Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “MAGNETRONS”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 235 records · Page 13

Compression and strong rarefaction in high power impulse magnetron sputtering discharges

Gas compression and strong rarefaction have been observed for high power impulse magnetron sputtering (HIPIMS) discharges using a copper target in argon. Time-resolved ion saturation currents of 35 probes were simultaneously recorded for HIPIMS discharges operating far above the self-sputtering runaway threshold. The argon background pressure was a parameter for the evaluation of the spatial and temporal development of the plasma density distribution. The data can be interpreted by a massive onset of the sputtering flux (sputter wind) that causes a transient densification of the gas, followed by rarefaction and the replacement of gas plasma by the metal plasma of sustained self-sputtering. The plasma density pulse follows closely the power pulse at low pressure. At high pressure, the relatively remote probes recorded a density peak only after the discharge pulse, indicative for slow, diffusive ion transport.

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗

Origin of the Delayed Current Onset in High Power Impulse Magnetron Sputtering

Repetitive pulses of voltage and current are applied in high power impulse magnetron sputtering. The current pulse usually lags the applied voltage by a significant time, which in some cases can reach many 10s of microseconds. The current time lag is generally highly reproducible and jitters less than 1percent of the delay time. This work investigates the time lag experimentally and theoretically. The experiments include several different target and gas combinations, voltage and current amplitudes, gas pressures, pulse repetition rates, and pulse durations. It is shown that in all cases the inverse delay is approximately proportional to the applied voltage, where the proportionality factor depends on the combination of materials and the conditions selected. The proportionality factor contains the parameters of ionization and secondary electron emission. The statistical time lag is negligible while the formative time lag is large and usually dominated by the ion motion (inertia), although, at low pressure, the long free path of magnetized electrons causing ionization contributes to the delay.

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗

Discharge Physics of High Power Impulse Magnetron Sputtering

High power impulse magnetron sputtering (HIPIMS) is pulsed sputtering where the peak power exceeds the time-averaged power by typically two orders of magnitude. The peak power density, averaged over the target area, can reach or exceed 107 W/m2, leading to plasma conditions that make ionization of the sputtered atoms very likely. A brief review of HIPIMS operation is given in a tutorial manner, illustrated by some original data related to the self-sputtering of niobium in argon and krypton. Emphasis is put on the current-voltage-time relationships near the threshold of self-sputtering runaway. The great variety of current pulse shapes delivers clues on the very strong gas rarefaction, self-sputtering runaway conditions, and the stopping of runaway due to the evolution of atom ionization and ion return probabilities as the gas plasma is replaced by metal plasma. The discussions are completed by considering instabilities and the special case of ?gasless? self-sputtering.

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗

The influence of working gas pressure on interlayer mixing in magnetron-deposited Mo/Si multilayers

Impact of Ar gas pressure (1-4 mTorr) on the growth of amorphous interlayers in Mo/Si multilayers deposited by magnetron sputtering was investigated by small-angle x-ray scattering ({lambda} = 0.154 nm) and methods of cross-sectional transmission electron microscopy. Some reduction of thickness of the amorphous inter-layers with Ar pressure increase was found, while composition of the layers was enriched with molybdenum. The interface modification resulted in raise of EUV reflectance of the Mo/Si multilayers.

47 OTHER INSTRUMENTATION↗

Accounting for the Complex Surface Structure in Ellipsometric Studies of the Effects of Magnetron Sputtering Modes on the Growth and Optical Properties of In{sub 2}O{sub 3} Films

The efficiency of invoking additional information on optical transmission in solving the inverse problem of ellipsometry by a minimization method is demonstrated in practice for In{sub 2}O{sub 3} fi doped and nondoped with Sn on Al{sub 2}O{sub 3} (012) substrates. This approach allows the thickness and refractive index of thin films with rough surfaces to be uniquely determined. Solutions of the inverse problem in the framework of one-, two-, and multilayer models are compared. The last provides the best description of the experimental data and the correct parameters of the samples. The dependences of the investigated properties of films produced with different magnetron sputtering modes are found using the above methods and models and do not contradict general concepts about the film formation by this material.

36 MATERIALS SCIENCE↗

Easy Controlled Properties of Quaternary FeNiCrCd Thin Films Deposited from a Single dc Magnetron Sputtering Under the Influence of Deposition Rate

The quaternary FeNiCrCd thin films were produced from a single FeNiCrCr source on a commercial flexible polymer substrate using one dc magnetron sputtering technique. For that, a series of the films with a thickness of 50 nm were produced at different deposition rates of 0.02, 0.04, 0.06, and 0.08 nm/s, separately. In this study, as far as concerned, this was the first time that structural and magnetic properties of FeNiCrCd thin films were investigated. According to compositional analysis, the Fe and Cr contents slightly decreased with increasing deposition rate while Ni was almost constant, whereas those of the amount of Cd atoms increased. However, the atomic amounts of Fe and Cd in the films are quite different from those of the source material. The change of the atomic contents in the films from the source may be attributed to the relatively different bond energy/melting point of metals which have different contents sputtered from source material since this physical parameter is very significant for the sputtering process. For crystal structural analysis, a combination of hexagonal close-packed (hcp) and body-centered cubic (bcc) were observed. The peak intensity of the bcc-dominated planes decreased while the hcp-dominant plane increased since the change in peak intensities is compatible with the compositional analysis with increasing deposition rate. And, the grain sizes decreased gradually from 40.1 to 23.4 nm, with increasing deposition rate from 0.02, to 0.08 nm/s. Also, the film surfaces transformed from a rough to smooth surfaces with decreasing grain sizes as deposition rate increased. For magnetic analysis, the saturation magnetization M{sub s} values decreased as 1030, 773, 730, and 217 emu/cm{sup 3} with increasing deposition rate as 0.02, 0.04, 0.06, and 0.08 nm/s, respectively. In the same manner, the coercivity H{sub c} values were found as 11, 7, 6, and 2 Oe with the deposition rate of 0.02, 0.04, 0.06, and 0.08 nm/s, respectively. The decrease of the H{sub c} may have primarily come from the transformation of rough to smooth surface of the films. It may also be said that the films showed soft magnetic properties due to their low H{sub c} values with increasing deposition rate. Thus, the magnetic properties of the quaternary FeNiCrCd alloy films were seen to be easily improved with the deposition rate parameter for potential use in different industrial applications.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Magnetic and Magnetotransport Characteristics of Cr-Substituted Ni{sub 55}Mn{sub 34}Sn{sub 11} Thin Films Grown by Magnetron Sputtering

Highly oriented Cr-substituted Ni{sub 55}Mn{sub 34}Sn{sub 11} Heusler thin films having thickness ~ 400 nm were deposited by Ultrahigh vacuum dc magnetron sputtering on MgO (100) substrates. At room temperature, the films exhibit a mixture of dominant L2{sub 1} cubic austenite phase, as revealed by the intense (002) and (004) peaks, along with small fraction of the orthorhombic–martensitic phase. Surface morphology of the thin films showed distribution of Cr-rich and Cr-deficit regions together with patterned and aligned magnetic domains, thus bringing out the inherent room temperature ferromagnetism of the film. At temperatures above the Curie temperature, T{sub C} ~ 321 K, the magnetic behaviour of the films is seen to follow the Curie law rather than the Curie–Weiss law. Ferromagnetic to antiferromagnetic transition appears at T{sub N} ~ 247 K, which gives rise to exchange bias at low temperatures due to the coexistence of the two magnetic orders. This phase coexistence also leads to the formation of a spin glass state deep into the martensitic region. The film exhibits metal-like nature at high temperature and semiconductor-like behaviour with the lowering of temperature. A reentrant metallic state is observed at T ≤ 38 K during cooling that persists up to ≤ 62 K in warming cycle. The hysteresis in the ρ–T curve spread over a very wide temperature range confirms the magnetic phase coexistence in the martensitic state in the present thin films. The magnetoresistance (MR) first increases (2.4% at 300 K and H = 50 kOe) with temperature and maximizes to around ~ 3.25% at T = 150 K and then starts decreasing. Its value in the glassy state is very small. This shows that a magnetic liquid like state is more conducive to larger MR.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Photocatalytic activity of anatase titanium dioxide nanostructures prepared by reactive magnetron sputtering technique

In this work, nanostructured titanium dioxide (TiO{sub 2}) photocatalysts with high optical and structural homogeneity were successfully synthesized by dc reactive magnetron sputtering technique. The TiO{sub 2} thin films were produced with high structural homogeneity without any heat treatment. Analysis of the X-ray diffraction patterns and UV–visible spectroscopy gave an indication that the structure of prepared films is anatase with energy band gap of 3.23 eV. The Fourier-transform infrared spectroscopy has confirmed the formation of Ti–O bond. The average size of TiO{sub 2} particles in the deposited films was ranging in 5–7 nm. These nanostructures are very applicable as photocatalysts as their photocatalytic activity was determined from the degradation rate with UV irradiation time as the first order reaction rate constant was determined to be 2.4 × 10{sup −3} min{sup −1}.

36 MATERIALS SCIENCE↗

Physical properties of RF magnetron sputtered GaN/n-Si thin film: impacts of RF power

GaN thin film was successfully produced on n-Si(100) substrate by RF magnetron sputter under different RF power. Experimental measurement techniques such as UV/Vis spectroscopy, field emission scanning electron microscopy (FE-SEM), X-ray diffraction (XRD), atomic force microscopy (AFM), and Micro-Raman Spectroscopy were used to research effects of Radio Frequency power on physical properties of produced thin film. It has been found that produced thin film was polycrystalline structure with (100) and (110) planes of hexagonal GaN from X-ray diffraction measurement result. It also proved that increasing RF power gives rise to deterioration in crystal quality of GaN thin film. Reason of this deterioration was discussed. It has been achieved that increasing RF power has resulted in decreasing optical band gap energy of GaN thin film. Reasons for these changes in optical band gap energy were explained. It was seen that some thin films were grown as layer-plus-island mode (Stranski–Krastanov growth mode) and others were grown as layer-by-layer growth mode (Frank van der Merwe mode) from AFM analysis. It has been found that increasing RF power has resulted in improvement of surface morphology of thin film from field emission scanning electron microscopy analysis. However, reaching RF power to 125 W leads to start to deteriorate of surface of GaN thin film. The reasons for this have been discussed. E{sub 1}(TO) transverse optical phonon mode of hexagonal GaN with different intensity was detected from Micro-Raman Spectroscopy measurement. The reasons for this difference have been discussed. It was concluded that RF power has played a significant role in growing high quality GaN thin film. Morphological, structural, and optical properties of GaN thin film were enhanced by controlling RF power, making them a potential candidate for LED, solar cell, diode application.

77 NANOSCIENCE AND NANOTECHNOLOGY↗

Role of oxygen concentrations on structural and optical properties of RF magnetron sputtered ZnO thin films

We report an investigation on the effect of oxygen flow rate on the structural and optical properties of zinc oxide thin films prepared by RF magnetron sputtering. The structural measurements were carried using grazing incidence X-ray diffraction, atomic force microscopy and Raman spectroscopy. The role of oxygen partial pressure on the crystallinity, the surface morphology and vibrational modes has been established. The optical properties of the films were investigated using FR-Basic-VIS/NIR fitted with FR-Monitor software for film thickness, refractive index and color determination. The film thickness is observed to increase when oxygen is introduced at 4 sccm but eventual decrease with increase in the flow rate an indication of initial increase in rate of deposition followed by reduction. Elaborate explanations of these trends are provided.

36 MATERIALS SCIENCE↗

Properties of Gallium Oxide Films Obtained by HF-Magnetron Sputtering

The results of an analysis of structure and phase composition of gallium oxide films obtained by HF-magnetron sputtering are presented. It is shown that in the interval 290–350 K, the increase in the film conductivity with increasing temperature is due to the excitation of electrons from a local level Е{sub t} located 0.95 eV below the conduction band bottom.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Preparation and Oxidation Performance of a NiCoCrAlYSiHf + NiAl Composite Coating Deposited by Arc Ion Plating and Magnetron Sputtering Techniques

A NiCoCrAlYSiHf+NiAl composite coating was deposited onto a second-generation single-crystal superalloy René N5 by methods of arc ion plating and magnetron sputtering. After vacuum annealing, the composite coating exhibited a gradient distribution of elements, in which Al was enriched in outer layer and Cr was enriched in inner layer. Compared with conventional NiCoCrAlYSiHf and β-NiAl coatings, the composite coating was evaluated in isothermal and cyclic oxidation tests at 1100 °C in ambient air. The results showed that the oxidation rate of the composite coating was lower than that of NiCoCrAlYSiHf coating. Meanwhile, the extent of interdiffusion between coating and substrate in the composite coating was slighter compared with that in the β-NiAl coating. Microstructure evolutions of the composite coating after annealing and further oxidation test are investigated.

36 MATERIALS SCIENCE↗

Properties of Nb3Sn films fabricated by magnetron sputtering from a single target

Superconducting Nb3Sn films were fabricated on sapphire and fine grain Nb substrates by magnetron sputtering from a single stoichiometric Nb3Sn target. The structural, morphological and superconducting properties of the films annealed for 24 h at temperatures of 800-1000 {\deg}C were investigated. The effect of the annealing time at 1000 {\deg}C was examined for 1, 12, and 24 h. The film properties were characterized by X-ray diffraction, scanning electron microscopy, atomic force microscopy, energy dispersive X-ray spectroscopy, and Raman spectroscopy. The DC superconducting properties of the films were characterized by a four-point probe measurement down to cryogenic temperatures. The RF surface resistance of films was measured over a temperature range of 6-23 K using a 7.4 GHz sapphire-loaded Nb cavity. As-deposited Nb3Sn films on sapphire had a superconducting critical temperature of 17.21 K, which improved to 17.83 K when the film was annealed at 800 {\deg}C for 24 h. For the films annealed at 1000 {\deg}C, the surface Sn content was reduced to ~11.3 % for an annealing time of 12 h and to ~4.1 % for an annealing time of 24 h. The Raman spectra of the films confirmed the microstructural evolution after annealing. The RF superconducting critical temperature of the as-deposited Nb3Sn films on Nb was 16.02 K, which increased to 17.44 K when the film was annealed at 800 {\deg}C for 24 h.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Improvement of adhesion and barrier properties of biomedical stainless steel by deposition of YSZ coatings using RF magnetron sputtering

The AISI 316L stainless steel (SS) has been widely used in both artificial knee and hip joints in biomedical applications. In the present study, yttria stabilized zirconia (YSZ, ZrO{sub 2} + 8% Y{sub 2}O{sub 3}) films were deposited on AISI 316L SS by radio-frequency magnetron sputtering using different power densities (50–250 W) and deposition times (30–120 min) from a YSZ target. The crystallographic orientation and surface morphology were studied using X-ray diffraction (XRD), scanning electron microscopy (SEM) and transmission electron microscopy (TEM). The effects of the surface modification on the corrosion performance of AISI 316L SS were evaluated in phosphate buffered saline (PBS) solution using an electrochemical test on both the virgin and coated samples. The YSZ coatings have a (111) preferred orientation during crystal growth along the c-axis for short deposition times (30–60 min), whereas a polycrystalline structure forms during deposition times from 90 to 120 min. The corrosion protective character of the YSZ coatings depends on the crystal size and film thickness. A significant increase in adhesion and corrosion resistance by at least a factor of 46 and a higher breakdown potential were obtained for the deposited coatings at 200 W (120 min). - Highlights: • Well-formed and protective YSZ coatings were achieved on AISI 316L SS substrates. • Films grown at high power and long deposition time have polycrystalline structures. • The crystal size varies from ∼ 5 to 30 nm as both power and deposition time increased. • The differences of corrosion resistance are attributed to internal film structure.

36 MATERIALS SCIENCE↗

Influence of vanadium incorporation on the microstructure, mechanical and tribological properties of Nb–V–Si–N films deposited by reactive magnetron sputtering

Composite Nb–V–Si–N films with various V contents (3.7–13.2 at.%) were deposited by reactive magnetron sputtering and the effects of V content on the microstructure, mechanical and tribological properties of Nb–V–Si–N films were investigated. The results revealed that a three-phase structure, consisting of face-centered cubic (fcc) Nb–V–Si–N, hexagonal close-packed (hcp) Nb–V–Si–N and amorphous Si{sub 3}N{sub 4}, co-exists in the Nb–V–Si–N films and the cubic phase is dominant. The hardness and critical load (L{sub c}) of Nb–V–Si–N films initially increased gradually and reached a summit, then decreased with the increasing V content in the films and the maximum values were 35 GPa and 9.8 N, respectively, at 6.4 at.% V. The combination of V into Nb–Si–N film led to the fracture toughness linearly increasing from 1.11 MPa·m{sup 1/2} at 3.7 at.% V to 1.67 MPa·m{sup 1/2} at 13.2 at.% V. At room temperature (RT), the average friction coefficient decreased from 0.80 at 3.7 at.% V to 0.55 at 13.2 at.% V for the Nb–V–Si–N films. The wear rate of Nb–V–Si–N films initially decreased and then increased after reaching a minimum value of about 6.35 × 10{sup −} {sup 7} mm{sup 3}/N·mm at 6.4 at.% V. As the rise of testing temperature from 200 °C to 600 °C, the average friction coefficient of Nb–V–Si–N films decreased with the increase of the testing temperature regardless of V content. However, the wear rate gradually increased for all films. The average friction coefficient and wear rate at RT and elevated temperatures were mainly influenced by the vanadium oxides with weakly bonded lattice planes. - Highlight: • Fcc-Nb–V–Si–N, hcp-Nb–V–Si–N and amorphous Si{sub 3}N{sub 4} co-existed in the films. • The amount of Si{sub 3}N{sub 4} decreased with increasing V content in the films. • Hardness of Nb–V–Si–N film (6.4 at.%) reached a maximum value of 35 GPa. • Addition of V led to the increase of fracture toughness. • Tribological properties were influenced by lubricant wear debris.

36 MATERIALS SCIENCE↗

Effect of annealing on Curie temperature and phase transition in La{sub 0.55}Sr{sub 0.08}Mn{sub 0.37}O{sub 3} epitaxial films grown on SrTiO{sub 3} (100) substrates by reactive radio frequency magnetron sputtering

Mn-poor LaSrMnO{sub 3} (LSMO) epitaxial films were grown on SrTiO{sub 3} (100) substrates by radio frequency magnetron sputtering in an argon and oxygen gas mix, and then the samples were annealed in air at various temperatures (T{sub a}). 2 theta-chi X-ray diffraction mapping, nano-beam diffraction analysis through transmission electron microscopy, and electron back scatter diffraction through scanning electron microscopy revealed that the crystal symmetry of the LSMO films changed from monoclinic/orthorhombic to rhombohedral on annealing in air. Curie temperature (T{sub C}) of the LSMO films was found to increase with increasing T{sub a}, and become higher than the room temperature at T{sub a} ≥ 861 °C, indicating that the cause of these changes was the filling of oxygen and the transition of the crystal symmetry into rhombohedral. - Highlights: •Mn-poor LSMO changed from monoclinic/orthorhombic to rhombohedral by oxygen supply. •Mn-poor LSMO was increased T{sub C} by changed crystal symmetry, and it showed T{sub C} above RT. •Annealed in air effectively supplied O{sub 2} more than O{sub 2} gas during sputtering •EBSD is useful to evaluate crystal symmetry of complex oxide film from the substrate.

36 MATERIALS SCIENCE↗

Length-scale-dependent nanoindentation creep behaviour of Ti/Al multilayers by magnetron sputtering

This study presented length-scale-dependent room temperature creep behaviour of Ti/Al multilayers by nanoindentation. Ti/Al multilayers with individual layer thickness ranging from 10 nm to 250 nm were prepared by a direct current magnetron sputtering method. Microstructural analysis showed that the prepared Ti/Al multilayers were polycrystalline, with strong Ti (0002) and Al (111) texture. Nanoindentation creep tests were performed to examine the time-dependent creep deformation, stress exponent, creep strain rate sensitivity and contact creep compliance of the multilayers at room temperature. It was found that both the maximum creep deformation and the creep strain rate sensitivity increase with an increase in the individual layer thickness, indicating a length-scale-dependent creep behaviour of the Ti/Al multilayers. The values of stress exponent were found to lay in the range of 15.74–61.46, implying that the creep behaviour of the multilayers was controlled by the dislocation creep mechanism. Finally, the contact creep compliances of the Ti/Al multilayers were well modelled by a two-element Kelvin-Voigt model. From this, it was determined that the creep numbers and retardation times increased with increased individual layer thickness.

77 NANOSCIENCE AND NANOTECHNOLOGY↗

Correlation between structural and mechanical properties of RF magnetron sputter deposited hydroxyapatite coating

Highlights: • Microstructure and mechanical properties of textured hydroxyapatite (HA) coatings were evaluated. • TEM results revealed two types of coating microstructure corresponding to the film texture. • Elastic performance of the coating was determined by the texture of the HA coating. • HA coating with (300) texture showed larger elastic recovery. - Abstract: In the present study hydroxyapatite (HA) thin films with a,b-plain and c-plain preferential orientation were prepared by means of RF-magnetron sputtering with water vapor addition into a working gas atmosphere to investigate the influence of microstructural features on mechanical performance of the coating at nanoscale. The mechanical properties of the HA coatings textured along a,b- and c-axes by nanoindentation conclusively highlight that elastic modulus, H/E ratio, H{sup 3}/E{sup 2} parameter and percent of elastic recovery are determined by preferential orientation of the film. Nanoindentation reveals that the HA films exhibiting (300) texture possess commensurate nanohardness and lower elastic modulus compared to (002) oriented films, indicating that the former films possess higher resistance to cracking. The (002) and (300) textured coatings exhibited a nanohardness of 4.7 ± 2.0 GPa and 4.4 ± 2.2 GPa, respectively. The elastic modulus of the HA film with (300) and (002) preferential orientation was 75 ± 40 GPa and 103 ± 40 GPa, respectively. The HA coating with (300) texture showed a higher percentage of elastic recovery of 92% within unloading than that of the (002) textured film (69%).

36 MATERIALS SCIENCE↗