At least 235 records · Page 13

Oxidation of porous stainless steel supports for metal-supported solid oxide fuel cells

Here, oxidation behavior of porous P434L ferritic stainless steel, used for the fabrication of metal-supported solid oxide fuel cells (MS-SOFC), is studied under anodic and cathodic atmospheres. Temperature- and atmosphere-dependence is determined for as-sintered and pre-oxidized stainless steel. Pre-oxidation reduced the long-term oxidation rate. For pre-oxidized samples, the oxidation rate in air exceeds that in humid hydrogen for temperatures above 700 °C. The influence of PrOx, LSCF-SDC, and Ni-SDC coatings is also examined. The coatings do not dramatically impact oxide scale growth. Oxidation in C-free and C-containing anodic atmospheres is similar. Addition of CO 2 , CH 4 , and CO to humidified hydrogen to simulate ethanol reformate does not significantly impact oxidation behavior. Cr transpiration in humid air is greatly reduced by the PrOx coating, and a PrCrO 3 reaction product is observed throughout the porous structure. A dense and protective chromia-based scale forms on steel samples during oxidation in all conditions. A thin silica enriched oxide layer also forms at the metal-scale interface. In general, the oxidation behavior at 700 °C is found to be acceptable.

25 ENERGY STORAGE↗

Silicon carbide as an oxidation-resistant high-temperature material. 1: Oxidation and heat corrosion behavior

The oxidation and corrosion behavior of SiC (in the form of a SiC powder) and hot-pressed and reaction-bound material were studied. The excellent stability of SiC in an oxidizing atmosphere is due to the development of protective SiO2 coatings. Any changes in these protective layers (e.g., due to impurities, reaction with corrosive media, high porosity of SiC, etc.) lead in most cases to increased rates of oxidation and thus restrict the field of SiC application.

Schlichting, J.↗

Morphological development and oxidation mechanisms of aluminum nitride whiskers

Hexagonal aluminum nitride (AlN) whiskers have been synthesized at 1873 K under a flowing nitrogen atmosphere. The synthesized whiskers are long straight filaments with diameters between 1 and 5 {mu}m and length in the cm range. In order to investigate its 'oxidation resistance', a series of experiments have been performed. The oxidation behavior was quite different in the experimental temperature range assigned, which can be attributed to the kinetic factor and the morphological development during oxidation process. It was chemical controlled at lower temperature while both chemical reaction and diffusion controlled at medium temperature. Further accelerating of temperature to 1473 K, AlN whiskers was peeled into smaller parts, which increased the oxidation rate and hence showed powder-like oxidation behavior. Our new kinetic theory has been applied to study the oxidation behavior of AlN whiskers. The comparison of the experimental data with the theoretical ones validates the applicability of the new model. - Hexagonal aluminum nitride (AlN) whiskers have been synthesized at 1873 K under a flowing nitrogen atmosphere. The synthesized whiskers are long straight filaments with diameters between 1 and 5 {mu}m and length in the cm range.

36 MATERIALS SCIENCE↗

The Role of Oxidation Resistance in High Temperature Alloy Selection for a Future with Green Hydrogen

Hydrogen is being considered integral to the future energy landscape but there is limited mechanistic understanding and a lack of predictive models to describe the combined effects of alloy and gas composition, temperature, thermal cycling and water vapor contents on the oxidation behavior of high-temperature materials. Experimental evaluations were combined with coupled thermodynamic-kinetic modeling to investigate the oxidation behavior of five representative Ni-based superalloys in two water vapor contents (10%, 60% H 2 O) under thermal cycling (1-h, 100-h cyles) conditions at 800°C and 1000°C. The alloy with the highest Ti content demonstrated the poorest cyclic oxidation behavior while the alloy with highest Cr and Al contents was expected to continue to support protective formation of a compact Al 2 O 3 scale. Finally, accelerated degradation of the chromia-forming alloys was observed in the higher water vapor content but the impact on transient oxidation of the alumina-forming alloys needs further investigations.

36 MATERIALS SCIENCE↗

Steam Oxidation Testing in the Severe Accident Test Station

After the March 2011 accident at Fukushima Daiichi, Oak Ridge National Laboratory (ORNL) began conducting high temperature steam oxidation testing of candidate materials for accident tolerant fuel (ATF) cladding in August 2011 [1-11]. The ATF concept is to enhance safety margins in light water reactors (LWR) during severe accident scenarios by identifying materials with 100× slower steam oxidation rates compared to current Zr-based alloys. In 2012, the ORNL laboratory equipment was expanded and made available to the entire ATF community as the Severe Accident Test Station (SATS) [4,12]. Compared to the current UO2/Zr-based alloy fuel system, an ATF alternative would significantly reduce the rate of heat and hydrogen generation in the core during a coolant-limited severe accident [13-14]. The steam oxidation behavior of candidate materials is a key metric in the evaluation of ATF concepts and also an important input into models [15-17]. However, initial modeling work of FeCrAl cladding has used incomplete information on the physical properties of FeCrAl. Also, the steam oxidation data being collected at 1200°-1700°C is unique as no prior work has considered steam oxidation of alloys at such high temperatures. Also, because many accident scenarios include steadily increasing temperatures, the required data are not traditional isothermal exposures but exposures with varying “ramp” rates. In some cases, the steam oxidation behavior has been surprising and difficult to interpret. Thus, more fundamental information continues to be collected. In addition, more work continues to focus on commercially-manufactured tube material. This report summarizes recent work to characterize the behavior of candidate alloys exposed to high temperature steam, evaluate steam oxidation behavior in various ramp scenarios and continue to collect integral data on FeCrAl compared to conventional Zr-based cladding.

21 SPECIFIC NUCLEAR REACTORS AND ASSOCIATED PLANTS↗

Microbeam X-Ray Absorption Near-Edge Spectroscopy of Alloying Elements in the Oxide Layers of Irradiated Zircaloy-2

Hydrogen pickup of zirconium-based fuel cladding and structural materials during in-reactor corrosion can degrade fuel components because the ingress of hydrogen can lead to the formation of brittle hydrides. In the boiling water reactor (BWR) environment, Zircaloy-2 fuel cladding and structural components such as water rods and channels can experience accelerated hydrogen pickup, whereas Zircaloy-4 components exposed to similar conditions do not. Because the principal difference between the two alloys is that Zircaloy-2 contains nickel, accelerated hydrogen pickup has been hypothesized to result from the presence of nickel. However, an understanding of the mechanism by which this acceleration occurs is still lacking. We investigated the link between hydrogen pickup and the oxidation behavior of alloying elements when incorporated into the oxide layers formed on zirconium alloys when corroded in the reactor. Synchrotron radiation microbeam X-ray absorption near-edge spectroscopy (XANES) at the Advanced Photon Source was performed on carefully selected BWR-corroded Zircaloy-2 water rods at an assembly-averaged burnup ranging from 32.8 to 74.6 GWd/MTU to determine the oxidation states of alloying elements, such as iron and nickel, within the oxide layers as a function of distance from the oxide-metal interface at high burnup. Samples were chosen for comparison based on having similar oxide thicknesses, processing, elevation, reactors, and fluences but different hydrogen pickup fractions. Examinations of the oxide layers formed on these samples showed that (1) the oxidation states of these alloying elements changed with distance from the oxide-metal interface, (2) these elements exhibited delayed oxidation relative to the host zirconium, and (3) nickel in Zircaloy-2 remained metallic in the oxide layer at a longer distance from the oxide-metal interface than iron. An analysis of these results showed an apparent correlation between the delayed oxidation of nickel and higher hydrogen pickup of Zircaloy-2 at high burnup.

alloying elements↗

Oxidation of high-temperature intermetallics; Proceedings of the Workshop, Cleveland, OH, Sept. 22, 23, 1988

The present conference on the high-temperature oxidation behavior of aerospace structures-applicable intermetallic compounds discusses the influence of reactive-element additions on the oxidation of Ni3Al base alloys, the effect of Ni3Al oxidation below 850 C on fracture behavior, the oxidation of FeAl + Hf, Zr, and B, the synergistic effect of Al and Si on the oxidation resistance of Fe alloys, and pack cementation coatings of Cr-Al on Fe, Ni, and Co alloys. Also discussed are the formation of alumina on Nb- and Ti-base alloys, the oxidation behavior of titanium aluminide alloys, silicide coatings for refractory metals, the oxidation of chromium disilicide, and the oxidation behavior of nickel beryllides.

Grobstein, Toni↗

Challenges in computationally designing high temperature Fe-based austenitic alloys: Addressing the role of Ni additions

Alumina-forming austenitic (AFA) alloys are relatively inexpensive high performance materials which combine the creep resistance of low-cost austenitic alloys and the oxidation resistance of expensive alumina forming alloys. However, a fundamental understanding of the role of key alloying elements such as Ni, Cr, Al, Nb, Ti, V, B and C in the experimentally observed oxidation behavior of these alloys is still lacking. The present work is a first in a series of studies aiming to quantitatively describe the role of Ni in promoting or disrupting protective Al 2 O 3 scale formation on AFA alloys. Here, ternary Fe-Al-xNi model alloys with three different Ni contents were isothermally exposed in an atmosphere with a low partial pressure of oxygen between 800–1000 °C for 24 h to evaluate the role of Ni in the observed internal oxidation behavior. Increasing Ni contents had no impact on the internal oxidation behavior of the alloys. The experimental and theoretical analyses in the present work suggested a negligible effect of the internal oxide precipitates on the inward diffusion of oxygen, typically expected in these systems, while simultaneously highlighting the barriers in the development of reliable models for computation-assisted design of these alloys.

36 MATERIALS SCIENCE↗

Very Long Term Oxidation of Titanium Aluminides Investigated

Titanium aluminides (TiAl) are of great interest for intermediate-temperature (600 to 850 C) aerospace and power-generation applications because they offer significant weight savings over today's nickel alloys. TiAl alloys are being investigated for low-pressure turbine blade applications, exhaust nozzle components, and compressor cases in advanced subsonic and supersonic engines. Significant progress has been made in understanding the fundamental aspects of the oxidation behavior of binary TiAl alloys. However, most of this work has concentrated on short term (<1000 hr), high-temperature (900 to 1000 C) exposures. Also, there is not much data available in the literature regarding the oxidation behavior of the quaternary and higher order engineering alloys. This is especially true for the very long term, low-temperature conditions likely to be experienced during aerospace applications. An investigation at the NASA Glenn Research Center at Lewis Field was undertaken to characterize the long-term oxidation behavior of various model and advanced titanium aluminides for periods up to 7000 hr at 704 C in air using a high-resolution field emission scanning electron microscope. Also, a unique surface treatment technique developed to improve the oxidation resistance of TiAl was evaluated. The alloys included in this investigation are listed in the table. The table also shows typical alloy compositions and the specific weight changes and scale thickness measured for each alloy after exposure to 700 C for 7000 hr in air.

Locci, Ivan E.↗

Very Long Term Oxidation of Ti-48Al-2Cr-2Nb at 704 C In Air

Introduction Titanium aluminides are of great interest for intermediate-temperature (600 C - 850 C) aerospace and power generation applications because of their high specific properties. Replacement of conventional superalloys by titanium aluminides offers the potential of significant weight savings. Extensive development efforts over the past IO years have led to the identification of y (TiAl) + alpha(sub 2) (Ti3Al) alloys, such as the G.E. alloy Ti48Al-2Cr-2Nb (all composition in at. %), which offer a balance of room temperature mechanical properties and high-temperature strength retention. The two phase gamma + alpha(sub 2) class of titanium aluminides also offers superior oxidation and embrittlement resistance compared to the alpha(sub 2) and orthorhombic classes of titanium aluminides. However, environmental durability is still a major concern. Significant progress has recently been made in understanding the fundamental aspects of the oxidation behavior of binary gamma + alpha(sub 2) Ti-Al alloys. However, most of this work has concentrated on short term (less than 1000 hours), high temperature (900 C - 1000 C) exposures. Also little data are available in the literature regarding the oxidation behavior of the quaternary and higher order gamma + alpha(sub 2) engineering alloys. This is especially true for the very long-term, low temperature conditions likely to be experienced during engineering applications. The present work addresses this regime to fill this gap by characterizing the oxidation behavior of Ti48Al-2Cr-2Nb for periods up to 9000 h at 704 C in air.

Locci, I. E.↗

The high temperature creep behavior of oxides and oxide fibers

A thorough review of the literature was conducted on the high-temperature creep behavior of single and polycrystalline oxides which potentially could serve as fiber reinforcements in ceramics or metal matrix applications. Sapphire when oriented with the basal plane perpendicular to the fiber axis (c-axis oriented) is highly creep resistant at temperatures in excess of 1600 C and applied loads of 100 MPa and higher. Pyramidal slip is preferentially activated in sapphire under these conditions and steady-state creep rates in the range of 10(exp -7) to 10 (exp -8)/s were reported. Data on the creep resistance of polycrystalline beryllia suggest that C-axiz oriented single crystal beryllia may be a viable candidate as a fiber reinforcement material; however, the issure of fabricability and moisture sensitivity must be addressed for this material. Yttrium aluminum garnet (YAG) also appears to be a fiber candidate material having a high resistance to creep which is due to it's complex crystal structure and high Peierl resistance. The high creep resistance of garnet suggests that there may be other complex ternary oxides such as single crystal mullite which may also be candidate materials for fiber reinforcements. Finally, CVD and single crystal SiC, although not oxides, do possess a high resistance to creep in the temperature range between 1550 and 1850 C and under stresses of 110 to 220 MPa. From a review of the literature, it appears that for high creep resistant applications sapphire, silicon carbide, yttrium aluminum garnet, mullite, and beryllia are desirable candidate materials which require further investigation.

Jones, Linda E.↗

Hysteresis in the Active Oxidation of SiC

Si and SiC show both passive oxidation behavior where a protective film of SiO2 forms and active oxidation behavior where a volatile suboxide SiO(g) forms. The active-to-passive and passive-to-active oxidation transitions are explored for both Si and SiC. Si shows a dramatic difference between the P(O2) for the two transitions of ~10-4 bar. The active-to-passive transition is controlled by the condition for SiO2/Si equilibrium and the passive-to-active transition is controlled by the decomposition of SiO2. In the case of SiC, the P(O2) for these transitions are much closer. The active-to-passive transition appears to be controlled by the condition for SiO2/SiC equilibrium. The passive-to-active transition appears to be controlled by the interfacial reaction of SiC and SiO2 and subsequent generation of gases at the interface which leads to scale breakdown.

Jacobson, Nathan S.↗

Properties of plasma sprayed bond coats

Increasing bond coat oxidation resistance has been clearly linked to increasing durability of the ceramic layer of TBC's. However, recent studies have shown that significant differences in TBC life can be achieved for different bond coats that have little or no difference in oxidation behavior. These results suggest bond coat properties other than oxidation resistance can also influence TBC life. A determination of which properties affect TBC life and an understanding of how these properties affect TBC life could be valuable in designing new, more durable TBC's. Unfortunately, there is little existing information on the physical and mechanical properties of bond coat materials and there are fewer comparative studies that can be used to determine which properties are important to TBC life. This paper compares the properties of three bond coat compositions that have similar oxidation behavior but different TBC lives. Analysis of the properties indicates that the coefficient of thermal expansion and stress relaxation (creep) behavior of the three alloys are strongly correlated to the observed differences in TBC life.

Brindley, W. J.↗

Research on Oxidation Wear Behavior of a New Hot Forging Die Steel

Dry sliding tests for the hot forging die steel DM were performed in air under the test temperature at 400-700 °C and the time of 0.5-4 h by a UMT-3 high-temperature wear tester. The wear behavior and characteristics were studied systematically to explore the general characters in severe oxidation conditions. The results showed that a mild-to-severe oxidation wear transition occurred with an increase in the test temperature and duration. The reason was clarified as the unstable M{sub 6}C carbides coarsening should be responsible for the severe delamination of tribo-oxide layer. More importantly, an intense oxidation wear with lower wear rates was found when the experimental temperature reaches 700 °C or after 4 h of test time at 600 °C, which was closely related to the degradation behavior during wear test. Furthermore, a new schematic diagram of oxidation wear of DM steel was proposed.

36 MATERIALS SCIENCE↗

Transient behavior of oxide fuels with controlled microstructure and Cr2O3 additive

Abstract Microstructure and Cr 2 O 3 doping profoundly impact the thermal-mechanical properties and fracture of oxides fuels. It is a challenge to study the transient behavior of nuclear fuels under loss-of-coolant-event (LOCA). In this study, the crack behavior of UO 2 pellets with controlled grain structure and Cr 2 O 3 doping was tested with rapid power ramping (300−900 °C per min) mimicking a prototypical LOCA heating profile. Dense micron-sized UO 2 pellets display well-maintained integrity without cracking with the ramping up to 1500 °C at a heating rate of 8 °C per second. Fracture occurs in both pure and Cr 2 O 3 -doped dense nano-sized UO 2 pellets. The Cr 2 O 3 doped oxide fuel pellet with a larger grain size (~ 22.2 μm) displays the best performance under LOCA testing due to its highest thermal conductivity under high temperature. FEA calculations suggest a temperature gradient across the fuel pellet during transient testing, resulting in residual stress and cracking, which can be correlated with their thermal-mechanical properties.

Zhao, Dong (ORCID:0000000191377257)↗

Behavior of oxidized platinum nanoparticles on an aligned carbon nanotube forest

We observed and analyzed the behavior of platinum nanoparticles (PtNPs) supported on aligned-carbon nanotubes (CNTs) at high temperatures by X-ray photoelectron spectroscopy and high-resolution transmission electron microscope observations. We found that the PtNPs moved toward the inner-side along each CNT on which they were deposited. The mechanism of this behavior is related to the redox reaction of Pt with the carbon atoms in the CNT. We also performed in-situ observation of this process at a high temperature using an environmental transmission electron microscope under an oxygen atmosphere. We found that the PtNPs penetrated down into a high-density aligned CNT forest along the tube axis and that the PtNPs changed their shape to fit the structure of the CNTs during their movement.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Oxidation of Al2O3 continuous fiber-reinforced/NiAl composites

The 1200 C and 1300 C isothermal and cyclic oxidation behavior of Al2O3 continuous fiber-reinforced/NiAl composites were studied. Oxidation resulted in formation of Al2O3 external scales in a similar manner as scales formed on monolithic NiAl. The isothermal oxidation of an Al2O3/NiAl composite resulted in oxidation of the matrix along the fiber/matrix interface near the fiber ends. This oxide acted as a wedge between the fiber and the matrix, and, under cyclic oxidation conditions, led to further oxidation along the fiber lengths and eventual cracking of the composite. The oxidation behavior of composites in which the Al2O3 fibers were sputter coated with nickel prior to processing was much more severe. This was attributed to open channels around the fibers which formed during processing, most likely as a result of the diffusion of the nickel coating into the matrix.

Doychak, J.↗

Oxidation of Slurry Aluminide Coatings on Cast Stainless Steel Alloy CF8C-Plus at 800oC in Water Vapor

A new, cast austenitic stainless steel, CF8C-Plus, has been developed for a wide range of high temperature applications, including diesel exhaust components, turbine casings and turbocharger housings. CF8C-Plus offers significant improvements in creep rupture life and creep rupture strength over standard CF8C steel. However, at higher temperatures and in more aggressive environments, such as those containing significant water vapor, an oxidation-resistant protective coating will be necessary. The oxidation behavior of alloys CF8C and CF8C-Plus with various aluminide coatings were compared at 800oC in air plus 10 vol% water vapor. Due to their affordability, slurry aluminides were the primary coating system of interest, although chemical vapor deposition (CVD) and pack cementation coatings were also compared. Additionally, a preliminary study of the low cycle fatigue behavior of aluminized CF8C-Plus was conducted at 800oC. Each type of coating provided substantial improvements in oxidation behavior, with simple slurry aluminides showing very good oxidation resistance after 4,000 h testing in water vapor. Preliminary low cycle fatigue results indicated that thicker aluminide coatings degraded high temperature fatigue properties of CF8C-Plus, whereas thinner coatings did not. Results suggest that appropriately designed slurry aluminide coatings are a viable option for economical, long-term oxidation protection of austenitic stainless steels in water vapor.

Coating↗