Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “Etching”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 217 records · Page 12

Metal etching with reactive gas cluster ion beams using pickup cell

Mixed gas cluster ion beams were formed using pickup cell for metal etching. O{sub 2} neutral clusters pick up acetic acid and formed mixed cluster beam. By using O{sub 2}-GCIB with acetic acid, enhancement of Cu etching was observed. Because of dense energy deposition by GCIB, etching of Cu proceeds by CuO formation, enhancement of chemical reaction with acetic acid and desorption of etching products. Surface roughening was not observed on poly crystalline Cu because of the small dependence of etching rate on crystal orientation. Halogen free and low-temperature metal etching with GCIB using pickup cell is possible.

36 MATERIALS SCIENCE↗

Understanding time-resolved processes in atomic-layer etching of ultra-thin Al{sub 2}O{sub 3} film using BCl{sub 3} and Ar neutral beam

We scrutinize time-resolved processes occurring in atomic-layer etching (ALET) of ultra-thin Al{sub 2}O{sub 3} film using BCl{sub 3} gas and Ar neutral beam by employing density functional theory calculations and experimental measurements. BCl{sub 3} gas is found to be preferentially chemisorbed on Al{sub 2}O{sub 3}(100) in trans form with the surface atoms creating O-B and Al-Cl contacts. We disclose that the most likely sequence of etching events involves dominant detachment of Al-associated moieties at early etching stages in good agreement with our concurrent experiments on tracking Al{sub 2}O{sub 3} surface compositional variations during Ar bombardment. In this etching regime, we find that ALET requires half the maximum reaction energy of conventional plasma etching, which greatly increases if the etching sequence changes.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Etching of germanium-tin using ammonia peroxide mixture

The wet etching of germanium-tin (Ge{sub 1-x}Sn{sub x}) alloys (4.2% < x < 16.0%) in ammonia peroxide mixture (APM) is investigated. Empirical fitting of the data points indicates that the etch depth of Ge{sub 1-x}Sn{sub x} is proportional to the square root of the etch time t and decreases exponentially with increasing x for a given t. In addition, X-ray photoelectron spectroscopy results show that increasing t increases the intensity of the Sn oxide peak, whereas no obvious change is observed for the Ge oxide peak. This indicates that an accumulation of Sn oxide on the Ge{sub 1-x}Sn{sub x} surface decreases the amount of Ge atoms exposed to the etchant, which accounts for the decrease in etch rate with increasing etch time. Atomic force microscopy was used to examine the surface morphologies of the Ge{sub 0.918}Sn{sub 0.082} samples. Both root-mean-square roughness and undulation periods of the Ge{sub 1-x}Sn{sub x} surface were observed to increase with increasing t. This work provides further understanding of the wet etching of Ge{sub 1-x}Sn{sub x} using APM and may be used for the fabrication of Ge{sub 1-x}Sn{sub x}-based electronic and photonic devices.

36 MATERIALS SCIENCE↗

High-efficiency selective boron emitter formed by wet chemical etch-back for n -type screen-printed Si solar cells

Front metal contact induced recombination and resistance are major efficiency limiting factors of large-area screen-printed n-type front junction Si solar cells with homogeneous emitter and tunnel oxide passivated back contact (TOPCON). Here, this paper shows the development of a selective boron emitter (p + /p ++ ) formed by a screen-printed resist masking and wet chemical etch-back process, which first grows a porous Si layer and subsequently removes it. Various wet-chemical solutions for forming porous Si layer are investigated. An industrial compatible process with sodium nitrite (NaNO 2 ) catalyst is developed to uniformly etch-back the ~47 Ω/ atmospheric pressure chemical vapor deposited heavily doped boron emitter to ~135 Ω/ by growing a 320 nm porous Si layer within 3 min and subsequently removing it. After etching back, the boron emitter was subjected to a thermal oxidation to lower the surface concentration and the emitter saturation current density J 0e . Various etched-back emitters were evaluated by measuring J 0e on symmetric test structures with atomic layer deposited aluminum oxide (Al 2 O 3 ) passivation. Very low J 0e of 21, 14, and 9 fA/cm 2 were obtained for the 120, 150, and 180 Ω/ etched-back emitters, respectively. A solar cell with a selective emitter (65/180 Ω/ ) formed by this etch-back technology and with an Al/Ag contact on the front and TOPCON on the back gave an open-circuit voltage (V oc ) of 682.8 mV and efficiency of 21.04% on n-type Czochralski Si wafer. Finally, this demonstrates the potential of this technology for next generation high-efficiency industrial n-type Si solar cells.

14 SOLAR ENERGY↗

Enhancement to the conductivity of surface transfer-doped (111) diamond through thermochemical surface etching

The use of a transition metal catalyzed thermochemical etching method for improving the carrier transport properties of the near-surface two-dimensional (2D) hole gas in surface transfer-doped hydrogen-terminated (111) diamond is demonstrated. Using Ni 0.8 Cr 0.2 films deposited and annealed to a temperature of 900 °C, with up to three etch cycles, preferential (111) surface etching produces large terraces exceeding 10 μm in size with a surface microroughness, σ 2 RMS λ, that is two orders of magnitude lower than for the pre-etched (111) surface. Magnetotransport measurements on hydrogen-terminated Hall bars engineered on the pre- and post-etched surfaces and rendered conductive by the adsorbed water layer formed on exposure to ambient conditions demonstrate that this etching causes an improvement in the hole mobility by an order of magnitude, resulting in a measured sheet resistivity of 1.04 kΩ/sq at a temperature of 4.2 K without gating.

42 ENGINEERING↗

Seasoning of plasma etching reactors: Ion energy distributions to walls and real-time and run-to-run control strategies

Wafer-to-wafer process reproducibility during plasma etching often depends on the conditioning of the inside surfaces of the reactor. Passivation of reactor surfaces by plasma generated species, often called seasoning, can change the reactive sticking coefficients of radicals, thereby changing the composition of the radical and ion fluxes to the wafer. Ion bombardment of the walls may influence these processes through activation of surface sites or sputtering, and so the spatial variation of ion energies on the walls is important. These seasoning processes may occur during a single etching process or on a wafer-to-wafer basis. The seasoning of plasma etching reactors will be discussed using results from a computational investigation of p-Si etching in chlorine plasmas. The transport of etch products, passivation of walls, and sputtered products from walls are accounted for, as well as differentiating the ion energy distributions to different surfaces. A real-time, closed-loop control of etch rate to counter the effects of seasoning was achieved using the bias voltage as an actuator.

36 MATERIALS SCIENCE↗

Low-damage low-k etching with an environmentally friendly CF{sub 3}I plasma

The feasibility of etching Cu/low-k interconnects by using a low global warming potential CF{sub 3}I plasma was studied. Low-damage etching was done and porous SiOC (p-SiOC, k<2.6) film with low roughness was produced. Exposing p-SiOC film to CF{sub 3}I plasma was found to suppress the decrease in the CH{sub 3} group and the increase in the k value compared to those of conventional CF{sub 4} and C{sub 4}F{sub 6} plasmas. These effects are due to the low UV intensity and small amount of F radicals of CF{sub 3}I plasma. The authors also found that the etching profile of CF{sub 3}I plasma was comparable with that of CF{sub 4} plasma. Since the etching selectivity (p-SiOC/ArF photoresist) of CF{sub 3}I plasma is higher than that of CF{sub 4} plasma, the remaining photoresist thickness increases after etching, thus suppressing line edge roughness (LER). The decreased LER mitigated degradation of IV and time dependent dielectric breakdown characteristics in Cu interconnects. They also found that the roughness on the bottom surface of the p-SiOC trench was reduced. These benefits are due to CF{sub 3}I plasma's low reactivity with the carbon in photoresists and p-SiOC films. Based on these findings, they believe that the environmentally friendly CF{sub 3}I gas has great promise as a p-SiOC etching material.

36 MATERIALS SCIENCE↗

Plasma etching of Hf-based high-k thin films. Part I. Effect of complex ions and radicals on the surface reactions

The effect of ion and radical compositions in BCl{sub 3}/Cl{sub 2} plasmas was assessed in this work with a focus on the formation of etch products in patterning hafnium aluminate, a potential high-k gate oxide material. The plasma composition became increasingly more complex as the percentage of boron trichloride was increased, which led to the formation of a significant amount of boron-containing species including B{sup +}, BCl{sup +}, BCl{sub 2}{sup +}, BCl{sub 3}{sup +}, B{sub 2}Cl{sub 3}{sup +}, and B{sub 2}OCl{sub 3}{sup +} in the plasma. The BCl{sub 2}{sup +} ions were found to be the dominant species in BCl{sub 3} containing plasmas at most conditions; however, increasing the pressure or decreasing the power led to an increase in the formation of higher mass ions. Several compositions of Hf{sub 1-x}Al{sub x}O{sub y} thin films ranging from pure HfO{sub 2} to pure Al{sub 2}O{sub 3} were etched in BCl{sub 3}/Cl{sub 2} plasmas as functions of ion energy and plasma composition. The etch product distributions were measured and the dominant metal-containing etch products were HfCl{sub x} and AlCl{sub x} in a Cl{sub 2} plasma and HfCl{sub x}, HfBOCl{sub 4}, and Al{sub x}Cl{sub y} in a BCl{sub 3} plasma, and their concentrations increased with increasing ion energy. Oxygen was detected removed in the form of ClO in Cl{sub 2} and as trichloroboroxin ((BOCl){sub 3}) in BCl{sub 3}. Both the etch rate and the etch product formation are enhanced in BCl{sub 3}/Cl{sub 2} plasmas, as compared to those in Cl{sub 2} plasmas, due to the change in the composition and reactivity of the dominant ions and radicals.

36 MATERIALS SCIENCE↗

X-ray photoelectron spectroscopy analysis of organic materials etched by charged water droplet impact

Electrospray droplet impact (EDI) has been developed for matrix-free secondary ion mass spectrometry for surface analysis. When a target is etched by EDI, the physical etching on the target is suppressed to minimal, i.e., the occurrence of shallow surface etching. A novel approach to shallow surface etching of polystyrene (PS) by EDI was investigated. The charged water droplets were irradiated to a bulk and a spin coated PS. After irradiation, these samples were analyzed by X-ray photoelectron spectroscopy (XPS) and atomic force microscopy. It was found that XPS spectra for PS were independent on the irradiation time by EDI. This indicates that EDI is a unique technique for the surface etching of the organic materials without leaving any damage on the etched surface.

36 MATERIALS SCIENCE↗

Sidewall damage in plasma etching of Si/SiGe heterostructures

Plasma etching is a critical tool in the fabrication of Si/SiGe heterostructure quantum devices, but it also presents challenges, including damage to etched feature sidewalls that affects device performance. Chemical and structural changes in device feature sidewalls associated with plasma-surface interactions are considered damage, as they affect band structure and electrical conduction in the active region of the device. Here the authors report the results of experiments designed to better understand the mechanisms of plasma-induced sidewall damage in modulation-doped Si/SiGe heterostructures containing a two-dimensional electron gas. Damage to straight wires fabricated in the heterostructure using plasma etching was characterized both by measuring the width of the nonconductive ''sidewall depletion'' region at the device sidewall and by measuring the noise level factor {gamma}{sub H}/N determined from spectra of the low frequency noise. Observed increases in sidewall depletion width with increasing etch depth are tentatively attributed to the increase in total number of sidewall defects with increased plasma exposure time. Excess negative charge trapped on the feature sidewall could be another contributing factor. Defects at the bottom of etched features appear to contribute minimally. The noise level shows a minimum at an ion bombardment energy of {approx}100 eV, while the sidewall depletion width is independent of bias voltage, within experimental uncertainty. A proposed explanation of the noise trend involves two competing effects as ion energy increases: the increase in damage caused by each bombarding ion and the reduction in total number of incident ions due to shorter etch times.

36 MATERIALS SCIENCE↗

Dry-etching properties of TiN for metal/high-k gate stack using BCl{sub 3}-based inductively coupled plasma

The etch rate of TiN film and the selectivities of TiN/SiO{sub 2} and TiN/HfO{sub 2} were systematically investigated in Cl{sub 2}/BCl{sub 3}/Ar plasmas as functions of Cl{sub 2} flow rate, radio-frequency (rf) power, and direct-current (dc) bias voltage under different substrate temperatures of 10 and 80 degree sign C. The etch rate of TiN films increased with increasing Cl{sub 2} flow rate, rf power, and dc-bias voltage at a fixed substrate temperature. In addition, the etch rate of TiN films at 80 degree sign C were higher than that at 10 degree sign C when other plasma parameters were fixed. However, the selectivities of TiN/SiO{sub 2} and TiN/HfO{sub 2} showed different tendencies compared with etch-rate behavior as a function of rf power and dc bias voltage. The relative-volume densities of Ar (750.0 nm), Cl (725.2 nm), and Cl{sup +} (386.6 nm) were monitored with an optical-emission spectroscopy. When rf power increased, the relative-volume densities of all studied particles were increased. X-ray photoelectron spectroscopy was carried out to detect nonvolatile etch by-products from the surface, and nonvolatile peaks (TiCl{sub x} bonds) in Ti 2p and Cl 2p were observed due to their high melting points. Based on the experimental results, we can conclude that the TiN etch is dependent on the substrate temperature when other plasma parameters are fixed. This can be explained by the enhanced chemical pathway with the assistance of ion bombardment.

36 MATERIALS SCIENCE↗

Infinitely high selective inductively coupled plasma etching of an indium tin oxide binary mask structure for extreme ultraviolet lithography

Currently, extreme ultraviolet lithography (EUVL) is being investigated for next generation lithography. Among the core EUVL technologies, mask fabrication is of considerable importance due to the use of new reflective optics with a completely different configuration than those of conventional photolithography. This study investigated the etching properties of indium tin oxide (ITO) binary mask materials for EUVL, such as ITO (absorber layer), Ru (capping/etch-stop layer), and a Mo-Si multilayer (reflective layer), by varying the Cl{sub 2}/Ar gas flow ratio, dc self-bias voltage (V{sub dc}), and etch time in inductively coupled plasmas. The ITO absorber layer needs to be etched with no loss in the Ru layer on the Mo-Si multilayer for fabrication of the EUVL ITO binary mask structure proposed here. The ITO layer could be etched with an infinitely high etch selectivity over the Ru etch-stop layer in Cl{sub 2}/Ar plasma even with a very high overetch time.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Deep GaN etching by inductively coupled plasma and induced surface defects

GaN etching was studied in Cl{sub 2}/Ar plasmas as a function of process parameters. In addition, for a better understanding of the etching mechanisms, Langmuir probe measurements and optical emission spectroscopy were carried out. Etch rate was found to depend strongly on bias power. After optimization, an etch rate greater than 1000 nm/min was achieved. A second part of this work is dedicated to the etched surface defects. An original method to estimate GaN dislocation density and to localize nanopipes in the material is presented. Columnar defects could also appear with impurities in the etching reactor. The authors also present a possible formation mechanism of those columnar defects.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Recouping etch rates in pulsed inductively coupled plasmas

Pulsed rf plasmas are increasingly being employed for plasma etching at future technological nodes. Although the plasma uniformity usually improves with pulsing, the lower time-averaged power decreases the etch rate and the lower throughput is undesirable. It is therefore important to evaluate different strategies to restore higher etch rates while retaining the advantages of pulsed plasmas. In this work, the impact of varying pulsing modes in an inductively coupled plasma on plasma characteristics and feature profile evolution are discussed using the results from a two-dimensional reactor scale plasma model coupled to a Monte Carlo based feature profile model. Results are discussed for poly-Si etching in an Ar/Cl{sub 2} gas mixture. The consequences of source-only and bias-only pulsing modes on discharge characteristics, ion energy distributions (IEDs) to the wafer, and feature profile evolution are discussed. Although the etch depth rates were found to be higher for source-only pulsing compared to the synchronized (source and bias) pulsing mode, the higher ion energies in the afterglow period during source-only pulsing may also increase ion bombardment damage. Compensation of power may allow for increased etch depth rates while retaining the benefits of synchronized pulsing. Further, power compensation level can be varied to achieve fine tuning of the IEDs to the wafer.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Plasma etching: Yesterday, today, and tomorrow

The field of plasma etching is reviewed. Plasma etching, a revolutionary extension of the technique of physical sputtering, was introduced to integrated circuit manufacturing as early as the mid 1960s and more widely in the early 1970s, in an effort to reduce liquid waste disposal in manufacturing and achieve selectivities that were difficult to obtain with wet chemistry. Quickly, the ability to anisotropically etch silicon, aluminum, and silicon dioxide in plasmas became the breakthrough that allowed the features in integrated circuits to continue to shrink over the next 40 years. Some of this early history is reviewed, and a discussion of the evolution in plasma reactor design is included. Some basic principles related to plasma etching such as evaporation rates and Langmuir–Hinshelwood adsorption are introduced. Etching mechanisms of selected materials, silicon, silicon dioxide, and low dielectric-constant materials are discussed in detail. A detailed treatment is presented of applications in current silicon integrated circuit fabrication. Finally, some predictions are offered for future needs and advances in plasma etching for silicon and nonsilicon-based devices.

36 MATERIALS SCIENCE↗

Dry etching techniques for active devices based on hexagonal boron nitride epilayers

Hexagonal boron nitride (hBN) has emerged as a fundamentally and technologically important material system owing to its unique physical properties including layered structure, wide energy bandgap, large optical absorption, and neutron capture cross section. As for any materials under development, it is necessary to establish device processing techniques to realize active devices based on hBN. The authors report on the advancements in dry etching techniques for active devices based on hBN epilayers via inductively coupled plasma (ICP). The effect of ICP radio frequency (RF) power on the etch rate and vertical side wall profile was studied. The etching depth and angle with respect to the surface were measured using atomic force microscopy showing that an etching rate ∼1.25 μm/min and etching angles >80° were obtained. Profilometer data and scanning electron microscope images confirmed these results. This work demonstrates that SF{sub 6} is very suitable for etching hBN epilayers in RF plasma environments and can serve as a guide for future hBN device processing.

36 MATERIALS SCIENCE↗

Smoothing single-crystalline SiC surfaces by reactive ion etching using pure NF{sub 3} and NF{sub 3}/Ar mixture gas plasmas

In pure NF{sub 3} plasma, the etching rates of four kinds of single-crystalline SiC wafer etched at NF{sub 3} pressure of 2 Pa were the highest and it decreased with an increase in NF{sub 3} pressure. On the other hand, they increased with an increase in radio frequency (RF) power and were the highest at RF power of 200 W. A smooth surface was obtained on the single-crystalline 4H-SiC after reactive ion etching at NF{sub 3}/Ar gas pressure of 2 Pa and addition of Ar to NF{sub 3} plasma increased the smoothness of SiC surface. Scanning electron microscopy observation revealed that the number of pillars decreased with an increase in the Ar-concentration in the NF{sub 3}/Ar mixture gas. The roughness factor (R{sub a}) values were decreased from 51.5 nm to 25.5 nm for the As-cut SiC, from 0.25 nm to 0.20 nm for the Epi-SiC, from 5.0 nm to 0.7 nm for the Si-face mirror-polished SiC, and from 0.20 nm to 0.16 nm for the C-face mirror-polished SiC by adding 60% Ar to the NF{sub 3} gas. Both the R{sub a} values of the Epi- and the C-face mirror-polished wafer surfaces etched using the NF{sub 3}/Ar (40:60) plasma were similar to that treated with mirror polishing, so-called the Catalyst-Referred Etching (CARE) method, with which the lowest roughness of surface was obtained among the chemical mirror polishing methods. Etching duration for smoothing the single-crystalline SiC surface using its treatment was one third of that with the CARE method.

36 MATERIALS SCIENCE↗

Impact of hydrofluorocarbon molecular structure parameters on plasma etching of ultra-low-K dielectric

The authors report a systematic study aimed at evaluating the impact of molecular structure parameters of hydrofluorocarbon (HFC) precursors on plasma deposition of fluorocarbon (FC) films and etching performance of a representative ultra-low-k material, along with amorphous carbon. The precursor gases studied included fluorocarbon and hydrofluorocarbon gases whose molecular weights and chemical structures were systematically varied. Gases with three different degrees of unsaturation (DU) were examined. Trifluoromethane (CHF{sub 3}) is the only fully saturated gas that was tested. The gases with a DU value of one are 3,3,3-trifluoropropene (C{sub 3}H{sub 3}F{sub 3}), hexafluoropropene (C{sub 3}F{sub 6}), 1,1,3,3,3-pentafluoro-1-propene (C{sub 3}HF{sub 5}), (E)-1,2,3,3,3-pentafluoropropene (C{sub 3}HF{sub 5} isomer), heptafluoropropyl trifluorovinyl ether (C{sub 5}F{sub 10}O), octafluorocyclobutane (C{sub 4}F{sub 8}), and octafluoro-2-butene (C{sub 4}F{sub 8} isomer). The gases with a DU value of two includes hexafluoro-1,3-butadiene (C{sub 4}F{sub 6}), hexafluoro-2-butyne (C{sub 4}F{sub 6} isomer), octafluorocyclopentene (C{sub 5}F{sub 8}), and decafluorocyclohexene (C{sub 6}F{sub 10}). The work was performed in a dual frequency capacitively coupled plasma reactor. Real-time characterization of deposition and etching was performed using in situ ellipsometry, and optical emission spectroscopy was used for characterization of CF{sub 2} radicals in the gas phase. The chemical composition of the deposited FC films was examined by x-ray photoelectron spectroscopy. The authors found that the CF{sub 2} fraction, defined as the number of CF{sub 2} groups in a precursor molecule divided by the total number of carbon atoms in the molecule, determines the CF{sub 2} optical emission intensity of the plasma. CF{sub 2} optical emission, however, is not the dominant factor that determines HFC film deposition rates. Rather, HFC film deposition rates are determined by the number of weak bonds in the precursor molecule, which include a ring structure, C=C, C≡C, and C–H bonds. These bonds are broken preferentially in the plasma, and/or at the surface and fragments arriving at the substrate surface presumably provide dangling bonds that efficiently bond to the substrate or other fragments. Upon application of a radio-frequency bias to the substrate, substrate etching is induced. Highly polymerizing gases show decreased substrate etching rates as compared to HFC gases characterized by a lower HFC film deposition rate. This can be explained by a competition between deposition and etching reactions, and an increased energy and etchant dissipation in relatively thicker steady state FC films that form on the substrate surface. Deposited HFC films exhibit typically a high CF{sub 2} density at the film surface, which correlates with both the CF{sub 2} fractions in the precursor molecular structure and the deposition rate. The FC films deposited using hydrogen-containing precursors show higher degrees of crosslinking and lower F/C ratios than precursors without hydrogen, and exhibit a lower etch rate of substrate material. A small gap structure that blocks direct ion bombardment was used to simulate the sidewall plasma environment of a feature and was employed for in situ ellipsometry measurements. It is shown that highly polymerizing precursors with a DU of two enable protection of low-k sidewalls during plasma exposure from oxygen-related damage by protective film deposition. Dielectric film modifications are seen for precursors with a lower DU.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗