Thermally Activated Delayed Fluorescence Sensitization for Highly Efficient Blue Fluorescent Emitters
Hyperfluorescence is emerging as a powerful strategy to develop optoelectronic devices with high-color purity and enhanced stability. It requires appropriate integration of a sensitizer displaying efficient thermally activated delayed fluorescence (TADF) and an emitter displaying strong, narrow-band fluorescence. Here, through a joint computational and experimental approach, we provide an unprecedented, end-to-end systems level description of the electronic and optical processes that take place in a hyperfluorescent emissive layer composed of a TADF sensitizer, bis(2,5-di(9H-carbazol-9-yl)phenyl)-1,3,4-oxadiazole (4CzDPO), and a fluorescent emitter, 2,5,8,11-tetra-tert-butylperylene (TBPe). We combine the photophysical properties measurement of the emissive layer with the computational determination of the electronic properties, film morphology, and excitation transfer phenomena. The Förster resonance energy transfer rates from 4CzDPO to TBPe are on the order of 1011 s–1, considerably higher than the radiative and non-radiative recombination rates for 4CzDPO. These features ensure nearly complete energy transfer to TBPe, leading to a five-fold increase in the photoluminescence quantum yields in the 4CzDPO:TBPe system in comparison to neat films of 4CzDPO. Furthermore, our approach highlights the factors that can provide efficient energy transfer from TADF molecules to fluorescent emitters, suppress energy transfer among TADF molecules, and avoid the need for a host material within the emissive layer.