Scaling of the surface migration length in nanoscale patterned growth
Scaling of the surface migration length in nanoscale patterned growth (NPG) is investigated as a function of the lateral dimension L{sub M} of a mask film fabricated on a substrate for selective epitaxy. By reducing L{sub M} below the surface migration length, any nucleation on the mask is avoided through the evaporation and surface out-diffusion of adatoms. The upper limit of L{sub M} for NPG L{sub M,c} corresponds to the surface migration length on the mask. An equation, identical to that for two-dimensional step-flow growth, is derived for NPG. However, the boundary conditions at the substrate-mask interface are affected by the surface potential difference and are different from those at the terrace edges of a homogeneous stepped surface. This results in a scaling law for surface migration length, which is proportional to the diffusion constant D and the critical incident flux F{sub c} in the form (D/F{sub c}){sup 1/{alpha}} with {alpha} decreasing from 4 to 2 as evaporation becomes dominant. NPG of GaAs for L{sub M,c}{approx}200 nm({alpha}{approx}3.8) is demonstrated at {approx}600 deg. C with molecular beam epitaxy.