Effect of impurity doping concentration on solar cell output

Experimental measurements were made of solar cell and related photovoltaic parameters for silicon with high concentrations of dopant impurities. The cell output peaked for doping levels around 10 to the 17th power per cu cm. Independent measurements of diffusion length and open circuit voltage at high doping levels showed severe reductions at concentrations above 10 to the 18th power per cu cm. Theoretical reasons are given to explain these reductions. Indication is given of the problems requiring solution before increased cell output can be achieved at high doping levels.

Iles, P. A.↗

Radiation effects on beta /10.6/ of pure and europium doped KCl

Changes in the optical absorption coefficient as the result of X-ray and electron bombardment of pure monocrystalline and polycrystalline KCl and of divalent europium doped polycrystalline KCl were determined. A constant heat flow calorimetric method was used to measure the optical absorption coefficients. Both 300 kV X-ray irradiation and 2 MeV electron irradiation produced increases in the optical absorption coefficient at room temperature. X-ray irradiation produced more significant changes in pure monocrystalline KCl than equivalent amounts of electron irradiation. Electron irradiation of pure and Eu-doped polycrystalline KCl produced increases in the absorption by as much as a factor of 20 over untreated material. Bleaching of the electron-irradiated doped KCl with 649 millimicron light produced a further increase.

Grimes, H. H.↗

Iron-doped lithium niobate as a read-write holographic storage medium

The response of iron-doped lithium niobate under conditions corresponding to hologram storage and retrieval is described, and the material characteristics are discussed. The optical sensitivity can be improved by heavy chemical reduction of lightly doped crystals such that most of the iron is in the divalent state, the remaining part being trivalent. The best reduction process found to be reproducible so far is the anneal of the doped crystal in the presence of a salt such as lithium carbonate. It is shown by analysis and simulation that a page-oriented read-write holographic memory with 1000 bits per page would have a cycle time of about 60 msec and a signal-to-noise ratio of 27 dB. This cycle time, although still too long for a practical memory, represents an improvement of two orders of magnitude over that of previous laboratory prototypes using a thermoplastic storage medium

Alphonse, G. A.↗

Surface recombination velocity and diffusion length of minority carriers in heavily doped silicon layers

Quantitative analysis of the electron beam-induced current and the dependence of the effective diffusion length of the minority carriers on the penetration depth of the electron beam were employed for the analysis of the carrier recombination characteristics in heavily doped silicon layers. The analysis is based on the concept of the effective excitation strength of the carriers which takes into consideration all possible recombination sources. Two dimensional mapping of the surface recombination velocity of P-diffused Si layers will be presented together with a three dimensional mapping of minority carrier lifetime in ion implanted Si. Layers heavily doped with As exhibit improved recombination characteristics as compared to those of the layers doped with P.

Gatos, H. C.↗

Transmutation doping of silicon solar cells

Normal isotopic silicon contains 3.05% of Si-30 which transmutes to P-31 after thermal neutron absorption, with a half-life of 2.6 hours. This reaction is used to introduce extremely uniform concentrations of phosphorus into silicon, thus eliminating the areal and spatial inhomogeneities characteristic of chemical doping. Annealing of the lattice damage in the irradiated silicon does not alter the uniformity of dopant distribution. Transmutation doping also makes it possible to introduce phosphorus into polycrystalline silicon without segregation of the dopant at the grain boundaries. The use of neutron transmutation doped (NTD) silicon in solar cell research and development is discussed.

Wood, R. F.↗

Reflectance spectra for sodium and potassium doped ammonia frosts - Implications for Io's surface

This paper reports measurements of the reflection spectra of sodium- and potassium-doped ammonia frosts as a function of alkali metal concentration for the wavelength range 0.35-2.5 microns. The purpose of the measurements was to determine whether or not the reflection spectra for such a solid was compatible with the spectra albedo of Io. The data show that, with a sufficiently large alkali metal concentration, the reflection spectra of the doped ammonia frosts do not display the characteristic ammonia features at 2.0 and 2.25 micron. The high reflectance of the more concentrated samples and the character of the observed reflection spectrum make it difficult to rule out sodium-doped ammonia frost as a surface constituent on Io on the basis of existing data.

Rosen, M. D. A.↗

Bandgap narrowing in moderately to heavily doped silicon

A theoretical model of bandgap narrowing in silicon at high doping levels has been developed. The model takes into account the electrostatic energy of interaction between a minority carrier and the majority carriers surrounding it, which reduces the thermal energy necessary for creation of an electron-hole pair. A pair energy similar to the excitonic binding energy of bound electron-hole pairs in insulators is obtained. Theoretical results are in excellent agreement with experimental results in the doping range from 3 times 10 to the 17th to 1.5 times 10 to the 20th/cu cm at room temperature. These results indicate that at high injection levels such as a transistor biased into the conductivity-modulation regime or a solar cell whose surface is established by ion implantation into an oxide layer, the bandgap narrowing is determined by the injected carrier concentration rather than by the doping level.

Lanyon, H. P. D.↗

Effect of W and WC on the oxidation resistance of yttria-doped silicon nitride

The effect of tungsten and tungsten carbide contamination on the oxidation and cracking in air of yttria-doped silicon nitride ceramics is investigated. Silicon nitride powder containing 8 wt % Y2O3 was doped with 2 wt % W, 4 wt % W, 2 wt % WC or left undoped, and sintered in order to simulate contamination during milling, and specimens were exposed in air to 500, 750 and 1350 C for various lengths of time. Scanning electron and optical microscopy and X-ray diffraction of the specimens in the as-sintered state reveals that the addition of W or WC does not affect the phase relationships in the system, composed of alpha and beta Si3N4, melilite and an amorphous phase. Catastrophic oxidation is observed at 750 C in specimens containing 2 and 4 wt % W, accompanied by the disappearance of alpha Si3N4 and melilite from the structure. At 1350 C, the formation of a protective glassy oxide layer was observed on all specimens without catastrophic oxidation, and it is found that pre-oxidation at 1350 C also improved the oxidation resistance at 750 C of bars doped with 4 wt % W. It is suggested that tungsten contamination from WC grinding balls may be the major cause of the intermediate-temperature cracking and instability frequently observed in Si3N4-8Y2O3.

Schuon, S.↗

Photovoltaic investigation of minority carrier lifetime in the heavily-doped emitter layer of silicon junction solar cell

The results of experiments on the recombination lifetime in a phosphorus diffused N(+) layer of a silicon solar cell are reported. The cells studied comprised three groups of Czochralski grown crystals: boron doped to one ohm-cm, boron doped to 6 ohm-cm, and aluminum doped to one ohm-cm, all with a shunt resistance exceeding 500 kilo-ohms. The characteristic bulk diffusion length of a cell sample was determined from the short circuit current response to light at a wavelength of one micron. The recombination rates were obtained by measurement of the open circuit voltage as a function of the photogeneration rate. The recombination rate was found to be dependent on the photoinjection level, and is positive-field controlled at low photoinjection, positive-field influence Auger recombination at a medium photoinjection level, and negative-field controlled Auger recombination at a high photoinjection level.

Ho, C.-T.↗

Defect behavior in electron-irradiated boron- and gallium-doped silicon

Production and anneal of defects in electron-irradiated, float-zone silicon solar cells were studied by DLTS. In boron- and gallium-doped, n+-p cells, dominant defects were due to the divacancy, carbon interstitial, and carbon complex. Results suggest that the DLTS peak normally ascribed to carbon complexes also involves gallium. For gallium- and, to a lesser extent, boron-doped samples, damaged lifetime shows substantial recovery only when the carbon-complex peak has annealed out at 400 C. In boron-doped, n+-p-p+ cells, a minority carrier trap (E1) was also observed by DLTS in cells with a boron p+, but not in those with an aluminum p+ back. A level at Ev + 0.31 eV appeared upon 150 C annealing (E1 out) in both p+ back types of samples.

Drevinsky, P. J.↗

EL2 distributions in doped and undoped liquid encapsulated Czochralski GaAs

The longitudinal and radial distributions of EL2 in undoped semi-insulating and intentionally doped n-type GaAs crystals grown by the liquid encapsulated Czochralski technique are compared. Longitudinal profiles in undoped crystals are controlled by changes in melt stoichiometry as the crystal is pulled from the melt. EL2 profiles along crystals doped above about 1 x 10 to the 17th/cu cm, on the other hand, are controlled primarily by the carrier concentration as a result of the suppression of EL2 by free electrons. Radial EL2 profiles are typically W shaped and M shaped in undoped and doped (above threshold) crystals, respectively. The origin of these radial profiles is discussed in terms of residual stress, melt stoichiometry, and the suppresion of EL2 by electrons. The results are also discussed in the light of the antisite model for EL2.

Holmes, D. E.↗

Influence of oxygen on defect production in electron-irradiated, boron-doped silicon

Deep level transient spectroscopy (DLTS) measurements were made on float-zone and crucible-grown, boron-doped silicon irradiated with 1-MeV electrons. The minority carrier trap attributed to a boron-related state, was not seen in low-resistivity, float-zone silicon. However, a new majority carrier trap was observed in these samples. In the case of more lightly doped material the minority carrier trap was present, and its introduction rate was lower in float-zone than in crucible-grown silicon. For 1- and 10-ohm-cm float-zone material that was oxidized during processing, the introduction rates for this trap were comparable to those for crucible-grown silicon. This behavior indicates that the minority carrier trap involves oxygen and that it may be due to a boron-oxygen complex. The majority carrier trap seen in heavily doped, float-zone silicon may also involve boron but not oxygen. Observed trap concentrations suggest that oxygen content in the regions examined by DLTS is affected by processing techniques. Other differences were observed in defect production and annealing behavior of electron-irradiated, float-zone and crucible-grown silicon.

Deangelis, H. M.↗

Experimental test for interpreting the increase in sensibility of doped CR-39

In recent years the sensibility of CR-39 to nuclear tracks has been increased by doping the corresponding monomer with dioctyl phtalate. At this regard, two theoretical approaches are current managed to explain this phenomenon: either the doping react with the active radicals in the chain blocking them, stopping crosslinking between chains, or alternatively that the doping gets between them giving wider space between the crosslinkined chains.

Laville, A.↗

Transit time and charge storage measurements in heavily doped emitters

A first direct measurement of the minority-carrier transit time in a transparent heavily doped emitter layer is reported. The value was obtained by a high-frequency conductance method recently developed and used for low-doped Si. The transit time coupled with the steady-state current enables the determination of the quasi-static charge stored in the emitter and the quasi-static emitter capacitance. Using a transport model, from the measured transit time, the value for the minority-carrier diffusion coefficient and mobility is estimated. The measurements were done using a heavily doped emitter of the Si p(+)-n-p bipolar transistor. The new result indicates that the position-averaged minority-carrier diffusion coefficients may be much smaller than the corresponding majority-carrier values for emitters having a concentration ranging from about 3 x 10 to the 19th per cu cm to 10 to the 20th per cu cm.

Neugroschel, A.↗

Measurement of minority carrier lifetime, mobility and diffusion length in heavily doped silicon

Carrier transport and recombination parameters in heavily doped silicon were examined. Data were presented for carrier diffusivity in both p- and n-type heavily doped silicon covering a broad range of doping concentrations from 10 to the 15th power to 10 to the 20th power atoms/cu cm. One of the highlights of the results showed that minority carrier diffusivities are higher by a factor of 2 in silicon compared to majority carrier diffusivities.

Swirhun, S. E.↗

Heavy doping effects in high efficiency silicon solar cells

The temperature dependence of the emitter saturation current for bipolar devices was studied by varying the surface recombination velocity at the emitter surface. From this dependence, the value was derived for bandgap narrowing that is in better agreement with other determinations that were obtained from the temperature dependence measure on devices with ohmic contacts. Results of the first direct measurement of the minority-carrier transit time in a transparent heavily doped emitter layer were reported. The value was obtained by a high-frequency conductance method recently developed and used for doped Si. Experimental evidence is presented for significantly greater charge storage in highly excited silicon near room temperature than conventional theory would predict. These data are compared with various data for delta E sub G in heavily doped silicon.

Lindholm, F. A.↗

Ohmic contact formation in semi-insulating GaAs using shallow heavily doped p-type layers

The paper describes a simple, safe, and effective method for forming shallow zinc-doped p-type layers on chromium-doped semiinsulating GaAs, using an open-tube diffusion technique. The resulting peak dopant concentration for the 850-C diffusion was 10 to the 20th/cu cm. The contact resistance of ohmic contacts fabricated on these layers was found to be about 0.00005 ohm/sq cm. The variation of the contact resistance across the wafer reflected the variation of the doping concentration.

Bose, Amitava↗

Self-consistent calculations and design considerations for a GaAs nipi doping superlattice solar cell

The authors present design constraints which show that a previously proposed GaAs nipi doping superlattice solar cell structure would not work as an efficient space solar cell. A structure based on the CLEFT process, which shows promise of being an efficient cell with very high radiation tolerance, is proposed. In order to test theoretically its viability and to optimize its design, self-consistent quantum mechanical calculations were made for a number of thicknesses of the n, i, and p layers and the dopings in the n and p layers. These results show that: 1) an i layer is not necessary; in fact, its presence makes it difficult to satisfy one of the key constraints; 2) a near-optimum design with 750-A thick n and p layers with dopings of 2.5E18/cu cm and a selective contact separation of 20 microns would yield both high efficiency and very high radiation tolerance.

Clark, Ralph O.↗