At least 235 records · Page 13

xLi2MnO3 (1-x)LiMeO2 and Li4Ti5O12 Cell Chemistry for Behind-the-Meter Storage Applications

Li- and Mn-rich layered oxide material (xLi2MnO3 (1-x)LiMeO2, Me = Ni, Mn, and etc., LMR-NM) is paired with Li4Ti5O12 (LTO) in a full cell and evaluated for the Behind-the-Meter Storage (BTMS) applications. The LMR-NM/LTO full cell shows very high capacities and excellent long-term cycle life. It delivers 192 mAh g-1 after 500 cycles at C/2 and 45 degrees C with a capacity retention of 75% and coulombic efficiency higher than 99.95%. It also has impressive rate capabilities. A capacity of 220 mAh g-1 is achieved at 2C which is 88 % of the initial capacity at C/10. The high cycling temperature clearly enhances electrochemical kinetics and activates more Li2MnO3 component, which gives high capacities, low cell impedance, and better rate capabilities. Moreover, it helps to form a relatively thick cathode-electrolyte interphase (CEI) film to suppress transition metal dissolution from the cathode surface. The upper cut-off voltage (UCV) of 3.0 V keeps the structural integrity of the cathode during cycling. A higher UCV of 3.2 V accelerates structural instabilities of the cathode as well as growth of the solid-electrolyte interphase (SEI) via transition metal dissolution and deposition on the anode surface. It results in higher cell impedance, worse capacity retention and faster capacity fade.

behind-the-meter storage↗

Long cycle and calendar life of Si-based Li-ion batteries enabled by localized high-concentration electrolytes and their surprising water tolerance

Silicon-based anodes promise an increase in energy density for Li-ion batteries, yet they suffer from a poor calendar life. Researchers have posited that fluorinated lithium salt forms reactive side products that destroy the solid electrolyte interphase (SEI), even without cycling. HF is one such reactive side product formed from trace water contamination in the electrolyte. Some electrolytes, such as localized high concentration electrolytes (LHCEs) may improve cell stability in highly reactive systems, such as Li metal and Si. In the present study, LHCEs containing 200-300 ppm of water retained up to 8% greater capacity (1200-1300 mAh/g Si) in calendar life tests over 200 days compared to dried electrolytes (< 20 ppm water). Calendar aging took place at 100% state of charge. Cells with 200-300 ppm water performed comparably to cells with 20 ppm water in cycle life tests (900-1000 mAh/g Si) . Even adding 1000 ppm water did not lead to rapid capacity fade in cells undergoing cycle life tests. Nano-FTIR spectroscopy revealed chemical and structural differences in the SEI for cells with 1000 ppm water compared to 200-300 ppm water. The SEI differences, including increased Li2O concentration, may have contributed to improved calendar life. This research reveals the capabilities of LHCEs to improve the calendar and cycle life of Si-based Li-ion batteries, despite the presence of a highly reactive contaminant.

25 ENERGY STORAGE↗

Ionic Interdiffusion at Cathode|Solid-Electrolyte Interface: A Machine Learning–Assisted Multiscale Investigation and Mitigation Strategies

Future lithium batteries are expected to use solid electrolytes to achieve higher energy density and fast charge capabilities. However, most solid electrolytes are thermodynamically unstable against layered oxide cathodes. In this study, the stability of LiCoO2 (LCO) cathode with Li10GeP2S12 (LGPS) solid electrolyte is investigated using ab initio molecular dynamics (AIMD) and machine learning molecular dynamics (MLMD). The propensity of ionic interdiffusion, formation of a passivating interphase layer, and corresponding decay in cell performance is addressed using a continuum model. Large-scale MLMD simulations confirm that the LCO|LGPS interface permits interdiffusion of cobalt (Co) and other ionic species, leading to the formation and growth of a resistive interphase and to dramatic capacity fade even in the first cycle. We examine the literature evidence that incorporating a thin layer of LiNb0.5Ta0.5O3 (LNTO) between LCO and LGPS prevents the interdiffusion of ions. Atomistic simulations suggest that substituting lithium (Li) in LNTO with Co is thermodynamically unfavorable, thereby inhibiting ionic interdiffusion. The stable Nb5+/Ta5+ states form a rigid metal-oxide framework, which consequently also prevents the substitution of niobium (Nb) or tantalum (Ta). However, continuum-level analysis suggests that the higher mechanical stiffness of LNTO can lead to interfacial delamination between the LCO and LNTO. This phenomenon reduces the effectiveness of the protective layer. This paper, therefore, highlights the need to develop novel interlayers that balance low ionic interdiffusion with low mechanical stiffness.

Ncube, Musawenkosi K.↗

Concentration dependent properties and plastic deformation facilitate instability of the solid-electrolyte interphase in Li-ion batteries

Lithium-ion batteries (LIBs) often suffer from capacity fading and poor cyclic performance due to mechanical degradation of the solid-electrolyte interphase (SEI). Here we perform numerical simulations and theoretical analysis to elucidate the role of plasticity in wrinkling and ratcheting behaviors of an SEI/electrode system. A coupled diffusion and finite deformation framework is formulated and numerically implemented as a user-element subroutine (UEL) to describe transient lithium diffusion and accompanying elastic–viscoplastic deformation of the electrode. It is found that concentration dependent properties and plastic deformation facilitate wrinkling in such a system. A wrinkled morphology may further lead to ratcheting and related failure under cycling. A phase diagram of four types of cyclic behaviorsis identified in terms of the charging rate and time. Our analysis suggests several potential strategies to avoid wrinkling and ratcheting instabilities, such as charging/discharging the electrode at a sufficiently slow rate, and/or introducing a thick artificial SEI with a pre-tension.

25 ENERGY STORAGE↗

Exploring battery material failure mechanisms through synchrotron X-ray characterization techniques

Rechargeable battery cycling performance and related safety have been persistent concerns. Here, it is crucial to decipher the capacity fading induced by electrode material failure via a range of techniques. Among these, synchrotron-based X-ray techniques with high flux and brightness play a key role in understanding degradation mechanisms. In this comprehensive review, we summarized recent advancements in degradation modes and mechanisms that revealed by synchrotron X-ray methodologies. Subsequently, an overview of X-ray absorption spectroscopy and X-ray scattering techniques are introduced for the characterizing failure phenomena at local coordination atomic environment and long-range order crystal structure scale, respectively. At last, we envision the future of material failure mechanism exploration.

25 ENERGY STORAGE↗

Inhomogeneous distribution of lithium and electrolyte in aged Li-ion cylindrical cells

Carbonate-based electrolytes in Li-ion batteries exhibit long range order in a frozen state, which enables their non-destructive analysis by diffraction methods. In the current study the spatial distribution of lithium and electrolyte inside the graphite anode was determined in cycled Li-ion cells using monochromatic spatially-resolved neutron diffraction measurements at 150 K. The results indicate a loss of lithium and electrolyte and their non-uniform distribution in the graphite anode in aged Li-ion cells. The observed lithium and electrolyte losses are directly correlated with two electrochemical performance degradation mechanisms, which are responsible for the cell capacity fade.

18650-type↗

Impact of secondary particle size and two-layer architectures on the high-rate performance of thick electrodes in lithium-ion battery pouch cells

Increasing lithium-ion battery gravimetric energy density to > 300 Wh/kg, while simultaneously meeting a cost target of $80/kWh, is of paramount importance to increasing the driving range and affordability of electric vehicles. One way to address this goal is to reduce inactive components by increasing electrode areal capacities, but conventional thick electrode designs typically perform poorly at high discharge rates due to Li + mass transport limitations. Here we compare the rate capability and cycle life of NMC 532/graphite pouch cells made with five different thick cathode and anode designs paired together in 25 combinations. We find that using different particle sizes to structure both the cathode and anode architectures in two-layer configurations results in a 2X capacity improvement over the worst-performing combination at high discharge rates (97 vs. 46 mAh/g at 2C). These different cathode/anode designs also translate to different cycle life performance, with many cells cycled at C/2 achieving ~80% capacity retention after 1000 cycles, and cells cycled at 2C showing different degrees of capacity fade. Altogether, these results demonstrate that simple, scalable changes in electrode design can significantly improve the performance of thick electrodes for high energy density batteries.

25 ENERGY STORAGE↗

Solvation-guided inhibition of manganese dissolution of lithium- and manganese- rich cathode via cyclic carbonate molecular engineering

Lithium and manganese-rich (LMR) layered oxides represent a leading class of high-energy cathode materials, but their practical realization is fundamentally limited by severe manganese (Mn) dissolution, a process that triggers structural degradation and rapid capacity fade. While mitigation efforts have predominantly focused on interfacial engineering, the intrinsic contribution of bulk electrolyte solvation to this degradation pathway remains largely unexplored, primarily due to the difficulty of deconvolving its effects from concurrent cathode-electrolyte interphase (CEI) formation. Here, we report an experimental design to isolate the role of solvation. We systematically varied the electrolyte solvent solvation power by substituting the strongly coordinating ethylene carbonate (EC) with its weaker coordinating fluorinated derivatives, fluoroethylene carbonate (FEC) and trans-4,5-Difluoro-1,3-dioxolan-2-one (DFEC), while maintaining a consistent interfacial chemistry. Remarkably, the electrolyte formulated with the weakest solvent, DFEC, exhibits superior cycling stability, suppressing Mn dissolution by up to 63% relative to the conventional EC-based system. Post-mortem analysis unequivocally attributes this performance enhancement to the preservation of the LMR cathode's structural integrity, a direct consequence of mitigated Mn dissolution. This work provides conclusive evidence that modulating bulk electrolyte solvation is a potent and direct strategy for stabilizing LMR cathodes, establishing a vital design principle for next-generation battery systems.

25 ENERGY STORAGE↗

Enhanced long-term cyclability in Li-Rich layered oxides by electrochemically constructing a Li x TM 3-x O 4 -type spinel shell

The poor long-term cycling stability, including the fast capacity fade and the severe voltage decay, has become the main concern hindering the practical application of Li-rich layered oxides, a promising cathode for high- energy-density Li-ion battery. Herein, we design and electrochemically construct a ~10 nm-thick Li x TM 3-x O 4 - type (TM ¼Ni, Co, Mn, 0 3 O 4 -type spinel phase and the good Liþconductivity of LiMn 2 O 4 -type spinel phase. Systemic structural and electrochemical analysis demonstrate that, it slows down the activation rate of Li 2 MnO 3 component and efficiently alleviates the lattice O loss at high voltage (>4.5 V) and Mn dissolution, thereby suppressing the structural degradation from the layered phase to the spinel phase in the bulk, eventually significantly enhancing the long-term cycling stability. This study adds richness into the Mn-based spinel phase system and provides a new heterostructure design strategy to improve the electrochemical performance of Li-rich layered cathodes and beyond.

25 ENERGY STORAGE↗

Unveiling decaying mechanism through quantitative structure-activity relationship in electrolytes for lithium-ion batteries

Understanding the decaying mechanism in lithium-ion batteries (LIBs) is critical to establishing a stable electrolyte system. Despite the advent of various novel electrolyte solvents designated for high-voltage LIBs, their working principles are not fully understood. Currently, oxidative decomposition of electrolytes is believed to be the major cause of capacity fade, and tremendous effort has been devoted to discovering a new electrolyte with enhanced anodic stability. However, the oxidative decomposition process cannot solely explain the rapid decay of some electrolyte systems with intrinsic high anodic stability when used with a high-nickel layered oxide cathode such as LiNi 0.6 Mn 0.2 Co 0.2 O 2 (NMC622). In this report, a study of the quantitative structure-activity relationship was conducted to deepen the mechanistic understanding of the decay in high-voltage LIBs. Here, the results obtained from the newly introduced molecular pair analysis and linear free-energy relationship (LFER) studies were highly consistent with the solvation-involved decaying mechanism in a high-nickel layered oxide cathode cycling at high voltage (> 4.5 V vs. Li/Li + ). There was no evidence correlating the solvation ability of electrolyte solvents with the decay of a high-nickel layered oxide cathode cycling at a relatively low voltage (< 4.3 V vs. Li/Li + ), nor with the high-voltage spinel cathode LiNi 0.5 Mn 1.5 O 4 (LNMO). Undoubtedly, the unveiled mechanistic insight provides a critical guideline for the development of an appropriate electrolyte system targeting different high-voltage cathode materials.

25 ENERGY STORAGE↗

Current Status and Future Directions of All-Solid-State Batteries with Lithium Metal Anodes, Sulfide Electrolytes, and Layered Ternary Oxide Cathodes

All-solid-state batteries (ASSBs) offer great promise as a next-generation energy storage technology with higher energy density, wider operating temperature range, and improved safety for electric vehicles. ASSBs employing lithium metal anodes (Li), sulfide-based solid-state electrolytes (SSE), and Ni-rich layered transition metal oxide cathodes (LiMO 2 , M = Ni, Mn, Co, Al) are particularly promising due to its superior electrochemical performance compared to other solid-electrolyte systems. However, the battery cycle life at high cathode mass loading and high current is still limited because the failure mechanism is not fully understood. Lithium dendrite growth at the anode or inside a solid electrolyte still represents as a serious risk of cell failure. Interfacial resistance increases attributed to electrolyte decomposition and interfacial void formation at both cathode–electrolyte and anode–electrolyte interfaces lead to gradual capacity fading. In this Review, we present the fundamental challenges and recent scientific understandings of each component in ASSBs. The novel diagnostic tools for these components, especially the interfaces buried under the surface that are often hard for characterization are mainly examined. Lastly, we offer a perspective for future research directions. We hope this Review will provide a timely snapshot of state-of-the-art research progress in ASSBs to accelerate the development of ASSBs.

25 ENERGY STORAGE↗

Unravelling high-temperature stability of lithium-ion battery with lithium-rich oxide cathode in localized high-concentration electrolyte

Lithium (Li)-rich manganese (Mn)-rich oxide (LMR) cathode materials, despite of the high specific capacity up to 250 mAh g-1 suffer from instability of cathode/electrolyte interfacial layer at high working voltages, causing continuous voltage decay and capacity fading, especially at elevated temperatures. In various battery systems, localized high-concentration electrolytes (LHCEs) have been widely reported as a promising candidate to form effective electrode/electrolyte interphases. Here, an optimized LHCE is studied in graphite (Gr)-based full cells being cycled at 25, 45 and 60 °C with the reference of a conventional LiPF6-based electrolyte. It is revealed that the LHCE can effectively suppress continuous electrolyte decompositions and mitigate the dissolution of Mn ions due to the formation of more protective electrode/electrolyte interphases on both anode and cathode, which, in turn, lead to significantly improved cycling stability and enhanced rate capability under the selected temperatures. The mechanistic understanding on the failure of the conventional LiPF6-containing electrolyte and the function of the LHCE in Gr||LMR cells under high temperatures provides valuable perspectives of electrolyte development for practical application of LMR cathodes in high energy density batteries over a wide temperature range.

Localized high-concentration electrolyte, Lithium-↗

Electrochemical-driven green recovery of lithium, graphite and cathode from lithium-ion batteries using water

The expected exponential increase in consumption of lithium-ion batteries (LIBs) would pose a unique challenge to the availability of near-critical resources like lithium and graphite in the upcoming decade. In this work, we present a lithium recovery process that utilizes a degradation mechanism, i.e., lithium plating, as a tool to concentrate metallic lithium at the anode/separator interface for convenient extraction at room temperature – using only water. Electrochemical characterization of fast charged (1–6 C) LIBs yielded a maximum capacity fade of 50% over ten cycles. The lithium plating was confirmed via voltage plateau analysis, coulombic efficiency, and DC resistance measurements. A maximum lithium plating condition was observed to exist between 4C and 5C, thereby limiting the energy consumption in the extraction process. Post-mortem film thickness measurement showed an incrementing film deposition with a maximum of 35 µm thickness. SEM and XPS analysis confirmed increasing concentration of a dense dendritic metallic lithium deposition on the anode/separator interface with C-rate. A green recovery process was adopted to extract the concentrated metallic lithium using distilled water. The lithium from the plated film, solid/electrolyte interface (SEI), electrolyte, anode, and cathode, was extracted as salts. A 37% improvement in lithium recoverability was achieved with fast charging under ambient conditions. XPS analysis showed ~92% of lithium yield with no residual lithium in the graphite. In addition, the battery-grade graphite was recovered with 97% purity after heat treatment of the washed anode film, and concentrated transition metals oxides in the cathode to 93% purity for convenient extraction.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Direct Observation of Electron Beam-Induced Phase Transition in MgCrMnO 4

Irreversible structural transformation in intercalation-type cathode materials, which has been frequently observed, has been perceived as a principal cause of capacity fading and voltage decay in (uni) multivalent batteries. Herein, we explored the electron beam-induced spinel to defective rocksalt phase transitions in MgCrMnO 4 , a potential multivalent cation intercalation cathode, using atomic-resolution imaging and spectroscopy in an aberration-corrected scanning transmission electron microscope. This dynamic electron beam irradiation study of specific structural transformations provides an atomistic understanding of the structural evolution observed in transition-metal oxide spinels during electrochemical cycling using multivalent cations, such as Mg 2+ . By combining an imaging study with first-principles modeling, we demonstrate that the mechanism of the spinel to defective rocksalt transformation in MgCrMnO 4 nanostructures is enabled by the presence of oxygen vacancies and is, therefore, very similar to that observed in transition-metal oxide spinels upon Li intercalation.

36 MATERIALS SCIENCE↗

Asymmetric Reaction Pathways of Conversion-Type Electrodes for Lithium-Ion Batteries

Metal oxides have been actively explored as promising conversion-type electrode materials for lithium ion batteries due to high deliverable capacity but still notorious for poor cyclability, capacity fading, voltage hysteresis, etc. Yet, the fundamental reason for the undesirable properties of metal oxides behind the repetitive conversion process is still obscure. In this work, we take advantage of synchrotron X-ray techniques as well as transmission electron microscopy to monitor the structural changes during both conversion (lithiation) and reconversion (delithiation) reactions. Difference in diffusion rates of lithium and metal plays a decisive role in determining the reaction pathway. We find lithium accommodation and extraction occur via different reaction routes: lithiation follows a kinetically driven way while delithiation adopts a route close to the thermodynamic ground state path. Thermodynamic structural evolution features the formation of an intermediate phase of Li-Metal (M)-O, suggesting lithium removal accompanies with the Li/M ionic exchange and rearrangement of oxygen framework. The slow diffusion of metal ions and the high kinetic and energy barrier for dissociating the intermediate phase are mainly responsible for uncompleted reconversion reaction, evidenced by remaining Li-M-O phase at the end of charge. Imperfect reconversion reaction eventually limits the utilization of lithium ions over the repeated cycling. Furthermore, this work sheds light on structural changes occurring at metal oxides during both conversion and reconversion processes, which is strongly linked with the performances of conversion-type materials in applications.

25 ENERGY STORAGE↗

Temperature-Dependent Reaction Pathways in FeS 2 : Reversibility and the Electrochemical Formation of Fe 3 S 4

The present study has used a variety of characterization techniques to determine the products and reaction pathways involved in the rechargeable Li–FeS 2 system. We revisit both the initial lithiation and subsequent cycling of FeS 2 employing an ionic liquid electrolyte to investigate the intermediate and final charge products formed under varying thermal conditions (room temperature to 100 °C). The detection of Li 2 S and hexagonal FeS as the intermediate phases in the initial lithiation and the electrochemical formation of greigite, Fe 3 S 4 , as a charge product in the rechargeable reaction differ significantly from previous reports. The conditions for Fe 3 S 4 formation are shown to be dependent on both the temperature (~60 °C) and the availability of sulfur to drive a FeS to Fe 3 S 4 transformation. Upon further cycling, Fe 3 S 4 transforms to a lower sulfur content iron sulfide phase, a process which coincides with the loss of sulfur based on the new reaction pathways established in this work. The connection between sulfur loss, capacity fade, and charge product composition highlights the critical need to retain sulfur in the active material upon cycling.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Surface Stabilization with Fluorine of Layered Ultrahigh-Nickel Oxide Cathodes for Lithium-Ion Batteries

High-nickel layered oxide cathodes are key to meet the demands of the electric vehicle industry because of their high specific capacity. However, commercialization of these materials is hindered by critical challenges, such as phase transitions, particle cracking, aggressive surface reactivity, and thermal instability. Cation doping along with surface coating has proven to be an effective way to circumvent some of these issues to a large extent. Herein, fluorine coating is employed on a high-nickel Li[Ni 0.95 Mn 0.015 Co 0.02 Al 0.01 Mg 0.005 ]O 2 (NMCAM) cathode via a solution route. Detailed structural and electrochemical analyses indicate fluorine largely decorates the surface at low enough calcination temperatures. The cathode with 1 mol % fluorine coating exhibits a capacity retention of 71% after 500 cycles as compared to 59% for the control sample when cycled to a high cutoff voltage of 4.3 V in a full cell configuration with graphite anode. Post-mortem analysis of cycled electrodes reveals that surface reactivity is a major contributor to capacity fade as compared to particle cracking. Fluorine coating reduces surface reactivity and the depth to which rock-salt phase is formed on the surface during cycling. The thermal stability is also enhanced after fluorine coating as the material shows less heat release at high states of charge. Furthermore, this work demonstrates an effective, economical, and scalable way to stabilize the surface with fluorine and enhance the electrochemical performance of high-nickel cathodes.

25 ENERGY STORAGE↗

Tin Metal Improves the Lithiation Kinetics of High-Capacity Silicon Anodes

Si-based anodes present a great promise for high energy density lithium-ion batteries. However, its commercialization is largely hindered by a grand challenge of a rapid capacity fade. Here, we demonstrate excellent cycling stability on a Si-Sn thin film electrode that outperforms pure Si or Sn counterpart under the similar conditions. Combined with the first-principles calculations, in situ transmission electron microscopy studies reveal a reduced volume expansion, increased conductivity, as well as dynamic rearrangement upon lithiation of the Si-Sn film. Here we attribute the improved lithiation kinetics to the formation of a conductive matrix that comprises a mosaic of nanostructured Sn, Li y Sn (specifically, Li 7 Sn 2 develops around the lithiation potential of Si), and Li x Si. This work provides an important advance in understanding the lithiation mechanism of Si-based anodes for next-generation lithium-ion batteries.