Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “solid electrolyte interphase”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 217 records · Page 12

A quantitative figure of merit for battery SEI films and their use as functional solid-state electrolytes

As a key passivation film that governs battery operation, the solid electrolyte interphase (SEI) has long been credited for enabling high-performance batteries or blamed for their eventual death. However, qualitative descriptions of the SEI often found in the literature (e.g., “conductive,” “passivating”) highlight our incomplete understanding of this layer, where even the most basic properties foundational to SEI function remain difficult to measure. Here, we quantify SEI conductivities and SEI transference numbers using a separator-free Cu|SEI|Li architecture that treats the SEI as a functional solid-state electrolyte (SSE). We find that while any SEI property alone (e.g., electronic conductivity) is weakly correlated (R 2 < 0.67) with battery performance (e.g., Coulombic efficiency), a strong correlation (R 2 > 0.99) can be achieved by defining the “SEI cT number” as a product between the SEI transference number (T) and the ratio of SEI conductivities (c). Analogous to the thermoelectric figure of merit (i.e., zT ), SEI cT quantitatively benchmarks the holistic impact of SEI properties on battery performance and underscores the pitfalls of citing such properties in isolation. Perhaps most strikingly, we demonstrate that Li metal deposition and stripping at room temperature is possible in our separator-free Cu|SEI|Li cell, confirming that the SEI can function precisely as an SSE. Together, these results enrich our understanding of the SEI, not just as a passivation layer but as a functional structure that can potentially have important implications for solid-state batteries.

Science & Technology - Other Topics↗

Highly reversible Li 2 RuO 3 cathodes in sulfide-based all solid-state lithium batteries

The practical application of high-capacity lithium-rich cathode materials in lithium-ion batteries has been largely restricted by severe side reactions with electrolytes. Herein, we report a highly stable lithium-rich Li 2 RuO 3 cathode by forming a passivating solid electrolyte interphase at the interface with a sulfide solid electrolyte such as Li 6 PS 5 Cl in all-solid-state lithium batteries (ASSLBs), which efficiently suppresses serious parasitic interfacial reactions and fast-increasing interfacial impedance normally observed in liquid electrolytes. The exceptionally high interfacial stability of the Li 2 RuO 3 /sulfide electrolyte interface contributes to a high reversible capacity of 257 mA h g –1 of Li 2 RuO 3 at 0.05C rate, and unprecedented cycling stability with 90% capacity retention after 1000 cycles at 1C rate. Iin this work, comprehensive experimental characterizations and first-principles calculations disclose that electronically insulating interfacial reaction products forming at the interface between the Li 2 RuO 3 cathode and Li 6 PS 5 Cl facilitate the formation of a stable and passivating interphase and block the continuous side reactions. Importantly, reversible oxygen redox activity of Li 2 RuO 3 is well-maintained in this configuration of ASSLBs even after 600 cycles, thus the common voltage decay of the Li-rich material is also significantly reduced. These new discoveries demonstrate the critical role of interface design for achieving prolonged cycling stability of lithium-rich cathode materials.

25 ENERGY STORAGE↗

Evolution and Degradation Patterns of Electrochemical Cells Based on the Analysis of Interfacial Phenomena at Li Metal Anode/Electrolyte Interfaces

In this work, we report the results of a theoretical–computational analysis of the solid electrolyte interphase (SEI) growth and degradation dynamics occurring in lithium metal batteries during cycling. We use ab initio-kinetic Monte Carlo simulations to generate a synthetic data set, which is analyzed by machine learning methods. We aim to determine: (i) how modifications in interfacial interaction energies between solid electrolyte interphase (SEI) blocks and between Li ions and SEI facets impact the Coulombic efficiency (CE) of the battery and (ii) what factors, including reactions, microscopic transport, and other interfacial events, may lead to cell performance “failure” during prolonged charge and discharge cycles, signaled as a sharp decay in the CE over cycling. The demonstration of our approach is done on a cell including a Li metal surface interfacing with a previously introduced state-of-the-art electrolyte, and the idea can be applied to any electrochemical system. Outcomes include the identification of the leading chemical, physical, and structural variables causing cell failure and relating them to the electrolyte formulation, thus paving the way to future more refined analysis and electrolyte design.

batteries↗

Localized high-concentration electrolytes get more localized through micelle-like structures

Liquid electrolytes in batteries are typically treated as macroscopically homogeneous ionic transport media despite having a complex chemical composition and atomistic solvation structures, leaving a knowledge gap of the microstructural characteristics. Here, we reveal a unique micelle-like structure in a localized high-concentration electrolyte, in which the solvent acts as a surfactant between an insoluble salt in a diluent. The miscibility of the solvent with the diluent and simultaneous solubility of the salt results in a micelle-like structure with a smeared interface and an increased salt concentration at the centre of the salt–solvent clusters that extends the salt solubility. These intermingling miscibility effects have temperature dependencies, wherein a typical localized high-concentration electrolyte peaks in localized cluster salt concentration near room temperature and is used to form a stable solid–electrolyte interphase on a Li metal anode. Importantly, these findings serve as a guide to predicting a stable ternary phase diagram and connecting the electrolyte microstructure with electrolyte formulation and formation protocols of solid–electrolyte interphases for enhanced battery cyclability.

25 ENERGY STORAGE↗

Review of Multifunctional Separators: Stabilizing the Cathode and the Anode for Alkali (Li, Na, and K) Metal–Sulfur and Selenium Batteries

Alkali metal batteries based on lithium, sodium, and potassium anodes and sulfur-based cathodes are regarded as key for next-generation energy storage due to their high theoretical energy and potential cost effectiveness. However, metal–sulfur batteries remain challenged by several factors, including polysulfides’ (PSs) dissolution, sluggish sulfur redox kinetics at the cathode, and metallic dendrite growth at the anode. Functional separators and interlayers are an innovative approach to remedying these drawbacks. Here we critically review the state-of-the-art in separators/interlayers for cathode and anode protection, covering the Li–S and the emerging Na–S and K–S systems. The approaches for improving electrochemical performance may be categorized as one or a combination of the following: Immobilization of polysulfides (cathode); catalyzing sulfur redox kinetics (cathode); introduction of protective layers to serve as an artificial solid electrolyte interphase (SEI) (anode); and combined improvement in electrolyte wetting and homogenization of ion flux (anode and cathode). It is demonstrated that while the advances in Li–S are relatively mature, less progress has been made with Na–S and K–S due to the more challenging redox chemistry at the cathode and increased electrochemical instability at the anode. Throughout these sections there is a complementary discussion of functional separators for emerging alkali metal systems based on metal–selenium and the metal–selenium sulfide. The focus then shifts to interlayers and artificial SEI/cathode electrolyte interphase (CEI) layers employed to stabilize solid-state electrolytes (SSEs) in metal–sulfur solid-state batteries (SSBs). The discussion of SSEs focuses on inorganic electrolytes based on Li- and Na-based oxides and sulfides but also touches on some hybrid systems with an inorganic matrix and a minority polymer phase. The review then moves to practical considerations for functional separators, including scaleup issues and Li–S technoeconomics. The review concludes with an outlook section, where we discuss emerging mechanics, spectroscopy, and advanced electron microscopy (e.g. cryo-transmission electron microscopy (cryo-TEM) and cryo-focused ion beam (cryo-FIB))-based approaches for analysis of functional separator structure–battery electrochemical performance interrelations. Finally, throughout the review we identify the outstanding open scientific and technological questions while providing recommendations for future research topics.

25 ENERGY STORAGE↗

The passivity of lithium electrodes in liquid electrolytes for secondary batteries

Rechargeable Li metal batteries are currently limited by electrolyte decomposition and rapid Li consumption. Li plating and stripping greatly depend on the solid electrolyte interphase formed at the Li metal-liquid electrolyte interface. This Review discusses the reactions occurring at this interface from a corrosion science perspective, highlighting the requirements for an ideal passivation layer. Rechargeable Li metal batteries are currently limited by safety concerns, continuous electrolyte decomposition and rapid consumption of Li. These issues are mainly related to reactions occurring at the Li metal-liquid electrolyte interface. Additionally, the formation of a passivation film (that is, a solid electrolyte interphase) determines ionic diffusion and the structural and morphological evolution of the Li metal electrode upon cycling. In this Review, we discuss spontaneous and operation-induced reactions at the Li metal-electrolyte interface from a corrosion science perspective. We highlight that the instantaneous formation of a thin protective film of corrosion products at the Li surface, which acts as a barrier to further chemical reactions with the electrolyte, precedes film reformation, which occurs during subsequent electrochemical stripping and plating of Li during battery operation. Finally, we discuss solutions to overcoming remaining challenges of Li metal batteries related to Li surface science, electrolyte chemistry, cell engineering and the intrinsic instability of the Li metal-electrolyte interface.

25 ENERGY STORAGE↗

A chemically stabilized sulfur cathode for lean electrolyte lithium sulfur batteries

Lithium sulfur batteries (LSBs) are promising next-generation rechargeable batteries due to the high gravimetric energy, low cost, abundance, nontoxicity, and high sustainability of sulfur. However, the dissolution of high-order polysulfide in electrolytes and low Coulombic efficiency of Li anode require excess electrolytes and Li metal, which significantly reduce the energy density of LSBs. Quasi-solid-state LSBs, where sulfur is encapsulated in the micropores of carbon matrix and sealed by solid electrolyte interphase, can operate under lean electrolyte conditions, but a low sulfur loading in carbon matrix (<40 wt %) and low sulfur unitization (<70%) still limit the energy density in a cell level. Here, we significantly increase the sulfur loading in carbon to 60 wt % and sulfur utilization to ∼87% by dispersing sulfur in an oxygen-rich dense carbon host at a molecular level through strong chemical interactions of C–S and O–S. In an all-fluorinated organic lean electrolyte, the C/S cathode experiences a solid-state lithiation/delithiation reaction after the formation of solid electrolyte interphase in the first deep lithiation, completely avoiding the shuttle reaction. The chemically stabilized C/S composite retains a high reversible capacity of 541 mAh⋅g −1 (based on the total weight of the C/S composite) for 200 cycles under lean electrolyte conditions, corresponding to a high energy density of 974 Wh⋅kg −1 . The superior electrochemical performance of the chemical bonding-stabilized C/S composite renders it a promising cathode material for high-energy and long-cycle-life LSBs.

25 ENERGY STORAGE↗

On the Efficacy of Repeat Voltage Holds for Conditioning and Calendar Life Testing of Graphite and Silicon Cells

Voltage-hold (V-hold) protocols have shown promise toward calendar lifetime analysis of cells with graphite (Gr) and silicon (Si) anodes. In this work, repeat V-holds are performed on Gr and Si cells paired with lithium iron phosphate cathodes to delineate their beneficial role in formation and conditioning. We find that V-hold at the top of charge supplements constant current cycling in conditioning the cell to higher capacities for both Gr and Si cells after the first V-hold. A reduced order model provides the irreversible capacity proportions of each V-hold. With each repeat V-hold, parasitic loss of lithium to the solid electrolyte interphase (SEI) decreases on both Gr and Si cells. Gr cells show the square-root-of-time capacity loss behavior within 200 h of V-hold, indicative of its fast relaxation and low impact of reference performance test cycles on the SEI growth. Lifetime estimates from repeat V-holds on Gr can reach years. Si exhibits longer transition times from kinetic to diffusion-limited SEI growth, evidenced by the 400 h and 200 h holds showing square-root-of-time and linear behavior, respectively. Lifetime predictions from repeat V-holds on Si only reach 1–2 months, highlighting its limitations. Recommended duration of V-holds for Si cells should be ≥400 h.

25 ENERGY STORAGE↗

Progress Towards Extended Cycle Life Si-based Anodes: Investigation of Fluorinated Local High Concentration Electrolytes

Silicon (Si) anodes are promising candidates for Li-ion batteries due to their high specific capacity and low operating potential. Implementation has been challenged by the significant Si volume changes during (de)lithiation and associated growth/regrowth of the solid electrolyte interphase (SEI). In this report, fluorinated local high concentration electrolytes (FLHCEs) were designed such that each component of the electrolyte (solvent, salt, diluent) is fluorinated to modify the chemistry and stabilize the SEI of high (30%) silicon content anodes. FLHCEs were formulated to probe the electrolyte salt concentration and ratio of the fluorinated carbonate solvents to a hydrofluoroether diluent. Higher salt concentrations led to higher viscosities, conductivities, and contact angles on polyethylene separators. Electrochemical cycling of Si-graphite/NMC622 pouch cells using the FLHCEs delivered up to 67% capacity retention after 100 cycles at a C/3 rate. Post-cycling X-ray photoelectron spectroscopy (XPS) analyses of the Si-graphite anodes indicated the FLHCEs formed a LiF rich solid electrolyte interphase (SEI). The findings show that the fluorinated local high concentration electrolytes contribute to stabilizing the Si-graphite electrode over extended cycling.

36 MATERIALS SCIENCE↗

Investigating the Chemical Reactivity of Lithium Silicate Model SEI Layers

Silicon anodes suffer from an unstable solid electrolyte interphase (SEI) layer that contributes to undesirable capacity fade with cycling. A key part to addressing this unstable SEI formation is to examine how certain components of the SEI react with the electrolyte over time. One SEI component that has not been thoroughly studied in the context of the chemical reactivity against the electrolyte is lithiated silicate. Four model silicate thin films with increasing lithium content were deposited by radio frequency (RF) magnetron sputtering to study how the lithiation of the native oxide on a silicon anode affects the chemical stability of the anode surface. SiO2, Li2Si2O5, Li2SiO3, and Li3SiOx films were exposed to 1.2 M LiPF6 in the 3:7 wt% ethylene carbonate/ethyl methyl carbonate (EC/EMC) electrolyte for periods of time that are representative of the amount of time it takes to undergo cell formations. Soaked samples were rinsed, dried, and characterized by a combination of attenuated total reflectance-infrared spectroscopy (ATR-IR), focused ion beam-secondary electron microscopy (FIB-SEM), and X-ray photoelectron spectroscopy (XPS) depth profiling. It was found that the rate of the decrease in film thickness of the silicates exposed to the electrolyte over time increases as a function of the lithium content in the thin film. This reaction involves HF etching and LiPF6 salt degradation leading to silicate loss and fluorination throughout the bulk. Understanding this chemical instability is critical to determining the overall mechanism of SEI degradation over time.

ADVANCED PROPULSION SYSTEMS,ENERGY STORAGE↗

Stress- and interface-compatible red phosphorus anode for high-energy and durable sodium-ion batteries

Sodium-ion battery is a promising candidate for energy storage application, but the absence of high-capacity and low-cost anode materials significantly limit their practical specific energy and cost. Red phosphorus (RP) possesses a high theoretical specific capacity but suffers from large volume change, low electronic conductivity and unstable solid-electrolyte interphase (SEI). Herein, a hierarchical micro/nanostructured antimony-doped RP/carbon anode was developed, which demonstrate extraordinary electrochemical performance with high initial Coulombic efficiency of ~90%, high areal (~1.7 mAh cm-2) capacity together with good cycle stability and rate capability. Combined experimental and computational studies consistently revealed that such a unique structural design can dramatically accommodate the mechanical stress and moreover effectively restrain the undesired decomposition of electrolyte solvents regardless of electrolytes formulation, resulting in superior structural integrity and thin/robust SEI formation during cycling. The present finding has offered an alternative strategy for stress management and interface engineering on high-capacity alloying-based anode materials.

Liu, Xiang↗

High-Power Lithium Metal Batteries Enabled by High-Concentration Acetonitrile-Based Electrolytes with Vinylene Carbonate Additive

To enable next-generation high power, high-energy-density lithium (Li) metal batteries (LMBs), an electrolyte possessing both high Li Coulombic efficiency (CE) at high-rate and good anodic stability on cathodes is critical. Acetonitrile (AN) is a well-known organic solvent for high anodic stability and high ionic conductivity, yet its application in LMBs is limited due to its poor compatibility with Li metal anode even at high salt concentration conditions. Here, we developed a highly concentrated AN-based electrolyte with vinylene carbonate (VC) additive to suppress Li+ depletion at high current densities. Addition of VC in the AN-based electrolyte leads to the formation of a polycarbonate-based solid electrolyte interphase which minimizes Li corrosion and leads to very high Li CE of up to 99.1% at a current density of 0.2 mA cm-2. Using such an electrolyte, fast charging of Li||NMC333 cells has been realized at a high current density of 3.6 mA cm-2, and stable cycling of Li||NMC622 cells with a high cathode loading of 4 mAh cm-2 has also been demonstrated.

Peng, Zhe↗

Enabling 4C Fast Charging of Lithium–Ion Batteries by Coating Graphite with a Solid–State Electrolyte

Enabling fast-charging (≥4C) of lithium-ion batteries is an important challenge to accelerate the adoption of electric vehicles. However, the desire to maximize energy density has driven the use of increasingly thick electrodes, which hinders rate capability. Herein, atomic layer deposition is used to coat a single-ion conducting solid electrolyte (Li 3 BO 3 -Li 2 CO 3 ) onto postcalendered graphite electrodes, forming an artificial solid-electrolyte interphase (SEI). When compared to uncoated control electrodes, the solid electrolyte coating: 1) eliminates natural SEI formation during preconditioning; 2) decreases interphase impedance by >75% compared to the natural SEI; and 3) extends cycle life under 4C charging conditions, enabling retention of 80% capacity after 500 cycles (compared to 12 cycles in the uncoated control) in pouch cells with >3 mAh cm –2 loading. Furthermore, this work demonstrates that 4C charging without Li plating can be achieved through purely interfacial modification without sacrificing energy density and sheds new light on the role of the SEI in Li plating and fast-charge performance.

25 ENERGY STORAGE↗

Electroanalytical Measurement of Interphase Formation at a Li Metal–Solid Electrolyte Interface

The interphase between Li metal and solid electrolytes dictates performance in Li metal batteries. For the solid electrolyte Lipon, in this study we electroanalytically measure a capacity loss of 1.03 ± 0.16 μAh/cm 2 when Lipon first contacts Li metal. Assuming this capacity is all lost to interphase formation, this corresponds to a maximum Li consumption of 5.0 ± 0.8 nm to form an interphase ~4.7 nm thick. From dynamic electrochemical impedance spectroscopy (dEIS) during Li plating, we determine that nonlinear chaotic spectra demark this interphase formation and that this occurs immediately upon initiation of Li plating. dEIS also reveals interfacial resistance during both plating and stripping that decreases as the amount of plated Li increases.

25 ENERGY STORAGE↗

Robust battery interphases from dilute fluorinated cations

Controlling solid electrolyte interphase (SEI) in batteries is crucial for their efficient cycling. Herein, we demonstrate an approach to enable robust battery performance that does not rely on high fractions of fluorinated species in electrolytes, thus substantially decreasing the environmental footprint and cost of high-energy batteries. In this approach, we use very low fractions of readily reducible fluorinated cations in electrolyte (~0.1 wt%) and employ electrostatic attraction to generate a substantial population of these cations at the anode surface. As a result, we can form a robust fluorine-rich SEI that allows for dendrite-free deposition of dense Li and stable cycling of Li-metal full cells with high-voltage cathodes. Our approach represents a general strategy for delivering desired chemical species to battery anodes through electrostatic attraction while using minute amounts of additive.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Irreparable Interphase Chemistry Degradation Induced by Temperature Pulse in Lithium‐Ion Batteries

Abstract While it is widely recognized that the operating temperature significantly affects the energy density and cycle life of lithium‐ion batteries, the consequence of electrode‐electrolyte interphase chemistry to sudden environmental temperature changes remains inadequately understood. Here, we systematically investigate the effects of a temperature pulse (T pulse) on the electrochemical performance of LiNi 0.8 Mn 0.1 Co 0.1 O 2 (NMC811) pouch full cells. By utilizing advanced characterization tools, such as time‐of‐flight secondary‐ion mass spectrometry, we reveal that the T pulse can lead to an irreversible degradation of cathode‐electrolyte interphase chemistry and architecture. Despite negligible immediate impacts on the solid‐electrolyte interphase (SEI) on graphite anode, aggregated cathode‐to‐anode chemical crossover gradually degrades the SEI by catalyzing electrolyte reduction decomposition and inducing metallic dead Li formation because of insufficient cathode passivation after the T pulse. Consequently, pouch cells subjected to the T pulse show an inferior cycle stability to those free of the T pulse. This work unveils the effects of sudden temperature changes on the interphase chemistry and cell performance, emphasizing the importance of a proper temperature management in assessing performance.

Cui, Zehao↗

Role of Salt Concentration on Interphase Dynamics and Chemistry of Silicon Anodes during Electrochemical Cycling

We investigated the chemistry and structure of the solid electrolyte interphase (SEI) grown over a silicon anode as a function of the lithium salt concentration. In these experiments, in situ neutron reflectivity measurements were performed to measure the thickness and composition of the SEI formed from 1.0 and 5.5 M lithium bis(trifluoromethane)sulfonimide (LiTFSI) in standard ethylene carbonate:dimethyl carbonate electrolytes. These measurements reveal the formation of a 350+ Å thick SEI layer that is predominantly organic (∼80%) and dimensionally stable when using a 1.0 M salt solution. In contrast, increasing the salt concentration to 5.5 M resulted in an SEI that exhibited thickness changes from 100 to 375 Å and became up to 30% inorganic. In conclusion, these compositional and structural changes point to the role of salt speciation on the resulting passivation of silicon electrodes and indicate the need to form more organic-like passivation layers to promote the calendar life of silicon anodes.

Electrodes↗