Unveiling the Role of Critical Impurities in Spent LiFePO 4 Cathodes for Scalable Direct Regeneration

Direct regeneration offers a promising alternative to recycling End-of-Life (EoL) batteries by restoring metal elements and preserving the material structure, yet scaling these technologies to handle practical cathode black mass (CBM) with impurities remains challenging. Here, this study investigates the evolution of impurities, including aluminum (Al), polyvinylidene difluoride (PVDF) binder, and residual carbon (C), during direct recycling of spent LiFePO 4 (LFP) cathodes and their impact on electrochemical performance. Using various ex situ and in situ analyses, it is shown that the formation of lithium fluoride (LiF) during the traditional direct recycling process hinders lithium diffusion and deteriorates the reversible capacity. To address this major challenge, the combination of pH-controlled hydrothermal purification and the two-step sintering process is proposed effectively to regenerate spent LFP cathodes, eliminating the negative effect of Al and fluorine (F) impurities while mitigating any potential impacts of carbon residuals. The regenerated LFP from spent CBM achieves superior performance, retaining 152.5 mAh g −1 at 0.1 C and 133 mAh g −1 at 1 C with 98.7% capacity retention after 200 cycles. This approach is further validated using three distinct waste feedstocks from battery modules, enhancing impurity management and scalability in direct recycling. These findings present a sustainable and economically viable solution for large-scale LFP regeneration.

25 ENERGY STORAGE↗

An Inorganic‐Rich Solid Electrolyte Interphase for Advanced Lithium‐Metal Batteries in Carbonate Electrolytes

Abstract In carbonate electrolytes, the organic–inorganic solid electrolyte interphase (SEI) formed on the Li‐metal anode surface is strongly bonded to Li and experiences the same volume change as Li, thus it undergoes continuous cracking/reformation during plating/stripping cycles. Here, an inorganic‐rich SEI is designed on a Li‐metal surface to reduce its bonding energy with Li metal by dissolving 4 m concentrated LiNO 3 in dimethyl sulfoxide (DMSO) as an additive for a fluoroethylene‐carbonate (FEC)‐based electrolyte. Due to the aggregate structure of NO 3 − ions and their participation in the primary Li + solvation sheath, abundant Li 2 O, Li 3 N, and LiN x O y grains are formed in the resulting SEI, in addition to the uniform LiF distribution from the reduction of PF 6 − ions. The weak bonding of the SEI (high interface energy) to Li can effectively promote Li diffusion along the SEI/Li interface and prevent Li dendrite penetration into the SEI. As a result, our designed carbonate electrolyte enables a Li anode to achieve a high Li plating/stripping Coulombic efficiency of 99.55 % (1 mA cm −2 , 1.0 mAh cm −2 ) and the electrolyte also enables a Li||LiNi 0.8 Co 0.1 Mn 0.1 O 2 (NMC811) full cell (2.5 mAh cm −2 ) to retain 75 % of its initial capacity after 200 cycles with an outstanding CE of 99.83 %.

Liu, Sufu↗

A Facile Potential Hold Method for Fostering an Inorganic Solid‐Electrolyte Interphase for Anode‐Free Lithium‐Metal Batteries

Abstract Anode‐free lithium batteries are regarded as an ultimate form of high‐energy‐density lithium‐ion batteries. Unfortunately, irreversible lithium loss during cycling plays a major role in degrading the overall cell performance in the anode‐free configuration. To alleviate the deterioration, building a robust solid‐electrolyte interface on an anode current collector is an indispensable requirement. Here, we present a facile in‐situ electrochemical method of a potential hold during the first charge to guide more salt‐derived (less solvent‐derived) decomposition on the anode interface. We show the distinctive decomposition potential of lithium salts and ether/carbonate solvents, where the Li‐solvation structures with salt contact‐ion‐pairs preferentially decompose to form LiF‐rich and less organic components, leading to enhanced lithium Coulombic efficiency in Li||Cu cells as well as mitigating the capacity fade of Cu||LiFePO 4 and Cu||LiNi 0.8 Mn 0.1 Co 0.1 O 2 cells.

Shin, Woochul↗

Lithium‐Containing Hybrid SEI Layer Enabling High Mass Loading and Anode‐Less Sodium Metal Batteries

Abstract The continuous rupturing and rebuilding of unstable solid electrolyte interphase (SEI) layer during cycling would block Na + diffusion and induce Na dendrite formation, ultimately limiting the practical application of high‐energy‐density sodium metal batteries. Herein, a hybrid SEI layer containing Li‐species is dexterously constructed on the surface of sodium metal anode. Li‐containing inorganic components (Li 3 N, LiF, and Li 2 CO 3 ) are introduced to stabilize the Na/electrolyte interface and enhance the mechanical and diffusion kinetic properties of the SEI layer, which can reduce the side reactions and gas generation, regulate Na + flux during cycling and promote rapid Na + migration for uniform dendrite‐free Na deposition. As a result, the constructed Na symmetric cells achieve low overpotential and long cycle life of 5900, 1800, and 500 h at current densities of 3, 10, and 30 mA cm −2 , respectively. Furthermore, the full cells paired with the Na₃V₂(PO₄)₃ cathode demonstrate high specific capacity and excellent cycle stability, even at an ultra‐high cathode loading of 39.3 mg cm −2 and a low N/P ratio (negative/positive electrode capacity ratio of 1.21).

Xia, Li [State Key Laboratory of Physical Chemistr↗

An Inorganic-Rich Solid Electrolyte Interphase for Advanced Lithium-Metal Batteries in Carbonate Electrolytes

In carbonate electrolytes, the organic-inorganic solid electrolyte interphase (SEI) formed on the lithium (Li) metal anode surface is strongly bonded to Li and experiences the same volume change as Li, thus it undergoes continuous cracking/reformation during plating/stripping cycles. Here we report, an inorganic-rich SEI is designed on a Li metal surface to reduce its bonding energy with Li metal by dissolving 4 M concentrated LiNO 3 in dimethyl sulfoxide (DMSO) as an additive for a fluoroethylene carbonate (FEC) based electrolyte. Due to the aggregate structure of NO 3 - ions and its participation in the primary Li + solvation sheath, abundant Li 2 O, Li 3 N, and LiN x O y grains are formed in the resulting SEI, in addition to the uniform LiF distribution from the reduction of PF 6 - ions. The inorganic-rich SEI’s weak bonding (high interface energy) to Li can effectively promote Li diffusion along the SEI/Li interface and prevent Li dendrite penetration into the SEI. As a result, our designed carbonate electrolyte enables a Li anode to achieve a high Li plating/stripping CE of 99.55% (1 mA cm -2 , 1.0 mAh cm -2 ) and the electrolyte also enables a Li||LiNi 0.8 Co 0.1 Mn 0.1 O 2 (NMC811) full cell (2.5 mAh cm -2 ) to retain 75%of its initial capacity after 200 cycles with an outstanding CE of 99.83%.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

A Facile Potential Hold Method for Fostering an Inorganic Solid-Electrolyte Interphase for Anode-Free Lithium-Metal Batteries

Anode-free lithium batteries are regarded as an ultimate form of high-energy-density lithium-ion batteries. Unfortunately, irreversible lithium loss during cycling plays a major role in degrading the overall cell performance in the anode-free configuration. To alleviate the deterioration, building a robust solid-electrolyte interface on an anode current collector is an indispensable requirement. Here, we present a facile in-situ electrochemical method of a potential hold during the first charge to guide more salt-derived (less solvent-derived) decomposition on the anode interface. Here we show the distinctive decomposition potential of lithium salts and ether/carbonate solvents, where the Li-solvation structures with salt contact-ion-pairs preferentially decompose to form LiF-rich and less organic components, leading to enhanced lithium Coulombic efficiency in Li||Cu cells as well as mitigating the capacity fade of Cu||LiFePO 4 and Cu||LiNi 0.8 Mn 0.1 Co 0.1 O 2 cells.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Lithium‐Containing Hybrid SEI Layer Enabling High Mass Loading and Anode‐Less Sodium Metal Batteries

The continuous rupturing and rebuilding of unstable solid electrolyte interphase (SEI) layer during cycling would block Na + diffusion and induce Na dendrite formation, ultimately limiting the practical application of high-energy-density sodium metal batteries. Herein, a hybrid SEI layer containing Li-species is dexterously constructed on the surface of sodium metal anode. Li-containing inorganic components (Li 3 N, LiF, and Li 2 CO 3 ) are introduced to stabilize the Na/electrolyte interface and enhance the mechanical and diffusion kinetic properties of the SEI layer, which can reduce the side reactions and gas generation, regulate Na + flux during cycling and promote rapid Na + migration for uniform dendrite-free Na deposition. As a result, the constructed Na symmetric cells achieve low overpotential and long cycle life of 5900, 1800, and 500 h at current densities of 3, 10, and 30 mA cm −2 , respectively. Furthermore, the full cells paired with the Na₃V₂(PO₄)₃ cathode demonstrate high specific capacity and excellent cycle stability, even at an ultra-high cathode loading of 39.3 mg cm −2 and a low N/P ratio (negative/positive electrode capacity ratio of 1.21).

Diffusion kinetic↗

Deciphering the Evolution of Current Distribution in Hybrid Silver Vanadium Oxide / Carbon Monofluoride Cathodes within Lithium Primary Batteries

For batteries to function effectively all active material must be accessible requiring both electron and ion transport to each particle. A common approach to generating the needed conductive network is the addition of carbon to create a composite electrode. An alternative approach is the electrochemically induced formation of conductive reaction products where the electrochemically generated materials are in intimate contact with the active material contributing to effective connection of each active particle. Furthermore, this study probes silver vanadium oxide (Ag 2 V 4 O 11 , SVO), carbon monofluoride (CF x ), and hybrid SVO/CF x electrodes in lithium batteries. Ex situ XRD identifies Ag 0 as a reduction product from SVO and LiF from CF x that can be followed as a function of depth-of-discharge (DOD). Spatially-resolved operando energy dispersive x-ray diffraction reveals that the presence of SVO alleviates reaction heterogeneity in the electrodes which are electron transfer limited in the absence of sufficient Ag 0 . Synchrotron X-ray tomography on discharged cathodes reveals the distribution of silver particles where the particles are more closely spaced near the current collector indicating multiple nucleation sites for their formation. Finally, operando isothermal microcalorimetry is used to determine the heat dissipation of the parent and hybrid battery types. Using material enthalpy potentials, we determine the current distribution between the two active materials for the discharging hybrid cathode adding further insight to the diffraction analysis. Taken together, these results provide a comprehensive understanding of hybrid SVO/CF x cathodes and give guidance on optimal compositions that balance power and energy density considerations.

36 MATERIALS SCIENCE↗

Probing the Li 4 Ti 5 O 12 Interface Upon Lithium Uptake by Operando Small Angle Neutron Scattering

The formation of a solid–electrolyte interphase (SEI) on the surface of Li 4 Ti 5 O 12 (LTO) has become a highly controversial topic, with arguments for it and against it. However, prior studies supporting the formation of an SEI layer have typically suggested that a layer forms upon cycling of a cell, although the layer is probed after disassembling. In this study, cubic mesostructured LTO is synthesized with crystallite domain sizes between 3 and 4 nm and uniform pores with diameters ≤8 nm. The mean pore size is controlled between 4–8 nm through the use of a triblock amphipathic copolymer with a tunable hydrophobic block as template and by thermal treatment. The LTO morphology obtained is spherical and evolves upon heat treatment. We report these materials show excellent electrochemical performance, including high rate capability and capacity retention. The LTO material is subjected to operando small-angle neutron scattering and X-ray photoelectron spectroscopy experiments, which reveal that the highly debated SEI forms at potentials as high as 2.2 V, first as a LiF-rich layer and subsequently by the growth of a carbonaceous layer. These SEI products form first on the smaller pores before forming on the mesopores.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Extreme Fast-Charging of Lithium-Ion Cells: Effect on Anode and Electrolyte

In this study, the effects of charge rate in coin cells containing NMC532/1506-Tgraphite are investigated. The cells are cycled at room temperature using charge rates of 1-, 2-, 4-, and 8-C and discharged at the 1-C rate for 50 cycles. The amounts of lithium and LiF are found to be highly correlated with charge time. Three decomposition products are identified in the organic electrolyte. The proposed, empirical formulae for these compounds are C 14 H 33 O 15 P 3 , C 16 H 37 O 15 P 3 , and C 11 H 22 O 7 PF; all are most likely organophosphates formed by the reaction of organic electrolyte decomposition products with LiPF 6 or P(=O)F 3 . The relative concentrations of these organics do not display sensitivity to charge rate. These results imply that a new performance fade mechanism is not introduced by electrolyte decomposition.

25 ENERGY STORAGE↗

Investigation of Corrosion Behavior of Carbide Phase Strengthened Nickel‐Based Alloy in Molten Fluoride Salt

The corrosion behavior of a high creep strength carbide-phase strengthened Ni-based alloy in molten FLiNaK (LiF-NaF-KF: 46.5-11.5-42 mol%) salt in the temperature range of 700°C–750°C has been investigated as a part of the development of structural alloys for fluoride salt-based molten salt reactors (MSRs). The alloy composition was designed based on Hastelloy-N, but with the goal of improving creep strength. Cr depletion depth, a measure of corrosion, was observed to be single micrometers after several hundred hours of corrosion testing. Sequential corrosion testing involving testing of pre-tested samples in fresh salt coupled with SEM-EDS, scanning transmission electron microscopy (STEM) examinations and thermodynamic and kinetic modeling, suggest that the corrosion rate at the alloy-salt interface is governed by diffusion of elements from the alloy bulk to the surface. The carbide phases in the corrosion-tested sample microstructure were identified to be largely M 6 C-type Mo-rich carbides and MC-type mixed carbides. Atom probe tomography (APT) showed some partitioning of Cr and Ti to the carbide phase and showed the carbide phases to be stable at the salt-facing surface.

Gordon, Ryan [Univ. of Wisconsin, Madison, WI (Uni↗

Delineating the Impact of Diluent on High-Concentration Electrolytes for Developing High-Voltage LiNi 0.5 Mn 1.5 O 4 Spinel Cathode

LiNi 0.5 Mn 1.5 O 4 (LNMO) is a high-voltage spinel cathode with low nickel content, making it an attractive candidate for next-generation lithium-ion batteries (LIBs). However, its application is limited by interfacial instability with conventional carbonate-based electrolytes at high voltages. In this work, a localized saturated electrolyte (LSE) capable of stably operating up to 4.85 V is investigated. Molecular dynamics simulations and Fourier transform infrared spectroscopy reveal that adding “non-solvating” 1,1,2,2-tetrafluoroethyl-2,2,3,3-tetrafluoropropyl ether diluent in the saturated electrolyte, more PF 6 − anions are present in the first solvation shell of Li + , at the expense of solvent molecules. This tailored solvation environment promotes the formation of a robust, LiF-rich cathode-electrolyte interphase that mitigates transition metal dissolution and parasitic side reactions. The optimized LSE enables excellent cycling performance, with 95% capacity retention in Li|LNMO half-cells after 100 cycles and 94% retention in Li 4 Ti 5 O 12 |LNMO full cells after 250 cycles, even at a practically relevant LNMO cathode loading of ≈15 mg cm −2 . In conclusion, these results highlight the benefits of electrolyte engineering and solvation structure control in advancing high-voltage LIB technologies.

LNMO cathode↗

Boron-Based Neutron Scintillator Screen Characterization with X-Rays and Neutrons

Recent work on boron-based neutron scintillator screens suggests these screens can offer superior performance when compared to commonly used screens. Borated neutron scintillator screens perform well in terms of light output (5-6 times greater than a standard Gadox screen) and detection effi-ciency (larger than standard LiF+ZnS screens). However, previously manu-factured boron-based screens have exhibited non-uniform surface coating and a poor mixture between phosphor and converter particles. The objective of this work was to evaluate newly fabricated scintillator screens to deter-mine if enhanced fabrication methods produced a more homogeneous distribution between neutron converter and scintillation phosphor particles. Uniformity of scintillator material deposition was also inspected. This new iteration of screens appeared more uniform than previous generations with the new coating method improving surface chemistry and scintillator material homogeneity. Additionally, a new methodology for screen characterization, involving the correlation of a neutron image taken with a borated scintillator screen to X-ray computed tomography of that same screen, was demonstrated to elucidate a relationship between scintillator screen thickness and relative light output of the screen under neutron exposure. This method suggested that the ideal thickness of scintillator material was ~150 µm to maximize light output of the screen.

36 - MATERIALS SCIENCE↗

Exploring Fission–Fusion Synergies to Accelerate Compatibility Understanding

To address the significant commercial interest in fusion energy, it will be necessary to accelerate the compatibility research associated with liquid breeders including Li, eutectic Pb–Li and LiF-BeF 2 (FLiBe) molten salt. Particularly for FLiBe, compatibility understanding is limited especially for fusion relevant materials such as reduced activation ferritic-martensitic steels, SiC and V alloys. The historical knowledge associated with molten salt reactors (MSRs) and recent work to commercialize MSRs can benefit fusion research. Recent experimental and modeling work has improved understanding and this knowledge can be applied to fusion relevant materials. For liquid metals (LMs), the comparisons to Li and Pb–Li are less direct but nevertheless can help guide the pathway toward commercialization. For Pb–Li, Al-rich coatings have been shown to inhibit dissolution and potentially increase operating temperatures. For commercialization, the experience with sensors and on-line cleanup can help guide future developments. Thus, it is worth considering the potential for fission-related research with LMs and molten salts to help accelerate fusion research.

36 MATERIALS SCIENCE↗

Assessing Stainless Steel Compatibility in Flowing FLiBe Salt

To address the considerable interest in LiF-BeF 2 (FLiBe) compatibility for fission and fusion reactor applications, static and flowing compatibility experiments were conducted to assess the compatibility with type 316H stainless steel. In static testing at 550° and 650 °C, small mass changes were measured and posttest characterization of the FLiBe showed increased levels of Fe, Cr, Ni and Mn in the salt. Adding Be in the static salt test reduced the dissolution of Fe and Ni. Further, an initial assessment of mass transfer in flowing FLiBe without a Be addition was conducted using a monometallic 316H thermal convection loop (TCL) operated for 1000 h with a peak temperature of 650 °C. Similar to prior results in flowing FLiNaK salt, the 316H specimens exhibited small mass losses in the hot leg. Posttest characterization of the 316H specimens suggested Cr surface depletion in the hot and cold legs and possibly Fe deposition in the cold leg. To further understand this behavior, Cr and Fe dissolution was measured in static FLiBe at 550–650 °C.

316H stainless steel↗

A neutron tomography study to visualize fluoride salt (FLiNaK) intrusion in nuclear-grade graphite

Manufactured graphite is a preferred material for in-core components of molten salt reactors and fluoride salt-cooled high-temperature reactors, which are in permanent contact with liquid salts. However, owing to the porous nature of nuclear graphite, under certain conditions, molten salts may intrude graphite's pores and affect graphite's properties and functionality. Therefore, a better understanding of molten salt intrusion (distribution across sample cross section and penetration depth) is needed to assess its effects. Here, in this work, we have demonstrated the use of neutron imaging (computed tomography) in the evaluation of salt penetration and distribution of a wide range of graphite grades with diverse microstructures that have been subjected to FLiNaK (LiF–NaF–KF) intrusion at 750 °C and 5 bar pressure for 12 h. Because of the great neutron attenuation contrast from scattering and adsorption between Li (from FLiNaK) and the graphite matrix, we have obtained direct visualization of FLiNaK salt distribution in the salt-impregnated graphites for the first time. Three-dimensional reconstructed images and cross-sectional concentration profiles demonstrate that salt penetration and density distribution are greatly dependent on the microstructural properties of the graphite grade.

22 GENERAL STUDIES OF NUCLEAR REACTORS↗

Viewing is understanding: Graphite microstructure effects on infiltrated molten salt distribution revealed by 3D neutron tomography

Molten salt infiltration in the pore network of nuclear graphite may cause unwanted changes to graphite's local structure and mechanical and thermal properties. A detailed and comprehensive understanding of molten salt intrusion (distribution across sample cross section and penetration depth) is needed to assess its effects. Here, in this work, we report on an improved methodology for the use of neutron imaging (computed tomography) to evaluate salt penetration and distribution of a wide range of graphite grades with diverse microstructures. Neutron tomography data were acquired on the same graphite sample before and after salt intrusion; the 3D reconstructed volumes were digitally co-registered and subtracted. The difference in neutron attenuation coefficient represents direct visualization of FLiNaK (LiF–NaF–KF) salt distribution in the salt-impregnated graphite samples. This improved methodology was applied to investigate the effect of exposure times (12 h and 336 h) and of graphite microstructure when exposed to FLiNaK at 750 °C and 3 bar (gauge) pressure, starting from flowing argon at near atmospheric pressure. The results show that medium-grained and fine-grained graphites evolve to equilibrium at significantly different rates: fast salt uptake in medium-grained graphites produces salt deposits throughout the volume of graphite specimens, whereas salt infiltration in fine-grained graphites is much slower and limited to exposed surfaces.

FLiNaK infiltration↗