Identification of a paramagnetic recombination center in silicon/silicon-dioxide interface
A paramagnetic recombination center having an orthorhombic symmetry with g[110] = 2.0095(2), g[001] = 2.0038(2), and g[110] = 2.0029(2) is found at the interface between silicon and native oxide. The center is referred to P{sub m} center and observed by a spin dependent recombination based electron paramagnetic resonance detection that has the sensitivity of {approx}10{sup 11} spins/cm{sup 2}. The employment of an isotopically enriched {sup 28}Si sample with the concentration of {sup 29}Si nuclear spins reduced to 0.017% leads to narrowing of the resonance line. This narrowing is the key for the accurate determination of the angular dependence of the g-factor.