At least 217 records · Page 12

Metallic Powder Core Tubular Wire (PCTW) Development for Additive Manufacturing

NASA Langley Research Center (LaRC) in Hampton, VA, and the Center for Welding, Joining, and Coating Research (CWJCR) in the Department of Metallurgical and Materials Engineering at the Colorado School of Mines (CSM) in Golden, CO, have collaborated for nearly fifteen years to develop metallic powder core tubular wire (PCTW) feedstock for additive manufacturing (AM) using electron beam deposition. The motivation for this development was to offset dealloying observed during deposition of titanium and aluminum alloy solid wire feedstock in the LaRC electron beam freeform fabrication (EBF3) system and to explore novel alloy compositions by tailoring the powder fill. EBF3 is a fusion-based AM process that is performed under vacuum and is consequently prone to vaporization loss of low vapor pressure alloying elements. Research spanning four graduate student research projects succeeded in developing the basic methodology to fabricate PCTW, the mass balance equations used to define the powder fill, microstructure control through particulate inoculation, and the feasibility of producing metal matrix composite materials. Metallic PCTW is comprised of a thin foil sheath wrapped around a powder blend. Fabrication of PCTW at CSM was accomplished using a tubular wire mill system to first bend a flat strip into a u-shaped cross section, deposit a powder fill, create a lap joint to seal the wire, and draw to final diameter. Powder management systems were developed to ensure uniform mixing of powder constituents and identify feed rates for optimum fill ratios. Processing parameters were successfully developed for titanium and aluminum alloy sheaths to account for material work hardening during drawing. Mass balance equations were developed to account for compositional contributions of the sheath and powder fill. PCTW composition can be adjusted through selection of the sheath or powder materials. PCTWs were successfully developed to offset Al loss in deposits of Ti-6-4 and Mg loss in Al 6061, resulting in deposits that were within the composition limits for each material. Ti-6-4 deposits were fabricated using PCTW comprised of commercially pure (CP) titanium sheath and a fill of pre-alloyed Ti-6-4 powder with additions of elemental Al and V powders. Additions of both elements were required to account for the CP Ti from the sheath, and Al was further enhanced to offset documented losses in EBF3 deposits. For Al 6061 deposits, composition was modulated through the choice of sheath material. The PCTW was made using an Al 5052 sheath to supplement Mg content and a fill composition of pre-alloyed 6061 powder with additions of Si and Cu.The slower solidification rate of the EBF3 process compared with laser powder bed fusion processes can lead to coarse-grained microstructures and mechanical property anisotropy. EBF3deposits of Ti-6-4 exhibited large epitaxially grown β grains, which result in degraded mechanical properties in the deposition direction. Microstructure refinement was achieved through a combination of electron beam modulation and the use of a PCTW designed for Ti-6-4 deposits and modified by the addition of powder made from Fe and B. Resulting deposits exhibited reductions in β grain size, α phase colony intercept length and lath width, and an increased volume fraction of β phase. The mechanism of microstructure refinement was related to precipitation of boride particles. Hardness testing confirmed that mechanical property anisotropy was reduced and an overall increase in hardness was achieved.Metal matrix composite (MMC) materials offer strength and stiffness benefits over unreinforced materials. Two methods were investigated using PCTW technology for producing Al 6061 basedMMC materials; the direct addition of SiC reinforcing particles and the in-situ generation of reinforcements through reaction synthesis of precursor powders. Al 6061 based MMCs reinforced with SiC exhibited particle clustering and formation of aluminum carbides during deposition. The application of a Ni coating to the SiC particles prior to incorporation into the powder fill eliminated aluminum carbide formation and aided particle distribution during deposition. Modulation of beam focus and power further reduced aluminum carbide formation and aided particle distribution. In reaction synthesis, precursor additions undergo an exothermic reaction during deposition to form new ceramic products, generally of finer scale than the initial precursor components. The product phases provide reinforcement in the MMC and act as nucleation sites during solidification, resulting in grain refinement, improved mechanical properties, and reduced susceptibility to solidification cracking. Higher tensile strength and stiffness were demonstrated in Al 6061 based MMCs with 2 vol% reinforcement. These combined research efforts demonstrate the potential of PCTW technology for customizing of alloy composition and achieving microstructure control. A manufacturing process for titanium- and aluminum-based PCTWs was developed based on iterative design, theoretical calculations, and empirical data. PCTW technology successfully mitigated Al loss from Ti-6-4 and Mg loss in Al 6061, resulted in grain refinement in Ti-6-4, and demonstrated fabrication of Al based MMCs

Marcia S Domack↗

Surface film effects on drop tube undercooling studies

The effects of various gaseous atmospheric constituents on drop-tube solidified samples of elemental metals were examined from a microstructural standpoint. All specimens were prepared from the purest available elements, so effects of impurities should not account for the observed effects. The drop-tube gas has a definite effect on the sample microstructure. Most dramatically, the sample cooling rate is effected. Some samples receive sufficient cooling to solidify in free fall while others do not, splating at the end of the drop tube in the sample catcher. Gases are selectively absorbed into the sample. Upon solidification gas can become less soluble and as a result forms voids within the sample. The general oxidation/reduction characteristics of the gas also affect sample microstructures. In general, under the more favorable experimental conditions including reducing atmospheric conditions and superheatings, examination of sample microstructures indicates that nucleation has been suppressed. This is indicated by underlying uniform dendrite spacings throughout the sample and with a single dendrite orientation through most of the sample. The samples were annealed yielding a few large grains and single or bi-crystal samples were commonly formed. This was especially true of samples that were inadvertently greatly superheated. This is in contrast with results from a previous study in which surface oxides were stable and contained numerous sites of nucleation. The number of nucleation events depends upon the surface state of the specimen as determined by the atmosphere and is consistent with theoretical expectations based upon the thermodynamic stability of surface oxide films. Oxide-free specimens are characterized by shiny surfaces, with no observable features under the scanning electron microscope at 5000X.

Ethridge, E. C.↗

M551 metals melting experiment

The Metals Melting Skylab Experiment consisted of selectively melting, in sequence, three rotating discs made of aluminum alloy, stainless steel, and tantalum alloy. For comparison, three other discs of the same three materials were similarly melted or welded on the ground. The power source of the melting was an electron beam unit. Results are presented which support the concept that the major difference between ground base and Skylab samples (i.e., large elongated grains in ground base samples versus nearly equiaxed and equal sized grains in Skylab samples) can be explained on the basis of constitutional supercooling, and not on the basis of surface phenomena. Microstructural observations on the weld samples and present explanations for some of these observations are examined. In particular, ripples and their implications to weld solidification were studied. Evidence of pronounced copper segregation in the Skylab A1 weld samples, and the tantalum samples studied, indicates a weld microhardness (and hence strength) that is uniformly higher than the ground base results, which is in agreement with previous predictions. Photographs are shown of the microstructure of the various alloys.

Li, C. H.↗

Bulk undercooling

Bulk undercooling methods and procedures will first be reviewed. Measurement of various parameters which are necessary to understand the solidification mechanism during and after recalescence will be discussed. During recalescence of levitated, glass-encased large droplets (5 to 8 mm diam) high speed temperature sensing devices coupled with a rapid response oscilloscope are now being used at MIT to measure local thermal behavior in hypoeutectic and eutectic binary Ni-Sn alloys. Dendrite tip velocities were measured by various investigators using thermal sensors or high speed cinematography. The confirmation of the validity of solidification models of bulk-undercooled melts is made difficult by the fineness of the final microstructure, the ultra-rapid evolution of the solidifying system which makes measurements very awkward, and the continuous modification of the microstructure which formed during recalescence because of precipitation, remelting and rapid coarsening.

Kattamis, T. Z.↗

The effectiveness of Coriolis dampening of convection during aircraft high-g arcs

Directional solidification data for metal samples in KC-135 parabolic maneuvers are examined to determine evidence for Coriolis dampening of convection. Microstructural and materials properties data are examined for iron carbon, immiscible, and superalloy systems. By comparison of low-g data and high-g data with those of one-g control samples, it is determined that there is no evidence that Coriolis dampening of convective flow is effective during the 1.8 g KC-135 high-g maneuvers. A first approximation model for the high-g arc is proposed. The model yields a centrifugal radius of 20,480 ft and an angular speed of 0.397 RPM. Comparison to centrifugal solidification experiments (for an equal acceleration) where Coriolis melt growth stabilization is significant indicates that the KC-135 high-g arc is less effective in dampening convection by a factor of 100. This large difference in Coriolis dampening of convection might be taken advantage of for experiments where separation of centrifugal acceeration and Coriolis acceleration is desirable.

Curreri, Peter A.↗

Solidification of undercooled metals

The present investigation is concerned with the subject of undercooling (i.e., supercooling) in the case of metal alloys, taking into account the effects of undercooling on microstructure and microsegregation in alloys which solidify in a crystalline manner. Techniques for obtaining a large degree of undercooling are discussed. These techniques make it possible to eliminate heterogeneous nucleants from the melt and to remove container nucleation effects. The nucleation behavior of small metal droplets is considered along with the formation of a dispersion of fine droplets in a suitable inert medium, the mixing of fine metal powders with glass powder, and the levitation melting technique. Attention is given to solidification with rapid interface velocity, aspects of dendritic morphology, and thermal measurements during solidification of undercooled droplets.

Flemings, M. C.↗

Structure-property relationships in eutectic composites

The preparation of a composite material of eutectic composition directly from the molten state is investigated. The manufacture of eutectic composites by unidirectional solidification is reviewed, and it is shown how two-phase composite structures of given relative volume fraction can be produced with a range of particle sizes. Crystallographic relationships and the thermal stability of interfaces in controlled eutectic structures are examined, the mechanical behavior of aligned eutectic microstructures is discussed, and characteristics of eutectic composites having mechanical properties of engineering significance are evaluated. Specific properties of the Ni-Nb eutectic alloy are reviewed to demonstrate the effect of structure control (through directional solidification) on the mechanical response of a eutectic composite. It is noted that unidirectionally solidified eutectic composites possess highly aligned and thermally stable microstructures and also exhibit excellent combinations of strength and ductility to very high temperature levels.

Hertzberg, R. W.↗

Minimizing Segregation during the Controlled Directional Solidification of Dendric Alloys

Gravity-driven convection induced in the liquid by density gradients of temperature or composition disrupts uniform dendritic growth during controlled directional solidification and promotes severe macrosegregation. The solute-rich region about the dendrite tip appears to play a pivotal role in channel initiation. Allen and Hunt referred to this region as an "initial transient" or dynamic region constituting steep concentration gradients. Experimental investigation also point to the role the tip region plays in developing microstructure. Hellawell and co-workers showed that flow-through dendritic channels could be effectively disrupted, and segregation minimized, during the gradient freezing of bulk castings by rotating the melt through a slight angle with respect to Earth's gravity vector. Adapting this principle to controlled directional solidification, it has been shown" that segregation in dendritic alloys can be minimized, and properties improved, by processing the sample near horizontal in conjunction with a slow axial rotation of the crucible. It is postulated that the observed microstructural uniformity arises by maintaining the developing solute field about the dendrite tip. Solute rejected during vertical directional solidification will rise or sink parallel to the primary dendrite arms during axial rotation setting the stage for accumulation, instabilities, and segregation. In contrast, during horizontal growth, the rejected solute will sink or rise perpendicular to the primary dendrite. Now, in the presence of a slight axial rotation, solute that was initially sinking (or rising) will find itself above (or below) its parent dendrite, i.e., still about the tip region. The following is intended to experimentally demonstrate the viability of this concept in coordination with a model that gives predictive insight regarding solute distribution about growing dendrites. Alloys based on the lead-tin eutectic system were used in this study. The system is well characterized, the constituent metals are available in a very pure form, and the thermophysical properties are well known. During solidification of hypoeutectic alloys, e.g., 55 wt pct Pb, the primary dendrites reject the less dense tin, and for the hypereutectic alloys, e.g., 75 wt pct Sn, the primary dendrites reject denser lead. Alloys were prepared by melting appropriate amounts of lead and tin in a glass crucible after which the homogeneous liquid was sucked directly into 5-mm i.d. glass tubes. The sample tube, containing approximately 30 cm of alloy, was then mechanically driven into the directional solidification furnace assembly and positioned such that approx. 20 cm of the sample was remelted. Subsequently, directional solidification was initiated by withdrawing the sample through a water-cooled jacket at a constant growth velocity of 2 ,microns/s. After 5 to 6 cm of growth, the sample was quickly removed from the furnace and quenched in a water bath to preserve the solid-liquid interface. Samples were directionally solidified vertically upward, nearly horizontally, and some in conjunction with an applied axial rotation of the crucible. Temperature gradients at the solid-liquid interface were measured with an in-siru K-type thermocouple. Solidified samples were cut perpendicular and parallel to the growth direction and conventionally prepared for microscopic examination.

Grugel, Richard N.↗

Experimental results and numerical modeling of solidification during aircraft high-g arcs

The question of how the Coriolis and gravity gradient forces during high-gravity maneuvers compare to that for common centrifuges is addressed. Microstructural examination of samples solidified during high-gravity arcs reveals no evidence of convection dampening. As a first approximation, the high-gravity arc is modeled as a centrifuge with a radius of 20,480 ft and angular speed of 0.318 rpm. Scaling analysis indicates that the Coriolis and gravity gradient expected on the aircraft high gravity arc are less than that for the centrifuges by a factor of 100. Detailed Navier-Stokes analysis of the fluid flow and thermal fields during solidification of aluminum and Cd-Te during KC-135 high gravity show that convective flows of about 1 mm/s are induced. The thermal field is only slightly modified by the convection. Coriolis and gravity gradient during solidification in KC-135 high-gravity arcs, even at accelerations that have been shown to produce significant convective flow dampening in the centrifuge systems, are found to have no significant influence on the melt thermal and flowfields.

Curreri, P. A.↗

Investigation of solidification in zero-gravity environment: M553 sphere forming experiment. Nickel-silver alloy evaluation

The processing of nickel-silver alloy specimens in space is discussed. Four specimens were melted only partially, while a fifth was melted completely and assumed after solidification a perfectly spherical shape. Growth of the solid was epitaxial on the unmelted material or on the retaining sting and occurred without undercooling. Solidification was dendritic in all cases with nonequilibrium silver particles forming monotectically between dendrite arms. Substantial loss of silver by evaporation took place. Evaporation of the silver within internal gas cavities on the melt was followed by surface condensation after completion of solidification and cooling, leading to a silver-rich lining in these cavities. The material gave no microstructural evidence of any reduction in liquid convection.

Kattamis, T. Z.↗

The effect of thermal cycling to 1100 degree C on the alpha (Mo) phase in directionally solidified gamma/gamma prime-alpha alloys

In gamma/gamma prime - alpha eutectic alloys (Ni-Mo-Al), the resistance of the alpha phase to morphological changes during thermal cycling was found to be dependent on the structure formed during directional solidification. Fine, smooth alpha fibers survived up to 1000 five minute cycles to 1100 C with minor microstructural contour changes, while coarser and irregularly shaped alpha fibers tended to spheroidize. A mechanism to explain this phenomenon is proposed. It is suggested that on heating to 1100 C, the alpha phase is likely to undergo morphological changes, until differential thermal expansion creates a stress free interface between the alpha phase and the gamma/gamma prime matrix.

Harf, F. H.↗

Interface Pattern Selection in Directional Solidification

The central focus of this research is to establish key scientific concepts that govern the selection of cellular and dendritic patterns during the directional solidification of alloys. Ground-based studies have established that the conditions under which cellular and dendritic microstructures form are precisely where convection effects are dominant in bulk samples. Thus, experimental data can not be obtained terrestrially under pure diffusive regime. Furthermore, reliable theoretical models are not yet possible which can quantitatively incorporate fluid flow in the pattern selection criterion. Consequently, microgravity experiments on cellular and dendritic growth are designed to obtain benchmark data under diffusive growth conditions that can be quantitatively analyzed and compared with the rigorous theoretical model to establish the fundamental principles that govern the selection of specific microstructure and its length scales. In the cellular structure, different cells in an array are strongly coupled so that the cellular pattern evolution is controlled by complex interactions between thermal diffusion, solute diffusion and interface effects. These interactions give infinity of solutions, and the system selects only a narrow band of solutions. The aim of this investigation is to obtain benchmark data and develop a rigorous theoretical model that will allow us to quantitatively establish the physics of this selection process.

Trivedi, Rohit↗

Influence of convection on microstructure

In eutectic growth, as the solid phases grow they reject atoms to the liquid. This results in a variation of melt composition along the solid/liquid interface. In the past, mass transfer in eutectic solidification, in the absence of convection, was considered to be governed only by the diffusion induced by compositional gradients. However, mass transfer can also be generated by a temperature gradient. This is called thermotransport, thermomigration, thermal diffusion or the Soret effect. A theoretical model of the influence of the Soret effect on the growth of eutectic alloys is presented. A differential equation describing the compositional field near the interface during unidirectional solidification of a binary eutectic alloy was formulated by including the contributions of both compositional and thermal gradients in the liquid. A steady-state solution of the differential equation was obtained by applying appropriate boundary conditions and accounting for heat flow in the melt. Following that, the average interfacial composition was converted to a variation of undercooling at the interface, and consequently to microstructural parameters. The results obtained show that thermotransport can, under certain circumstances, be a parameter of paramount importance.

Wilcox, William R.↗

Macrosegregation Caused by Convection Associated with Directional Solidification through Cross-Section Change

Al-7 wt% Si and Pb-6 wt% Sb alloy samples were directionally solidified (DS), with liquid above and solid below and gravity pointing down, in cylindrical graphite crucibles through an abrupt cross-section change. Fraction eutectic distribution in the microstructure, primary dendrite spacing and primary dendrite trunk diameters have been measured in the DS samples in the vicinity of section change in order to examine the effect of convection associated with the combined influence of thermosolutal factors and solidification shrinkage. It is observed that convection not only produces extensive radial and axial macrosegregation near cross-section change, it also affects the dendritic array morphology. Primary dendrite spacing and primary dendrite trunk diameter, both, are influenced by this convection. In addition to the experimental results, preliminary results from a numerical model which includes solidification shrinkage and thermosolutal convection in the mushy zone in its analysis will also be presented

Ghods, M.↗

Processing eutectics in space

Experimental work is reported which was directed toward obtaining interface shape control while a numerical thermal analysis program was being made operational. An experimental system was developed in which the solid-liquid interface in a directionally solidified aluminum-nickel eutectic could be made either concave to the melt or convex to the melt. This experimental system provides control over the solid-liquid interface shape and can be used to study the effect of such control on the microstructure. The SINDA thermal analysis program, obtained from Marshall Space Flight Center, was used to evaluate experimental directional solidification systems for the aluminum-nickel and the aluminum-copper eutectics. This program was applied to a three-dimensional ingot, and was used to calculate the thermal profiles in axisymmetric heat flow. The results show that solid-liquid interface shape control can be attained with physically realizable thermal configurations and the magnitudes of the required thermal inputs were indicated.

Douglas, F. C.↗

Cast Iron With High Carbon Content

Method proposed for solidifying high-carbon cast iron without carbon particles segregating at upper surface. Solidification carried out in low gravity, for example on airplane flying free-fall parabolic trajectory. Many different microstructures obtained by proposed technique, and percentage by weight of carbon retained in melt much higher than at present.

Curreri, P. A.↗

A study of reduced chromium content in a nickel-base superalloy via element substitution and rapid solidification processing

A study of reduced chromium content in a nickel base superalloy via element substitution and rapid solidification processing was performed. The two elements used as partial substitutes for chromium were Si and Zr. The microstructure of conventionally solidified materials was characterized using microscopy techniques. These alloys were rapidly solidified using the chill block melt spinning technique and the rapidly solidified microstructures were characterized using electron microscopy. The spinning technique and the rapidly solidified microstructures was assessed following heat treatments at 1033 and 1272 K. Rapidly solidified material of three alloys was reduced to particulate form and consolidated using hot isostatic pressing (HIP). The consolidated materials were also characterized using microscopy techniques. In order to evaluate the relative strengths of the consolidated alloys, compression tests were performed at room temperature and 1033 K on samples of as-HIPed and HIPed plus solution treated material. Yield strength, porosity, and oxidation resistance characteristics are given and compared.

Powers, William O.↗

Influence of convection of spiral structures in lead-tin eutectic

Convection was generated during directional solidification by the accelerated crucible rotation technique (spin up/spin down). This stirring increased the rotation rate of the microstructure and reduced the length solidifying cooperatively, but had no influence on the lamellar spacing.

Popov, Dimitar↗