Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “titanium alloys”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 217 records · Page 12

A Novel Surface Treatment for Titanium Alloys

High-speed commercial aircraft require a surface treatment for titanium (Ti) alloy that is both environmentally safe and durable under the conditions of supersonic flight. A number of pretreatment procedures for Ti alloy requiring multi-stages have been developed to produce a stable surface. Among the stages are, degreasing, mechanical abrasion, chemical etching, and electrochemical anodizing. These treatments exhibit significant variations in their long-term stability, and the benefits of each step in these processes still remain unclear. In addition, chromium compounds are often used in many chemical treatments and these materials are detrimental to the environment. Recently, a chromium-free surface treatment for Ti alloy has been reported, though not designed for high temperature applications. In the present study, a simple surface treatment process developed at NASA/LaRC is reported, offering a high performance surface for a variety of applications. This novel surface treatment for Ti alloy is conventionally achieved by forming oxides on the surface with a two-step chemical process without mechanical abrasion. This acid-followed-by-base treatment was designed to be cost effective and relatively safe to use in a commercial application. In addition, it is chromium-free, and has been successfully used with a sol-gel coating to afford a strong adhesive bond after exposure to hot-wet environments. Phenylethynyl containing adhesives were used to evaluate this surface treatment with sol-gel solutions made of novel imide silanes developed at NASA/LaRC. Oxide layers developed by this process were controlled by immersion time and temperature and solution concentration. The morphology and chemical composition of the oxide layers were investigated using scanning electron microscopy (SEM), X-ray photoelectron spectroscopy (XPS), and Auger electron spectroscopy (AES). Bond strengths made with this new treatment were evaluated using single lap shear tests.

Lowther, S. E.↗

The effect of alloy composition on the mechanism of stress corrosion cracking of titanium alloys in aqueous environments

Emphasis has been placed on determining the interrelations among the composition, phase structure, deformation, and fracture properties of the alpha phase in susceptible alpha-beta alloys. The program is divided into two parts: (1) evaluation of the aqueous stress corrosion susceptibility of a series of alloys that contain various alpha-soluble elements; and (2) investigations of the metallurgical aspects of the mechanism of aqueous stress corrosion cracking.

Williams, D. N.↗

The effect of alloy composition on the mechanism of stress-corrosion cracking of titanium alloys in aqueous environments

A detailed study was made of the relation between the size distribution of Ti3Al particles in a Ti-8Al alloy and the tensile properties measured in air and in saltwater. The size distribution of Ti3Al was varied by isothermal aging for various times at temperatures in the range 770 to 970 K (930 to 1290 F). The aging kinetics were found to be relatively slow. Quantitative measurements of the particle coarsening rate at 920 K (1200 F) showed good agreement with the predicted behavior for coarsening controlled by matrix diffusion, and suggested that the specific free energy of the Ti3Al alpha interface in negligible small. In all cases, the Ti3Al particles were sheared by the glide dislocations. It was concluded that there is a definite correlation between the presence of deformable Ti3Al particles and an alloy's susceptibility to aqueous stress corrosion cracking. Furthermore, the appearance of the surface slip lines and the dislocation substructure in deformed specimens suggest that the specific effect of the Ti3Al particles is to cause a nonhomogeneous planar slip character and an enhanced chemical potential of the slip bands.

Wood, R. A.↗

Environmental Studies on Titanium Aluminide Alloys

Titanium aluminides are attractive alternatives to superalloys in moderate temperature applications (600 to 850 C) by virtue of their high strength-to-density ratio (high specific strength). These alloys are also more ductile than competing intermetallic systems. However, most Ti-based alloys tend to degrade through interstitial embrittlement and rapid oxidation during exposure to elevated temperatures. Therefore, their environmental behavior must be thoroughly investigated before they can be developed further. The goals of titanium aluminide environmental studies at the NASA Lewis Research Center are twofold: characterize the degradation mechanisms for advanced structural alloys and determine what means are available to minimize degradation. The studies to date have covered the alpha 2 (Ti3Al), orthorhombic (Ti2AlNb), and gamma (TiAl) classes of alloys.

Brindley, William J.↗

Improved diffusion welding and roll welding of titanium alloys

Auto-vacuum cleaning technique was applied to titanium parts prior to welding. This provides oxide-free welding surfaces. Diffusion welding can be accomplished in as little as five minutes of hot pressing. Roll welding can be accomplished with only ten percent deformation.

Holko, K. H.↗

Development and fracture mechanics data for 6Al-6V-2 Sn titanium alloy

Fracture mechanics properties of 6Al-6V-2Sn titanium in the annealed, solution-treated, and aged condition are presented. Tensile, fracture toughness, cyclic flaw growth, and sustained-load threshold tests were conducted. Both surface flaw and compact tension-specimen geometries were employed. Temperatures and/or environments used were -65 F (220 K) air, ambient, 300 F (422 K) air, and room-temperature air containing 10 and 100% relative humidity.

Fiftal, C. F.↗

The Solidification Velocity of Undercooled Nickel and Titanium Alloys with Dilute Solute

The study of solidification velocity is important for two reasons. First, understanding the manner in which the degree of undercooling of the liquid and solidification velocity affect the microstructure of the solid is fundamental. Second, there is disagreement between theoretical predictions of the relationship between undercooling and solidification velocity and experimental results. Thus, the objective of this research is to accurately and systematically quantify the solidification velocity as a function of undercooling for dilute nickel-and titanium-based alloys. The alloys chosen for study cover a wide range of equilibrium partition coefficients, and the results are compared to current theory.

Algoso, Paul R.↗

Nickel Titanium Alloys, Methods of Manufacture Thereof and Article Comprising the Same

Disclosed herein is a shape memory alloy comprising 48 to 50 atomic percent nickel, 15 to 30 atomic percent hathium, 1 to 5 atomic percent aluminum; with the remainder being titanium. Disclosed herein too is a method of manufacturing a shape memory alloy comprising mixing together to form an alloy nickel, hafnium, aluminum and titanium in amounts of 48 to 50 atomic percent nickel, 15 to 30 atomic percent hafnium, 1 to 5 atomic percent aluminum; with the remainder being titanium; solution treating the alloy at a temperature of 700 to 1300.degree. C. for 50 to 200 hours; and aging the alloy at a temperature of 400 to 800.degree. C. for a time period of 50 to 200 hours to form a shape memory alloy.

Manuel, Michele Viola↗

Development of Low Density Titanium Alloys for Structural Applications

In this report the results of a program designed to reduce the density of titanium by adding magnesium are presented. Because these two elements are immiscible under conventional ingot metallurgy techniques, two specialized powder metallurgy methods namely, mechanical alloying (MA) and physical vapor deposition (PVD) were implemented. The mechanical alloying experiments were done both at the University of Idaho and at the Defense Research Agency in UK. Since titanium is reactive with interstitial elements, a secondary goal of this research was to correlate solubility extensions with interstitial contamination content, especially oxygen and nitrogen. MA was carried out in SPEX 8000 shaker mils and different milling containers were utilized to control the level of contamination. Results showed that solubilities of Mg in Ti were obtained up to 28 at.% (16.4 wt. %) Mg in Ti for Ti-39.6 at. % (25 wt. %) Mg alloys, which greatly exceed those obtained under equilibrium conditions. This reflects a density reduction of approximately 26 %. Contamination of oxygen and nitrogen seemed to increase the solubility of magnesium in titanium in some cases; however, we were not able to make a clear correlation between contamination levels with solubilities. Work at the DRA has emphasized optimization of present PVD equipment, specifically composition and temperature control. Preliminary PVD data has shown Ti-Mg deposits have successfully been made up to 2 mm thick and that solubility extensions were achieved. The potential for density reduction of titanium by alloying with magnesium has been demonstrated; however, this work has only scratched the surface of the development of such low density alloys. Much research is needed before such alloys could be implemented into industry. Further funding is required in order to optimize the MA/PVD processes including contamination control, determination of optimal alloy compositions, microstructure development, and mechanical property determination.

Froes, F. H.↗

Improving intrinsic oxygen reduction activity and stability: Atomic layer deposition preparation of platinum-titanium alloy catalysts

Improved activity and stability Pt-based catalysts for the oxygen reduction reaction (ORR) are needed to perpetuate the deployment of polymer electrolyte fuel cells (PEFCs) in the transportation sector. In this study, we use atomic layer deposition of TiO 2 and Pt coupled with thermal reductive annealing to prepare Pt 3 Ti electrocatalysts. The atomic level synthetic control resulted in Pt 3 Ti nanoparticles with high ORR performance, including a mass activity of 1.84 A/mg Pt and excellent electrochemical stability. The Pt 3 Ti nanoparticles show excellent specific activity — 5.3-fold higher than commercial Pt/C and 3-fold higher than polycrystalline Pt, exceeding the performance of any PtTi catalysts reported to date. Combined experimental and computational efforts indicate that Pt enrichment on the Pt 3 Ti enhances the activity, and the intrinsic stability of the Pt 3 Ti phase provides durability. Subsequently, this knowledge, along with the facile fabrication of alloys by atomic layer deposition, can be leveraged to designed improved performance catalysts.

25 ENERGY STORAGE↗

Defect And Damage Characterization Of Additively Manufactured Titanium Alloy Ti-5553 Using Traditional Computed Tomography Volume Segmentation And Machine Learning Algorithms

The mechanical response of a component is affected by defects, such as porosity, arising from the laser powder bed fusion (LPBF) fabrication process. Thus, it is important to develop accurate and efficient inspection methods for identifying porosity. In this work, porosity identified in an X-ray computed tomography (XCT) volume of a Ti-5553 coupon was compared to pores identified in a serial sectioned volume that represented the ground truth. The porosity of the XCT scan was identified using contrast-based, ISO-based, and machine learning (ML) methods for segmentation. Large inherent porosity was easy to identify, but the ISO thresholding still struggled due to the intensity gradient resulting from both the beam hardening in XCT and the uneven lighting of the serial sectioning panels. Further, the results show that ML-based methods were better suited for identifying small pores and reducing the amount of false positives. Additionally, high strain-rate impact testing was done on some of the XCT samples as well as post-mortem XCT inspection, and the same suite of segmentation and quantification tools were used to identify the large spallation cavities. The comparison of porosity pre- and post-mortem provides insight on the influence of the LPBF porosity on the formation of spall cavities.

36 MATERIALS SCIENCE↗

Stress corrosion cracking of titanium alloys

Experiments were conducted to study (1) the basic electrochemical behavior of titanium in acid chloride solutions and (2) the response of the metal to dynamic straining in the same evironment. The aim of this group of experiments was to simulate, as nearly as possible, the actual conditions which exist at the tip of a crack. One of the foremost theories proposed to explain the propagation of stress corrosion cracks is a hydrogen embrittlement theory involving the precipitation of embrittling titanium hydrides inside the metal near the crack tip. An initial survey of the basic electrochemical literature indicated that surface hydrides play a critical role in the electrochemistry of titanium in acid solutions. A comprehensive analysis of the effect of surface films, particularly hydrides, on the electrochemical behavior of titanium in these solution is presented.

May, R. C.↗

A preliminary report on the effect of elevated temperature exposure on the mechanical properties of titanium-alloy honeycomb-core sandwich panels.

A study has been initiated to determine the effects of elevated-temperature exposure on the room-temperature mechanical properties of titanium honeycomb-core sandwich panels fabricated by brazing or spot diffusion bonding. Only flatwise tensile properties following exposure have been determined to date. Preliminary results indicate very little change in the flatwise tensile strength of sandwich panels fabricated by spot diffusion bonding following exposures of 10,000 hr at 600 and 800 F and 1000 hr at 1000 F. Titanium panels fabricated by using a Ti-Zr-Be braze alloy are susceptible to oxidation at elevated temperature and experience flatwise tensile strength degradation after continuous exposures of 7500 hr at 600 F, 1000 hr at 800 F, and less than 100 hr at 1000 F. It is possible that the exposure life of the brazed panels may be substantially increased if the panel edges are sealed to prevent oxidation of the braze alloy.

Bales, T. T.↗