High-temperature oxidation of a rapidly solidified amorphous Ta-Ir alloy
The oxidation products formed at 500 and 700 C on an amorphous Ta-44.5 at. pct Ir alloy in an Ar-0.1 percent O2 gas mixture were characterized using SEM, XRD, EPMA, TEM, STEM, AES, and XPS. Initially, a thin (3-4 nm) layer of Ta2O5 formed at the surface of the alloy. Continued growth of the Ta2O5, which occurred very rapidly, involved diffusion of oxygen anions from the Ta2O5/gas interface to the alloy/Ta2O5 interface, where tantalum was selectively oxidized. Because the oxide grew more quickly than iridium could diffuse back into the alloy, the iridium coalesced into platelets of crystalline iridium-rich alloy that were oriented approximately parallel to the oxide/alloy interface, and which became embedded in a matrix of Ta2O5. The unoxidized core remained in the glassy state. The oxidation process and/or the dissolution of oxygen into the unoxidized alloy caused the alloy to become embrittled.