Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “SLAGS”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 217 records · Page 12

The evolution of strength and crystalline phases for alkali-activated ground blast furnace slag and fly ash-based geopolymers

The increase in strength and evolution of crystalline phases in inorganic polymer cement, made by the alkali activation of slag, Class C and Class F fly ashes, was followed using compressive strength test and synchrotron X-ray diffraction. In order to increase the crystallinity of the product the reactions were carried out at 80 deg. C. We found that hydrotalcite formed in both the alkali-activated slag cements and the fly ash-based geopolymers. Hydroxycancrinite, one member of the ABC-6 family of zeolites, was found only in the fly ash geopolymers. Assuming that the predominantly amorphous geopolymer formed under ambient conditions relates to the crystalline phases found when the mixture is cured at high temperature, we propose that the structure of this zeolitic precursor formed in Na-based high alkaline environment can be regarded as a disordered form of the basic building unit of the ABC-6 group of zeolites which includes poly-types such as hydroxycancrinite, hydroxysodalite and chabazite-Na.

36 MATERIALS SCIENCE↗

Density and water content of nanoscale solid C-S-H formed in alkali-activated slag (AAS) paste and implications for chemical shrinkage

Alkali-activated slag (AAS) paste was analyzed using small-angle neutron scattering (SANS). The scattering response indicates that the microstructure consists of a uniform matrix of hydration product with a high surface area studded with unhydrated cores of slag particles. In contrast with portland cement paste, no surface fractal scattering regime was detected, and elevated temperature curing (at 60 Degree-Sign C) had no detectable effect on the microstructure at any length scale studied. The specific surface area of the AAS pastes is about 25% higher than that of a portland cement paste cured under the same conditions. The composition and mass density of the nanoscale solid C-S-H phase formed in the AAS paste was determined using a previously developed neutron scattering method, in conjunction with a hydration model. The result ((CaO){sub 0.99}-SiO{sub 2}-(Al{sub 2}O{sub 3}){sub 0.06}-(H{sub 2}O){sub 0.97}, d = (2.73 {+-} 0.02) g/cm{sup 3}) is significantly lower in calcium and in water as compared to portland cement or pure tricalcium silicate paste. These values were used to calculate the chemical shrinkage that would result from complete hydration of the AAS paste. The result, (12.2 {+-} 1.5) cm{sup 3} of volumetric shrinkage per 100 g of unhydrated cement, is about twice the amount of chemical shrinkage exhibited by normal cement pastes.

36 MATERIALS SCIENCE↗

Influence of the composition of cement kiln dust on its interaction with fly ash and slag

Cement kiln dust (CKD), a by-product of the cement industry, contains significant amounts of alkali, free lime, chloride and sulfate. Wide variation reported in the chemical composition of CKDs limits their potential application as a sustainable binder component in concrete. In the current study, the performance of two different CKDs as components in a novel binder is evaluated. Several binders are developed by blending CKDs with fly ash or slag. Binders with 70% CKD were prepared at a water-to-binder ratio of 0.4, and heat-cured at 75 °C to accelerate the strength development. The hydration progress was monitored using X-ray diffraction, and morphological examination was performed using scanning electron microscopy (SEM) and transmission electron microscopy (TEM). Ettringite and calcium aluminosilicate hydrate (C-A-S-H) were identified as the main hydration products in the hardened binder system. Strength development of CKD-based binder was found to be significantly influenced by its free lime and sulfate contents. -- Highlights: •Interaction of cement kiln dust with fly ash and slag was explored. •CKD with higher free lime and sulfate content increased the strength of binder. •C-S-H like reaction gel with fibrillar morphology is observed in CKD-based binders.

36 MATERIALS SCIENCE↗

Isothermal calorimetry and in-situ XRD study of the NaOH activated fly ash, metakaolin and slag

Much is unknown about the reaction processes responsible for the formation and polycondensation of geopolymers and other alkali activated materials. In this work, isothermal calorimeter and in-situ XRD were adopted to study the heat and mineral evolution of NaOH activated fly ash, metakaolin and ground granulated blast furnace slag. Both activator concentration and temperature have profound influences on duration of exothermal geopolymerization peaks. NaOH activated fly ash is more temperature dependable, with much higher activation energy than metakaolin and slag. The dissolution of source precursor is rapid and the formation of new phases can be detected by the end of the initial dissolution period. The in-situ XRD measurement together with the PONKCS analysis method promotes quantitative estimation of amorphous evolution during alkali activation.

36 MATERIALS SCIENCE↗

Moisture transport and sorption in cement based materials containing slag or silica fume

This paper presents the moisture dependency of moisture transport and moisture fixation in mortars with OPC, slag and silica fume. Water vapor desorption isotherms were measured with gravimetric methods and the moisture dependency of moisture transport was investigated with cup-tests. The results show an ongoing evolution of water vapor desorption isotherms from eight months to four years. The evolution is more pronounced for mortars containing slag. The results also show that there is a significant difference in moisture dependency of the moisture transport properties above 70% relative humidity; some mortars exhibit a clear moisture dependency in moisture transport whereas others do not. At a relative humidity below 70%, the water to binder ratio is more decisive for moisture transport than the type of binder. These results are of value for service-life models, where they represent important input data, and for understanding the evolution of the microstructure at later ages.

36 MATERIALS SCIENCE↗

Rheology of activated phosphorus slag with lime and alkaline salts

The present study aimed to determine the rheological behavior of activated phosphorus slag (AAPS) with a combination of Ca(OH){sub 2} and Na{sub 2}CO{sub 3} (CNC activator) or Na{sub 2}SO{sub 4} (CNS activator) compared to OPC paste. The findings showed that the rheology of AAPS pastes fit with the Herschel-Bulkley model and behaved like a shear-thinning fluid. The AAPS pastes rheology is affected by concentration and nature of activator. The shear stress in AAPS pastes was lower than OPC paste, and increased with increasing the activator concentration. In early ages, reaction products of PS/CNC pastes included calcite-type compounds with the formed gel while gypsum compounds formed in the PS/CNS pastes. This resulted in higher shear stress and lower workability for PS/CNC pastes compared to PS/CNS pastes. The formed gel due to interaction between Ca{sup 2+} ions of CNC activator and Si{sup 4+} ions of Phosphorus slag caused an increase in the shear stress for PS/CNC during the time.

36 MATERIALS SCIENCE↗

Early reactivity of sodium silicate-activated slag pastes and its impact on rheological properties

The fast loss of fluidity of sodium silicate-activated slag (SS-AAS) systems have been widely studied in the literature. In this study, the rheology of these cements has been correlated with the evolution of the reaction products formed over time. For this purpose, a combination of experimental characterization techniques, to study the pore solution composition and microstructure of SS-AAS pastes and thermodynamic calculations have been applied. The initial precipitation of ill-defined N-A-S-H and C-N-A-S-H producta leads to a fast increase of the storage modulus after 40 min of reaction. These products are formed from the reaction of the Na{sup +} ions and silicate ions of the activator with the Ca{sup 2+} and aluminate species dissolved from the slag. However, when a shear is applied, the structure breaks down and fluidity is recovered, that infers that the attractive forces between the particles are low at the early stages of hydration.

36 MATERIALS SCIENCE↗

Comparison of liquid absorption-release of superabsorbent polymers in alkali-activated slag and Portland cement systems: An NMR study combined with additional methods

In this study, {sup 1}H low-field NMR was used to compare the liquid absorption-release behaviour of superabsorbent polymers (SAPs) in Portland cement (PC) paste, NaOH-activated slag (SH-AAS) paste, and water glass-activated slag (WG-AAS) paste. The liquid absorption of SAPs in the PC paste was lower than that in the SH-AAS paste and the WG-AAS paste. The liquid release was also faster, which was mainly due to the higher Ca{sup 2+} concentration in the pore fluid of the PC system. In the AAS system, although the Ca{sup 2+} concentration in the pore fluid was low, the Na{sup +} concentration was much higher than that in the PC system due to the activator. The Ca{sup 2+} in the PC system is an important factor affecting the swelling of SAPs, while in the AAS system, the swelling limitation of SAPs is the result of the combined effects of Ca{sup 2+} and Na{sup +}, with Na{sup +} being dominant.

36 MATERIALS SCIENCE↗

Coordination environment of Si in calcium silicate hydrates, silicate minerals, and blast furnace slags: A XANES database

Understanding the silicate polymerization of calcium silicate hydrate (C-S-H) gel and its crystalline polymorphs is important in cement science. NMR can determine Si environments, but the measurement can be time-consuming and provides no spatial information. X-ray absorption near-edge structure (XANES) spectroscopy is a fast tool for probing Si coordination, possibly with spatial information. However, there lacks an understanding of Si K-edge XANES spectra of cement-related silicate phases. Here, a Si K-edge XANES spectral database of nanocrystalline C-S-H, C-S-H minerals, blast-furnace slags, and metakaolin is provided. Si K-edge of C-S-H minerals shifts to higher energies with higher polymerized Si and lower CaSi connectivity in the Si second nearest neighbor shell. Si K-edge energy shows weak correlations with Ca/Si ratio, average SiO bond length, and SiO{sub 4} distortion due to the structural complexity of silicates. The substitution of Al for Si shifts the Si K-edge of tobermorite and slags to higher energies.

36 MATERIALS SCIENCE↗

Experimental evidence for the acceleration of slag hydration in blended cements by the addition of CaCl2

Cements with high substitution rates of ground granulated blast furnace slags (GGBS) have the potential to significantly lower CO{sub 2} emissions of concrete, but their early age strength is often below those of traditional OPC cements. One way of mitigating this drawback is to use accelerating admixtures. In this study, the effect of CaCl{sub 2} additions on the hydration of blended cements was investigated by measuring compressive strength, porosity, heat release and propagation of ultrasound in blends containing 70 wt% of GGBS. The onset of formation of aluminate phases was monitored using in-situ XRD. The effect of CaCl{sub 2} on slag hydration was isolated by replacing GGBS by an inert quartz filler. Results showed that compressive strength values at one, two and seven days were increased by 50% by the CaCl{sub 2} addition. The increases in compressive strength corresponded to a reduction in pore space. GGBS hydration contributed to the heat development, structuration and compressive strength of the blended cements from 15 h. The addition of CaCl{sub 2} led to an earlier onset of the GGBS reaction, at around 10 h, and increased the rate of GGBS hydration during the first seven days. The time of onset of the GGBS contribution was also the moment when AFm precipitation started. In CaCl{sub 2}-containing blends, Cl was incorporated in AFm.

36 MATERIALS SCIENCE↗

Autogenous shrinkage and hydration property of alkali activated slag pastes containing superabsorbent polymer

In this paper, the superabsorbent polymer (SAP) was applied as internal curing agent to study its effect on the autogenous shrinkage and hydration property of alkali activated slag (AAS) pastes. Liquid absorption and release processes of SAP in AAS pastes were characterized by {sup 1}H nuclear magnetic resonance ({sup 1}H NMR). Moreover, the microstructure and mechanical strength of AAS pastes containing SAP were also revealed. The results showed that the autogenous shrinkage of AAS pastes containing SAP was reduced by about 80.6%, 72.1% and 72.6%, respectively as the silicate modulus (Ms) increased from 0.8 to 1.4. The addition of SAP delayed the second exothermic peak, but increased the cumulative heat of AAS pastes. In addition, internal curing by SAP could promote the generation of C-A-S-H gels and hydrotalcite-like phases and increase the reaction degree of slag, particularly for AAS pastes with higher Ms, being attributed to the continuous release of entrained water and alkali activator solutions in SAP with the increase of hydration time. Furthermore, the addition of SAP would increase capillary pore size and pore volume of AAS pastes, and thus lead to the decrease of compressive strength.

36 MATERIALS SCIENCE↗

A microstructural investigation of a Na2SO4 activated cement-slag blend

The reactivity and early strength of cement:slag binders is usefully enhanced by the addition of sodium sulfate though the underlying mechanisms of the relationship between the enhanced hydration reactions and the structural aspects of the strength behavior remain unclear. In this study, microstructural development in the presence of Na{sub 2}SO{sub 4} was investigated utilizing mercury intrusion porosimetry (MIP), NMR relaxometry, and XRD. Increased rates of early strength development and decreased rates of late strength development due to the presence of added Na{sub 2}SO{sub 4} were linked to effects on capillary porosity refinement. While degree of hydration at later age was shown to have been lower in the presence of Na{sub 2}SO{sub 4}, and may have been responsible for the higher capillary porosity, a clear alteration in the pathway of microstructural development had occurred with inhibition to hydration of the slag component due to earlier microstructural development proposed.

36 MATERIALS SCIENCE↗

THE IMPACT OF DISSOLVED SALTS ON PASTES CONTAINING FLY ASH, CEMENT AND SLAG

The degree of hydration of a mixture of cementitious materials (Class F fly ash, blast furnace slag and portland cement) in highly concentrated alkaline salt solutions is enhanced by the addition of aluminate to the salt solution. This increase in the degree of hydration, as monitored with isothermal calorimetry, leads to higher values of dynamic Young's modulus and compressive strength and lower values of total porosity. This enhancement in performance properties of these cementitious waste forms by increased hydration is beneficial to the retention of the radionuclides that are also present in the salt solution. The aluminate ions in the solution act first to retard the set time of the mix but then enhance the hydration reactions following the induction period. In fact, the aluminate ions increase the degree of hydration by {approx}35% over the degree of hydration for the same mix with a lower aluminate concentration. An increase in the blast furnace slag concentration and a decrease in the water to cementitious materials ratio produced mixes with higher values of Young's modulus and lower values of total porosity. Therefore, these operational factors can be fine tuned to enhance performance properties of cementitious waste form. Empirical models for Young modulus, heat of hydration and total porosity were developed to predict the values of these properties. These linear models used only statistically significant compositional and operational factors and provided insight into those factors that control these properties.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Adsorption of superplasticizer admixtures on alkali-activated slag pastes

Alkali-activated slag (AAS) binders are obtained by a manufacturing process less energy-intensive than ordinary Portland cement (OPC) and involves lower greenhouse gasses emission. These alkaline cements allow the production of high mechanical strength and durable concretes. In the present work, the adsorption of different superplasticizer admixtures (naphthalene-based, melamine-based and a vinyl copolymer) on the slag particles in AAS pastes using alkaline solutions with different pH values have been studied in detail. The effect of the superplasticizers on the yield stress and plastic viscosity of the AAS and OPC pastes have been also evaluated. The results obtained allowed us to conclude that the adsorption of the superplasticizers on AAS pastes is independent of the pH of the alkaline solutions used and lower than on OPC pastes. However, the effect of the admixtures on the rheological parameters depends directly on the type and dosage of the superplasticizer as well as of the binder used and, in the case of the AAS, on the pH of the alkaline activator solution. In 11.7-pH NaOH-AAS pastes the dosages of the superplasticizers required to attain similar reduction in the yield stress are ten-fold lower than for Portland cement. In this case the superplasticizers studied show a fluidizing effect considerably higher in 11.7-pH NaOH-AAS pastes than in OPC pastes. In 13.6-pH NaOH-AAS pastes, the only admixture observed to affect the rheological parameters is the naphthalene-based admixture due to its higher chemical stability in such extremely alkaline media.

36 MATERIALS SCIENCE↗

Effect of the inherent alkalis of alkali activated slag on the risk of alkali silica reaction

Alkali silica reaction (ASR) occurred in the alkali activated slag (AAS) concrete was evaluated by a revised mortar prism method. The mortars were made of blast furnace slags activated by alkali silicate solution possessing different modulus (0.5, 0.75, 1 and 2) as well as cations (sodium and potassium) and standard sand with a volume replacement of 25 vol% by borosilicate glass beads. Their changes in length and dynamic elastic modulus were monitored up to 7 months. The results showed that ASR has taken place among some mortars, which were evident under both light microscopy and electron microscopy with EDX analysis. The results also revealed that high alkali content did promote the risk of ASR but the degradation due to ASR was affected in a much more complex way.

36 MATERIALS SCIENCE↗

Performance of fly ash concrete with ferronickel slag fine aggregate against alkali-silica reaction and chloride diffusion

Ferronickel slag (FNS) is an industrial by-product of ferronickel alloy production at a high temperature which can be a promising potential to be used as fine aggregate to produce more sustainable concrete. In this study, the performance of concrete containing ferronickel slag sand and fly ash relating to alkali-silica reaction (ASR) and chloride contamination was investigated. ASR-induced expansion, chloride diffusion resistance, and chloride binding capacity of FNS concrete were determined through concrete prism tests (CPT), accelerated diffusion test, and bulk diffusion test. Thermogravimetric analysis (TGA) was conducted to measure the amount of Portlandite and Friedel's salt in concrete. Concrete with 50 wt% FNS sand as fine natural aggregate replacement and 25 wt% of cement replacement by fly ash showed a remarkable potential to be used not only as a low-carbon concrete with comparable mechanical properties to conventional concrete but also with a better performance against ASR and chloride contamination.

36 MATERIALS SCIENCE↗

Modelling of High-Chromia Refractory Spalling in Slagging Coal Gasifiers

The economic viability of converting coal into clean burning liquid fuels in slagging coal gasifiers is compromised by the limited service lifetime of hot-face refractories. One of the most severe refractory degradation mechanisms is spalling, which can occur by either volume expansion phenomena (compressive stresses) or by volume shrinkage phenomena (tensile stresses). A volume shrinkage model is benchmarked to high-chromia refractory material properties and performance under gasifier operating conditions. The model is found to be appropriate for first order estimates of gasifier refractory lifetime when the apparent diffusivity of volatized Cr in the refractory includes the effects of slag-filled pores and cracks.

Failure Analysis↗

Accelerated carbonation of steel slags in a landfill cover construction

Steel slags from high-alloyed tool steel production were used in a full scale cover construction of a municipal solid waste (MSW) landfill. In order to study the long-term stability of the steel slags within the final cover, a laboratory experiment was performed. The effect on the ageing process, due to i.e. carbonation, exerted by five different factors resembling both the material characteristics and the environmental conditions is investigated. Leaching behaviour, acid neutralization capacity and mineralogy (evaluated by means of X-ray diffraction, XRD, and thermogravimetry/differential thermal analysis, TG/DTA) are tested after different periods of ageing under different conditions. Samples aged for 3 and 10 months were evaluated in this paper. Multivariate data analysis was used for data evaluation. The results indicate that among the investigated factors, ageing time and carbon dioxide content of the atmosphere were able to exert the most relevant effect. However, further investigations are required in order to clarify the role of the temperature.

54 ENVIRONMENTAL SCIENCES↗