Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “Layered oxides”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 217 records · Page 12

Unraveling Na and F coupling effects in stabilizing Li, Mn-rich layered oxide cathodes via local ordering modification

Regardless of the prevailing capacity and energy density of lithium, manganese-rich layered oxide (LMR-NMC) cathodes, continuous decay of voltage and overall energy density during cycling hinders this material from commercialization in Li-ion batteries. Although significant work focuses on single doping of Na and F, analysis in portraying the benefit of these ions in diminishing the structural distortion during activation cycle is in doubt. In this study, the effects of co-doping Na and F into the LMR-NMC structure in stabilizing the structure and mitigating oxygen loss during the first cycle are closely examined via in situ x-ray measurements. Na and F co-doping shows a 30% lower degree of Li + /Ni 2+ mixing in the Li layer (C2/m structure), 50% reduced Debye-Waller factor of Mn-O bonding, increase reversible TM migration, and faster Li diffusion relative to the pristine material. Due to the utilization of Ni redox chemistry below 4.4 V, less oxygen redox is required for charge compensation at high voltage. This study offers the first instance to quantitatively evaluate the effects of co-doping Na and F in LMR-NMC cathode in order to minimize voltage degradation by altering the local ordering of O3-type structure, which may rationalize strategies to overcome the issues of the material.

25 ENERGY STORAGE↗

First-Cycle Simulation for Li-Rich Layered Oxide Cathode Material x Li 2 MnO 3 • (1- x )Li M O 2 ( x = 0.4)

Here, lithium-rich layered oxides (LRLO) x Li 2 MnO 3 • (1- x )Li M O 2 continue to attract attention owing to their promise of high capacity and energy density as lithium-ion battery cathodes, despite the degradation of atomic structure and energy density (voltage fade) with cycling. First-principles DFT calculations for the model systems M = Co and M = Mn 0.5 Ni 0.5 provide insights into the atomic-scale transformations in the bulk during the first charge and discharge of LRLO. The simulations were performed with the VASP code at the GGA+ U level. Molecular dynamics simulations were conducted at T = 1000 K (charge) and 2000 K (discharge) to accelerate the dynamics. Considerable Co migration to the Li layer occurs during the first charge for the system with M = Co, but the Li M O 2 component remains substantially intact for the system with M = Mn 0.5 Ni 0.5 . First-charge oxygen dimerization in the M = Co system occurs in both the Li M O 2 and the Li 2 MnO 3 components of the material, and exceeds than for M = Mn 0.5 Ni 0.5 , where dimerization is essentially confined to the Li 2 MnO 3 component. About half of the oxygen dimers created during the voltage plateau dissociate during the first discharge. Analysis of the redox suggests that some Mn 3+ is generated during the first charge for the system M = Co.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Effect of oxide layer growth conditions on radiation detection performance of Ni/SiO 2 /epi-4H-SiC MOS capacitors

We report high resolution radiation detection has been demonstrated using Ni/SiO2/n-4H-SiC metal-oxidesemiconductor vertical capacitors fabricated using highly crystalline 4H-SiC epilayers. The oxide layers have been grown thermally using two different approaches: i) in-air, and ii) oxygen-ambience oxidation. The devices fabricated using the former method exhibited dark currents one order of magnitude higher than that in the latter. The observed difference has been attributed to the back-contact series resistance and capacitance. Regardless of the difference in the device parameters, detectors prepared using both of the methods exhibited very high energy resolutions of ≤ 0.5% for 5486 keV alpha particles emitted by an 241Am radioisotope. Capacitance mode deep level transient spectroscopic (DLTS) studies revealed similar type of electrically active defects along with Z1/2 and EH5 deep level defects in both the types of devices. The DLTS scans also revealed positive polarity peaks in these devices which indicate emission from minority carrier trap centers. The activation energy corresponding to the peak was found to be ~1.2 eV which has been assigned to HK3 defects responsible for hole trapping in 4H-SiC. The possibility of appearance of the positive peak due to non-negligible impedance of the back-contact has been ruled out based on the observation that the centroid of the observed peak did not change with detectors having different device parameters.

36 MATERIALS SCIENCE↗

Distinction between Intrinsic and X-ray-Induced Oxidized Oxygen States in Li-Rich 3d Layered Oxides and LiAlO 2

Resonant inelastic X-ray scattering (RIXS) at the O K-edge is considered a prime technique to identify bulk oxidized oxygen formation, but its fundamental interpretation is not straightforward. In this study, we intentionally induce RIXS signatures of oxidized oxygen upon beam exposure in LiAlO 2 polymorphs that are easily distinguished because of their wide band gaps. After careful consideration of beam exposure effects on Li[Li 0.144 Ni 0.136 Mn 0.544 Co 0.136 ]O 2 (LR-NMC), we conclude that oxidized oxygen features are inherent at high states of charge and are lost upon aggressive beam exposure. The extracted oxidized oxygen line shapes from our X-ray irradiation studies for both LiAlO 2 (induced) and LR-NMC (inherent) are found to have an additional oxidized oxygen RIXS feature not observed in O 2 gas studies. This study highlights the unique insight of O K-edge RIXS into determining the nature and stability of oxidized oxygen states.

36 MATERIALS SCIENCE↗

Whole-Voltage-Range Solid-Solution Reaction in Layered Oxide Cathode of Sodium-Ion Batteries

Layered manganese-based oxides (LMOs) are promising cathode materials for sodium-ion batteries (SIBs) due to their versatile structures. However, the Jahn–Teller effect of Mn 3+ induces severe distortion of MnO 6 octahedra, and the resultant low symmetry is responsible for the gliding of MnO 2 layers and then inferior multiple-phase transitions upon Na + extraction/insertion. Here, hexagonal P2-Na 0.643 Li 0.078 Mn 0.827 Ti 0.095 O 2 is synthesized through the incorporation of Li and Ti into the distorted orthorhombic P'2-Na 0.67 MnO 2 to function as a phase-transition-free oxide cathode. Further, it is revealed that Li in both the transition-metal and Na layers enhances the covalency of Mn–O bonds and allows degeneracy of Mn 3d e g orbitals to favor the formation of hexagonal phase, and the high strength of Ti–O bonds reduces the electrostatic interaction between Na and O for suppressed Na + /vacancy rearrangements. These collectively lead to a whole-voltage-range solid-solution reaction between 1.8 and 4.3 V with a small volume variation of 1.49%. This rewards its excellent cycling stability (capacity retention of 90% after 500 cycles) and rate capability (89 mAh g -1 at 2000 mA g -1 ).

25 ENERGY STORAGE↗

Simulation of First-Charge Oxygen-Dimerization and Mn-Migration in Li-Rich Layered Oxides x Li 2 MnO 3 ·(1 – x )Li M O 2 and Implications for Voltage Fade

The instabilities of Li-rich layered oxide xLi 2 MnO 3 •(1-x)LiMO 2 (lithium-ion-battery cathode materials) during the first charge are investigated using first-principles dynamical simulation. To complement our earlier simulations for (x = 0.4, M = Ni 0.5 Mn 0.5 ), we address here: pure Li 2 MnO 3 ; small x; M compositions that include Co; a composite with Co spinel: Li 2 MnO 3 •Li 2 M 2 O 4 ; a Li 2 MnO 3 slab. Lastly, we discuss how the threshold fraction f of Li 2(1-f) MnO 3 delithiation at which instabilities occur at the surface, fth(surface), differs from that in the bulk, f th (bulk). Approaches to inhibit voltage fade are discussed.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Platinum-induced structural collapse in layered oxide polycrystalline films

Effect of a platinum bottom electrode on the SrBi{sub 5}Fe{sub 1−x}Co{sub x}Ti{sub 4}O{sub 18} layered oxide polycrystalline films was systematically studied. The doped cobalt ions react with the platinum to form a secondary phase of PtCoO{sub 2}, which has a typical Delafossite structure with a weak antiferromagnetism and an exceptionally high in-plane electrical conductivity. Formation of PtCoO{sub 2} at the interface partially consumes the cobalt dopant and leads to the structural collapsing from 5 to 4 layers, which was confirmed by X-ray diffraction and high resolution transmission electron microscopy measurements. Considering the weak magnetic contribution from PtCoO{sub 2}, the observed ferromagnetism should be intrinsic of the Aurivillius compounds. Ferroelectric properties were also indicated by the piezoresponse force microscopy. In this work, the platinum induced secondary phase at the interface was observed, which has a strong impact on Aurivillius structural configuration and thus the ferromagnetic and ferroelectric properties.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Catalytically enhanced thermal decomposition of chemically grown silicon oxide layers on Si(001)

The thermal decomposition of Si dioxide layers formed by wet chemical treatment on Si(001) has been studied by low-energy electron microscopy. Independent nucleations of voids occur into the Si oxide layers that open by reaction at the void periphery. Depending on the voids, the reaction rates exhibit large differences via the occurrence of a nonlinear growth of the void radius. This non-steady state regime is attributed to the accumulation of defects and silicon hydroxyl species at the SiO{sub 2}/Si interface that enhances the silicon oxide decomposition at the void periphery.

71 CLASSICAL AND QUANTUM MECHANICS, GENERAL PHYSIC↗

Probing Thermal Stability of Li-Ion Battery Ni-Rich Layered Oxide Cathodes by means of Operando Gas Analysis and Neutron Diffraction

Thermal stability is a crucial parameter that must be considered within the overall performance metrics of Ni-rich layered oxide cathodes. While the intrinsic structural stability of the cathode materials under thermal conditions is important, it is also critical to consider their reaction with electrolytes. In this study, operando gas analysis, ex situ neutron diffraction, and differential scanning calorimetry were combined to give a broader picture of the thermal stability of Ni-rich NMC cathodes. Li 1– x Ni 0.8 Mn 0.1 Co 0.1 O 2 (NMC811) composite materials with four different states of charge were investigated with and without the presence of an electrolyte. It has been found that electrolyte can greatly accelerate both the structural and thermal decomposition of the cathode materials. A higher state of charge will also make cathode materials more susceptible to thermal shock. Without an electrolyte, O 2 release inducing a structural change from layered to rock salt was the major observation during thermal runaway. However, all samples retained some levels of layered structure after annealing up to 300 °C without the electrolyte. In comparison, almost all the O3-type layered phase transformed to the rock-salt phase for the cathode materials heated with the electrolyte at the same experimental conditions. Moreover, the amount of CO 2 increased by nearly two orders of magnitude when annealing cathode materials with electrolyte in operando gas analysis experiments. More delithiated NMC811 samples released larger amounts of CO 2 at earlier onset temperatures, resonating well with the differential scanning calorimetry (DSC) results showing that more delithiated samples release more heat during thermal shock.

25 ENERGY STORAGE↗

The Formation of Oxide Layers on a Titanium Surface by Irradiation with Femtosecond Laser Pulses

By subjecting technical grade titanium to irradiation with femtosecond laser pulses with high energy density, we create a microporous nanocrystalline oxide layer with a thickness of ∼50 μm on its surface. The structure and phase composition of the modified surface layers are studied using X-ray diffraction and high-resolution scanning and transmission electron microscopies.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

An Ordered P2/P3 Composite Layered Oxide Cathode with Long Cycle Life in Sodium-Ion Batteries

Developing stable cathode materials represents a crucial step toward long-life sodium-ion batteries. P2-type layered oxides are important as cathodes for their reversibility, but their long-term performance in full cells remains a key challenge. Herein, we report Na 0.75 Co 0.125 Cu 0.125 Fe 0.125 Ni 0.125 Mn 0.5 O 2 with an intergrowth of ordered P2 and P3 phases, studied by neutron diffraction and Rietveld refinement. A stable electrochemical performance is achieved in Na half cells with 100% capacity retention at a rate of C/10 after 100 cycles (initial capacity of 90 mAh/g), 96% capacity retention at a rate of 1 C after 500 cycles (initial capacity of 70 mAh/g), and 85% capacity retention at a rate of 5 C after 1000 cycles (initial capacity of 55 mAh/g). Stable full cell performance is achieved with 84.2% capacity retention after 1000 cycles at a rate of 1 C. Synchrotron X-ray diffraction, spectroscopy, and imaging are applied to elucidate the relationship between chemical/structural evolution and battery performance. A reversible local and global structural evolution is observed during initial cycles. Meanwhile, the challenges with enabling prolonged cycling (beyond 1000 cycles) may be associated with Fe dissolution and formation of a copper oxide phase. This study implies that cathodes with complex chemical and structural formations may stabilize electrochemical performance and highlights the importance of decoupling the contribution of each transition metal to performance degradation.

25 ENERGY STORAGE↗

Insights into the Performance Degradation of Oxygen-Type Manganese-Rich Layered Oxide Cathodes for High-Voltage Sodium-Ion Batteries

The cost of batteries is becoming as important as the energy density for large-scale electrochemical energy storage application. Sodium manganese-rich layered oxides (P-type and O-type) are thus one of the promising cathode materials for rechargeable batteries because of the relatively low cost of manganese and sodium. The O-type cathodes are more promising for practical application owing to their high sodium-ion stoichiometry. However, most of these materials suffer from rapid capacity decay during high-voltage cycling. We used synchrotron X-ray probes coupled with electrochemical techniques to disclose the structural evolution of α-NaMnO 2 during solid-state synthesis and electrochemical cycling. During high-voltage cycling, a substantial increase of interfacial microstrain from both stacking faults and Mn cation migration was found to pin down this material’s layered structures and simultaneously block the diffusion pathways of Na + , thus leading to the performance degradation. The findings presented in this work can guide future development of high-performance sodium-ion cathode materials.

25 ENERGY STORAGE↗

Lithium-Ion Mobility in Layered Oxide Li 2 (La 0.75 Li 0.25 )(Ta 1.5 Ti 0.5 )O 7 Containing Lithium on both Intra and Inter‐Stack Positions

With the aid of neutron diffraction and electrochemical impedance spectroscopy, we have demonstrated the effect of the increase in lithium concentration and distribution on Li-ion conductivity. This has been done through the synthesis of a layered oxide Li 2 (La 0.75 Li 0.25 )(Ta 1.5 Ti 0.5 )O 7 , with the so-called Ruddlesden-Popper type structure, where bilayer stacks of (Ta/Ti)O 6 octahedra are separated by lithium ions, located in inter-stack spaces. There are also intra-stack spaces that are occupied by a mixture of La and Li, as confirmed by neutron diffraction. The distribution of lithium over both inter- and intra-stack positions leads to the enhancement of Li-ion conductivity in Li 2 (La 0.75 Li 0.25 )(Ta 1.5 Ti 0.5 )O 7 compared to Li 2 La(TaTi)O 7 , which has a lower concentration of lithium ions, located only in inter-stack spaces. Furthermore, the analyses of real and imaginary components of electrochemical impedance data confirm the enhanced mobility of ions in Li 2 (La 0.75 Li 0.25 )(Ta 1.5 Ti 0.5 )O 7 . While the Li-ion conductivity needs further improvement for practical applications, the success of the strategy implemented in this work offers a useful methodology for the design of layered ionic conductors.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Suppressing Atmospheric Degradation of Sulfide-Based Solid Electrolytes via Ultrathin Metal Oxide Layers

Sulfide-based solid-state electrolytes (SSEs) are promising materials with superior Li-ion conductivity; however, their poor atmospheric stability limits commercial manufacturing at scale. Here, we investigate the impact of ultrathin metal oxide layers deposited via atomic layer deposition (ALD) on the stability of Li 6 PS 5 Cl (LPSCl). Al 2 O 3 layers grown directly on LPSCl particles significantly stabilize the surface chemistry and Li-ion transport properties relative to uncoated material upon exposure to both an ambient atmosphere (22% relative humidity, RH) and humidified O 2 (100% RH). Detailed investigations indicate that coatings impede the surface and bulk degradation kinetics of exposed materials, even for coatings as thin as ∼1 Å. Furthermore, this suggests that stabilization is due to more than just a physical barrier. Shifts in valence band edge positions of coated LPSCl indicate that ALD coatings alter the surface electronic structure and resulting oxidation tendency of underlying LPSCl, suggesting new avenues to improving the environmental stability of sulfide SSEs.

Atmospheric chemistry↗

Boosting electrochemical reaction and suppressing phase transition with a high-entropy O3-type layered oxide for sodium-ion batteries

Complex phase transitions induced by interlayer slides in layered cathode materials lead to poor cycling stability and rate capability for sodium-ion batteries. Herein, we design and prepare a new six-component high-entropy oxide (HEO) layered cathode O3–Na(Fe 0.2 Co 0.2 Ni 0.2 Ti 0.2 Sn 0.1 Li 0.1 )O 2 to enable highly reversible electrochemical reaction and phase-transition behavior. The HEO cathode exhibits good cycling performance (capacity retention of ~81% after 100 cycles at 0.5C) and outstanding rate capability (capacity of ~81 mA h g –1 at 2.0C) due to the higher sodium diffusion coefficient (above 5.75 × 10 –11 cm 2 s –1 ) than most reported O3-type cathodes. Moreover, the high-entropy cathode has superior compatibility with the hard carbon anode and delivers a specific capacity of 90.4 mA h g –1 (energy density of ~267.5 W h kg –1 ). Ex situ X-ray diffraction proves that the high-entropy designing effectively suppresses the intermediate phase change to achieve reversible O3–P3 phase evolution, and in turn stabilizes the layered structure. X-ray absorption spectroscopy and Mössbauer spectrum of 57 Fe suggest that Ni 2+ /Ni 3.5+ , Co 3+ /Co 3.5+ , and part of Fe 3+ /Fe 3.5+ redox reaction contribute the charge compensation. Finally, the enhanced performance can be attributed to the disordered distribution of multi-component transition metals in HEO suppressing the ordering of electric charges and sodium vacancies, thereby inhibiting the interlayer slide and phase transition.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Layered Oxide Cathodes for Li-Ion Batteries: Oxygen Loss and Vacancy Evolution

Loss of oxygen in layered transition metal oxides is a major reason for the structural degradation and thus the fade of electrochemical performance in the cathodes for Li-ion batteries. Via in-situ transmission electron microscopy observations of LiNi 0.80 Co 0.15 Al 0.05 O 2 (NCA), we found that the oxygen loss in the layered cathode is a two-stage process with distinct release rates. The initial rapid oxygen loss generates a high concentration of oxygen vacancies that results in the formation of an amorphized, vacancy-containing rock-salt layer in the surface. In the second stage, the slower rate of oxygen loss allows recrystallization of this defective phase via coalescing of atomic oxygen vacancies, which results in the formation of a cavity-containing surface layer with a crystalline rock-salt structure over the layered phase in the bulk. Comparison of the in-situ results with electrochemically cycled NCA cathodes confirms this two-stage process of oxygen loss. Furthermore, these results provide unprecedented microscopic details regarding the structural degradation of layered oxides arising from oxygen loss and have broader implications in manipulating the oxygen activity in the electrode.

36 MATERIALS SCIENCE↗

Toward the Stable and Reversible Lattice Oxygen Redox in Li-Rich Layered Oxides

Conventional wisdom on utilizing cation redox in intercalation materials for energy storage has been challenged by a new class of cathode materials where oxygen anions actively participate in the reversible electrochemical reaction. This type of Li-rich layered oxides (LRLO) have captured great interests in the field of energy storage materials as they are considered as one of the most promising cathode materials for future high energy density lithium-ion and lithium metal batteries. However, the activation of solid-state oxygen redox reaction usually causes some detrimental effects on the electrochemical performance (e.g., O 2 loss, voltage fade) preventing the practical application of LRLO (Y. S. Meng et al., Nature Energy, 2018, 3, 641-647; X. Yu et al., Nature Energy, 2018, 3, 690-698). Till now, the charge-compensation mechanism associated with oxygen reduction/oxidation is still under fierce debate. For instance, J.M. Tarascon et al. proposed the presence of peroxo-like species (O 2 n- , O-O: 2.45 Å) in lattice oxygen redox based on the research results of 4d/5d-TM LRLO (Science, 2015, 350, 1516-1521; Nature Materials, 2017, 16, 580-586). In contrast, P. Bruce et al. clearly demonstrated that there is no peroxide species formed in 3d-TM LRLO (Nature Chemistry, 2016, 8, 684-691). The controversial viewpoints regarding oxygen reduction/oxidation at solid state may be originated from the intrinsic complexity of this class of materials and the limitations of the characterization techniques. Our work reveals the origin of stable and reversible lattice oxygen redox in 3d TM LRLO, specifically, the localized structure distortion (i.e., short O-O pairs) accompanying the oxygen redox is favorable for the stability of the average layered lattice structure, maintaining the high-voltage character and topotactic structure-reversibility of LRLO. With a model compound (Li 1.2 Mn 0.54 Co 0.13 Ni 0.13 O 2 ), we for the first time observe a local occurrence of short O-O pair (~2.39 Å) concomitant with the lattice oxygen redox via neutron pair distribution function. It was found that the distance of this short O-O pair is very similar to that of O-O dimer in peroxo-like species, but our quantum mechanical calculation results suggest that the bonding nature of this short O-O pair (in which potential π-type overlap dominated) is quite different from that of peroxo-like O-O dimer (in which σ-type bond formed). Based on these understandings in our work, an optimization guidance for LRLO is unambiguously presented: designing a robust layered structure with high-covalency TMs while constructing a flexible local structure (e.g., honeycomb structure) with high-ionicity TMs to accommodate the local distortion induced by oxygen redox, thus achieving the reversible high energy density in LRLO.

Zhang, Minghao↗

Insights into the Crossover Effects in Cells with High‐Nickel Layered Oxide Cathodes and Silicon/Graphite Composite Anodes

Abstract Silicon anodes are regarded as one of the most promising alternatives to graphite (Gr) anodes due to their ultrahigh capacity, abundance, and low cost. Coupling Si‐based anodes with high‐nickel layered oxide cathodes LiNi x Mn y Co 1− x − y O 2 (NMC, x ≥ 0.8) can enhance the driving range for electric vehicles. Transition‐metal (TM) ion dissolution and deposition has been a long‐known failure mode for Gr‐based lithium‐ion batteries. However, the mechanistic insight associated with TM ion deposition on Si‐based anodes has rarely been reported. Herein, the impact of in situ deposited TM ions on SiO x /Gr composite anodes and the individual influences of Ni, Mn, and Co on the structural and electrochemical stability along with the underlying degradation mechanisms are presented. TM ion dissolution causes a greater deleterious impact on Si than on Gr, with different TM ions exhibiting different influences on anode‐electrolyte interphase formation. Specifically, Ni deposit induces more aggressive salt decomposition; Co deposit has negligible effect on salt decomposition, but significantly accelerates solvent decomposition; and Mn deposit aggravates both salt and solvent decompositions, resulting in worse full cell performance. The extent of degradation decreases in the order Mn 2+ > Ni 2+ > Co 2+ . The systematic comparisons presented can guide further development of high energy systems.

Zhang, Xianhui↗