At least 217 records · Page 12

Filament Formation and Melt Spinning of Coal-Based Mesophase Pitch for Carbon Fiber Production

High-performance carbon fibers excel as high specific strength and modulus materials, and are utilized in composites applications ranging across aerospace, automotive, energy, infrastructure, and sports equipment sectors. Compared to PAN-based carbon fiber, mesophase pitch-based carbon fiber has lower tensile strength but provides a higher modulus, higher thermal conductivity, and a lower cost potential. However, challenges in stable, continuous melt spinning processing are a serious limiting factor. Unlike typical melt spinning of long, linear chain polymers, mesophase pitch is a comprised of relatively shorter polycyclic aromatic hydrocarbons which form a liquid crystal. In its ‘green’ or ‘as-spun’ state, the fibers are very fragile. Moreover, its temperature of processing is quite high, often approaching 400ºC. Complex flow dynamics combined with short length and time scale heat transfer render its melt spinning a formidable processing challenge. Improved understanding of the root causes for nascent filament breakage and spinning instabilities are needed. This work aims to determine fundamental phenomena that govern mesophase pitch filament formation by comparison of required draw force and uninterrupted spinning minutes with applied draw down ratio. The effect of perturbations on spinning stability are analyzed using capillary rheometry, microscopy of elongating filaments, and filtration.

01 COAL, LIGNITE, AND PEAT↗

Effect of processing on Polymer/Composite structure and properties

Advances in the vitality and economic health of the field of polymer forecasting are discussed. A consistent and rational point of view which considers processing as a participant in the underlying triad of relationships which comprise materials science and engineering is outlined. This triad includes processing as it influences material structure, and ultimately properties. Methods in processing structure properties, polymer science and engineering, polymer chemistry and synthesis, structure and modification and optimization through processing, and methods of melt flow modeling in processing structure property relations of polymer were developed. Mechanical properties of composites are considered, and biomedical materials research to include polymer processing effects are studied. An analysis of the design technology of advances graphite/epoxy composites is also reported.

Source record↗

Friction and wear of polyethylene oxide polymer having a range of molecular weights

Sliding friction and wear experiments were conducted at light loads (25 to 250 g) with various molecular weights of the polyethylene oxide polymer sliding on itself and iron. Results of the experimental investigation indicate that: (1) the coefficient of friction for the polymer decreases with increasing molecular weight; (2) friction coefficient is higher for the polymer sliding on itself than it is for the polymer sliding on iron; (3) at sufficiently high loads localized surface melting occurs and the friction coefficient is the same for the polymer sliding on itself and iron; (4) fracture cracks develop in the sliding wear track at higher but not lower sliding velocities, reflecting a strain rate sensitivity to crack initiation, and (5) the friction coefficient for the polymer sliding on iron increases with the formation of a polymer film on the iron surface.

Buckley, D. H.↗

Imide Cyclotriphosphazene/Hexafluoroisopropylidene Polymers

Useful physical and chemical properties observed in compounds obtained by thermally-induced melt polymerization of maleimido-phenoxy cyclotriphosphazenes linked through hexafluoroisopropylidene-diphthalimide groups. Polymers exhibit high strength, high thermal stability, and high char yields, and appear to be excellent candidates for fabricating composite materials.

Fohlen, G. M.↗

Uniqueness of relaxation times determined by dielectric spectroscopy

Dielectric spectroscopy is extremely powerful to study molecular dynamics, because of the very broad frequency range. Often multiple processes superimpose resulting in spectra that expand over several orders of magnitude, with some of the contributions partially hidden. For illustration, we selected two examples, (i) normal mode of high molar mass polymers partially hidden by conductivity and polarization and (ii) contour length fluctuations partially hidden by reptation using the well-studied polyisoprene melts as example. The intuitive approach to describe experimental spectra and to extract relaxation times is the addition of two or more model functions. Here, we use the empirical Havriliak-Negami function to illustrate the ambiguity of the extracted relaxation time, despite an excellent agreement of the fit with experimental data. We show that there are an infinite number of solutions for which a perfect description of experimental data can be achieved. However, a simple mathematical relationship indicates uniqueness of the pairs of the relaxation strength and relaxation time. Sacrificing the absolute value of the relaxation time enables to find the temperature dependence of the parameters with a high accuracy. For the specific cases studied here, the time temperature superposition (TTS) is very useful to confirm the principle. However, the derivation is not based on a specific temperature dependence, hence, independent from the TTS. We compare new and traditional approaches and find the same trend for the temperature dependence. The important advantage of the new technology is the knowledge of the accuracy of the relaxation times. Relaxation times determined from data for which the peak is clearly visible are the same within the experimental accuracy for traditional and new technology. However, for data where a dominant process hides the peak, substantial deviations can be observed. Finally, we conclude that the new approach is particularly helpful for cases in which relaxation times need to be determined without having access to the associated peak position.

36 MATERIALS SCIENCE↗

Effects of Melt Processing on Evolution of Structure in PEEK

We report on the effects of melt processing temperature on structure formation in Poly(ether-ether-ketone), PEEK. Real time Small Angle X-ray Scattering, SAXS, and thermal analysis are used to follow the melting behavior after various stages of processing. Assignment of peaks to structural entities within the material, the relative perfection of the crystals, and the possibility of their reorganization, are all influenced by the melt processing history. With the advent of high intensity synchrotron sources of X-radiation, polymer scientists gain a research tool which, when used along with thermal analysis, provides additional structural information about the crystals during growth and subsequent melting. PEEK is an engineering thermoplastic polymer with a very high glass transition temperature (145 C) and crystal melting point (337 C). PEEK has been the subject of recent studies by X-ray scattering in which melt and cold crystallization were followed in real-time. X-ray scattering and thermal studies have been used to address the formation of dual endothermic response which has been variously ascribed to lamellar insertion, dual crystal populations, or melting followed by re-crystallization. Another important issue is whether all of the amorphous phase is located in interlamellar regions, or alternatively whether some is located in "pockets" away from the crystalline lamellar stacks. The interpretation of scattering from lamellar stacks varies depending upon whether such amorphous pockets are formed. Some groups believe all of the amorphous phase is interlamellar. This leads to selection of a smaller thickness for the crystals. Other groups suggest that most amorphous phase is not interlamellar, and this leads to the suggestion that the crystal thickness is larger than the amorphous layer within the stacks. To investigate these ideas, we used SAXS and Differential Scanning Calorimetry to compare results of single and dual stage melt crystallization of PEEK using a treatment scheme involving annealing/crystallization at T(sub a1) followed by annealing at T(sub a2) where either T(sub a1) < T(sub a2) or T(sub a1) > T(sub a2). We proposed a model to explain multiple melting endotherms in PPS, treated according to one or two-stage melt or cold crystallization. Key features of this model are that multiple endotherms: (1) are due to reorganization/recrystallization after cold crystallization; and, (2) are dominated by crystal morphology after melt crystallization at high T. In other words, multiple distinct crystal populations are formed by the latter treatment, leading to observation of multiple melting. PEEK 45OG pellets (ICI Americas) were the starting material for this study. Films were compression molded at 400 C, then quenched to ice water. Samples were heated to 375 C in a Mettler FP80 hot stage and held for three min. to erase crystal seeds before cooling them to T(sub a1) = 280 C . Samples were held at T(sub a2) for a period of time, then immediately heated to 360 C. In the second treatment samples were held at T(sub a1) = 31 C for different crystallization times t(sub c) then cooled to 295 C and held 15 min. In situ (SAXS) experiments were performed at the Brookhaven National Synchrotron Light Source with the sample located inside the Mettler hot stage. The system was equipped with a two-dimensional position sensitive detector. The sample to detector distance was 172.7 cm and the X-ray wavelength was 1.54 Angstroms. SAXS data were taken continuously during the isothermal periods and during the heating to 360 C at 5 C/min. Each SAXS scan was collected for 30 sec. Since the samples were isotropic, circular integration was used to increase the signal to noise ratio. After dual stage melt crystallization with T(sub a1) < T(sub a2) the lower melting endotherm arises from holding at T(sub a1). During cooling a broad distribution of crystals forms, and the low-melting tail is perfected during T(sub al). Heating to T(sub a2) melts these imperfect crystals and allows others with greater average long spacing to form in their place. After dual stage crystallization with T(sub a1) > T(sub a2), the amount of space remaining for additional growth at T(sub a2) depends upon the holding time at T(sub a1). The long period of crystals formed at T(sub a2) is smaller than that formed at T(sub a1) due to growth in a now-restricted geometry. Perfection of crystals is seen as an increase of the intensity of the population scattering at higher s, while the intensity of the population scattering at lower s stays constant. During heating from below to above the minor endotherm, we see rapid decrease of the intensity of the X-ray scattering corresponding to the population of crystals scattering in the shoulder. Another important observation is that after the sample is annealed at 295 C, the shoulder intensity is restored once again. The population scattering at higher s remains longer before it disappears in the sample treated to the second stage of melt crystallization, compared to the sample crystallized with a single stage. This could be interpreted as an effect of continued perfection of the less perfect population, which is also reflected in the increased melting temperature of the smaller endotherm as the holding time at 295 C increases. In the corresponding DSC scans we see a shift in the area and the peak temperature of the lower melting endotherm with an increase of the annealing time.

Georgiev, Georgi↗

Evaluation of Graphite Fiber/Polyimide PMCs from Hot Melt vs Solution Prepreg

Carbon fiber reinforced high temperature polymer matrix composites (PMC) have been extensively investigated as potential weight reduction replacements of various metallic components in next generation high performance propulsion rocket engines. The initial phase involves development of comprehensive composite material-process-structure-design-property-in-service performance correlations and database, especially for a high stiffness facesheet of various sandwich structures. Overview of the program plan, technical approaches and current multi-team efforts will be presented. During composite fabrication, it was found that the two large volume commercial prepregging methods (hot-melt vs. solution) resulted in considerably different composite cure behavior. Details of the process-induced physical and chemical modifications in the prepregs, their effects on composite processing, and systematic cure cycle optimization studies will be discussed. The combined effects of prepregging method and cure cycle modification on composite properties and isothermal aging performance were also evaluated.

Shin, E. Eugene↗

Evaluation of Graphite Fiber/Polyimide PMCs from Hot Melt versus Solution Prepreg

Carbon fiber reinforced high temperature polymer matrix composites (PMC) have been extensively investigated as potential weight reduction replacements of various metallic components in next generation high performance propulsion rocket engines. The initial phase involves development of comprehensive composite material-process-structure-design-property in-service performance correlations and database, especially for a high stiffness facesheet of various sandwich structures. Overview of the program plan, technical approaches and current multi-team efforts will be presented. During composite fabrication, it was found that the two large volume commercial prepregging methods (hot-melt vs. solution) resulted in considerably different composite cure behavior. Details of the process-induced physical and chemical modifications in the prepregs, their effects on composite processing, and systematic cure cycle optimization studies will be discussed. The combined effects of prepregging method and cure cycle modification on composite properties and isothermal aging performance were also evaluated.

Shin, Eugene E.↗

Fundamentals of Scalable Nanoparticle Assembly in Engineering Polymres

Systematically improving the properties of polymer nanocomposites is contingent on effectively controlling nanoparticle (NP) dispersion; further, it is necessary to attain this at scale if these methods are to impact practical applications. While most past work has focused on amorphous polymers, ≈ 70% of all polymers sold annually are semicrystalline. Inspired by this apparent disconnect, our work in the current DOE funded grant and this renewal proposal employs a novel handle, polymer crystallization, to organize NPs into the various amorphous zones of the lamellar semicrystalline morphology (interlamellar, interfibrillar and interspherulitic domains) of stereoregular polymers. We hypothesize that the isothermal crystallization rate of a polymer host, G, and NP diffusivity, are the two relevant control parameters in this context. In the case where the NPs are miscible in the melt, they remain spatially well-dispersed when the polymer is crystallized at a rate that is fast relative to NP diffusion. In contrast, monolayer-thick NP sheets with intersheet spacing of ~10-100nm form in slowly crystallized samples. This sheet stacking is remarkably similar to that seen in natural materials, e.g., Nacre. There is also ordering of the NPs at the larger interfibrillar scale. Importantly, the relative fraction of engulfed, interlamellar and interfibrillar NPs is determined by G. Further, the modulus of these materials can increase by a factor of 2-3 due to the organization state of the NPs, while leaving fracture toughness unaffected. We have established the broad applicability of this approach in two polymers, polyethylene (PE) and polyethyleneoxide (PEO). To achieve this goal we developed a method for grafting long PE chains from NPs with controlled graft density and molecular weight, giving us the ability to tailor their dispersion in the PE melt prior to crystallization. In this renewal proposal, we will develop the fundamental, quantitative understanding that will allow us to independently tailor polymer crystallization rate, NP diffusivity and NP agglomeration state in semicrystalline polymers so as to facilely control NP ordering and hence properties. A program that tightly integrates experiment and theory is proposed, and a key outcome of this research will be a three-dimensional design map for different regimes of NP organization (and hence properties) that can be achieved by polymer crystallization. A second independent outcome is the role of directional solidification and how it competes with the rates of polymer crystallization and NP mobility to affect the organization of the NP.

36 MATERIALS SCIENCE↗

Morphology of poly-3-hexyl-thiophene blends with styrene–isoprene–styrene block-copolymer elastomers from X-ray and neutron scattering

The nano- and micron scale morphology of poly(3-hexylthiophene) (P3HT) and polystyrene-block-polyisoprene-block-polystyrene (PS–PI–PS) elastomeric blends is investigated through the use of ultra-small and small angle X-ray and neutron scattering (USAXS, SAXS, SANS). It is demonstrated that loading P3HT into elastomer matrices is possible with little distortion of the elastomeric structure up to a loading of ~5 wt%. Increased loadings of conjugated polymer is found to significantly distort the matrix structure. Changes in processing conditions are also found to affect the blend morphology with especially strong dependence on processing temperature. Processing temperatures above the glass transition temperature (T g ) of polystyrene and the melting temperature (T m ) of the conjugated polymer additive (P3HT) creates significantly more organized mesophase domains. P3HT blends with PS–PI–PS can also be flow-aligned through processing, which results in an anisotropic structure that could be useful for the generation of anisotropic properties (e.g. conductivity). Moreover, the extent of flow alignment is significantly affected by the P3HT loading in the PS–PI–PS matrix. The work adds insight to the morphological understanding of a complex P3HT and PS–PI–PS polymer blend as conjugated polymer is added to the system. Here, we also provide studies isolating the effect of processing changes aiding in the understanding of the structural changes in this elastomeric conjugated polymer blend.

36 MATERIALS SCIENCE↗

15 years of spin-echo spectroscopy at SNS-NSE: Looking back and looking forward

High-resolution neutron spin echo (NSE) spectroscopy offers unique insights into the mobility of molecular (sub)structures excited by thermal fluctuations (i.e., Brownian motion) of “soft matter” as polymers in solution and in the melt, in biological matter (e.g., protein motions), membranes, and glasses. The ability to tag substructures using H, D contrast variation to resolve the relevant timescales of dynamics on selected molecular items in liquids, soft matter, and melts is a significant advantage of NSE. Also slow magnetic fluctuations on molecular length scales in the range of nanoseconds, e.g., in spin glasses or topological spin structures, can be accessed. This paper reviews the highlights and peculiarities of the SNS-NSE, based at the pulsed neutron source SNS, during its first 1.5 decades of operation. An outlook and perspectives of research in the domain of high-resolution spectroscopy is given.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Subsurface Spectroscopy of Thermal Degradation Inside an Inert Plastic Bonded Explosive (PBX) Simulant Using Feedback-Assisted Wavefront Shaping

We characterize the subsurface thermal degradation of an inert analog of high-explosive molecular crystals (Eu:Y(acac) 3 (DPEPO)) (EYAD) embedded inside of a plastic bonded explosive simulant using feedback-assisted wavefront shaping-based fluorescence and Raman spectroscopies. This technique utilizes wavefront shaping to focus pump light inside a heterogeneous material onto a target particle, which significantly improves its spectroscopic signature. We find that embedding the EYAD crystals in the heterogeneous polymer results in improved thermal stability, relative to bare crystal measurements, with the crystal remaining fluorescent to >612 K inside of the heterogeneous material, while the bare crystal’s fluorescence is fully quenched by 500 K. We hypothesize that this improvement is due to the polymer restricting the effects of EYAD melting, which occurs at 400 K and is the primary mechanism for spectroscopic changes in the temperature range explored.

Anderson, Benjamin R.↗

Hot forming graphite/polyimide structures

Hot forming process has been developed in which structural shapes and panels are fabricated directly from stabilized graphite/polyimide preforms. Process can be used with thermosetting polymers that have high-temperature melt phase just before final cure. This phase allows fibers to move without destroying matrix-to-fiber adhesion. One of key advantages of this process is that prestages preforms are very stable and do not require refrigerated storage.

Baucom, R. M.↗

A new brominated polymeric additive for flame retardant glass-filled polybutylene terephthalate

Attention is called to the undesirable effects (poor ultraviolet light stability and blooming) sometimes introduced by brominated flame retarders. A brominated polymeric additive (BPA) with little or none of these undesirable side effects is compared with decabromobiphenyl oxide (DBBPO). The additive bears the product name F-2300. It is found to be more easily dispersed than DBBPO. The F-2300 is as effective as the DBBPO in the oxygen index test. The improved efficiency of the F-2300 may be explained by its better dispersion in polybutylene terephthalate (PBT). Glass-filled PBT containing F-2300 is found to be more resistant to UV degradation than DBBPO-containing formulas. Formulations with F-2300 therefore have a longer useful outdoor life. F-2300 is a diglycidyl-type polymer containing 50 percent aromatically bound bromine. Its melting point is 112 C, and it is stable up to 372 C. It is pointed out that since its melts at a relatively low temperature, it can be introduced into the formulation as a large agglomerate and still be dispersed evenly throughout the polymer.

Nir, Z.↗

Levitation of superconducting composites

The inverse levitation of a high temperature superconductor polymer composite consisting of powdered quench melt growth Ba2YCu3O(7-delta) and cyanoacrylate is reported. Magnetic hysteresis loop measurements for the composite are compared to those measured for the bulk material prior to powdering. Differences in the flux pining capability between the two material forms are small but significant.

Chiang, C. K.↗

High-Temperature Shape Memory Polymers

physical conformation changes when exposed to an external stimulus, such as a change in temperature. Such materials have a permanent shape, but can be reshaped above a critical temperature and fixed into a temporary shape when cooled under stress to below the critical temperature. When reheated above the critical temperature (Tc, also sometimes called the triggering or switching temperature), the materials revert to the permanent shape. The current innovation involves a chemically treated (sulfonated, carboxylated, phosphonated, or other polar function group), high-temperature, semicrystalline thermoplastic poly(ether ether ketone) (Tg .140 C, Tm = 340 C) mix containing organometallic complexes (Zn++, Li+, or other metal, ammonium, or phosphonium salts), or high-temperature ionic liquids (e.g. hexafluorosilicate salt with 1-propyl-3- methyl imidazolium, Tm = 210 C) to form a network where dipolar or ionic interactions between the polymer and the low-molecular-weight or inorganic compound forms a complex that provides a physical crosslink. Hereafter, these compounds will be referred to as "additives". The polymer is semicrystalline, and the high-melt-point crystals provide a temporary crosslink that acts as a permanent crosslink just so long as the melting temperature is not exceeded. In this example case, the melting point is .340 C, and the shape memory critical temperature is between 150 and 250 C. PEEK is an engineering thermoplastic with a high Young fs modulus, nominally 3.6 GPa. An important aspect of the invention is the control of the PEEK functionalization (in this example, the sulfonation degree), and the thermal properties (i.e. melting point) of the additive, which determines the switching temperature. Because the compound is thermoplastic, it can be formed into the "permanent" shape by conventional plastics processing operations. In addition, the compound may be covalently cross - linked after forming the permanent shape by S-PEEK by applying ionizing radiation ( radiation, neutrons), or by chemical crosslinking to form a covalent permanent network. With respect to other shape memory polymers, this invention is novel in that it describes the use of a thermoplastic composition that can be thermally molded or solution-cast into complex "permanent" shapes, and then reheated or redissolved and recast from solution to prepare another shape. It is also unique in that the shape memory behavior is provided by a non-polymer additive.

Yoonessi, Mitra↗