Sintered MRE 2 (Fe, Co) 14 B magnets by DyF 3 blending or diffusion treatment were investigated. “Base-line” magnets with a thickness of 1.5 mm were coated (painted) with DyF 3 powder and heated to promote Dy diffusion at 800–900 °C, i.e., “Diffusion” magnets. For comparison, the magnet alloy powder for making Base-line magnets was blended with 3–5 wt.% DyF 3 powder and then made into sintered magnets, i.e., “Blended” magnets. The coercivity and (BH) max of Base-line magnets were 9.7 kOe and 32.7 MGOe, respectively, while the coercivity of Diffusion magnets was increased to 15 kOe and the (BH) max was nearly unchanged at 31.4 MGOe. Blended magnets with 5 wt% DyF 3 had a coercivity of 17.8 kOe, but the (BH) max was reduced to 25.4 MGOe, due to a considerable reduction of remanence. The total Dy concentration in the MRE 2 (Fe, Co) 14 B Diffusion magnets with a β value of -0.5%/°C was 5.3 wt%, while typical commercial Nd-based Nd 2 Fe 14 B magnets require at least 7.5 wt% Dy to achieve the same β. Therefore, the MRE 2 (Fe, Co) 14 B Diffusion magnets exhibited better temperature stability.