Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “crosslink”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 217 records · Page 12

Potential seal candidates for high-energy propellants

Five potential seal candidates (linear Tefzel, linear Halar, crosslinked Halar, Viton ECD-006, and phosphazine fluoroelastomer) were evaluated for the orbital maneuvering system of the space shuttle. Since this system employs nitrogen tetroxide (N2O4) and monomethyl hydrazine (MMH) as hypergolic propellants, the seal candidates were selected on the basis of projected chemical resistance as well as rheological behavior. Chemical resistance to these high-energy fuels was determined via conventional isothermal and thermal cycling immersion tests. Rheological measurements, however, were performed on O-rings molded from the subject seal candidates. Properties determined, such as cyclic work and hysteresis, stress relaxation, and indicated modulus, therefore, relate to the O-ring seals themselves.

Merz, P. L.↗

Polymeric foams stable at high temperatures

Crosslinked poly(N-arylenebenzimidazoles) are stable up to 370 C. Polymers are made by mixing appropriate stoichiometric amounts of tetramine and aromatic dicarboxylic acid anhydride with phenol or alkyl-substituted phenol.

Riccitiello, S. R.↗

Isomer effects on polyimide properties

Polyimide polymers which are thermally stable and processable are developed. The addition of alkyl substituents to an aromatic ring in the polymer backbone is examined along with polyimide precursor amines containing functional groups that allow for post-cure crosslinking. The synthesis of key monomers is reported, including 2,4,6-tris (m-aminobenzyl) 1,3,5-trimethyl benzene and 2,4,6-tris (p-aminobenzyl) 1,3,5-trimethyl benzene. The preparation of a key monomer, 2,5,3-triamino benzophenone, is reported.

Stump, B. L.↗

Development of anion-selective membranes

Methods were studied of preparing anion-exchange membranes that would have low resistance, high selectivity, and physical and chemical stability when used in acidic media in a redox energy storage system. Of the twelve systems selected for study, only the system that was based on crosslinked poly-4-vinylpyridinium chloride produced physically strong membranes when equilibrated in l M HCl. The resistivity of the best membrane was 12 ohm-cm, and the transference number for chloride ions was 0.81.

Lacey, R. E.↗

Development of polyphenylquinoxaline graphite composites

Six polyphenylquinoxalines (PPQ) containing pendant cyano (CN) groups were synthesized. The polymers were characterized in terms of inherent viscosity, glass transition temperature, softening temperature and weight loss due to aging in air at 316 C (600 F). The potential for crosslinking PPQs by trimerization of pendant CN groups was investigated. A polymer derived from 1 mole 3,3,4,4 -tetraaminobenzophenone, .2 mole p-bis(p -cyanophenoxyphenylglyoxalyl)benzene and .8 mole p-bis(phenylglyoxalyl)benzene was selected for more extensive characterization in HM-S graphite fiber-reinforced composites. Mechanical properties were determined using composites made from HM-S fiber and polymer and composites made from HM-S fiber, polymer and a potential CN group trimerization catalyst. Composite mechanical properties, inter-laminar shear strength and flexure properties, were determined over the temperature range of +21 C to 316 C.

Shdo, J. D.↗

Thermal analysis of PMR-polyimides by dielectrometry

A preliminary study was conducted to determine the dielectric properties of glass fabric reinforced composites as influenced by the reactions occurring during the preparation of crosslinked polyimides by the PMR process. The variables studied included: formulated molecular weight, staging temperature and time; rate of temperature increase to cure temperature; and cure temperature and time. The changes of capacitance and, particularly, of dissipation factor were found to be strongly dependent on each of the variables studied.

Gluyas, R. E.↗

A description of the mechanical behavior of composite solid propellants based on molecular theory

Both the investigation and the representation of the stress-strain response (including rupture) of gum and filled elastomers can be based on a simple functional statement. Internally consistent experiments are used to sort out the effects of time, temperature, strain and crosslink density on gum rubbers. All effects are readily correlated and shown to be essentially independent of the elastomer when considered in terms of non-dimensionalized stress, strain and time. A semiquantitative molecular theory is developed to explain this result. The introduction of fillers modifies the response, but, guided by the framework thus provided, their effects can be readily accounted for.

Landel, R. F.↗

Syntheses and degradations of fluorinated heterocyclics

The relative stability of two ring systems, the triazine rings and 1,2,4-oxadiazoles, which offer potential crosslinks useful for curing perfluoroalkyl ether elastomers, has been investigated. Tris (perfluoro-n-heptyl)-s-triazine, the perfluoroether substituted-s-triazine, 1,4-bis/(5-perfluoro-n-heptyl)-1,2,4-oxadiazolyl/benzene, its perfluoroalkyl ether substituted analog, and 3,5-bis-(perfluoro-n-heptyl)-1,2,4-oxadiazole were synthesized and subjected to thermal and oxidative degradation at 235 and 325 C and to hydrolytic degradation at 235 C. The perfluoroalkyl ether substituted triazine and 3,5-bis(perfluoro-n-heptyl)-1,2,4-oxadiazole were found to be stable under all conditions investigated.

Paciorek, K. L.↗

Variability of ultimate properties of elastomers

The measurement of the ultimate properties of elastomers is characterized by variability in the data. For example, when a sufficient number of specimens is tested, distributions in the values of the stress-at-break, strain-at-break, and time-to-break are commonly obtained. It is pointed out that such variability can be rationalized on the basis of variations in both the degree of crosslinking and in the size of naturally occurring flows present in the elastomer.

Fedors, R. F.↗

Study of improved resins for advanced supersonic technology composites. Part 1: Heteroaromatic polymers containing ether groups. Part 2: Curing chemistry of aromatic polymers and composite studies

Fourteen ether-containing, aromatic dianhydrides have been synthesized from N-phenyl-3 or 4-nitrophthalimide and various bisphenols. The process involves nucleophilic displacement of activated nitro groups with bisphenolate ions. Ether-containing dianhydrides were indefinitely stable in the presence of atmospheric moisture. One-step, high temperature solution polymerization of the ether-containing dianhydrides with m-phenylene diamine, 4,4'-oxydianiline and 1, 3-bis(4-aminophenoxy)benzene afforded 42 polyetherimides. The polyetherimides were all soluble in m-cresol except two which were found to be crystalline. The glass transition temperatures of the polyetherimides ranged from 178 to 277 C. Soluble polybenzimidazopyrrolones containing ether groups were also prepared from the same ether-containing dianhydrides and aromatic tetraamines by one-step solution polymerization. Using low molecular weight polyetherimides, various thermoset resin systems were developed and tested as matrices for fiber-reinforced composites. The curing chemistry involving reaction of the phthalonitrile group and the o-diaminophenyl group was found to be generally applicable to crosslinking various aromatic polymers other than polyimides.

Takekoshi, T.↗

Oil and fat absorbing polymers

A method is described for forming a solid network polymer having a minimal amount of crosslinking for use in absorbing fats and oils. The polymer remains solid at a swelling ratio in oil or fat of at least ten and provides an oil absorption greater than 900 weight percent.

Marsh, H. E., Jr.↗

Cross Linking and Degradation Mechanisms in Model Sealant Candidates

Model compounds were investigated as to which type of heterocyclic ring is the most advantageous for curing sealants based on perfluoroalkylether chains. The relative thermal, thermal oxidative, hydrolytic, and fuel stability of potential crosslinks were determined. Specifically substituted materials were synthesized and evaluation of their stabilities in air, inert atmosphere, water, and Jet-A fuel at 235 and 325 C was made. Three heterocyclic ring systems were considered, namely, triazine, 1,2,4- and 1,3,4-oxadiazoles.

Paciorek, K. L.↗

Analysis of the thermal reaction products of para polyphenylene by combined gas chromatography-mass spectrometry

Analysis of the volatiles and sublimate produced when para-polyphenylene is pyrolyzed to constant weight under vacuum in the temperature range from 380 to 1000 C indicates that the polymer undergoes thermal degradation in two stages. The first stage involved dehydrohalogenation, which is essentially a curing reaction that produces crosslinking between polyphenylene chains resulting from the loss of chlorine from the polymer in the form of hydrogen chloride. The second stage of the thermal degradation is dehydrogenation because hydrogen is the major volatile species. Increasing amounts of polycyclic aromatic hydrocarbons (phenanthrene and 9, 10 benzphenanthrene) in the sublimate, concomitant with increasing C/H ratios of the polymeric residue with pyrolysis temperature, is consistent with the buildup of polynuclear structures in the polymer matrix.

Fewell, L. L.↗

Accelerated heat-aging studies on fluororubber in various media

Heat-aging studies were conducted on fluororubber (copolymers of vinylidene fluoride and perfluoropropylene) using N,N-dicinnamylidene-1,6-hexanediamine, a Schiff's base of 1,6-hexanediamine, and MgO as acid acceptor. The principal technique employed was chemical stress relaxation for determining network changes brought about in the heat-aged fluororubber. This technique was backed up by swelling measurements, gel permeation chromatography, and IR spectroscopy. Stress relaxation curves are plotted for a wide range of variation in parameters (time, crosslinking density, state of curing, temperature, intermittent and continuous relaxation).

Kalfayan, S. H.↗

Reduced variable technique for predicting grain behavior

The use of reduced variables to account for the time-temperature dependence of the relaxation modulus is a standard and universally adopted technique in the stress analysis of solid propellant grains. Recent work has suggested that the reduced variable technique can also be used to account for the dependence of the relaxation modulus on the crosslink density of an elastomer system. By combining variables, it is now possible to determine the relaxation modulus as a function of both mechanical and chemical parameters over a long period of time. The problems involved, the pitfalls to be avoided, and suggested techniques to be used in acquiring data are discussed.

Lewis, G. W.↗

Development and evaluation of elastomeric materials for geothermal applications

A material for a casing packer for service for 24 hours in a geothermal environment was developed by synthesis of new elastomers and formulation of available materials. Formulation included use of commercial elastomer gumstocks and also crosslinking of plastic (high Tg) materials. Fibrous reinforcement of fluorocarbon rubbers was emphasized. Organic fiber reinforcement did not increase hot properties significantly. Glass fiber reinforcement gave significant increase in tensile properties. Elongation was reduced, and the glass-reinforced composition examined so far did not hold up well in the geothermal environment. Colloidal asbestos fibers were also investigated. A few experiments with polyphenyl ether gave material with low tensile and high compression set. Available high styrene SBR compositions were studied. Work to date suggests that new synthetic polymers will be required for service in geothermal environments.

Mueller, W. A.↗

On the form of the strain energy function for a family of SBR materials

Styrene-butadiene materials with varying crosslink densities are analyzed through use of a strain energy function of the type introduced by Valanis and Landel (1967). A form of the strain energy function derived from strip biaxial tests proves to be accurate when checked against uniaxial and other biaxial test results.

Arenz, R. J.↗

Heat- and chemical-resistant oxdiazole elastomers

Heat and chemical resistant polymers with triazine crosslinks are prepared by thermal condensation reactions to form 1,2,4-oxdiazole linkages. They are compounded with variety of fillers, extenders, and modifiers for numerous applications in which stability, impermiability to liquids and gases, good plasticity, and elasticity or rigidity are important.

Rosser, R. W.↗