Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “shear tests”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 217 records · Page 12

The feasibility of producing aluminum-lithium structures for cryogenic tankage applications by laser beam welding

Aluminum-lithium alloys exhibit high strength, high elastic modulus, and low density as well as excellent cryogenic mechanical properties making them ideal material candidates for cryogenic tanks. NASA has proposed the use of 'built-up' structure for panels fabricated into cryogenic tanks replacing current conventional machining. Superplastically formed stiffeners would be joined to sheet (tank skin) that had been roll formed to the radius of the tank in order to produce panels. Aluminum-lithium alloys of interest for producing the built-up structure include alloy 2095-T6 stiffeners to 2095-T8 sheet and alloy 8090-T6 stiffeners to 2090-T83 sheet. Laser welding, with comparable joint properties, offers the following advantages over conventional welding: higher production rates, minimal degradation within the heat affected zones, and full process automation. This study established process parameters for laser beam welding, mechanical property determinations, metallographic characterization, and fabrication of prototype panels. Tensile tests representing partial penetration of the skin alloys provided joint efficiencies between 65 and 77 percent, depending upon alloy and degree of penetration. Results of tension shear tests of lap welds indicated that the combination of 2095-T6 to 2090-T8 exhibited significantly higher weld shear strength at the interface in comparison to welds of 8090-T6 to 2090-T83. The increased shear strength associated with 2095 is believed to be due to the alloy's ability to precipitation strengthening (naturally age) after welding.

Martukanitz, R. P.↗

An Experimental and Analytical Evaluation of a Biaxial Test for Determining Shear Properties of Composite Materials

The results of an experimental and analytical investigation of a biaxial tension/compression test for determining shear properties of composite materials are reported. Using finite element models of isotropic and orthotropic laminates, a specimen geometry was optimized. A kinematic fixture was designed to introduce an equal and opposite pair of forces into a specimen with a one inch square test section. Aluminum and several composite laminates with the optimized geometry and a configuration with large stress gradients were tested in the fixture. The specimens were instrumented with strain gages in the center of the test section for shear stiffness measurements. Pure shear strain was measured. The results from the experiments correlated well with finite element results. Failure of the specimens occurred through the center of the test section and appeared to have initiated at the high stress points. The results lead to the conclusion that the optimized specimen is suitable for determining shear modulus for composite materials. Further revisions to the specimen geometry are necessary if the method is to give shear strength data.

Kennedy, John M.↗

Wear testing of friction stir spot welding tools for joining of DP 980 Steel

Friction stir spot welding has been shown to be a viable method of joining ultra high strength steel (UHSS), both in terms of joint strength and process cycle time. However, the cost of tooling must be reasonable in order for this method to be adopted as an industrial process. Several tooling materials have been evaluated in prior studies, including silicon nitride and polycrystalline cubic boron nitride (PCBN). Recently a new tool alloy has been developed, where a blend of PCBN and tungsten rhenium (W-Re) was used in order to improve the toughness of the tool. Wear testing results are presented for two of these alloys: one with a composition of 60% PCBN and 40% W-Re (designated as Q60), and one with 70% PCBN and 30% W-Re (designated at Q70). The sheet material used for all wear testing was DP 980. Tool profiles were measured periodically during the testing process in order to show the progression of wear as a function of the number of spots produced. Lap shear testing was done each time a tool profile was taken in order to show the relationship between tool wear and joint strength. For the welding parameters chosen for this study the Q70 tool provided the best combination of wear resistance and joint strength.

Friction Stir↗

Influence of alkali-silica reaction on the shear capacity of reinforced concrete beams with minimum transverse reinforcement

A growing number of critical concrete infrastructure are affected by alkali-silica reaction (ASR) damage such as the Seabrook Nuclear Power Plant in New Hampshire, Parker arch-gravity dam in Arizona, and several highway bridges in California and Texas. ASR causes expansion and cracking and degrades the concrete mechanical properties. Despite a wealth of material level studies there is still limited large-scale experimental data regarding the effects of ASR on reinforced concrete (RC) members. Due to the brittle nature of the shear failure in RC structures, this study focuses on the shear response of full-scale ASR damaged RC beams with minimum shear reinforcement. Six RC beams were built with different levels of ASR susceptibility and conditioned in different environments during which continuous expansion monitoring was performed. The beams all contained reactive fine aggregate (sand) and two of them had additional alkali, 1.25% by weight of cement, to accelerate ASR. The highest expansion rate of the beams happened during the first 150 days and the expansions stayed constant after 240 days and 330 days for beams conditioned in outdoor and laboratory conditions, respectively, until the last measurement at 575 days. The highest expansion, 0.4%, was seen in the beams with additional alkali and conditioned outside with regular water spray. Out of the six beams, three were selected at different levels of ASR damage and two shear tests were performed on the minimally reinforced spans close to the ends of each beam. Results indicated that beams gain shear strength from ongoing cement hydration in the presence of moisture for ASR expansions less than 0.2%. Compared to one of the beams with 0.2% ASR expansion, one of the other samples with 0.4% expansion lost 6% of its shear strength, 25% of its shear stiffness, and showed about two times larger shear cracks and shear deformations at peak load. Finally, the shear reinforcement yielded at 20% less load in the beam with 0.4% expansion compared to the beam with 0.2% expansion.

42 ENGINEERING↗

Fine Pitch Bonding for High Density Interconnects

CTE (coefficient of thermal expansion) mismatch between two wafers has potential for brittle failure when large areas are bonded on top of one another (wafer to wafer or wafer to die bonds). To address this type of failure, we proposed patterning a polymer around metallic interconnects. For this project, utilized benzo cyclobutene (BCB) to form the bond and accommodate stress. For the metal interconnects, we used indium. To determine the benefits of utilizing BCB, mechanical shear testing of die bonding with just BCB were compared to die bonded just with oxide. These tests demonstrated that BCB, when cured for only 30 minutes and bonded at 200°C, the BCB was able to withstand shear forces similar to oxide. Furthermore, when the BCB did fail, it experienced a more ductile failure, allowing the silicon to crack, rather than shatter. To demonstrate the feasibility of using BCB between indium interconnects, wafers were pattered with layers of BCB with vias for indium or ENEPIG (electroless nickel, electroless palladium, immersion gold). Subsequently, these wafers were pattered with a variety of indium or ENEPIG interconnect pitches, diameters, and heights. These dies were bonded under a variety of conditions, and those that held a bond, were cross-sectioned and imaged. Images revealed that certain bonding conditions allow for interconnects and BCB to achieve a void-less bond and thus demonstrate that utilizing polymers in place of oxide is a feasible way to reduce CTE stress.

36 MATERIALS SCIENCE↗

Strength Tests on Thin-walled Duralumin Cylinders in Torsion

This report is the first of a series presenting the results of strength tests on thin-walled cylinders and truncated cones of circular and elliptical section; it comprises the results obtained to date from torsion (pure shear) tests on 65 thin-walled duralumin cylinders of circular section with ends clamped to rigid bulkheads. The effect of variations in the length/radius and radius/thickness ratios on the type of failure is indicated, and a semi-empirical equation for the shearing stress at maximum load is given.

TRUNCATED - CYLINDERS, CIRCULAR - STRENGTH↗

Analyses of Failure Mechanisms in Woven Graphite/Polyimide Composites with Medium and High Modulus Graphite Fibers Subjected to In-Plane Shear

The application of the Iosipescu shear test for the room and high temperature failure analyses of the woven graphite/polyimide composites with the medium (T-650) and igh (M40J and M60J) modulus graphite fibers is discussed. The M40J/PMR-II-50 and M60J/PMR-II-50 composites were tested as supplied and after thermal conditioning. The effect of temperature and conditioning on the initiation of intralaminar damage and the shear strength of the composites was established.

Kumosa, M.↗

Mechanical response and microprocesses of reconsolidating crushed salt at elevated temperature

Design, analysis and performance assessment of potential salt repositories for heat-generating nuclear waste require knowledge of thermal, mechanical, and fluid transport properties of reconsolidating granular salt. So, to inform salt repository evaluations, we have undertaken an experimental program to determine Bulk and Young’s moduli and Poisson’s ratio of reconsolidated granular salt as a function of porosity and temperature and to establish the deformational processes by which the salt reconsolidates. Our tests were conducted at 100, 175, and 250 °C. In hydrostatic tests, confining pressure is increased to 20 MPa with periodic unload/reload loops to determine K. Volume strain increases with increasing temperature. In shear tests at 2.5 and 5 MPa confining pressure, after confining pressure is applied, the crushed salt is subjected to a differential stress, with periodic unload/reload loops to determine E and ν. At predetermined differential stress levels the stress is held constant and the salt consolidates. Displacement gages mounted on the samples show little lateral deformation until the samples reach a porosity of ~10 %. Interestingly, vapor is vented only for 250 °C tests and condenses at the vent port. It is hypothesized that the brine originates from fluid inclusions, which were made accessible by heating and intragranular deformational processes including decrepitation. Furthermore, identification and documentation of consolidation processes are inferred from optical and scanning electron microstructural observations. As a result, densification at low porosity is enhanced by water film on grain boundaries that enables solution-precipitation phenomena.

58 GEOSCIENCES↗

Corrosion behaviour of friction-bit-joined and weld-bonded AA7075-T6/galvannealed DP980

Joining of aluminium alloys 7075-T6 and galvannealed dual phase 980 steel was achieved by friction bit joining (FBJ) and weld-bonding (FBJ + adhesive) processes. Accelerated laboratory-scale corrosion tests were performed on both FBJ only and weld-bonded specimens to study joint strength under a corrosive environment. Static lap shear tests showed that both FBJ only and weld-bonded cases generally retained more than 80% of the joint strength of non-corroded specimens at the end of corrosion testing. The presence of Zn/Fe coating on the steel substrate resulted in improved corrosion resistance for FBJ specimens, compared to joints produced with bare steel. An optical microscopy was used for cross-sectional analysis of corroded specimens. Some corrosion on the joining bit was observed near the bit head. However, the joining bit was still intact on the steel substrate, indicating that the primary bond was sound.

36 MATERIALS SCIENCE↗

Space Shuttle Columbia Aging Wiring Failure Analysis

A Space Shuttle Columbia main engine controller 14 AWG wire short circuited during the launch of STS-93. Post-flight examination divulged that the wire had electrically arced against the head of a nearby bolt. More extensive inspection revealed additional damage to the subject wire, and to other wires as well from the mid-body of Columbia. The shorted wire was to have been constructed from nickel-plated copper conductors surrounded by the polyimide insulation Kapton, top-coated with an aromatic polyimide resin. The wires were analyzed via scanning electron microscope (SEM), energy dispersive X-Ray spectroscopy (EDX), and electron spectroscopy for chemical analysis (ESCA); differential scanning calorimetry (DSC) and thermal gravimetric analysis (TGA) were performed on the polyimide. Exemplar testing under laboratory conditions was performed to replicate the mechanical damage characteristics evident on the failed wires. The exemplar testing included a step test, where, as the name implies, a person stepped on a simulated wire bundle that rested upon a bolt head. Likewise, a shear test that forced a bolt head and a torque tip against a wire was performed to attempt to damage the insulation and conductor. Additionally, a vibration test was performed to determine if a wire bundle would abrade when vibrated against the head of a bolt. Also, an abrasion test was undertaken to determine if the polyimide of the wire could be damaged by rubbing against convolex helical tubing. Finally, an impact test was performed to ascertain if the use of the tubing would protect the wire from the strike of a foreign object.

McDaniels, Steven J.↗

Microstructural characterization and mechanical property of active soldering anodized 6061 Al alloy using Sn-3.5Ag-xTi active solders

Active solders Sn-3.5Ag-xTi varied from x = 0 to 6 wt.% Ti addition were prepared by vacuum arc re-melting and the resultant phase formation and variation of microstructure with titanium concentration were analyzed using X-ray diffraction, optical microscopy and scanning electron microscopy. The Sn-3.5Ag-xTi active solders are used as metallic filler to join with anodized 6061 Al alloy for potential applications of providing a higher heat conduction path. Their joints and mechanical properties were characterized and evaluated in terms of titanium content. The mechanical property of joints was measured by shear testing. The joint strength was very dependent on the titanium content. Solder with a 0.5 wt.% Ti addition can successfully wet and bond to the anodized aluminum oxide layers of Al alloy and posses a shear strength of 16.28 {+-} 0.64 MPa. The maximum bonding strength reached 22.24 {+-} 0.70 MPa at a 3 wt.% Ti addition. Interfacial reaction phase and chemical composition were identified by a transmission electron microscope with energy dispersive spectrometer. Results showed that the Ti element reacts with anodized aluminum oxide to form Al{sub 3}Ti-rich and Al{sub 3}Ti phases at the joint interfaces. - Highlights: Black-Right-Pointing-Pointer Active solder joining of anodized Al alloy needs 0.5 wt.% Ti addition for Sn-3.5Ag. Black-Right-Pointing-Pointer The maximum bonding strength occurs at 3 wt.% Ti addition. Black-Right-Pointing-Pointer The Ti reacts with anodized Al oxide to form Al{sub 3}Ti-rich and Al{sub 3}Ti at joint interface.

36 MATERIALS SCIENCE↗

Experimental study of fracture slip due to stress perturbation in fractured geo-resources

Anthropogenic activities such as underground fluid injection/extraction, well stimulation, and dam impoundment will perturb the state-of-stress in the subsurface, which could activate critically stressed pre-existing fractures and faults. Fault and fracture activation can induce seismicity, change flow behavior, and damage asperities on the fracture surface to alter reservoir permeability. Here, in this study, triaxial shear tests were conducted on saw cut and rough fracture Barre granite specimens to better characterize how a decrease in normal stress and increase in shear stress will influence crystalline rock fracture hydromechanical properties. In a triaxial set up, confining pressure (CP) and differential stress (DS) were used to induce normal and shear stress on a 45° oriented fracture. Fracture slip and the corresponding stress relaxation was observed when the confining stress decreased. Fracture permeability increased when the fracture slipped. Moreover, new micro-cracks observed by x-ray images indicated the creation of new flow paths for fluid movement. The experimental outcomes of this study indicate that decrease in normal stress due to stress perturbations along the faults/fractures in the extensional stress regime can induce the slip along the fracture. This could have a significant influence on slope stability in quarries, stimulation and injection strategy in deep geo-resources, and potentially minimize the risk of induced seismicity. The observed stress dependency of hydraulic aperture in rough fracture during pre- and post-slip stages could provide key inputs for field-scale simulation of geo-resources.

58 GEOSCIENCES↗

Room temperature mechanical properties of shuttle thermal protection system materials

Tests were conducted at room temperature to determine the mechanical properties and behavior of materials used for the thermal protection system of the space shuttle. The materials investigated include the LI-900 RSI tiles, the RTV-560 adhesive and the .41 cm (.16 thick) strain isolator pad (SIP). Tensile and compression cyclic loading tests were conducted on the SIP material and stress-strain curves obtained for various proof loads and load cyclic conditioning. Ultimate tensile and shear tests were conducted on the RSI, RTV, and SIP materials. The SIP material exhibits highly nonlinear stress-strain behavior, increased tangent modulus and ultimate tensile strength with increased loading rate, and large short time load relaxation and moderate creep behavior. Proof and cyclic load conditioning of the SIP results in permanent deformation of the material, hysteresis effects, and much higher tensile tangent modulus values at large strains.

Sawyer, J. W.↗

Mechanically fastened joints in woven fabric composites

Strength analysis for composite bolted joints involves the mating of a stress analysis with an appropriate mode specific failure criterion for each of the primary failure modes. The stress analysis and failure criteria are independent of each other and can be manipulated separately in order to optimize the strength analysis package formed by their coupling. Material properties tests were conducted on rubber toughened graphite-epoxy material to measure the basic strength and stiffness in the warp and fill directions and in shear. Test matrices are summarized for investigations of laminate configuration, stacking sequence, fastener diameter, edge distance, fastener half spacing, laminate thickness, and fastener torque. A three dimensional finite element analysis computer program was written and failure criteria for net tension, shearout, and bearing were determined.

Wilson, D. W.↗

Joint Strength Optimization and Damping Assessment of NiTi-Polymer Matrix Hybrid Composites

Approaches to optimize the adhesive joint strength between shape memory alloy ribbons and carbon fiber-reinforced epoxy composites were investigated for potential use as either an actuating structure or a dampening composite for structural applications. The interfacial bond strength between nickel-titanium (NiTi) and a polymer matrix composite (PMC) was measured by double lap shear testing as a function of NiTi surface treatment and adhesive material. The effect of NiTi surface treatment on damping was investigated using dynamic mechanical analysis. Lap shear data show that treating the surfaces of NiTi ribbons by light sandblasting and primer application increased the interfacial bond strength by 20 percent over the baseline composite structure. Lap shear data also reveal that out of three different film adhesives investigated, samples bonded with AF 191U and Hysol® 9696U display the highest adhesive joint strengths. Optical microscopy reveals that most samples failed by either cohesive failure within the adhesive or by adhesive failure at either the adhesive/PMC or NiTi/adhesive interface. Adhering NiTi to the PMC did not appear to negatively impact damping performance; however, a more thorough examination into NiTi's role on vibration damping should be investigated.

lap shear↗

Stress analysis and buckling of J-stiffened graphite-epoxy panel

A graphite epoxy shear panel with bonded on J stiffeners was investigated. The panel, loaded to buckling in a picture frame shear test is described. Two finite element models, each of which included the doubler material bonded to the panel skin under the stiffeners and at the panel edges, were used to make a stress analysis of the panel. The shear load distributions in the panel from two commonly used boundary conditions, applied shear load and applied displacement, were compared with the results from one of the finite element models that included the picture frame test fixture.

Davis, R. C.↗