Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “MAGNETRON SPUTTERING”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 217 records · Page 12

Ti-Nb thin films deposited by magnetron sputtering on stainless steel

Thin films of Ti-Nb alloys were deposited on AISI 316L stainless steel substrate by magnetron sputtering, and the structure, composition, morphology, and microstructure of the films were analyzed by means of x-ray diffraction (XRD), (scanning) transmission electron microscopy (TEM) coupled with energy-dispersive x-ray spectroscopy, atomic force microscopy (AFM), and x-ray photoelectron spectroscopy (XPS). Thin films of four compositions were produced: Ti{sub 85}Nb{sub 15} (Ti-26 wt. % Nb), Ti{sub 80}Nb{sub 20} (Ti-33 wt. % Nb), Ti{sub 70}Nb{sub 30} (Ti-45 wt. % Nb), and Ti{sub 60}Nb{sub 40} (Ti-56 wt. % Nb). Structural characterization by XRD indicated that only the β phase was present in the thin films and that the increase in the Nb content modified the alloy film texture. These changes in the film texture, also detected by TEM analysis, were attributed to different growth modes related to the Nb content in the alloy films. The mean grain sizes measured by AFM increased with the Nb amount (from 197 to 222 nm). XPS analysis showed a predominance of oxidized Ti and Nb on the film surfaces and an enrichment of Ti.

36 MATERIALS SCIENCE↗

The correlation between the radial distribution of high-energetic ions and the structural as well as electrical properties of magnetron sputtered ZnO:Al films

The origin of the pronounced radial distributions of structural and electrical properties of magnetron sputtered ZnO:Al films has been investigated. The film properties were correlated with the radially resolved ion-distribution functions. While the positive ions exhibit low energies and a radial distribution with a maximum intensity opposite the center of the target, the negative ions can have energies up to several hundred eV, depending on the target potential, with a radial distribution with two maxima opposite the erosion tracks. The most prominent positive ion is that of the working gas (Ar{sup +}), while the highest flux of the negative ions is measured for negative oxygen O{sup −}. The radial distribution of the flux of the high-energetic negative ions can clearly be related to the radial variations of the structural (c-axis lattice parameter, crystallite size) and electronic (resistivity) properties for sputtering from the planar target, which points to the decisive role of the high-energetic negative oxygen ions for the film quality. The relation between the negative ion bombardment and the structural as well as electronic properties can be explained by a qualitative model recently developed by us. The same target has also been investigated in the eroded state. In this case, the limited acceptance angle of the mass spectrometer leads to a misinterpretation of the radial distribution of the flux of the high-energetic negative ions. This effect can be explained by a simulation, based on the assumption that the high-energetic negative ions are mainly accelerated in the cathode (target) sheath perpendicular to the uneven substrate surface.

36 MATERIALS SCIENCE↗

Parameters of ZnO films with p-type conductivity deposited by high-frequency magnetron sputtering

It is demonstrated that a reduction in the defect concentration in ZnO films formed by high-frequency magnetron sputtering allows effective doping with acceptor impurities both in the cation (Li) and anion (N{sup +}) sublattices and p-type conductivity with reproducible charge-carrier parameters (concentration and mobility) to be obtained. ZnO films are doped with nitrogen by annealing in a high-frequency gas discharge atmosphere. Hall measurements by the Van der Pauw technique show that the deposition of thin Eu layers on the ZnO film surface increases the concentration and mobility of majority charge carriers. The embedding of metal impurities with different ionic radii (Ag and Au) in the cation sublattice of the ZnO films to compensate misfit stresses makes it possible to enhance the concentration of radiative-recombination centers.

36 MATERIALS SCIENCE↗

On the electron energy in the high power impulse magnetron sputtering discharge

The temporal variation of the electron energy distribution function (EEDF) was measured with a Langmuir probe in a high power impulse magnetron sputtering (HiPIMS) discharge at 3 and 20 mTorr pressures. In the HiPIMS discharge a high power pulse is applied to a planar magnetron giving a high electron density and highly ionized sputtered vapor. The measured EEDF is Maxwellian-like during the pulse; it is broader for lower discharge pressure and it becomes narrower as the pulse progresses. This indicates that the plasma cools as the pulse progresses, probably due to high metal content of the discharge.

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗

One-step aluminium-assisted crystallization of Ge epitaxy on Si by magnetron sputtering

In this work, one-step aluminium-assisted crystallization of Ge on Si is achieved via magnetron sputtering by applying an in-situ low temperature (50 °C to 150 °C) heat treatment in between Al and Ge depositions. The effect of heat treatment on film properties and the growth mechanism of Ge epitaxy on Si are studied via X-ray diffraction, Raman and transmission electron microscopy analyses. Compared with the conventional two-step process, the one-step aluminium-assisted crystallization requires much lower thermal budget and results in pure Ge epitaxial layer, which may be suitable for use as a virtual substrate for the fabrication of III-V solar cells.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Effects of off-stoichiometry and density on the magnetic and magneto-optical properties of yttrium iron garnet films by magnetron sputtering method

Yttrium iron garnet films were deposited on Si and Si/CeO{sub 2} substrates by magnetron sputtering method followed by postannealing. By varying the fabrication parameters such as sputtering atmosphere, sputtering power, and annealing atmosphere, single phase garnet films were obtained with different off-stoichiometry and film density. The dependence of cation ratio, magnetic and magneto-optical characteristics, and absorption coefficient were systemically investigated. The results reveal that a proper oxygen pressure in both sputtering and annealing process give rise to a small cation ratio of (Fe{sup 2+} or Fe{sup 4+})/Fe{sup 3+}, thus is beneficial to obtain large saturation magnetization, large Faraday rotation, and small optical absorption. The sputtering power can also affect the properties of the film through changing the film density. Our results indicate that the properties of sputtering deposited yttrium iron garnet (YIG) film can be easily tuned and optimized by modifying the off-stoichiometry and density of the film, thus provides flexibility to fabricate YIG film for extensive applications.

36 MATERIALS SCIENCE↗

Preliminary study of CdTe and CdTe:Cu thin films nanostructures deposited by using DC magnetron sputtering

Growth and properties of CdTe and CdTe:Cu thin films nanostrucures deposited by using dc magnetron sputtering are reported. Scanning electron microscope (SEM) was used to observe the surface morphologies of the thin films. At growth conditions of 250 °C and 14 W, CdTe films did not yet evenly deposited. However, at growth temperature and plasma power of 325 °C and 43 W, both CdTe and CdTe:Cu(2%) have deposited on the substrates. In this condition, the morphology of the films indicate that the films have a grain-like nanostructures. Grain size diameter of about 200 nm begin to appear on top of the films. Energy Dispersive X-rays spectroscopy (EDX) was used to investigate chemical elements of the Cu doped CdTe film deposited. It was found that the film deposited consist of Cd, Te and Cu elements. XRD was used to investigate the full width at half maximum (FWHM) values of the thin films deposited. The results show that CdTe:Cu(2%) thin film has better crystallographic properties than CdTe thin film. The UV-Vis spectrometer was used to investigate the optical properties of thin films deposited. The transmittance spectra showed that transmittance of CdTe:Cu(2%) film is lower than CdTe film. It was found that the bandgap energy of CdTe and CdTe:Cu(2%) thin films of about 1.48 eV.

36 MATERIALS SCIENCE↗

Electrochemical Performance of rf Magnetron Sputtered LiCoO{sub 2} Thin Film Positive Electrodes

Thin films of LiCoO{sub 2} were grown by rf magnetron sputtering technique and studied the influence of In situ annealing treatment on microstructural and electrochemical properties of the films. Annealing treatment in presence of O{sub 2} ambient develops characteristic (104) plan in relative to (003) plane texture indicating that the films have HT-layered structure with R3-bar m symmetry. The effect is discussed in terms of grain size, cycling stability, reversibility and the specific discharge capacity.

36 MATERIALS SCIENCE↗

Physical properties of epitaxial ZrN/MgO(001) layers grown by reactive magnetron sputtering

Single-crystal ZrN films, 830 nm thick, are grown on MgO(001) at 450 °C by magnetically unbalanced reactive magnetron sputtering. The combination of high-resolution x-ray diffraction reciprocal lattice maps, high-resolution cross-sectional transmission electron microscopy, and selected-area electron diffraction shows that ZrN grows epitaxially on MgO(001) with a cube-on-cube orientational relationship, (001){sub ZrN}‖(001){sub MgO} and [100]{sub ZrN}‖[100]{sub MgO}. The layers are essentially fully relaxed with a lattice parameter of 0.4575 nm, in good agreement with reported results for bulk ZrN crystals. X-ray reflectivity results reveal that the films are completely dense with smooth surfaces (roughness = 1.3 nm, consistent with atomic-force microscopy analyses). Based on temperature-dependent electronic transport measurements, epitaxial ZrN/MgO(001) layers have a room-temperature resistivity ρ{sub 300K} of 12.0 μΩ-cm, a temperature coefficient of resistivity between 100 and 300 K of 5.6 × 10{sup −8}Ω-cm K{sup −1}, a residual resistivity ρ{sub o} below 30 K of 0.78 μΩ-cm (corresponding to a residual resistivity ratio ρ{sub 300Κ}/ρ{sub 15K} = 15), and the layers exhibit a superconducting transition temperature of 10.4 K. The relatively high residual resistivity ratio, combined with long in-plane and out-of-plane x-ray coherence lengths, ξ{sub ‖} = 18 nm and ξ{sub ⊥} = 161 nm, indicates high crystalline quality with low mosaicity. The reflectance of ZrN(001), as determined by variable-angle spectroscopic ellipsometry, decreases slowly from 95% at 1 eV to 90% at 2 eV with a reflectance edge at 3.04 eV. Interband transitions dominate the dielectric response above 2 eV. The ZrN(001) nanoindentation hardness and modulus are 22.7 ± 1.7 and 450 ± 25 GPa.

36 MATERIALS SCIENCE↗

High-Power Impulse Magnetron Sputter Deposition of Ultrathick Amorphous Carbon

Diamond-like carbon (DLC) is a material of interest for inertial confinement fusion (ICF) ablators. However, the deposition of ultrathick DLC coatings, as required for ICF ablator fabrication, remains a challenge. Here, in this study, we use high-power impulse magnetron sputtering to deposit DLC and demonstrate a set of process parameters leading to high-purity, amorphous DLC coatings with a low compressive residual stress of <400 MPa. Coatings with thicknesses of up to 80 μm are demonstrated.

amorphous carbon↗

Oblique angle deposition of boron carbide films by magnetron sputtering

Many applications of boron carbide (B4C) films entail deposition on non-planar substrates, necessitating a better understanding of oblique angle deposition phenomena. Here, we systematically study the effect of substrate tilt on properties of B 4 C films with thicknesses up to 10 μm deposited by direct current magnetron sputtering. Results show that all films are amorphous and columnar with an average column width of ~100 nm, independent of substrate tilt. Column tilt angles are limited to ~20° even for substrate tilt of 80°. Film density, residual stress, and the refractive index weakly (within ≲20%) depend on substrate tilt. Furthermore, oxygen impurities bond preferentially with carbon atoms in inter-columnar regions. Substrate tilt has a major effect on mechanical properties that decrease by ~50%, suggesting weak interconnection between nano-columns. Implications of these observations for the deposition onto non-planar substrates are discussed.

36 MATERIALS SCIENCE↗

Gold-tantalum alloy films deposited by high-density-plasma magnetron sputtering

Gold-tantalum alloy films are of interest for biomedical and magnetically-assisted inertial confinement fusion applications. Here, we systematically study the effects of substrate tilt (0°–80°) and negative substrate bias (0–100 V) on properties of ≲3-μm-thick films deposited by high-power impulse magnetron sputtering (HiPIMS) from a Au–Ta alloy target (with 80 at. % of Ta). Results reveal that, for all the substrate bias values studied, an increase in substrate tilt leads to a monotonic decrease in film thickness, density, residual compressive stress, and electrical conductivity. Larger substrate bias favors the formation of a body-centered cubic phase, with films exhibiting lower column tilt and higher density, electrical conductivity, and residual compressive stress. Furthermore, these changes are attributed to metal atom ionization effects, based on the lack of correlation with distributions of landing energies and incident angles of depositing species as calculated by Monte Carlo simulations of ballistic collisions and gas phase atomic transport. By varying substrate tilt and bias in HiPIMS deposition, properties of Au–Ta alloy films can be controlled in a very wide range, including residual stress from –2 to +0.5 GPa, density from 12 to 17 g/cm 3 , and the electrical resistivity from 50 to 4500 μΩ cm, enabling optimum deposition conditions to be selected for specific applications.

36 MATERIALS SCIENCE↗

FePt:C/Fe graded and nongraded films with controllable coercivity fabricated by magnetron sputtering and postannealing

Graded and nongraded FePt:C(hard)/Fe(soft) films with different structures are fabricated by magnetron sputtering and postannealing. Due to the interdiffusion between FePt and C layers during the annealing process, films with a continuous variation in anisotropy are realized by varying the C concentration in the FePt hard layer. In comparison to the FePt/Fe bilayer, the coercivities of graded and nongraded films are effectively reduced. However, the mechanisms of reduction are different. Moreover, adding a nonmagnetic C layer not only tailors the gradient of anisotropy, but also weakens the intergranular exchange interaction.

36 MATERIALS SCIENCE↗

Highly phosphorus-doped crystalline Si layers grown by pulse-magnetron sputter deposition

The electrical properties of highly phosphorus-doped crystalline silicon films deposited by pulse-magnetron sputtering were studied. The films were grown, 450 nm thick, on Si(100) and Si(111) wafers at low substrate temperatures T{sub s} of 450-550 deg. C and post-treated by rapid thermal annealing (RTA) and plasma hydrogenation (PH). In the case of films grown on Si(100), at all values of T{sub s} postgrowth treatment by RTA resulted in an increase in the dopant activation up to 100% and of the Hall mobility to about bulklike values of 50 cm{sup 2} V{sup -1} s{sup -1}. This result suggests high structural quality of the films on Si(100). The Si(111) films, which are typically more defective, exhibit a completely different behavior with a strong dependence of the electrical dopant activation and the Hall mobility on T{sub s}. By post-treatment a maximum P donor activation level of 22% could be obtained. The variation in the post-treatment procedure (RTA+PH and PH+RTA) for the films deposited at high T{sub s} showed that PH results only in minor changes in the film properties. The different influence of RTA and PH is discussed in terms of the different defect structure of the films. These investigations reveal that high T{sub s} and after-treatment by RTA are the main preconditions for optimal electrical film properties.

36 MATERIALS SCIENCE↗

Evolution of the plasma composition of a high power impulse magnetron sputtering system studied with a time-of-flight spectrometer

The plasma of a high power impulse magnetron sputtering system has been investigated using a time-of-flight spectrometer. The target materials included high sputter yield materials (Cu, Ag), transition metals (Nb, Cr, Ti), and carbon (graphite); the sputtering gases were argon, krypton, and nitrogen, and two different target thicknesses were selected to consider the role of the magnetic field strength. Measurements for selected combinations of those parameters give quantitative information on the transition from gas-dominated to metal-dominated (self-sputtering) plasma, on the fractions of ion charge states, and in the case of molecular gases, on the fraction of atomic and molecular ions.

36 MATERIALS SCIENCE↗

Properties of silicon homojunctions with pulse-magnetron sputtered crystalline n{sup +}-emitter layers

Highly phosphorus doped crystalline silicon films were grown by pulse-magnetron sputter deposition on (100) and (111) oriented silicon wafer substrates at low temperatures of 450-550 deg. C. Rapid thermal annealing (RTA) and plasma hydrogenation (PH) were applied as postgrowth treatments. To explore the nature of the junction transport processes the I-V characteristics were studied in different device geometries as a function of temperature. The analysis suggests that depending on the substrate orientation (hkl) both postgrowth treatments influence the bulk-related current component J{sub 0b}{sup (hkl)} of the saturation current density in different manners and introduce additional conduction paths at the perimeter of the measured diode structures. For diodes grown on Si(100) postgrowth treatment by RTA results in a decrease in J{sub 0b}{sup (100)} to respectable 4x10{sup -11} A cm{sup -2}, whereas no major influence of RTA for the Si(111) based junctions could be obtained. They prove to be sensitive to PH post-treatment, which resulted in a reduction in J{sub 0b}{sup (111)} to 8x10{sup -11} A cm{sup -2}. The perimeter induced excess current is most strongly pronounced for the hydrogenated diodes on Si(111) and much less relevant for the RTA treated Si(100) structures.

36 MATERIALS SCIENCE↗

Current-voltage-time characteristics of the reactive Ar/N{sub 2} high power impulse magnetron sputtering discharge

The discharge current and voltage waveforms have been measured in a reactive high power impulse magnetron sputtering (HiPIMS) Ar/N{sub 2} discharge with a Ti target for 400 {mu}s long pulses. We observe that the current waveform in the reactive Ar/N{sub 2} HiPIMS discharge is highly dependent on the pulse repetition frequency, unlike the non-reactive Ar discharge. The current is found to increase significantly as the frequency is lowered. This is attributed to an increase in the secondary electron emission yield during the self-sputtering phase, when the nitride forms on the target at low frequencies. In addition, self-sputtering runaway occurs at lower discharge voltages when nitrogen is added to the discharge. This illustrates the crucial role of self-sputtering in the behavior of the reactive HiPIMS discharge.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Influence of vanadium incorporation on the microstructure, mechanical and tribological properties of Nb–V–Si–N films deposited by reactive magnetron sputtering

Composite Nb–V–Si–N films with various V contents (3.7–13.2 at.%) were deposited by reactive magnetron sputtering and the effects of V content on the microstructure, mechanical and tribological properties of Nb–V–Si–N films were investigated. The results revealed that a three-phase structure, consisting of face-centered cubic (fcc) Nb–V–Si–N, hexagonal close-packed (hcp) Nb–V–Si–N and amorphous Si{sub 3}N{sub 4}, co-exists in the Nb–V–Si–N films and the cubic phase is dominant. The hardness and critical load (L{sub c}) of Nb–V–Si–N films initially increased gradually and reached a summit, then decreased with the increasing V content in the films and the maximum values were 35 GPa and 9.8 N, respectively, at 6.4 at.% V. The combination of V into Nb–Si–N film led to the fracture toughness linearly increasing from 1.11 MPa·m{sup 1/2} at 3.7 at.% V to 1.67 MPa·m{sup 1/2} at 13.2 at.% V. At room temperature (RT), the average friction coefficient decreased from 0.80 at 3.7 at.% V to 0.55 at 13.2 at.% V for the Nb–V–Si–N films. The wear rate of Nb–V–Si–N films initially decreased and then increased after reaching a minimum value of about 6.35 × 10{sup −} {sup 7} mm{sup 3}/N·mm at 6.4 at.% V. As the rise of testing temperature from 200 °C to 600 °C, the average friction coefficient of Nb–V–Si–N films decreased with the increase of the testing temperature regardless of V content. However, the wear rate gradually increased for all films. The average friction coefficient and wear rate at RT and elevated temperatures were mainly influenced by the vanadium oxides with weakly bonded lattice planes. - Highlight: • Fcc-Nb–V–Si–N, hcp-Nb–V–Si–N and amorphous Si{sub 3}N{sub 4} co-existed in the films. • The amount of Si{sub 3}N{sub 4} decreased with increasing V content in the films. • Hardness of Nb–V–Si–N film (6.4 at.%) reached a maximum value of 35 GPa. • Addition of V led to the increase of fracture toughness. • Tribological properties were influenced by lubricant wear debris.

36 MATERIALS SCIENCE↗