At least 217 records · Page 12

A Bi-Layer Dense/Porous Solid Electrolyte Interphase for Enhanced Lithium-Metal Stability

Due to its high theoretical capacity and low electrochemical potential, lithium metal is a highly investigated anode for next-generation high-energy batteries. However, the unstable chemical and topographical heterogeneous surface of lithium gives rise to safety and efficiency concerns that prevent it from being utilized in practical applications. Exposure to electrolyte leads to non-uniform, mixed organic-inorganic solid-electrolyte interphase (SEI) formation, starting a cascading to non-uniform flux distribution, consumption of active materials, and dendrite growth. The SEI is the key feature that will lead to harnessing the capabilities possible with lithium metal. In this work, the formation of a closed-host bi-layer solid electrolyte interphase (SEI) improves the stability of lithium anode. This is successfully realized by forming an interconnected porous LiF-rich artificial SEI in contact with Li metal, and a dense, stable in-situ formed upper layer SEI. The porous layer increases the number of Li/LiF interfaces, which reduces local volume fluctuations and improves Li+ diffusion along these interfaces. Additionally, the tortuous porous structure guides uniform Li+ flux distribution and mechanically suppresses dendrite propagation. The dense upper layer of the SEI accomplishes a closed-host design through reaction with LiNO3 additive and prevents continuous consumption of active materials seen without the additive included in the electrolyte. The duality of a dense top layer with porous bottom layer led to extended cycle life and improved rate performance, evidenced with symmetric cell testing, as well as full cell testing paired with sulfur and LiFePO4 (LFP) cathodes. This work is a good example of a rational design of the SEI, based on comprehensive consideration of various critical factors to improve Li-metal anode stability, and highlights a new pathway to improve cycling and rate performances of Li metal batteries.

25 ENERGY STORAGE↗

Increasing the Pressure‐Free Stripping Capacity of the Lithium Metal Anode in Solid‐State‐Batteries by Carbon Nanotubes

Abstract Lithium metal is the key anode material for solid‐state‐batteries as its successful implementation will drastically increase their energy and power densities. However, anode contact loss during stripping leads to dendrites upon plating and subsequent cell failure. Design strategies to mitigate these issues are crucial to enable the use of lithium metal anodes. This paper reports the dissolution kinetics of composite anodes made of lithium metal and carbon nanotubes (CNTs) with a garnet‐type solid electrolyte (SE). In addition to an enhancement of the effective diffusion within the anode, its dissolution is fundamentally changed from being 2D to 3D. By maintaining contact with the SE, the CNTs facilitate lithium transport to the interface, which yields more than 20 mAh cm −2 discharge capacity at 100 µ A cm −2 without the application of external stack pressure ( > 1 MPa). Conclusions drawn from electrochemical data on the anode microstructure are validated using cryo‐focused‐ion‐beam scanning electron microscopy and correlated with the mechanical properties. Micro‐indentation, acoustic analysis, and stress–strain testing show that mechanical properties of the anode, like yield strength and hardness, are adjustable. Overall, it is shown that the mechanical and electrochemical properties of Li–CNT composite electrodes can be tailored to suit the requirements of a practical cell.

Fuchs, Till↗

Ion‐Conducting, Electron‐Blocking Layer for High‐Performance Solid Electrolytes

Lithium metal batteries bring greater promise for energy density, often relying on solid‐state electrolytes to meet critical benchmarks. However, Li dendrite formation is a prevailing problem that limits the cycle life and Coulombic efficiency of solid‐state Li metal batteries. For the first time, a thin (<100 nm) layer of electronically insulating, ionically conducting lithium phosphorus oxynitride (LiPON) is applied using atomic layer deposition between a Li anode and garnet Li 7 La 3 Zr 2 O 12 (LLZO). The performance of a conformal LiPON layer as an electron barrier in symmetric Li‐LLZO cells is observed through potential step chronoamperometry, galvanostatic cycling, electron microscopy, and various spectroscopic techniques. The LiPON‐coated LLZO achieves 100 times lower electronic conductance than LLZO alone. Cycling carried out at 0.1 mA cm −2 for 100 cycles demonstrates that suppression of electron pathways into the bulk solid electrolyte improves the cycle life of a lithium metal cell. These findings suggest an electronic conductivity effect in solid‐state electrolytes. A strategy is demonstrated to design thin‐film (LiPON)‐modulated bulk solid‐state electrolytes (LLZO) capable of maintaining high ionic conductivity and electrochemical stability while reducing the effective electronic conductivity, which results in significantly decreased dendrite formation, improved cycle life, and greater interfacial integrity between the electrolyte and a Li anode.

Hitz, Emily M.↗

Lithicone‐Protected Lithium Metal Anodes for Lithium Metal Batteries with Nickel‐Rich Cathode Materials

The high energy density advantage of lithium (Li) metal batteries (LMBs) makes them increasingly desirable; however, problems such as strong reactivity and dendrite growth of Li metal anode limit their practical uses. In this work, a novel Li‐containing glycerol (LiGL) or lithicone protection layer on a 50 μm thick Li metal anode is employed for improving the performance of LMBs. This LiGL layer was accurately deposited via a molecular layer deposition (MLD) process at 150 °C, using lithium tert‐butoxide and glycerol as precursors. The as‐formed LiGL coating layer is highly tunable in its thickness by simply adjusting MLD cycles and shows a good stability and outstanding ionic transport properties. The LiGL layer is found to effectively mitigate side reactions and enhance cycling stability in both symmetric cells and full cells. Specifically, the LMBs with LiGL@Li anode of 400 MLD cycles and LiNi 0.6 Mn 0.2 Co 0.2 O 2 cathode enable a capacity retention of ≈87%, much higher than ≈35% of the cells with bare Li after 200 cycles at a charge/discharge current density of 2.1 mA cm −2 . This work paves a feasible way for practical LMBs with improved capacity and stability through applying an innovative protection layer on Li metal anodes.

25 ENERGY STORAGE↗

The Critical Stack Pressure to Alter Void Generation at Li/Solid-Electrolyte Interfaces during Stripping

The lithium stripping process generates vacancies, which may accumulate as voids and lead to uneven current distribution and dendrite growth in the following plating cycles. A stack pressure is typically required during stripping, but how to optimize the stack pressure is not clear. In this work, extremely lithiophilic Li/Li 2 O and lithiophobic Li/LiF interfaces were used to reveal the combining effect of interface interaction and stack pressure induced lithium creep on the stripping critical current density (CCD). A multiscale simulation scheme with Density Functional Theory (DFT), kinetic Monte Carlo (KMC) simulations, and an analytical model was developed. The analytical model predicted lithiophobic interfaces require a higher stack pressure than lithiophilic interfaces to reach the same CCD. The KMC simulations also showed higher stack pressure is needed at lithiophobic interfaces to accelerate Li vacancy diffusion into the bulk and maintain a flat surface. This stack pressure needs to be high enough to alter the Li forward-and-backward hopping barriers at the interface. This multiscale simulation scheme illustrates the importance to include the chemical-mechanical effects during Li stripping morphology evolution. It can be used to design ideal interlayer coating materials to maintain a flat Li surface during cycling.

25 ENERGY STORAGE↗

Low-temperature and high-rate-charging lithium metal batteries enabled by an electrochemically active monolayer-regulated interface

Stable operation of rechargeable lithium (Li)-based batteries at low temperatures is vital for cold-climate applications but is plagued with dendritic Li plating and unstable solid-electrolyte interphase (SEI). Here we report high-performance Li-metal batteries under low-temperature and high-rate-charging conditions. This is realized by utilizing a self-assembled monolayer of electrochemically active molecules on current collectors that regulates the nanostructure and composition of SEI and deposition morphology of Li metal anodes. A multilayer SEI containing a LiF-rich inner phase and amorphous outer layer effectively seals the Li surface in contrast to the conventional impassive SEI at low temperatures. As a result, galvanic Li corrosion and self-discharge were suppressed; stable Li deposition was realized from -60º to 45ºC; and a Li|LiCoO 2 cell with a capacity of 2.0 mAh cm -2 displayed a 200-cycle life at -15ºC with a recharge time of 45 minutes.

25 ENERGY STORAGE↗

Understanding the Selective Deposition of Li Metal on Nonuniform Electrode Surfaces Using Atomic Force Microscopy

The use of lithium metal in secondary batteries has been impeded by its tendency to form dendrites: branching conductive structures of metal that can lead to capacity loss and, ultimately, internal shorts in the battery. Patterned electrodes, in addition to artificially increasing the current density of cells by increasing the surface area available for reaction, also generate a nonuniform electric field in the vicinity of the electrode surface. This nonuniform electric field, though rapidly screened by the electrolyte, can promote inhomogeneous deposition and Solid Electrolyte Interphase formation. As the consequence of these effects is not theoretically apparent since Solid Electrolyte Interphase volume and conductivity changes can, in principle, offset variations in local current density, we have performed experiments to examine the deposition of Li on nonuniform electrode surfaces using Atomic Force Microscopy. In this work, we measure the local variations in topography, SEI thickness, and composition, and discuss their implications for the formation of dendrites in Li metal.

25 ENERGY STORAGE↗

Lithium Nucleation of Anode-Free Solid-State Batteries with a Dry Compressible Interlayer

Anode-free lithium batteries offer promising advantages, including increased energy density and the ability to address common mechanistic failures within the cell, thus increasing safety. One way that can make this possible is to control lithium nucleation. This could be achieved by reducing the overpotential required and implanting lithophilic nucleation sites in an anodic interlayer to aid in lithium ion transport and plating. The concept has been utilized in solid-state battery systems where electrolytes are solids with further improved safety and structural longevity. In this presentation, we discuss the use of a silver-holey graphene-based anodic interlayer that can be fabricated via direct dry compression without the use of solvent or binder. The addition of silver to the holey graphene matrix creates a route to lithium plating via a lower-energy intermediate. This idea is supported by the presence of a lithium-silver alloy that forms during the activation step. It is understood that the embedded silver acts as a nucleation site for lithium ions, thereby assisting in even plating. This control, combined with the added cushion of the holey graphene itself, can help reduce dendrite formation, ultimately increasing the safety and lifetime of the solid-state batteries.

Solid state batteries↗

Computational Elucidation of Mechanical Degradation in NMC Cathodes: Impact on Cell Performance

Next-generation lithium ion batteries are expected to demonstrate superior energy and power density with longer cycle life for successful electrification of the automobile, aviation, and marine industries. Adoption of lithium metal anodes with solid electrolytes can help to achieve that goal given that the dendrite-related issues are solved eventually. Another possibility is to use Ni-rich high-capacity NMC cathode materials with liquid and/or solid electrolytes, which presently experiences rapid capacity fade while charged to higher voltages. Several mechanical and chemical degradation mechanisms are active within these NMC-based cathode particles. Recent experimental research activities attempted to correlate the mechanical damage with the capacity fade experienced by Ni-rich LiNi x Mn y Co z O 2 (x+y+z = 1) (NMC) cathodes. Here, a computational framework is developed in this study capable of quantifying the evolution of inter primary particle and cathode/electrolyte interfacial fracture experienced by the poly- and single-crystalline NMC cathodes during charge/discharge operation. Influences of mechanical degradation on the overall cell capacity, while operating with liquid and/or solid electrolytes, are successfully characterized. Decreasing the size of the cathode primary particles, or the size of the single-crystalline cathodes, can mitigate the overall mechanical degradation, and subsequent capacity fade, experienced by NMC cathodes. The developed theoretical methodology can help the engineers and scientists to better understand the mechanical degradation mechanism prevalent in Ni-rich NMC cathodes and build superior lithium ion-based energy storage devices for the application in next-generation devices.

25 ENERGY STORAGE↗

Anion modification for stable solid electrolyte interphase in anode-free lithium metal batteries

The durability of anode-free Li metal batteries is largely limited by the undesired Li plating/stripping irreversibility on the current collector due to the infinite volume change, uncontrollable Li dendrite growth, and continuous parasitic reactions between Li metal and the electrolyte. To address these challenges, the formation of a stable and robust solid electrolyte interphase (SEI) with high ionic conductivity and strong mechanical strength is critical. Here, we developed an advanced electrolyte by introducing LiNO 3 into the localized high concentration electrolyte (LHCE) with lithium bis(fluorosulfonyl)imide (LiFSI) salt, 1,2-dimethoxyethane (DME) solvent, and 1,1,2,2-tetrafluoroethyl-2,2,3,3-tetrafluoropropylether (TFTE) diluent to in situ construct a LiF and Li x N y O z co-enriched passivation layer on the Cu current collector. The synergetic effect of high mechanical strength of LiF and high ionic conductivity of Li x N y O z endows the Li metal anode with a high Coulombic efficiency (CE) of 99.35%. In conclusion, in anode-free Li metal pouch cell using LiFePO 4 (LFP) as a cathode holds an exceptionally improved capacity retention under the charging/discharging rate of 1/3 C, demonstrating great promise for developing dendrite-free and safe Li metal batteries.

25 ENERGY STORAGE↗

Effects of Applied Interfacial Pressure on Li-Metal Cycling Performance and Morphology in 4 M LiFSI in DME

Lithium-metal anodes can theoretically enable 10x higher gravimetric capacity than conventional graphite anodes. However, Li-metal anode cycling has proven difficult due to porous and dendritic morphologies, extensive parasitic solid electrolyte interphase reactions, and formation of dead Li. We systematically investigate the effects of applied interfacial pressure on Li-metal anode cycling performance and morphology in the recently developed and highly efficient 4 M lithium bis(fluorosulfonyl)imide in 1,2-dimethoxyethane electrolyte. We present cycling, morphology, and impedance data at a current density of 0.5 mA/cm 2 and a capacity of 2 mAh/cm 2 at applied interfacial pressures of 0, 0.01, 0.1, 1, and 10 MPa. Cryo-focused ion beam milling and cryo-scanning electron microscopy imaging in cross section reveal that increasing the applied pressure during Li deposition from 0 to 10 MPa leads to greater than a fivefold reduction in thickness (and therefore volume) of the deposited Li. This suggests that pressure during cycling can have a profound impact on the practical volumetric energy density for Li-metal anodes. A “goldilocks zone” of cell performance is observed at intermediate pressures of 0.1–1 MPa. Increasing pressure from 0 to 1 MPa generally improves cell-to-cell reproducibility, cycling stability, and Coulombic efficiency. However, the highest pressure (10 MPa) results in high cell overpotential and evidence of soft short circuits, which likely result from transport limitations associated with increased pressure causing local pore closure in the separator. All cells exhibit at least some signs of cycling instability after 50 cycles when cycled to 2 mAh/cm 2 with thin 50 μm Li counter electrodes, though instability decreases with increasing pressure. In contrast, cells cycled to only 1 mAh/cm 2 perform well for 50 cycles, indicating that capacity plays an important role in cycling stability.

25 ENERGY STORAGE↗

Impact of Salt Chemistry and Interlayer Architecture on Solid Electrolyte Interphase Composition and Performance

Reversible lithium metal anodes require interphases that are chemically stable, mechanically robust, and compatible with scalable processing. Here, we use slot-die-coated, salt-rich PEO interlayers to design SEI nanolayers on Cu current collectors and isolate how salt anion chemistry controls interphase composition and lithium plating/stripping behavior in architectures relevant to Li plating and anode-free cells. Mesoscale modeling shows that dendrite initiation at SEI defects is governed by a tradeoff among interphase thickness, ionic conductivity, and stiffness through defect-driven current focusing, motivating controlled formation from thin precursor layers. Using UHV-transferred XPS and ToF-SIMS depth profiling after controlled Li deposition, we find that fluorinated sulfonylimide salts (LiTFSI, LiFSI) form mixed inorganic/organic interphases containing LiF and PEO-derived alkoxides, with LiFSI producing a more LiF-dominant Li-facing surface than LiTFSI under identical conditions. In contrast, LiNO 3 -containing interlayers yield a comparatively thick nitrate-derived interphase that reduces upon Li contact to an N-rich inorganic layer (Li–N/N 3− , LiN x O y ). In Cu| |Li cells, these designed interlayers reduce interfacial resistance and improve Coulombic efficiency (CE) and critical current density (CCD) relative to uncoated controls, with LiFSI- and LiNO 3 -based interlayers providing the highest CE/CCD. Overall, the results demonstrate a manufacturing-relevant approach to engineer SEI nanolayers by salt chemistry, providing pathways to improve reversible lithium metal anodes while reducing reliance on LiTFSI.

anion chemistry↗

Method of improved performance in metal electrodes for batteries

Disclosed are methods for pre-conditioning or pre-treating the surface of a metal (e.g., lithium) electrode such that the cycle life and efficiency of the electrode within an electrochemical cell are improved through the prevention of dendrite growth. The pretreatment process includes the use of an alternating current to modify the surface properties of the metal electrode, such that a more uniform flux of metal ions is transferred across the electrode-electrolyte Interface in subsequent electrodeposition and electrodissolution processes. As a result, an electrode treated with such a process exhibits improved performance and durability, including markedly lower overpotentials and largely improved metal (e.g., lithium) retention in strip plate tests as compared with untreated electrodes.

Dasgupta, Neil P.↗

Lithium Growth on Alloying Substrates and Effect on Volumetric Expansion

The widespread implementation of next-generation Li metal anodes is limited, in part, due to the formation of dendritic and/or mossy electrodeposits during cycling. These morphologies can lead to battery failure due to the formation of short circuits and significant volumetric expansion at the anode. One strategy to control the electrodeposition of Li metal is to use lithiophilic materials at the anode. Here, we evaluate the impact of Ag and Au on the early stages of Li metal electrodeposition and cycling. The alloying substrates decrease the voltage for Li reduction and improve Li wetting/adhesion. We probe volumetric expansion directly through dilatometry measurements and find that the degree of volumetric expansion is less when lithium is cycled on an alloying substrate compared to a non-alloying substrate (Cu). Dilatometry experiments reveal that Au has the least amount of volumetric expansion and coin cell cycling experiments indicate that Ag yields more stable cycling compared to Au or Cu. The evaluation of in situ cross-sectional images of cycled coin cells shows that Ag has the lowest volumetric expansion in a coin cell format.

alloys↗

Mechanical and electrical changes in electrochemically active polyimide binders for Li-ion batteries

Polyimide binders are often used in electrodes made with silicon for lithium-ion batteries for their mechanical strength and adhesion, which help mitigate mechanical issues associated with large volumetric expansion. These binders can be electrochemically active, but it is difficult to characterize what physical and chemical changes occur due to a composite electrode with multiple components and processes at play. Here, in this work, we study electrodes consisting only of polyimide binder and conductive carbon, using scanning probe-based techniques—contact resonance, force volume, and scanning spreading resistance microscopy—along with cryo-scanning transmission electron microscopy, electron energy loss spectroscopy, and energy dispersive X-ray spectroscopy. We show that lithium becomes trapped in the binder during cycling and results in large initial capacity losses, the formation of dendrite-like features, column-like domains of significantly increased mechanical modulus, and a slight increase in electronic resistivity.

25 ENERGY STORAGE↗

Local Ultrasonic Resonance Spectroscopy of Lithium Metal Batteries for Aerospace Applications

As next-generation aircraft and vehicles continue to develop, so do their associated energy demands. Lithium metal batteries are a leading candidate to fulfill this energy requirement, but these batteries are prone to internal dendrite defects that can lead to catastrophic thermal runaway events. Current battery management systems are capable of mitigating such risks, but are unable to detect such defects until thermal runaway has already begun. Various nondestructive evaluation (NDE) techniques, particularly ultrasonic NDE, can directly monitor internal battery parameters giving them the potential to detect critical defects prior to catastrophic failure. However, most of the current battery NDE research has focused on improved battery state-of-charge (SOC) and stateof- health (SOH) monitoring with little emphasis on critical defect detection. Thus, a measurement technique sensitive to subtle battery defects is needed. In addition, the complex mechanics of ultrasound in porous, thin, multilayered batteries prompt the use of physics-based simulation to guide inspections. In this work, an ultrasonic NDE technique has been developed utilizing frequency domain analysis of local battery resonances to detect the presence of battery defects. This technique is a practical extension of local ultrasonic resonance spectroscopy (LURS) – which previously required non-contact laser ultrasonics – to measurements with piezoelectric contact and immersion scan transducers. To extend the technique to work with piezoelectric transducers, ultrasonic battery measurements were compared to a sans-battery calibration measurement. Then, a linear systems deconvolution was used to eliminate the transfer functions of extraneous factors such as the transducer and electronics, leaving only the frequency-dependent battery reflection coefficient. The LURS technique was first validated on stainless steel and aluminum plates, producing reflection coefficients in line with analytical and numerical finite element modeling (FEM) results. Functioning Li-metal pouch cells were then seeded with lithium chip defects prior to LURS measurements. The presence of these defects is shown to cause a measurable shift in the battery’s through-thickness local resonances. 2D, frequency-domain poroelastic models of ultrasonic propagation in a single-cell lithium metal pouch battery were created and corroborated these findings. Thus, this work has both extended and proven the feasibility of the LURS technique in the detection of local battery defects.

Ultrasound↗

Fundamental Study of Uranium Dendrites Electrochemically Separated in Molten Salt with the Presence of Cerium

In this study, uranium was electrochemically separated in the presence of cerium in eutectic LiCl-KCl at varying concentrations of cerium and varying overpotentials. Harvested dendrites were then examined and analyzed for their morphological features and elemental composition using various analytical techniques. Conclusions: Increasing the applied overpotential causes the dendrites to evolve from relatively simple and large platelet-like crystals (25 mV), to a grid-like network with crystals having jagged and smooth features (50 mV, 100 mV), and finally into a very chaotic and complex crystal morphology (200 mV) for all uranium-cerium compositions explored. Varying the uranium:cerium concentration ratio did not have much effect on the uranium dendrite morphologies. EDS results show that cerium is not co-deposited on the surface of the dendrite crystals, ICP-MS results do show a presence of cerium in the volumetric composition. This is likely due to salt occlusion during the dendrite formation. XRD has been performed on several samples at the 25 mV overpotential with 1 wt% U and 0 wt% Ce in the molten salt eutectic. These results indicate that there is not salt occlusion within the dendrites during electrochemical separation. Additionally, the uranium metal quickly oxidizes during preparation for XRD.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

A self-healing plastic ceramic electrolyte by an aprotic dynamic polymer network for lithium metal batteries

Abstract Oxide ceramic electrolytes (OCEs) have great potential for solid-state lithium metal (Li 0 ) battery applications because, in theory, their high elastic modulus provides better resistance to Li 0 dendrite growth. However, in practice, OCEs can hardly survive critical current densities higher than 1 mA/cm 2 . Key issues that contribute to the breakdown of OCEs include Li 0 penetration promoted by grain boundaries (GBs), uncontrolled side reactions at electrode-OCE interfaces, and, equally importantly, defects evolution (e.g., void growth and crack propagation) that leads to local current concentration and mechanical failure inside and on OCEs. Here, taking advantage of a dynamically crosslinked aprotic polymer with non-covalent –CH 3 ⋯CF 3 bonds, we developed a plastic ceramic electrolyte (PCE) by hybridizing the polymer framework with ionically conductive ceramics. Using in-situ synchrotron X-ray technique and Cryogenic transmission electron microscopy (Cryo-TEM), we uncover that the PCE exhibits self-healing/repairing capability through a two-step dynamic defects removal mechanism. This significantly suppresses the generation of hotspots for Li 0 penetration and chemomechanical degradations, resulting in durability beyond 2000 hours in Li 0 -Li 0 cells at 1 mA/cm 2 . Furthermore, by introducing a polyacrylate buffer layer between PCE and Li 0 -anode, long cycle life >3600 cycles was achieved when paired with a 4.2 V zero-strain cathode, all under near-zero stack pressure.

36 MATERIALS SCIENCE↗