Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “degradable”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 217 records · Page 12

The degradation of space shuttle TPS metals in dissociated oxygen.

The interaction of space shuttle orbiter Thermal Protection System (TPS) metals with the chemical environment to which it is exposed during reentry is considered with emphasis on the effects of dissociated oxygen. Experimental results comparing the interactions of atomic (dissociated) and molecular oxygen with five candidate shuttle TPS metals, Ni-20Cr-2ThO2, Ni-20Cr-3.5Al-2ThO2, Ni-16Cr-15Fe-2Mn-.5Si-.3La-2ThO2, Haynes Alloy Number 188, and Ti-6Al-4V at their maximum planned use temperature are presented. As measured by metal recession, weight change, rate of oxide scale formation, and scale spalling, the first four metals show enhanced degradation in a dissociated oxygen environment. The enhanced degradation appears to result from differing rates of alloy constituent reactions in the two environments. The dissociated oxygen environmental tests are found to better assess the usefulness of shuttle skin materials for the planned mission than do conventional molecular (either flowing or static) oxidation experiments.-

Gilbreath, W. P.↗

Observations on degradation of UV systems on Nimbus spacecraft

Broad band photometer experiments in the 1200 to 3000 A have been operating on Nimbus 3 and 4 since April 1969 for the purpose of determining the nature of variations in the UV solar irradiance. An Ebert-Fastie double monochromator has been measuring the solar irradiance and earth radiance from 2500 to 3400 A for the determination of global atmospheric ozone distributions since April 1970. From prelaunch testing and an evaluation of the flight data it is concluded that the principal source of degradation is probably the spacecraft. The degradation produces a characteristic signal loss and change in angular response of the system which might be explained by micron sized droplets becoming a permanent residue under the influence of solar UV radiation.

Heath, D. F.↗

Water and processes of degradation in the Martian landscape

It is shown that erosion has been active on Mars so that many of the surface landforms are products of degradation. Unlike earth, erosion has not been a universal process, but one areally restricted and intermittently active so that a landscape is the product of one or two cycles of erosion and large areas of essentially undisturbed primitive terrain; running water has been the principal agent of degradation. Many features on Mars are most easily explained by assuming running surface water at some time in the past; for a few features, running water is the only possible explanation.

Milton, D. J.↗

A model to predict the degradation of a SiGe thermopile.

Discussion of the various phenomena which affect the available output power of a typical radioisotope thermoelectric generator (RTG), including estimates of the magnitude of these effects. Power degradation, as well as the corresponding changes in operating temperature, are calculated by means of a computer code which systematically accounts for the time- and temperature-dependent variables. A model for predicting available output power of an RTG is developed which includes changes in performance due to fuel decay, alteration of bulk thermoelectric properties, changes in electrode contacts, geometry changes due to material sublimation, and degradation of the thermal insulation.

Stapfer, G.↗

Diffusional creep and creep-degradation in dispersion-strengthened Ni-Cr base alloys.

Dispersoid-free regions were observed in the dispersion-strengthened alloy TD-NiCr (Ni-20 Cr-2 ThO2) after slow strain rate testing (stress rupture, creep, and fatigue) in air from 1145 to 1590 K. Formation of the dispersoid-free regions appears to be the result of diffusional creep. The net effect of creep in TD-NiCr is the degradation of the alloy to a duplex microstructure. Creep degradation of TD-NiCr is further enhanced by the formation of voids and intergranular oxidation in the dispersoid-free bands. Void formation was observed after as little as 0.13% creep deformation at 1255 K. The dispersoid-free regions apparently provide sites for void formation and oxide growth since the strength and oxidation resistance of Ni-20 Cr-2 ThO2.

Whittenberger, J. D.↗

Restoration of degraded images by composite gratings in a coherent optical processor.

A study has been made on restoration of degraded images utilizing spatial filtering techniques in a coherent optical processor. This study differs from other coherent approaches in that the spatial filters employed contain only composite gratings that are quite simple to produce. A general method of synthesizing the appropriate composite gratings for linearly smeared as well as multiply exposed and out-of-focus images will be presented in some detail with experimental results. The extension of the method of synthesis to other types of degradation is briefly discussed.

Jablonowski, D. P.↗

A study of the effects of solid phase reactions on the thermal degradation and ballistic properties of solid propellants

The thermal stability of perchlorate composite propellants was studied at 135 and 170 C. The experimental efforts were concentrated on determining the importance of heterogeneous oxidizer-fuel reactions in the thermal degradation process. The experimental approach used to elucidate the mechanisms by which the oxidizer fuel composites thermally degrade was divided into two parts: (1) keeping the fuel constant and varying the nature of the oxidizers, and (2) holding the oxidizer constant and varying the fuel components. The fuel component primarily utilized in the first phase was polyethylene. Oxidizers included KClO4, KClO3, NH4ClO4 and NH4ClO4 doped with materials such as chlorate, phosphate and arsenate. In the second phase the oxidizer used was primarily NH4ClO4 while the fuels included saturated and unsaturated polybutadiene prepolymers and a series of bonding agents. Techniques employed in the current study include thermogravimetric measurements, differential thermal analysis, infrared, mass spectrometry, electron microscopy, and appropriate wet chemical analysis.

Schmidt, W. G.↗

Effects of diffusion on aluminum depletion and degradation of NiAl coatings

Experimental demonstration of the effects of diffusion on aluminum depletion and degradation in NiAl coatings on superalloys. Pack aluminized IN 100 and Mar-M200 were vacuum annealed at 1100 C to allow diffusion to proceed independently of oxidation. As-coated and as-diffused coatings were compared before and after cyclic furnace oxidation at 1100 C. The extent of degradation was judged by specific weight change, metallography, and electron microprobe analyses.

Smialek, J. L.↗

Research study on high energy radiation effect and environment solar cell degradation methods

The most detailed and comprehensively verified analytical model was used to evaluate the effects of simplifying assumptions on the accuracy of predictions made by the external damage coefficient method. It was found that the most serious discrepancies were present in heavily damaged cells, particularly proton damaged cells, in which a gradient in damage across the cell existed. In general, it was found that the current damage coefficient method tends to underestimate damage at high fluences. An exception to this rule was thick cover-slipped cells experiencing heavy degradation due to omnidirectional electrons. In such cases, the damage coefficient method overestimates the damage. Comparisons of degradation predictions made by the two methods and measured flight data confirmed the above findings.

Horne, W. E.↗

Measurements of capillary system degradation

The effects of vibration, flow transients, and warm gas pressurization on capillary acquisition system performance were evaluated. The degradation observed under wide band random and high frequency sinusoidal vibration was of a substantially different nature from that obtained under low frequency sinusoidal vibration. With the former, ingestion of small gas bubbles into the liquid region was correlated by a hydrostatic model, while the capillary stability was destroyed and liquid was lost from the liquid region with the latter. No degradation was observed as a result of flow transients in a flight-type multichannel screen device, but it was observed in a transparent laboratory device. Liquid hydrogen outflow tests were conducted with a multilayer dual-screen-liner system with both helium and hydrogen pressurant gases. The tendency towards dryout of the device with hydrogen pressurant was found to increase with increasing pressurant temperature and length of prepressurization period. Dryout did not occur with helium pressurant.

Warren, R. P.↗

Image degradation in aerial imagery duplicates

A series of Earth Resources Aircraft Program data flights were made over an aerial test range in Arizona for the evaluation of large cameras. Specifically, both medium altitude and high altitude flights were made to test and evaluate a series of color as well as black-and-white films. Image degradation, inherent in duplication processing, was studied. Resolution losses resulting from resolution characteristics of the film types are given. Color duplicates, in general, are shown to be degraded more than black-and-white films because of the limitations imposed by available aerial color duplicating stock. Results indicate that a greater resolution loss may be expected when the original has higher resolution. Photographs of the duplications are shown.

Lockwood, H. E.↗

Chemiluminescence Study on Thermal Degradation of Aircraft Tire Elastomers

Since the autoxidative process accounts in part for the degradation of rubber, including aircraft tires, it was felt that a study of the chemiluminescence from unsaturated elastomers could contribute significantly to an understanding of the degradation mechanism. The study revealed similarities in chemiluminescence behavior between four elastomers which were investigated, and it shows that similar oxidation mechanisms occur. Oxidative chemiluminescence was observed from purified samples of cis-1,4-polybutadiene, cis-1,4-polyisoprene, trans-polypentenamer, and 1,2-polybutadiene in an oxygen atmosphere at 25-150 C. The elastomer samples were placed in a 600 watt oven which is equipped with gas inlets for introducing any desired atmosphere. Chemiluminescence emission from the samples was focused with a two inch quartz lens onto the detector of a 12" photomultiplier which is connected to a photon counter. A strip-chart recorder, connected to the counter, permitted automatic data collection. Diagrams of the apparatus are included. The chemical reactions which occurred from the thermal decomposition of the polymer samples are described, and results (and tabulated data) are discussed.

Mendenhall, G. D.↗

Degradation of a Multilayer Insulation Due to a Seam and a Penetration

The degradation of the thermal performance of a multilayer insulation due to the presence of a seam and a penetration was studied. The multilayer insulation had 30 aluminized Mylar radiation shields with silk net spacers. The seam, an offset butt joint, caused a heat input of 0.169 watt per meter in addition to the basic insulation thermal performance of 0.388 watt per square meter obtained before the installation of the butt joint. The penetration, a fiberglass tank support strut, provided a heat input (including the degradation of the insulation) of 0.543 watt in addition to the basic insulation thermal performance of 0.452 watt per square meter obtained before the penetration.

Sumner, I. E.↗

Syntheses and degradations of fluorinated heterocyclics

The relative stability of two ring systems, the triazine rings and 1,2,4-oxadiazoles, which offer potential crosslinks useful for curing perfluoroalkyl ether elastomers, has been investigated. Tris (perfluoro-n-heptyl)-s-triazine, the perfluoroether substituted-s-triazine, 1,4-bis/(5-perfluoro-n-heptyl)-1,2,4-oxadiazolyl/benzene, its perfluoroalkyl ether substituted analog, and 3,5-bis-(perfluoro-n-heptyl)-1,2,4-oxadiazole were synthesized and subjected to thermal and oxidative degradation at 235 and 325 C and to hydrolytic degradation at 235 C. The perfluoroalkyl ether substituted triazine and 3,5-bis(perfluoro-n-heptyl)-1,2,4-oxadiazole were found to be stable under all conditions investigated.

Paciorek, K. L.↗

Characterization of degraded nickel cadmium cells

Various cells were cycled until degradation and then tested to determine the electrochemical characterization of the cells with regard to charge control. A constant voltage charged to a temperature-biased voltage, using up to an 8-voltage limit was used for the evaluation. Graphs show severe discharge voltage degradation with cycling and periodic capacity discharge; voltage extremes for cells with and without periodic capacity discharges; voltage extremes for cells with high rate discharge; voltage-temperature levels used for charge control; end of charge current and discharge voltage for 5 percent DOD cycling; cell capacity following 5 percent DOD cycling; and the end of discharge voltage and typical charge current profiles for the 20 percent DOD cycling.

Gross, S.↗

Analytical predictions of selenide RTG power degradation

A mathematical model for the performance and degradation analysis of an RTG using the newly developed selenide thermoelectric materials has been developed at JPL. The computerized model is quite comprehensive and enables the accurate detailing of the electrical and thermal effects that take place within the thermocouple under any desired set of operation conditions, including heat input, ambient temperature and load conditions. The paper discusses the logic flow of the computer model and presents the time and temperature dependent results for various degradation mechanisms and rates as they have been established to date.

Noon, E. L.↗

Measurement requirements and techniques for degradation studies and lifetime prediction testing of photovoltaic modules

Tests of weathering and aging behavior are being developed to characterize the degradation and predict the lifetimes of low-cost photovoltaic arrays. Environmental factors which affect array performance include UV radiation, thermal energy, water, oxygen (generally involved in synergistic effects with UV radiation or high temperatures), physical stress, pollutants (oxides of nitrogen, sulfur dioxide and ozone), abrasives and dirt. A survey of photovoltaic array testing has shown the need to establish quantitative correlations between certain measurable properties (carbonyl formation, glass transition temperature, and molecular weight change) and modes of degradation and failure.

Noel, G. T.↗

Performance degradation mechanisms and modes in terrestrial photovoltaic arrays and technology for their diagnosis

Accelerated life-prediction test methodologies have been developed for the validation of a 20-year service life for low-cost photovoltaic arrays. Array failure modes, relevant materials property changes, and primary degradation mechanisms are discussed as a prerequisite to identifying suitable measurement techniques and instruments. Measurements must provide sufficient confidence to permit selection among alternative designs and materials and to stimulate widespread deployment of such arrays. Furthermore, the diversity of candidate materials and designs, and the variety of potential environmental stress combinations, degradation mechanisms and failure modes require that combinations of measurement techniques be identified which are suitable for the characterization of various encapsulation system-cell structure-environment combinations.

Noel, G. T.↗