Probabilistic Composite Design

Probabilistic composite design is described in terms of a computational simulation. This simulation tracks probabilistically the composite design evolution from constituent materials, fabrication process, through composite mechanics and structural components. Comparisons with experimental data are provided to illustrate selection of probabilistic design allowables, test methods/specimen guidelines, and identification of in situ versus pristine strength, For example, results show that: in situ fiber tensile strength is 90% of its pristine strength; flat-wise long-tapered specimens are most suitable for setting ply tensile strength allowables: a composite radome can be designed with a reliability of 0.999999; and laminate fatigue exhibits wide-spread scatter at 90% cyclic-stress to static-strength ratios.

Chamis, Christos C.↗

Interfacial adhesion of carbon fibers

Relative adhesion strengths between AS4, AS1, and XAS carbon fibers and thermoplastic polymers were determined using the embedded single filament test. Polymers studied included polycarbonate, polyphenylene oxide, polyetherimide, polysulfone, polyphenylene oxide blends with polystyrene, and polycarbonate blends with a polycarbonate polysiloxane block copolymer. Fiber surface treatments and sizings improved adhesion somewhat, but adhesion remained well below levels obtained with epoxy matrices. An explanation for the differences between the Hercules and Grafil fibers was sought using X ray photon spectroscopy, wetting, scanning electron microscopy and thermal desorption analysis.

Bascom, Willard D.↗

Microstructural, Strength, and Creep Characterization of Sylramic™, Sylramic™-iBN and Super Sylramic™-iBN SiC Fibers

The chemical composition, microstructure, strength, and thermal stability of polymer-derived Sylramic™ SiC fibers fabricated by Dow Corning and COI Ceramics, Inc., and nitrogen-treated Sylramic™ SiC fibers, referred to as Sylramic™-iBN and Super Sylramic™-iBN SiC fibers, were investigated and compared. The baseline Sylramic™ SiC fibers fabricated by both vendors as well as the nitrogen-treated Sylramic™ SiC fibers are composed mostly of β-SiC (~97 wt%) with small amounts of TiB2 (~2 wt%), amorphous carbon (~1 wt%) and trace amounts of B4C. Most of the amorphous carbon is segregated at the core/interior of the fibers. Both baseline and nitrogen-treated Sylramic™ SiC fibers have similar grain size and pore size distribution, except for a thin layer of in-situ grown crystalline BN (30 to 70 nm) on the surface of Sylramic™-iBN and Super Sylramic™-iBN fibers. Wide variation in strength within a batch as well as between batches is observed in both baseline and nitrogen-treated Sylramic™ SiC fibers but both types of fibers are microstructurally stable at temperatures to 1800°C in argon and nitrogen environments compared to Nicalon™-S and Tyranno®-SA SiC fibers. Under the same creep condition, Super Sylramic™-iBN fibers show better creep resistance compared to Sylramic™, Sylramic™-iBN, Hi-Nicalon™-S, and Tyranno®-SA fibers. Possible reasons for strength variability and the mechanism of in-situ BN formation on Sylramic™ SiC fibers are discussed.

SiC fibers↗

A revisit to high-rate mode-II fracture characterization of composites with Kolsky bar techniques.

Nowadays composite materials have been extensively utilized in many military and industrial applications. For example, the newest Boeing 787 uses 50% composite (mostly carbon fiber reinforced plastic) in production. However, the weak delamination strength of fiber reinforced composites, when subjected to external impact such as ballistic impact, has been always potential serious threats to the safety of passengers. Dynamic fracture toughness is a critical indicator of the performance from delamination in such impact events. Quasi-static experimental techniques for fracture toughness have been well developed. For example, end notched flexure (ENF) technique, which is illustrated in Fig. 1, has become a typical method to determined mode-II fracture toughness for composites under quasi-static loading conditions. However, dynamic fracture characterization of composites has been challenging. This has resulted in conflictive and confusing conclusions in regard to strain rate effects on fracture toughness of composites.

36 MATERIALS SCIENCE↗

Methods for producing silicon carbide architectural preforms

Methods are disclosed for producing architectural preforms and high-temperature composite structures containing high-strength ceramic fibers with reduced preforming stresses within each fiber, with an in-situ grown coating on each fiber surface, with reduced boron within the bulk of each fiber, and with improved tensile creep and rupture resistance properties for each fiber. The methods include the steps of preparing an original sample of a preform formed from a pre-selected high-strength silicon carbide ceramic fiber type, placing the original sample in a processing furnace under a pre-selected preforming stress state and thermally treating the sample in the processing furnace at a pre-selected processing temperature and hold time in a processing gas having a pre-selected composition, pressure, and flow rate. For the high-temperature composite structures, the method includes additional steps of depositing a thin interphase coating on the surface of each fiber and forming a ceramic or carbon-based matrix within the sample.

DiCarlo, James A.↗

Pendulum impact resistance of tungsten fiber/metal matrix composites.

The impact properties of copper, copper-10 nickel, and a superalloy matrix reinforced with tungsten fibers were studied. In most cases the following increased composite impact strength: increased fiber or matrix toughness, decreased fiber-matrix reaction, increased test temperature, hot working and heat treatment. Notch sensitivity was reduced by increasing fiber or matrix toughness. The effect of fiber content depended on the relative toughness of the fibers and matrix. Above 530 K a 60 volume per cent superalloy matrix composite had a greater impact strength than a turbine blade superalloy, whereas below 530 K a hot worked 56 volume per cent composite had a greater impact strength than the superalloy.

Winsa, E. A.↗

Time-Dependent Stress Rupture Strength Degradation of Hi-Nicalon Fiber-Reinforced Silicon Carbide Composites at Intermediate Temperatures

The stress rupture strength of silicon carbide fiber-reinforced silicon carbide composites with a boron nitride fiber coating decreases with time within the intermediate temperature range of 700 to 950 degree Celsius. Various theories have been proposed to explain the cause of the time-dependent stress rupture strength. The objective of this paper is to investigate the relative significance of the various theories for the time-dependent strength of silicon carbide fiber-reinforced silicon carbide composites. This is achieved through the development of a numerically based progressive failure analysis routine and through the application of the routine to simulate the composite stress rupture tests. The progressive failure routine is a time-marching routine with an iterative loop between a probability of fiber survival equation and a force equilibrium equation within each time step. Failure of the composite is assumed to initiate near a matrix crack and the progression of fiber failures occurs by global load sharing. The probability of survival equation is derived from consideration of the strength of ceramic fibers with randomly occurring and slow growing flaws as well as the mechanical interaction between the fibers and matrix near a matrix crack. The force equilibrium equation follows from the global load sharing presumption. The results of progressive failure analyses of the composite tests suggest that the relationship between time and stress-rupture strength is attributed almost entirely to the slow flaw growth within the fibers. Although other mechanisms may be present, they appear to have only a minor influence on the observed time-dependent behavior.

Progressive Failure Analysis↗

Fundamental analysis of the failure of polymer-based fiber reinforced composites

A mathematical model is described which will permit predictions of the strength of fiber reinforced composites containing known flaws to be made from the basic properties of their constituents. The approach was to embed a local heterogeneous region (LHR) surrounding the crack tip into an anisotropic elastic continuum. The model should (1) permit an explicit analysis of the micromechanical processes involved in the fracture process, and (2) remain simple enough to be useful in practical computations. Computations for arbitrary flaw size and orientation under arbitrary applied load combinations were performed from unidirectional composites with linear elastic-brittle constituent behavior. The mechanical properties were nominally those of graphite epoxy. With the rupture properties arbitrarily varied to test the capability of the model to reflect real fracture modes in fiber composites, it was shown that fiber breakage, matrix crazing, crack bridging, matrix-fiber debonding, and axial splitting can all occur during a period of (gradually) increasing load prior to catastrophic fracture. The computations reveal qualitatively the sequential nature of the stable crack process that precedes fracture.

Kanninen, M. F.↗

Discontinuous Aligned Carbon Fiber Intermediates for Automotive and Related Applications

This work focused on preferentially aligning discontinuous carbon fibers in wet-laid or air-laid processes. It is well known that aligned fibers provides higher directional strength and stiffness. Discontinuous fibers further allow higher degree of draw and formability as the gaps in the fibers allow for higher material movement. The current processes are limited in their ability to align carbon fibers during processing. The aligned fibers have several benefits - (a) in applications where chopped fibers can replace continuous fibers for targeted strength and stiffness metrics, but at a substantially reduced cost; (b) they can tolerate deeper draws than continuous fiber composites in thermo-stamping and compression molding processes; (c) they can be tailored for pultrusion and unidirectional applications. Although pultrusion is primarily a process that adopts continuous fibers, stitch bonded entangled discontinuous fibers can provide unique intermediates. This is analogous to natural coir fibers which get aligned and entangled to produce ropes/rods for example, (d) they can be processed in cross-ply and multi-directional formats, like composite laminates. In this work Neenah Paper partnered with IACMI, UT and ORNL to evaluate structure-process-property relationships with Zoltek carbon fiber. A few process parameters such as machine speed, weight basis, fiber length, effect of fiber sizing, direction of mat lay-up etc. were investigated. The produced mats were converted to thermoplastic composite laminates using polyamide 6 (PA6, nylon) resin. The specific objective of this project is to produce a wet-laid nonwoven carbon fiber mat with a high degree of unidirectional fiber alignment, using discontinuous carbon fibers. The report provides details about the processing, characterization, and lower-upper bound properties.

36 MATERIALS SCIENCE↗

Transverse Strength of SCS-6 Silicon Carbide Fibers

A diametral compression test was used to measure the transverse strength of SCS-6 SiC fibers before and after heat treatment. Subjecting fibers to diametral compression successfully produced transverse tensile failure in the form of fiber cracking along the same diametral plane in which the compressive load was applied. An analysis of the hoop stress along the diametral plane, in which the effects of the C core were included, showed that there is a large tensile hoop stress concentration in the SiC sheath at the interface between the C core and the SiC sheath, where the stress is 6.3 times greater than the stress present in a solid SiC fiber under identical loading. This high tensile hoop stress concentration promotes crack initiation near the core and significantly limits the capability of these fibers to withstand transverse compressive loading. The maximum tensile hoop stresses, located at the interface between the C core and SiC sheath, at the measured failure loads were 850 MPa for the as-received SCS-6 fiber and 1210 MPa for fibers exposed to a 1-h heat treatment at 1850°C in 138 MPa of Ar.

Jeffrey I. Eldridge↗

Strength advantages of chemically polished boron fibers before and after reaction with aluminum

In order to determine their strength potential, the fracture properties of different types of commercial boron fibers were measured before and after application of secondary strengthening treatments. The principal treatments employed were a slight chemical polish, which removed low strength surface flaws, and a heat treatment in oxygen, which contracted the fibers and thereby compressed intrinsic bulk flaws. Those fiber types most significantly strengthened were 200 to 400 micrometers (8 to 16 mil) diameter boron on tungsten fibers produced in a single chemical vapor deposition reactor. The slight polish increased average tensile strenghts from 3.4 to 4.4 CN/m2 (500 to 640 ksi) and reduced coefficients of variation from about 15 to 3 percent. The oxygen heat treatment plus slight polish further improved average strengths to 5.5 GN/m2 (800 ksi) with coefficients near 3 percent. To ascertain whether these excellent properties could be retained after fabrication of B/Al composites, as produced and polished 203 micrometers (8 mil) fibers were thinly coated with aluminum, heat treated at B/Al fabrication temperatures, and then tested in tension and flexure at room temperature. The pre-polished fibers were observed to retain their superior strengths to higher temperatures than the as-produced fibers even though both were subjected to the same detrimental reaction with aluminum.

Dicarlo, J. A.↗

Overview of SBIR Phase II Work on Hollow Graphite Fibers

Ultra-Lightweight materials are enabling for producing space based optical components and support structures. Heretofore, innovative designs using existing materials has been the approach to produce lighter-weight optical systems. Graphite fiber reinforced composites, because of their light weight, have been a material of frequent choice to produce space based optical components. Hollow graphite fibers would be lighter than standard solid graphite fibers and, thus, would save weight in optical components. The Phase I SBIR program demonstrated it is possible to produce hollow carbon fibers that have strengths up to 4.2 GPa which are equivalent to commercial fibers, and composites made from the hollow fibers had substantially equivalent composite strengths as commercial fiber composites at a 46% weight savings. The Phase II SBIR program will optimize processing and properties of the hollow carbon fiber and scale-up processing to produce sufficient fiber for fabricating a large ultra-lightweight mirror for delivery to NASA. Information presented here includes an overview of the strength of some preliminary hollow fibers, photographs of those fibers, and a short discussion of future plans.

Stallcup, Michael↗

Effect of impact damage and open holes on the compression strength of tough resin/high strain fiber laminates

Structural damage and design-based inclusions such as cutouts can reduce significantly the strength of graphite-epoxy laminates. One composite mechanics research activity at the Langley Research Center is to assess and improve the performance of composite structures in strength are common to both tension and compression loaded laminates; however, the problem associated with compression performance is the most illusive to solve. Compression failure involves both shear crippling and delamination modes. Several graphite-epoxy material systems proposed for improved damage-tolerance were studied. Material parameters included both tough resin formulations and high strain fibers.

Williams, J. G.↗

Large-diameter carbon-composite monofilaments

Large-diameter carbon composite monofilaments with high strength and high modulus were produced by pregging multifiber carbon bundles with suitable organic resins and pyrolysing them together. Two approaches were developed to increase the utilization of fiber tensile strength by minimizing stress concentration defects induced by dissimilar shrinkage during pyrolysis. These were matrix modification to improve char yield and strain-to-failure and fiber-matrix copyrolysis to alleviate matrix cracking. Highest tensile strength and modulus were obtained by heat treatments to 2873 K to match fiber and matrix strain-to-failure and develop maximum monofilament tensile-strength and elastic modulus.

Bradshaw, W. G.↗

Melt-spinnable polyacrylonitrile copolymer precursors for carbon fibers

This paper describes the feasibility of achieving melt-processable polyacrylonitrile copolymer precursors for producing high strength carbon fibers. High molecular weight poly(acrylonitrile-ran-methyl acrylate) (PAN-MA) copolymers with high acrylonitrile content were mixed were various binary melting point modifiers with one component being water to produce systems that formed stable melts at temperatures below the temperature corresponding to the onset of PAN-MA crosslinking. The structure of the copolymer was 96.5 ± 0.13 mol% AN and 4.40 ± 0.13 mol % MA by 1H NMR with an Mw = 238 kDa and polydispersity of 1.9 determined by size exclusion chromatography. A reduction in the Tm of the copolymer of 200 °C was established for one of the copolymer/melting point modifier systems, which corresponds to the greatest reduction in a PAN-based copolymer melting temperature yet reported. From isothermal DSC and pressurized capillary rheometry experiments it was found that the stability of the resulting melts shows a strong temperature dependence, but does not show a strong dependence on shear-rate. Copolymer mixtures consisting of H2O and acetonitrile or adiponitrile were found to be suitable for melt-extrusion at 170 °C with viscosities ranging from 1800 to 2000 Pa*s and stabilities of the melts ≥1 h.

36 MATERIALS SCIENCE↗

Void effects on the interlaminar shear strength of unidirectional graphite-fiber-reinforced composites

A study was conducted to evaluate the effect of voids on the interlaminar shear strength (ILSS) of a polyimide matrix composite system. The graphite/PMR-15 composite was chosen for study because of the extensive amount of experience that has been amassed in the processing of this material. Void contents were calculated and the void geometry and distribution were noted using microscope techniques such as those used in metallography. A good empirical correlation between ILSS and composite density was found. The most acceptable relationship between the ILSS and density was found to be a power equation that closely resembles theoretically derived expressions. It was found that void-free composites could be processed in matched metal die molds at pressures greater than 1.4 MPa and less than 6.9 MPa.

Bowles, Kenneth J.↗

Method to measure orientation of discontinuous fiber embedded in the polymer matrix from computerized tomography scan data

Usage of discontinuous glass fibers in injection and compression molded resin components is rapidly increasing to improve their mechanical properties. Since added fiber contributes to more strength along the fiber direction compared to transverse direction, the mechanical properties of such components strongly depend on the fiber orientation. Thus it is important to estimate the fiber orientation distribution in such materials. Here, we are presenting recently developed method to estimate fiber orientation from 3D image of fibers generated using micro CT scan. Typically the 3D images from CT scan are very large and it becomes difficult to separate each fiber and extract end point information. In this paper a novel method to address this challenge is presented. The micro-CT images were broken into finite volume, reducing data size, and then each fiber was reduced to its own center line, further reducing the data size, using Mimics Innovation Suite (Materialise NV). These 3D centerlines were then used to quantify the 2nd order orientation tensor. Our results from the proposed method are compared with the measurements using well established industry standard approach called method of ellipses for validation. The key challenges in estimating the fiber orientation are identified and future improvements are proposed.

36 MATERIALS SCIENCE↗