Dendrite Growth Morphology Modeling in Liquid and Solid Electrolytes

The main goal of this project is to develop a multi-scale modeling approach that connects micron-scale phase-field models and atomic-scale density functional theory (DFT)-based simulations via parameter- and relationship-passing in order to predict Li-metal dendrite morphology evolution, in both liquid and solid electrolytes. The key hypothesis of the DFT-informed phase-field multiscale modeling approach is that it can capture the electrochemical-mechanical driving forces and incorporate the roles of nano-meter-thin solid electrolyte interphase (SEI) in liquid electrolytes as well as of the microstructures of micro-meter-thick solid electrolytes (SEs) for all-solid-state batteries. In this project, we have formulated and implemented phase-field models to incorporate the electrochemical driving forces in liquid electrolytes and then incorporate mechanical driving forces to simulate dendrite growth in solid electrolytes with resolved microstructures. We have implemented two treatments for the SEI: an explicit model to include the microstructure of the SE or SEI in the phase field model and an implicit model to simulate the impact of nano-meter thick SEI in liquid electrolytes by varying the electrode/electrolyte interfacial properties. The key interfacial properties, including the electronic and ionic transport properties, the charge transfer reaction kinetics, and mechanical properties, were computed by DFT-based calculations. At the DFT-based model, one key advancement is to directly predict the charge transfer reaction kinetics at a complex Li/SEI/electrolyte interface by linking DFT with density functional tight binding (DFTB) calculations. As the main accomplishments, we have demonstrated two successful predictions in both solid electrolyte and liquid electrolyte based on this multiscale approach. The predicted intergranular Li dendrite growth in LLZO revealed the importance of trapped electrons at internal interfaces in the microstructure of LLZO. The predicted electroplating morphology of mossy Li and faceted Mg agreed well with experiments. The insights provided by the multiscale model and the model enabled electrolyte and SEI design will accelerate the development of Li-metal electrode for high energy density batteries, that meet DOE’s target on cell density (>350 Wh/kg) and cost below $100/kWhuse for EV applications.

25 ENERGY STORAGE↗

Understanding Solid-Electrolyte Interphase Formation at the Lithium Metal Anode of Lithium-Sulfur Batteries

Lithium-sulfur (Li-S) batteries are one of the most promising chemistries for the next generation of energy storage devices. In a standard Li-S cell, the metallic lithium anode is an essential component of the battery due to its low density, extremely high theoretical specific capacity, and very low negative electrochemical potential. However, several challenges related to the use of Li metal have prevented this battery technology from becoming commercially available. For instance, Li-anodes are highly reactive, which results in the continuous decomposition of the electrolyte and the formation of the solid-electrolyte interphase (SEI) layer. This, combined with the non-uniform deposition of Liions during plating at the anode surface, can seriously affect the performance, cycling, and safety of the battery. In addition, it has been suggested that a controlled SEI formation at the metallic Li anode can yield enhanced battery performance. Hence, a comprehensive understanding of how the SEI layer is formed can help elucidate improvements in this battery technology. In this work, the formation of the SEI layer in Li-S batteries is investigated using density functional theory (DFT) and ab initio molecular dynamics (AIMD) simulations. The stability of liquid organic-based electrolyte components, salt concentration, electron-rich environments, and the use of inorganic solid-state electrolyte (SSE) materials are explored in order to provide molecular-level fundamental insights into how the nature and composition of the electrolyte can alter the initial stages of the SEI formation. The products of electrolyte decomposition and electro-/chemical reaction pathways of liquid electrolyte component such as solvent and salts are predicted from AIMD simulations of electrolyte-anode interfaces. Energetics of reactions from DFT ground-state optimizations are also presented to confirm the decomposition mechanisms. Some significant differences are then drawn regarding the use of low and high salt concentrations. Simulations under electron-rich environments show additional multielectron electrochemical reactions of solvent and salt decomposition taking place due to the excess of electrons and the presence of radical anions in the solution. Finally, the initial stages of formation, stability, and main constituents of interfaces between Li-metal and Sbased electrodes with sulfide-based SSEs are characterized in detail.

25 ENERGY STORAGE↗

Enabling 4C Fast Charging of Lithium–Ion Batteries by Coating Graphite with a Solid–State Electrolyte

Enabling fast-charging (≥4C) of lithium-ion batteries is an important challenge to accelerate the adoption of electric vehicles. However, the desire to maximize energy density has driven the use of increasingly thick electrodes, which hinders rate capability. Herein, atomic layer deposition is used to coat a single-ion conducting solid electrolyte (Li 3 BO 3 -Li 2 CO 3 ) onto postcalendered graphite electrodes, forming an artificial solid-electrolyte interphase (SEI). When compared to uncoated control electrodes, the solid electrolyte coating: 1) eliminates natural SEI formation during preconditioning; 2) decreases interphase impedance by >75% compared to the natural SEI; and 3) extends cycle life under 4C charging conditions, enabling retention of 80% capacity after 500 cycles (compared to 12 cycles in the uncoated control) in pouch cells with >3 mAh cm –2 loading. Furthermore, this work demonstrates that 4C charging without Li plating can be achieved through purely interfacial modification without sacrificing energy density and sheds new light on the role of the SEI in Li plating and fast-charge performance.

25 ENERGY STORAGE↗

Performance degradation due to anodic failure mechanisms in lithium-ion batteries

Here, we report a mechano-chemical model for anodic degradation during fast-charging of nickel-manganese-cobalt (NMC)/graphite (C) cell due to SEI growth, lithium plating/stripping, dead lithium storage, and film fracture of composite SEI and plated lithium film. Degradation of the battery is analyzed for a range of charging rates from 1 to 6 C-rates, and the influence of plating mechanisms – lithium plating and dead lithium deposition and recovery during stripping – on the film resistance of the anode are accounted for in the model. Dynamic evolution of the interfacial properties is modeled using rule-of-mixture approach. Model predictions of plating associated stress fields are used to compute critical energy release rate for film cracking. The results indicate an increased tendency of fracture for thinner SEI film with lithium plating at higher charging rates. The process of reforming the cracked film absorbs a significant portion of the electrode current thereby reducing the cell capacity and plating efficiency. The mechano-chemical model provides an extensive analytical framework for understanding the synergistic coupling of anodic degradation mechanisms, prognosticating conditions of SEI failure, and evaluating the capacity fade and efficiency of lithium-ion battery.

25 ENERGY STORAGE↗

Insights into Spontaneous Solid Electrolyte Interphase Formation at Magnesium Metal Anode Surface from Ab Initio Molecular Dynamics Simulations

Spontaneous chemical reactivity at multivalent (Mg, Ca, Zn, Al) electrode surfaces is critical to solid electrolyte interphase (SEI) formation, and hence, directly affects the longevity of batteries. Here, we report an investigation of the reactivity of 0.5 M Mg(TFSI)2 in 1,2-dimethoxyethane (DME) solvent at a Mg(0001) surface using ab initio molecular dynamics (AIMD) simulations and detailed Bader charge analysis. Based on the simulations, the initial degradation reactions of the electrolyte strongly depend on the structure of the Mg(TFSI)2 species near the anode surface. At the surface, the dissociation of Mg(TFSI)2 species occurs via cleavage of the N-S bond for the solvent separated ion pair (SSIP) and via cleavage of the C-S bond for the contact ion pair (CIP) configuration. In the case of the CIP, both TFSI anions undergo spontaneous bond dissociation reactions to form atomic O, C, S, F, and N species adsorbed on the surface of the Mg anode. These products indicate that the initial SEI layer formed on the surface of the pristine Mg anode consists of a complex mixture of multiple components such as oxides, carbides, sulfides, fluorides, and nitrides. We believe that the atomic level insights gained from these simulations will lay the groundwork for the rational design of tailored and functional interphases that are critical for the success of multivalent battery technology.

Agarwal, Garvit↗

Quantitative Analysis of Origin of Lithium Inventory Loss and Interface Evolution over Extended Fast Charge Aging in Li Ion Batteries

During the extreme fast charging (XFC) of lithium-ion batteries, lithium inventory loss (LLI) and reaction mechanisms at the anode/electrolyte interface are crucial factors in performance and safety. Determining the causes of LLI and quantifying them remain an essential challenge. We present mechanistic research on the evolution and interactions of aging mechanisms at the anode/electrolyte interface. We used NMC 532 /graphite pouch cells charged at rates of 1, 6, and 9 C up to 1000 cycles for our investigation. The cell components were characterized after cycling using electrochemical measurements, inductively coupled plasma optical emission spectroscopy, 7 Li solid-state nuclear magnetic resonance spectroscopy, and high-performance liquid chromatography/mass spectrometry. The results indicate that cells charged at 1 C exhibit no Li plating, and the increase of SEI thickness is the dominant source of the Li loss. In contrast, Li loss in cells charged at 9 C is related to the formation of the metallic plating layers (42%) the SEI layer (38.1%) and irreversible intercalation into the bulk graphite (19%). XPS analysis suggests that the charging rate has little influence on the evolution of SEI composition. The interactions between competing aging mechanisms were evaluated by a correlation analysis. In conclusion, the quantitative method established in this work provides a comprehensive analytical framework for understanding the synergistic coupling of anodic degradation mechanisms, forecasting SEI failure scenarios, and assessing the XFC lithium-ion battery capacity fade.

25 ENERGY STORAGE↗

Stable Potassium Metal Anodes with an All-Aluminum Current Collector through Improved Electrolyte Wetting

This is the first report of successful potassium metal battery anode cycling with an aluminum-based rather than copper-based current collector. Dendrite-free plating/stripping is achieved through improved electrolyte wetting, employing an aluminum-powder-coated aluminum foil “Al@Al,” without any modification of the support surface chemistry or electrolyte additives. The reservoir-free Al@Al half-cell is stable at 1000 cycles (1950 h) at 0.5 mA cm -2 , with 98.9% cycling Coulombic efficiency and 0.085 V overpotential. The pre-potassiated cell is stable through a wide current range, including 130 cycles (2600 min) at 3.0 mA cm -2 , with 0.178 V overpotential. Al@Al is fully wetted by a 4 m potassium bis(fluorosulfonyl)imide-dimethoxyethane electrolyte (θCA = 0°), producing a uniform solid electrolyte interphase (SEI) during the initial galvanostatic formation cycles. On planar aluminum foil with a nearly identical surface oxide, the electrolyte wets poorly (θCA = 52°). This correlates with coarse irregular SEI clumps at formation, 3D potassium islands with further SEI coarsening during plating/stripping, possibly dead potassium metal on stripped surfaces, and rapid failure. The electrochemical stability of Al@Al versus planar Al is not related to differences in potassiophilicity (nearly identical) as obtained from thermal wetting experiments. Additionally, planar Cu foils are also poorly electrolyte-wetted and become dendritic. The key fundamental takeaway is that the incomplete electrolyte wetting of collectors results in early onset of SEI instability and dendrites.

25 ENERGY STORAGE↗

A Solution-Processable High-Modulus Crystalline Artificial Solid Electrolyte Interphase for Practical Lithium Metal Batteries

The solid electrolyte interphase (SEI) has been identified as a key challenge for Li metal anodes. The brittle and inhomogeneous native SEI generated by parasitic reactions between Li and liquid electrolytes can devastate battery performance; therefore, artificial SEIs (ASEIs) have been proposed as an effective strategy to replace native SEIs. Herein, as a collaboration between academia and industrial R&D teams, a multifunctional (crystalline, high modulus, and robust, Li + ion conductive, electrolyte-blocking, and solution processable) ASEI material, LiAl-FBD (where “FBD” refers to 2,2,3,3-tetra-fluoro-1,4-butanediol), for improving Li metal battery performance is designed and synthesized. The LiAl-FBD crystal structure consists of Al 3+ ions bridged by FBD 2– ligands to form anion clusters while Li + ions are loosely bound at the periphery, enabling an Li + ion conductivity of 9.4 × 10 –6 S cm –1 . Further, the fluorinated, short ligands endow LiAl-FBD with electrolyte phobicity and high modulus. The ASEI is found to prevent side reactions and extend the cycle life of Li metal electrodes. Specifically, pairing LiAl-FBD coated 50 μm thick Li with industrial 3.5 mAh cm –2 NMC811 cathode and 2.8 μL mAh –1 lean elec-trolyte, the Li metal full cells show superior cycle life compared to bare ones, achieving 250 cycles at 1 mA cm –2 .

25 ENERGY STORAGE↗

Fine‐Tuning Li‐Ion Solvation Structure by Enhanced Solvent‐Diluent Interactions for Long‐Cycling Lithium Metal Batteries

Achieving durable lithium (Li) metal anodes in liquid electrolytes remains challenging, primarily due to the instability of the formed solid-electrolyte interphases (SEIs). Modulating the Li-ion solvation structures is pivotal in forming a stable SEI for stabilizing Li metal anodes. Here a strategy is developed to fine-tune the Li-ion solvation structures through enhanced dipole–dipole interactions between the Li-ion-coordinated solvent and the non-Li-ion-coordinating diluent, for creating a stable SEI in the developed binary salt electrolyte. The enhanced dipole–dipole interactions weaken the coordination between Li-ions and the solvents while strengthening the interaction between Li-ions and dual anions, thereby facilitating the Li-ion transport and a robust anion-derived SEI with a distinct bilayer structure. Consequently, the developed electrolyte exhibited exceptional electrochemical performance in high energy-density Li||LiNi 0.8 Mn 0.1 Co 0.1 O 2 (NMC811) cells, with long calendar life, stable cyclability at 1 C, and reliable operation between 25 and −20 °C, and it also demonstrat remarkable cycling stability for a Li||NMC811 pouch cell with projected energy density of 402 Wh kg −1 , maintaining 80% capacity retention over 606 cycles under practical conditions.

25 ENERGY STORAGE↗

Stabilizing the Solid‐Electrolyte Interphase with Polyacrylamide for High‐Voltage Aqueous Lithium‐Ion Batteries

Abstract The introduction of “water‐in‐salt” electrolyte (WiSE) concept opens a new horizon to aqueous electrochemistry that is benefited from the formation of a solid‐electrolyte interphase (SEI). However, such SEI still faces multiple challenges, including dissolution, mechanical damaging, and incessant reforming, which result in poor cycling stability. Here, we report a polymeric additive, polyacrylamide (PAM) that effectively stabilizes the interphase in WiSE. With the addition of 5 molar % PAM to 21 mol kg −1 LiTFSI electrolyte, a LiMn 2 O 4 ∥L‐TiO 2 full cell exhibits enhanced cycling stability with 86 % capacity retention after 100 cycles at 1 C. The formation mechanism and evolution of PAM‐assisted SEI was investigated using operando small angle neutron scattering and density functional theory (DFT) calculations, which reveal that PAM minimizes the presence of free water molecules at the anode/electrolyte interface, accelerates the TFSI − anion decomposition, and densifies the SEI.

Hou, Xu↗

Stabilizing the Solid‐Electrolyte Interphase with Polyacrylamide for High‐Voltage Aqueous Lithium‐Ion Batteries

Abstract The introduction of “water‐in‐salt” electrolyte (WiSE) concept opens a new horizon to aqueous electrochemistry that is benefited from the formation of a solid‐electrolyte interphase (SEI). However, such SEI still faces multiple challenges, including dissolution, mechanical damaging, and incessant reforming, which result in poor cycling stability. Here, we report a polymeric additive, polyacrylamide (PAM) that effectively stabilizes the interphase in WiSE. With the addition of 5 molar % PAM to 21 mol kg −1 LiTFSI electrolyte, a LiMn 2 O 4 ∥L‐TiO 2 full cell exhibits enhanced cycling stability with 86 % capacity retention after 100 cycles at 1 C. The formation mechanism and evolution of PAM‐assisted SEI was investigated using operando small angle neutron scattering and density functional theory (DFT) calculations, which reveal that PAM minimizes the presence of free water molecules at the anode/electrolyte interface, accelerates the TFSI − anion decomposition, and densifies the SEI.

25 ENERGY STORAGE↗

Probing the Li 4 Ti 5 O 12 Interface Upon Lithium Uptake by Operando Small Angle Neutron Scattering

The formation of a solid–electrolyte interphase (SEI) on the surface of Li 4 Ti 5 O 12 (LTO) has become a highly controversial topic, with arguments for it and against it. However, prior studies supporting the formation of an SEI layer have typically suggested that a layer forms upon cycling of a cell, although the layer is probed after disassembling. In this study, cubic mesostructured LTO is synthesized with crystallite domain sizes between 3 and 4 nm and uniform pores with diameters ≤8 nm. The mean pore size is controlled between 4–8 nm through the use of a triblock amphipathic copolymer with a tunable hydrophobic block as template and by thermal treatment. The LTO morphology obtained is spherical and evolves upon heat treatment. We report these materials show excellent electrochemical performance, including high rate capability and capacity retention. The LTO material is subjected to operando small-angle neutron scattering and X-ray photoelectron spectroscopy experiments, which reveal that the highly debated SEI forms at potentials as high as 2.2 V, first as a LiF-rich layer and subsequently by the growth of a carbonaceous layer. These SEI products form first on the smaller pores before forming on the mesopores.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

In situ probing the origin of interfacial instability of Na metal anode

The unstable and fragile solid electrolyte interphase (SEI) has restricted the application of Na metal anodes. Despite numerous research efforts being put into understanding its chemical composition and physical properties, direct observation of its formation remains a challenge due to the lack of temporal and spatial resolution. Here, through combined in situ probing techniques, we exhibit two pivotal stages associated with SEI instability during the often -neglected formation process. It is revealed that Na metal that is not uniformly passivated at the initial (passivating) stage will trigger unrestricted electrolyte decomposition and homogeneous components distribution during the subsequent (growing) stage. SEI with homogenously distributed components is found to have higher solubility than that with a layered structure evolved from a compact passivation layer. Furthermore, through demonstrating an SEI dissolution model that is closely related to its formation process and compositional distribution, this work sheds light on an uncharted territory of Na metal batteries.

25 ENERGY STORAGE↗

Evolution of solid electrolyte interphase and active material in the silicon wafer model system

Alloying anode materials for lithium-ion batteries, such as silicon (Si), are an important focus of materials research due to the demand for increased energy density for electric vehicles and stationary grid storage. However, progress towards next generation anode materials has been hindered by poor capacity retention due to the instability of the Si active material and the solid electrolyte interphase (SEI). Herein, the evolution of the active Si material and the SEI are simultaneously investigated from the perspective of chemical, structural, morphological, and electronic evolution in the Si wafer model system through its cycling life, using time-of-flight secondary ion mass spectrometry (TOF-SIMS), scanning transmission electron microscopy (STEM), atomic force microscopy (AFM), and scanning spreading resistance microscopy (SSRM). The results illustrate a dynamic evolution of the SEI and active Si material through cycling. Through an improved understanding of evolution of SEI and Si active material within the Si wafer model system, mitigation strategies may be designed to extend the lifetime of Si anodes.

25 ENERGY STORAGE↗

Electrode roughness dependent electrodeposition of sodium at the nanoscale

Na metal is an attractive anode material for rechargeable Na ion batteries, however, the dendritic growth of Na can cause serious safety issues. Along with modifications of solid-electrolyte interphase (SEI), engineering the electrode has been reported to be effective in suppressing Na dendritic growth, likely by reducing localized current density accumulation. However, fundamental understanding of Na growth at the nanoscale is still limited. Here, we report an in-situ study of Na electrodeposition in electrochemical liquid cells with the electrodes in different surface roughness, e.g., flat or sharp curvature. Real time observation using transmission electron microscopy (TEM) reveals the Na electrodeposition with remarkable details. Relatively large Na grains (in the micrometer scale) are achieved on the flat electrode surface. The local SEI thickness variations impact the growth rate, thus the morphology of individual grains. In contrast, small Na grains (in tens of nanometers) grow explosively on the electrode at the point with sharp curvature. The newly formed Na grains preferentially deposit at the base of existing grains close to the electrode. Further studies using continuum-based computational modeling suggest that the growth mode of an alkali metal (e.g. Na) is strongly influenced by the transport properties of SEI. Our direct observation of Na deposition in combination with the theoretical modeling provides insights for comprehensive understanding of electrode roughness and SEI effects on Na electrochemical deposition.

25 ENERGY STORAGE↗

Lithium metal stripping mechanisms revealed through electrochemical liquid cell electron microscopy

An understanding of lithium stripping is as important as that of lithium plating to achieve significant advances in using lithium metal anodes for high-energy rechargeable batteries. However, there have been limited studies on lithium stripping compared to lithium plating. Here we report the lithium stripping mechanisms revealed through in-situ electrochemical liquid cell transmission electron microscopy (TEM). We directly observe and compare the stripping behavior of the in-situ grown lithium dendrites and lithium nanograins covered by a lithium fluoride-rich solid-electrolyte interphase (SEI). Furthermore, we find the sporadic lithium stripping behavior and three important modes that can describe the stripping of individual lithium deposits, regardless of their morphology: (i) symmetric stripping, (ii) surface-preferred asymmetric stripping, and (iii) interface-preferred asymmetric stripping. In addition, SEI chemical mapping with high spatial resolution shows a remarkable SEI loss at the end of the lithium metal stripping, which illustrates the importance of SEI protection in the subsequent cycles.

25 ENERGY STORAGE↗

Quantifying lithium loss in amorphous silicon thin-film anodes via titration-gas chromatography

Silicon with a high theoretical capacity (3,579 mAh/g) is a promising anode candidate for lithium-ion batteries. However, commercialization is still impeded by low Coulombic efficiency, caused by solid electrolyte interphase (SEI) formation and trapped lithium (Li)-silicon (Si) alloy during repeated volume change. Quantifying capacity losses from each factor is crucial to formulate rational design strategies for further improvement. In this work, titration-gas chromatography and cryogenic transmission electron microscopy are applied to characterize the evolution of trapped Li-Si alloy and SEI growth in a silicon thin-film anode. It is found that continuous growth of the SEI is the dominant factor for lithium inventory loss during cycling, with only a marginal increase in trapped Li-Si alloy. This study offers a quantitative approach to differentiate Li in the SEI from trapped Li in Li-Si alloy through a silicon thin-film anode, providing unique insights into identifying critical bottlenecks for developing Si anodes.

25 ENERGY STORAGE↗

Compositions and Formation Mechanisms of Solid-Electrolyte Interphase on Microporous Carbon/Sulfur Cathodes

We report the formation mechanism and compositions of a solid-electrolyte interphase (SEI) on a microporous carbon/sulfur (MC/S) cathode in Li–S batteries using a carbonate-based electrolyte (1 M LiPF 6 in ethylene carbonate (EC)/dimethyl carbonate, v:v = 1:1). Through characterizations using 1D and 2D solution-phase nuclear magnetic resonance spectroscopy, coupled with model chemical reactions and DFT calculations, we have identified two critical roles of Li + in steering the SEI formation. First, the preferential solvation of Li + by EC in the mixed carbonate electrolyte renders EC as the dominant participant in the SEI formation, and second, Li + coordination to the EC carbonyl alters activation barriers and changes the reaction pathways relative to Na + . The main organic components in the SEI are identified as lithium ethylene monocarbonate and lithium methyl carbonate, which are virtually identical to those formed on Li and graphite anodes of lithium-ion batteries but via a different pathway.

25 ENERGY STORAGE↗