent material shear strength for a sample diffusion-bonded for 6 h.

36 MATERIALS SCIENCE↗