At least 235 records · Page 13

Materials for Advanced Ultra-Supercritical (AUSC) Steam Turbines – AUSC Component Demonstration

The work by the United States Department of Energy (U.S. DOE)/Ohio Coal Development Office (OCDO) Advanced Ultra-Supercritical (AUSC) Steam Boiler and Turbine Materials Consortia from 2001 through September 2015 was primarily focused on lab scale and pilot scale materials testing. The field testing included air-cooled probes and steam-cooled “loops” that were installed into existing utility boilers to gain exposure of these materials to realistic conditions of high temperature and corrosion due to the constituents in the coal ash. Successful research and development resulted in identification of metallic alloy materials and fabrication processes suited for power generation applications with metal temperatures up to approximately 1472°F (800°C). These materials or alloys have shown, in extensive laboratory tests and shop fabrication studies, to have excellent applicability for high-efficiency low CO2 transformational power generation technologies. However, as valuable as these material field tests have been for obtaining information, their scale is significantly below that required to minimize the risk associated with a power company building a multi-billion-dollar AUSC power plant. To decrease the identified risk barriers to full-scale implementation of these advanced materials, the U.S. DOE/OCDO AUSC Steam Boiler and Turbine Materials Consortia identified the key areas of the technology that need to be tested at a larger scale. Based upon the recommendations and outcome of a Consortia-sponsored workshop with the U.S.’s leading utilities, a Component Test (ComTest) Program for AUSC was proposed. The AUSC ComTest program would define materials performance requirements, plan for overall advanced system integration, design critical component tests, fabricate components for testing from advanced materials, and carry out the tests. A Pre-FEED evaluation of the test facility including the evaluation of three potential sites has been completed and previously reported. This report describes the Front-End Engineering Design (FEED), Detailed Engineering and the Environmental Assessment of the ComTest project. A significant amount of work was accomplished during Phase 1 to identity the components, as well as the component size, that would be manufactured from advanced alloys such as INCONEL 740H or HAYNES 282 alloys. Pathways to supply these components for ComTest have been identified as well as any further development that would be required. Every project of this nature has challenges and this project was no exception. The greatest challenge has been the project cost. Largely due to the infrastructure and balance of plant equipment upgrades required for Youngstown Thermal, the estimated project cost for the “base case” project was greater than originally budgeted. The project team spent a significant amount of time exploring opportunities for reducing the project cost. These options included: • Youngstown Thermal was exploring building a Combined Heat and Power (CHP) unit at their facility. The Youngstown Thermal staff, supported by Thermal Engineering Group, worked with the project team to determine whether it was economically desirable to supply ComTest with steam and other utilities, which would be supplied by the CHP project. • The project team also evaluated opportunities to optimize the project scope to reduce cost, such as reducing project scope by eliminating the Superheater Outlet Header test. • Southern Company had offered two sites as possible host locations for ComTest. Both sites had infrastructure in place such as steam from an existing unit, natural gas, cooling water and ample electrical power that would be required to be added at the Youngstown Thermal site. Utilizing this existing infrastructure could reduce the project cost. An additional project challenge was the departure of Babcock and Wilcox from the project in September 2016. This project setback was overcome by GE Power’s willingness to assume the design of the ComTest superheater. Since the project could not proceed without the superheater, this was a very positive project development. The merger of the GE Power and Alstom Power steam turbine divisions created synergies leading to the conclusion that instead of building a small-scale turbine, a more practical and useful endeavor would be to validate the manufacturing technology and supplier readiness for fabricating and machining full scale steam turbine components. Consequently, in March 2017, GE Power decided that a steam turbine test would not be necessary as part of the ComTest demonstration. Removing the operational testing of the steam turbine from ComTest further reduced the total project cost. Additionally, there was an opportunity to move ComTest from Youngstown Thermal to one of the Southern Company sites and operate ComTest at supercritical steam conditions and test the steam turbine main stop/control valve at a temperature and pressure that would be representative of the conditions of a high pressure steam turbine inlet valve. The steam could also possibly be returned to the host boiler so there would be no economic penalty of using this steam for ComTest. Relocating the project could further reduce the project cost due to the infrastructure already in place, including high pressure natural gas and cooling water, and the potential for heat integration, allowing a reduction of operating costs. Due to these potential cost reductions, it was decided to move the project away from Youngstown Thermal in March 2017. As integrating ComTest at the Southern Company site was explored, an issue was raised regarding the integration of the ComTest cycle with the plant steam cycle. Steam would be supplied to ComTest at nominally ~3865 psia and 775°F. The steam would be heated with natural gas to 1400°F for the valve test and then cooled to 1000°F so that the steam would be returned to the host boiler at the same conditions as their high pressure steam turbine inlet. However, there were concerns raised that the addition of the energy (natural gas) to the steam could trigger a New Source Review on the unit. Southern Company did not want ComTest to cause this review, so condensing all of the steam exiting ComTest and returning it to the host steam cycle as condensate was explored to insure there would be no implication that ComTest was adding energy to the host plant’s steam cycle. Ultimately, Southern Company decided that they wanted to “decouple” ComTest from the operating unit, making ComTest self-supporting, similar to the Youngstown Thermal “base case.” Without the steam turbine, the project team reached a consensus that operating the ComTest Superheater and steam turbine valves at the typical pressure of a package boiler (~1000 psig) would not generate enough useful technical information to justify the cost of the test. Therefore, it was decided in the December 2017 project quarterly meeting to cancel the operational phase of ComTest. Throughout the engineering phase of ComTest, manufacturing and supply chain challenges were identified. When GE Power recommended dropping the steam turbine test from ComTest, they identified many important manufacturing issues that should be evaluated and demonstrated. Other challenges had been raised by the GE Power group designing the superheater as well as those engineering components such as pressure relief and steam turbine bypass valves. In the December 2017 meeting, the project team decided that it was more beneficial to the AUSC technology to pursue these manufacturing and supply chain issues as Phase 2 of the ComTest project. This report is organized in the following manner: • Section 2 discusses the ComTest project background and organization. • Section 3 discussed project management. • Section 4 discusses the design of the ComTest AUSC components – the Superheater, steam turbine and Superheater Outlet Header. • Section 5 discusses the implementation of ComTest at Youngstown Thermal and the Southern Company site. • Section 6 discusses the development of the AUSC Supply Chain • Section 7 discusses the recommended plan for Phase 2 of ComTest

01 COAL, LIGNITE, AND PEAT↗

Nondestructive ultrasonic characterization of a triple-weld-bead wire arc additively manufactured ER70S-6 S-curved wall

Understanding build-scale microstructural variation in wire arc additive manufacturing (WAAM) of low-carbon steels is essential for ensuring consistent structure–property relationships throughout large components. Conventional destructive characterization techniques, such as scanning electron microscopy (SEM) and electron backscatter diffraction (EBSD), are time-intensive and limited to localized regions, making comprehensive evaluation of large WAAM structures challenging. In this study, a nondestructive ultrasonic approach was employed to characterize a 252 mm tall ER70S-6 S-curved WAAM wall produced using a triple-bead deposition strategy. Optical and SEM analysis revealed a repeating dual-region microstructure consisting of uniform polygonal ferrite at melt pool centers and heterogeneous ferrite with coarse and fine grains near melt pool boundaries, attributed to cyclic thermal conditions. Longitudinal ultrasonic backscatter imaging was used to evaluate the continuity of this periodicity along the full build height. The ultrasonic response exhibited a consistent repeating pattern that correlated with the observed layer-wise microstructural variation. X-ray computed tomography confirmed the absence of detectable porosity, indicating that ultrasonic contrast is primarily governed by grain morphology. Overall, the results indicate that longitudinal backscatter ultrasound is a promising nondestructive characterization technique for validating microstructural variations along the s-curved WAAM wall, with significant potential for microstructure optimization and process control.

36 MATERIALS SCIENCE↗

Fluid Flow Phenomena during Welding

MOLTEN WELD POOLS are dynamic. Liquid in the weld pool in acted on by several strong forces, which can result in high-velocity fluid motion. Fluid flow velocities exceeding 1 m/s (3.3 ft/s) have been observed in gas tungsten arc (GTA) welds under ordinary welding conditions, and higher velocities have been measured in submerged arc welds. Fluid flow is important because it affects weld shape and is related to the formation of a variety of weld defects. Moving liquid transports heat and often dominates heat transport in the weld pool. Because heat transport by mass flow depends on the direction and speed of fluid motion, weld pool shape can differ dramatically from that predicted by conductive heat flow. Temperature gradients are also altered by fluid flow, which can affect weld microstructure. A number of defects in GTA welds have been attributed to fluid flow or changes in fluid flow, including lack of penetration, top bead roughness, humped beads, finger penetration, and undercutting. Instabilities in the liquid film around the keyhole in electron beam and laser welds are responsible for the uneven penetration (spiking) characteristic of these types of welds.

36 MATERIALS SCIENCE↗

Non-Intrusive Load Monitoring of EBW Processes A Second Study [Slides]

The Objective is to Determine if induced off-nominal welding disturbances: (1) Beam arc out (weld on high vapor pressure aluminum plate); (2) Pulsed beam voltage; (3) Pulsed beam current; and (4) Pulsed beam focus current can be observed in the input power to the high-voltage cabinet powering the EB gun, ie Non-Instrusive Load Monitoring (NILM).

36 MATERIALS SCIENCE↗

Transition of creep damage region in dissimilar welds between Inconel 740H Ni-based superalloy and P92 ferritic/martensitic steel

Highlights: • The fresh martensite formed in P92-sided CGHAZ during PWHT due to high Ni content. • Transition from type I to type IV cracking was observed with increasing temperature. • Creep damaged area changed depending on the dominant creep mechanism. • The transition value of Larson-Miller parameter would be within 25,063–26,168. - Abstract: Characterization of microstructures and creep fracture characteristics of dissimilar welds between Ni-based Inconel 740H superalloy and ferritic/martensitic P92 steel has been investigated. The welds were produced by shielded metal arc (SMA) welding process with the AWS A5.11 Class ENiCrFe-3 filler metal, commonly known as Inconel 182 superalloy. Postweld heat treatment (PWHT) at 760 °C for 4 h was conducted to temper the martensite in heat-affected zone (HAZ) of P92 and to form γ′ strengthener in Inconel 740H. The deposited Inconel 182 austenitic weld metal had a columnar microstructure, and grew epitaxially from the Inconel 740H base metal. The weld interface between P92 and weld metal was characterized by the discrete line with a minimal inter-diffusion, where the fresh untempered martensite was found to be formed during PWHT due to higher Ni contents diffused from Inconel 182 into P92. The P92 base metal and Inconel 182 weld metal displayed low hardness values (~240 Hv), and the sharp hardness increase was detected at coarse-grained HAZ of P92 while the hardness minimum occurred at the fine-grained HAZ (FGHAZ). Fracture location after creep was found to shift from the P92-sided fusion line to the FGHAZ of P92 with increasing creep temperature. The carbon migration from the P92 into the weld metal was not significant at lower creep temperature (600 °C), where the crack initiation at the P92-sided fusion line appeared to be related with a significant strain incompatibility across the fusion line. At both 650 °C and 700 °C where diffusion-controlled creep was more pronounced, the type IV cracking was observed. This may be attributed to the strain localization at the weak grain boundaries of FGHAZ due to the smaller grain size as well as the lack of grain boundary strengthening by carbides.

36 MATERIALS SCIENCE↗

Methodology for Estimating Thermal and Neutron Embrittlement of Austenitic Stainless Steel Welds During Service in Light Water Reactors

The effect of thermal aging on the degradation of fracture toughness and Charpy-impact properties of austenitic stainless steel (SS) welds has been characterized at reactor temperatures. The solidification behavior and the distribution and morphology of the ferrite phase in SS welds are described. Thermal aging of the welds results in moderate decreases in Charpy-impact strength and fracture toughness. The upper-shelf Charpy-impact energy of aged welds decreases by 50–80 J/cm2. The decrease in fracture toughness J-R curve, or JIc is relatively small. Thermal aging has minimal effect on the tensile strength. The fracture properties of SS welds are insensitive to filler metal; the welding process has a significant effect. The large variability in the data makes it difficult to establish the effect of the welding process on fracture properties of SS welds. Consequently, the approach used for evaluating thermal and neutron embrittlement of austenitic SS welds relies on establishing a lower-bound fracture toughness J-R curve for unaged and aged, and non-irradiated and irradiated, SS welds. The existing fracture toughness J-R curve data for SS welds have been reviewed and evaluated to define lower-bound J-R curve for submerged arc (SA)/shielded metal arc (SMA)/manual metal arc (MMA) welds and gas tungsten arc (GTA)/tungsten inert gas (TIG) welds in the unaged and aged conditions. At reactor temperatures, the fracture toughness of GTA/TIG welds is a factor of about 2.3 higher than that of SA/SMA/MMA welds. Thermal aging decreases the fracture toughness by about 20%. The potential combined effects of thermal and neutron embrittlement of austenitic SS welds are also described. Lower-bound curves are presented that define the change in coefficient C and exponent n of the power-law J-R curve and the JIc value for SS welds as a function of neutron dose. The potential effects of reactor coolant environment on the fracture toughness of austenitic SS welds are also discussed.

Chopra, O. K.↗

LDRD 19A42-015, Multi-Wire Arc Additive Manufacturing

Additive manufacturing (AM) techniques can efficiently and cost-effectively fabricate components with both geometrical and compositional complexities, where functionally-graded compositions in a component allow multiple service requirements to be simultaneously addressed, such as corrosion and high temperature structural requirements. High cost alloy compositions need only be deposited in local areas where they are needed. A multi-wire arc additive manufacturing (m-WAAM) system was developed to enable functionally-graded, additively manufactured complex structures. The m-WAAM system utilizes multiple filler wire alloys, allowing control of composition and composition gradients in the component during additive fabrication. Ultimately, this project successfully developed a high deposition rate, arc-based, additive manufacturing process with the truly novel capability of enabling spatial composition tailoring during the build of the component. System capabilities and process science will be studied in a follow-on LDRD starting next year.

36 MATERIALS SCIENCE↗

Integrated Recycling Test Fuel Fabrication

The Integrated Recycling Test is a collaborative irradiation test that will electrochemically recycle used light water reactor fuel into metallic fuel feedstock. The feedstock will be fabricated into a metallic fast reactor type fuel that will be irradiation tested in a drop in capsule test in the Advanced Test Reactor on the Idaho National Laboratory site. This paper will summarize the fuel fabrication activities and design efforts. Casting development will include developing a casting process and system. The closure welding system will be based on the gas tungsten arc burst welding process. The settler/bonder system has been designed to be a simple system which provides heating and controllable impact energy to ensure wetting between the fuel and cladding. The final major pieces of equipment to be designed are the weld and sodium bond inspection system. Both x-radiography and ultrasonic inspection techniques have been examine experimentally and found to be feasible, however the final remote system has not been designed. Conceptual designs for radiography and an ultrasonic system have been made.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Microstructure and Corrosion Properties of Laser-Welded SAF 2507 Super Duplex Stainless Steel Joints

SAF 2507 super duplex stainless steel has been welded using laser beam (LB) welding and laser/gas metal arc hybrid (LGH) welding processes. The pitting and intergranular corrosion properties of the welding joints have been tested using electrochemical testing and microstructure observations. The volume fraction of the ferrite phase reaches 70% in the weld zone of the LB welding joint, while the volume fraction of the ferrite phase is 60% for the welding joint of LGH due to the introduction of Ni from welding wire. The pitting corrosion resistance of the welding joint for LB is better than that of LGH. The pitting corrosion is easily conceived in the heat-affected zone (HAZ) because of the formation of Cr{sub 2}N in the HAZ during welding.

36 MATERIALS SCIENCE↗

Microstructures and mechanical properties of a welded CoCrFeMnNi high-entropy alloy

The response of the CoCrFeMnNi high-entropy alloy to weld thermal cycles was investigated to determine its applicability as an engineering structural material. Two processes were used: high-energy-density, low-heat-input electron beam (EB) welding and low-energy-density, high-heat-input gas tungsten arc (GTA) welding. Weldability was determined through comprehensive microstructural and mechanical property characterisation of the welds. The welds did not develop solidification cracking or heat-affected zone cracks. The microstructures in weld fusion zones are similar to that in the as-cast materials, consisting of large columnar grains with dendrite. The dendrite arm spacing and the extent of elemental segregation were less in the welds than in the cast ingot, and also were less pronounced in the EB weld than in the GTA weld. Compositional microsegregation between dendritic cores and interdendritic regions of the welds was insignificant. Both welds exhibited slightly higher yield strengths than the base metal. The EB weld possessed comparable tensile strength and ductility to that of the base metal. In comparison, the GTA weld maintained ∼80% of the base metal's tensile strength and 50% of the ductility.

36 MATERIALS SCIENCE↗

In-situ Radiography of Hydrogen Porosity Growth and Development in Aluminum Welds

In aluminum welding, hydrogen contamination is the main cause of the welding defect, porosity. Porosity in welds can adversely affect the mechanical properties such as tensile strength, fatigue life and ductility. There have been a variety of solutions to help reduce porosity in aluminum welds including finding the source of hydrogen. However, in some cases the amount of hydrogen may be drastically reduced but impossible to completely eliminate. Another approach to this issue is to understand where a pore originates and how it moves and grows within the weld pool. This information may lead to a more innovative method for pore elimination during gas tungsten arc (GTA) welding of aluminum.

42 ENGINEERING↗

Assessment of Stress Corrosion Cracking Resistance of Activated Tungsten Inert Gas-Welded Duplex Stainless Steel Joints

The stress corrosion cracking behavior of duplex stainless steel (DSS) weld joint largely depends on the ferrite-austenite phase microstructure balance. This phase balance is decided by the welding process used, heat input, welding conditions and the weld metal chemistry. In this investigation, the influence of activated tungsten inert gas (ATIG) and tungsten inert gas (TIG) welding processes on the stress corrosion cracking (SCC) resistance of DSS joints was evaluated and compared. Boiling magnesium chloride (45 wt.%) environment maintained at 155 °C was used. The microstructure and ferrite content of different weld zones are correlated with the outcome of sustained load, SCC test. Irrespective of the welding processes used, SCC resistance of weld joints was inferior to that of the base metal. However, ATIG weld joint exhibited superior resistance to SCC than the TIG weld joint. The crack initiation and final failure were in the weld metal for the ATIG weld joint; they were in the heat-affected zone for the TIG weld joint.

36 MATERIALS SCIENCE↗

Analysis of the Corrosion Behavior of an A-TIG Welded SS 409 Weld Fusion Zone

AISI 409 (SS 409) ferritic stainless steel is generally used as the thick gauge section in freight train wagons, in ocean containers, and in sugar refinery equipment. Activating the flux tungsten inert gas (A-TIG) welding process can reduce the welding cost during fabrication of thick sections. However, corrosion behavior of the A-TIG weld fusion zone is a prime concern for this type of steel. In the present work, the effect of the A-TIG welding process parameters on the corrosion behavior of a weld fusion zone made of 8-mm-thick AISI 409 ferritic stainless-steel plate has been analyzed. Potentiodynamic polarization tests were performed to evaluate the corrosion behavior. The maximum corrosion potential (E{sub corr}) was shown by the weld made using a welding current of 215 A, a welding speed of 95 mm/min, and a flux coating density of 0.81 mg/cm{sup 2}. The minimum E{sub corr} was observed in the weld made using a welding current of 190 A, a welding speed of 120 mm/min, and a flux coating density of 1.40 mg/cm{sup 2}. The current study also presents the inclusive microstructure–corrosion property relationships using the collective techniques of scanning electron microscopy, energy-dispersive x-ray spectroscopy, and x-ray diffraction.

36 MATERIALS SCIENCE↗

Neutron diffraction illustrates residual stress behavior of welded alloys used as radioactive confinement boundary

Corrosion-resistant welded alloys are frequently used as a leak-tight boundary in critical applications that require confinement of hazardous and/or radioactive substances, including an increasing population of spent nuclear fuel (SNF) canisters. The behavior of residual stresses generated as a result of irregular elastic–plastic deformation during processes such as welding is one of today's key issues to a full understanding of the aging mechanisms that may compromise the confinement boundary. Whether such processes and any subsequent weld repairs, not subjected to post-weld heat treatment, would negatively affect the initial material by introducing through-thickness tensile stresses remains an open question. Here we report the first residual stress measurements using neutron diffraction on the welded joints of a SNF canister. We found significant tensile residual stresses in the as welded sample, indicating that initiation and through-thickness growth of cracks may be possible. Following repair, we observed a stress redistribution and introduction of beneficial compressive stresses. We anticipate our results will improve understanding of confinement susceptibility to aging and guide improvements in repair techniques.

36 MATERIALS SCIENCE↗

A Versatile Remediation Module for Remote Repair of Spent Nuclear Fuel and High-Level Waste Storage Containers

Oak Ridge National Laboratory (ORNL) successfully demonstrated the Versatile Remediation Module (VRM), a prototype module designed and built by ORNL for on-site remote repair of welded stainless steel storage containers for spent nuclear fuel and high-level radioactive waste. This paper describes the VRM prototype and its design features and components to support continued long-term storage or off-site transportation of spent nuclear fuel and high-level radioactive waste currently stored in storage containers. A remote (100 ft away from the simulated radiative environment) demonstration of the VRM was successfully performed on a full-scale mock-up welded stainless steel canister. The VRM is designed with features to accommodate remediation techniques beyond those currently selected and described in this paper. Therefore, many of the VRM’s features may benefit other remote nuclear or nonnuclear applications. The VRM is envisioned to serve as a development center to facilitate and enhance further development of new remediation technologies.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Structurally Integrated Coatings for Wear and Corrosion

Wear and corrosion of structures cuts across industries and continues to challenge materials scientists and engineers to develop cost effective solutions. Industries typically seek mature technologies that can be implemented for production with rapid or minimal development and have little appetite for the longer-term materials research and development required to solve complex problems. The collaborative work performed in this project addressed the complexity of this problem in a multi-year program that industries would be reluctant to undertake without government partnership. This effort built upon the prior development of Advanced Abrasion Resistant Materials conduct by Caterpillar Inc. under DOE Cooperative Agreement No. DE-FC26-01NT41054. In this referenced work, coatings were developed that exhibited significant wear life improvements over standard carburized heat treated steel in abrasive wear applications. The technology used in this referenced work, arc lamp fusing of thermal spray coatings, was one of the primary technical paths in this work effort. In addition to extending the capability of the coating technology to address corrosion issues, additional competitive coating technologies were evaluated to insure that the best technology was developed to meet the goals of the program. From this, plasma transferred arc (PTA) welding was selected as the second primary technology that was investigated. Specifically, this project developed improved, cost effective surfacing materials and processes for wear and corrosion resistance in both sliding and abrasive wear applications. Materials with wear and corrosion performance improvements that are 4 to 5 times greater than heat treated steels were developed. The materials developed were based on low cost material systems utilizing ferrous substrates and stainless steel type matrix with hard particulates formed from borides and carbides. Affordability was assessed against other competing hard surfacing or coating techniques, balanced with overall materials performance. State-of-the-art design and simulation capabilities were used to guide materials and process refinement. Caterpillar was the lead of the multi-partner collaborative project. Specific tasks were performed by the partners base on their unique capabilities. The project team was selected to include leaders in the field of material development, processing, modeling, and material characterization. Specifically, industrial members include the suppliers Deloro Stellite and Powder Alloy Corporation., who provided the experimental alloys and who aided in the development of the costs for the alloys, the Missouri University of Science and Technology and Iowa State University, who provided help in the alloy development and material characterization, QuesTek Innovations, a small company specializing the microstructural modeling of materials, and the DOE laboratories, Oak Ridge National Laboratory and National Energy Technology Laboratory (Albany), who provided unique coating process capability and wear characterization testing. The technologies developed in this program are expected to yield energy savings of about 50% over existing technologies, or 110 trillion BTUs per year by 2020 when fully implemented. Primary applications by Caterpillar are to replace the surface of machine components which are currently carburized and heat treated with new cladding materials with double the wear life. The new cladding technologies will consume less energy than carburizing. Thus, nearly 50% energy savings can be expected as a result from elimination of the heat treat process and the reduce wear of the materials. Additionally, when technologies from this project are applied on titanium or other non-ferrous substrates to make lighter weight, more wear resistant, and more efficient structures, significant fuel savings can be realized. With the anticipated drastic reduction in cost for refining titanium-containing ores, the usage of titanium alloys in earthmoving and related machinery is expected to increase multiple folds in the next decade. A major technical hurdle associated with the implementation of titanium alloys for heavy machinery is that of overcoming poor wear resistance. Proof of concept of the technologies developed in this project has been demonstrated by both laboratory testing of coupons and field testing of selected components. Further development will be required in order to have fully validated materials and process for production introduction and several technical hurdles remain to be addressed particular for use of the arc lamp fusing technology. The current project has reduced the risk of failure and provided sufficient data to encourage further investment by industry.

36 MATERIALS SCIENCE↗

Oxidation Behavior of Welded Fe-Based and Ni-Based Alloys in Supercritical CO 2

Next-generation supercritical CO 2 (sCO 2 ) power cycles will require different classes of alloy throughout the operational temperatures to optimize tradeoff of creep strength, oxidation performance and cost. This will necessitate joining methods such as welding, which might pose compatibility concerns at the joined interfaces. In this study, similar and dissimilar metal welds were generated from a variety of candidate alloys for sCO 2 systems including ferritic/martensitic steels, austenitic steels, and Ni-based superalloys. Samples were extracted from different regions of the welds and exposed to sCO 2 at 550 °C and 20 MPa for 2500 h, then characterized to understand their behavior in this environment. Unsurprisingly, the local oxidation behavior was largely dictated by the Cr content in the underlying metal. High-Cr austenitic steels and Ni alloys formed slow-growing Cr-rich oxide scales with minimal carburization of the underlying metal, while low-Cr ferritic/martensitic steels formed fast-growing Fe-rich oxide scales with significant carburization. Most welds did not show any unusual oxidation behavior at the interfaces, considering the local Cr content. The one exception was the 347H similar metal weld, where a larger grain size and complex grain structure in the fusion zone led to a significantly higher rate of Fe-rich oxide nodule formation compared to the base metal. This suggests that microstructural changes at joined interfaces can play an important role on the oxidation-limited lifetimes in future sCO 2 systems. The composition changes across the interfaces enabled study of the effect of Fe on the growth rate of Cr-rich oxides and of the origins of the sub-surface recrystallization zone that forms beneath them.