Bulk synthesis of radiation resistant W – Ti – Cr – V compositionally complex alloys

Refractory compositionally complex alloys are candidate material systems for next generation advanced nuclear reactors. This work showcases the first successful bulk synthesis of low activation W–Ti based refractory compositionally complex alloys using arc melting and provides insights on using additive manufacturing for these compositions using directed energy deposition. Both techniques produce equiaxed grains composed of a tungsten matrix with Ti–V–Cr dendritic boundaries. The arc melted specimen possesses a multi-modal grain size distribution, while the directed energy deposition specimen possesses a more gaussian distribution of grain size. Both arc melted and directed energy deposition specimens demonstrate high thermal stability up to 900 °C, as well as promising radiation resistance with low loop formation and the presence of homogeneously distributed helium cavities maintaining small diameters at ≥10 dpa under simultaneous light (helium) and heavy (krypton) ion irradiation at 900 °C.

Arc melting (AM)↗

Effects of temperature on helium bubble behaviour in Fe–9Cr alloy

In the present study, Fe–9Cr model alloys were irradiated by 275 keV He + ions at 500 to 800 °C to a peak damage level and implanted helium content of 0.5 dpa and 0.75 at% He, respectively. Effects of temperature on He bubble behaviour were studied by transmission electron microscopy (TEM) to reveal the temperature effects. The bubble spatial distribution changes from homogenous at 500 and 600 °C to heterogeneous at 700 and 800 °C, due to preferential bubble precipitation on dislocations and grain boundaries at high temperature. Faceted bubbles with low energy faces along the {001} planes were present at all four temperatures and are attributed to surface energy minimization. Bubble precipitation on the GBs became more pronounced with increasing temperature. Meanwhile, the cavity swelling increased with increasing temperature, from 0.59% at 500 °C to 8.21% at 800 °C with a sharp increase above 700 °C. By analysing the temperature dependence of bubble size and density, a transition temperature between low and high temperature regimes was obtained in terms of different activation energies which are related to different bubble nucleation and formation mechanisms.

36 MATERIALS SCIENCE↗

Defect evolution in Ni and solid-solution alloys of NiFe and NiFeCoCr under ion irradiation at 16 and 300 K

Single-phase concentrated solid-solution alloys (SP-CSAs) have shown unique chemical complexity at the levels of electrons and atoms, and their defect evolution is expected to be different from conventional dilute alloys. Single crystals of Ni, NiFe and NiFeCoCr are chosen as model systems to understand the chemical complexity on defect formation and damage accumulation in SP-CSAs under ion irradiation. The high-quality crystals were irradiated at 16 and 300 K to different ion fluences, to form irradiated region with little to heavy damages. Additionally, the ion-induced damage was determined using Rutherford backscattering spectrometry technique along a channeling direction (RBS/C) and the level of lattice damage in irradiated Ni and SP-CSAs was quantified from Monte Carlo (MC) simulations. The results are interpreted using the Multi Step Damage Accumulation model to reveal material damage accumulation kinetics. Key findings of the study are that in case of room temperature irradiations the damage level measured for complex alloys at the highest irradiation fluence of 2 × 10 15 cm -2 (~3 dpa) is significantly higher than that obtained for pure nickel samples and suggest two-step damage accumulation process with a defect transformation taking place at a fluence of about 1.5 × 10 15 cm -2 . Furthermore, structural and damage kinetic differences clearly imply that, with increasing degree of chemical complexity and high solid-solution strengthening effects from Ni to NiFe and to NiFeCoCr, the enhanced lattice stiffness resists to randomization of atomic configurations and inhibits the growth of extended defects.

36 MATERIALS SCIENCE↗

Dislocation loop evolution and radiation hardening in nickel-based concentrated solid solution alloys

Effects of chemical composition, ion irradiation dose and temperature on unfaulting of irradiation induced Frank dislocation loops to perfect loops in two nickel based single-phase solid solution alloys, Ni–20Fe and NiFe–20Cr, have been studied. The fraction of Frank loops decreases with irradiation dose from 7.2 to 38.4 dpa at 500°C, but with more Frank loops remaining in the ternary alloy. However, perfect loops and dislocation networks become the dominant features of defects at 580°C in both alloys. The results indicate a thermally assisted loop unfaulting process that may be hindered by more sluggish defect motion in the alloy with more chemical components. Nano-indentation with both continuous stiffness method and single indentation method are used to measure radiation hardening. Loop unfaulting in both alloys irradiated at 580°C reduced radiation hardening while significant hardening is observed after irradiation at 500°C. The quasi-static single indentation method exhibits lower hardness results compared to continuous stiffness method, because dislocations induced from the cyclic loading in the latter method get relaxed and stabilized, resulting in higher resistance to the indenter.

36 MATERIALS SCIENCE↗

Disordering of helium gas bubble superlattices in molybdenum under ion irradiation and thermal annealing

Self-organization of gas bubbles causes the formation of an ordered array of nanoscale gas bubbles (a gas bubble superlattice), a highly efficient mechanism for gas storage under irradiation. Here, the stability of helium (He) gas bubble superlattices in molybdenum (Mo) under krypton (Kr) ion irradiation and thermal annealing has been investigated. The He gas bubble superlattices gradually become disordered under Kr ion irradiation at 300° C, and the order-disorder transformation process completes at 2.5 dpa. Both transmission electron microscopy (TEM) and synchrotron-based small-angle X-ray scattering (SAXS) reveal that the order-disorder transformation of He gas bubble superlattices is associated with a slight increase in the average bubble size. Phase-field modeling indicates that the inhomogeneous growth and coarsening of bubbles/voids cause the disordering of imperfect superlattices under irradiation and implies that highly ordered superlattices could potentially exhibit much stronger resistance to irradiation damage. Under thermal annealing, the He gas bubble superlattices in Mo become unstable and disordered at 1000° C with the bubble size increasing from ~1.1 to ~1.6 nm. The finding in this research provides insights into the disordering mechanisms of defect superlattices as well as guidance for designing stable defect superlattices in harsh environments.

73 NUCLEAR PHYSICS AND RADIATION PHYSICS↗

D retention and depth profile behavior for single crystal tungsten with high temperature neutron irradiation

Single crystalline W (tungsten) samples irradiated at 633, 963 and 1073 K by neutrons to a damage level of 0.1 dpa were exposed to a high-flux D (deuterium) plasma at 673, 873 and 973 K, respectively, in TPE (Tritium Plasma Experiment) at INL (Idaho National Laboratory). Deuterium desorption was analyzed by TDS (Thermal Desorption Spectroscopy), and D depth profiles were determined by NRA (Nuclear Reaction Analysis) at SNL (Sandia National Laboratories). HIDT (Hydrogen Isotope Diffusion and Trapping) simulation code was applied to evaluate D behavior for neutron-damaged W at higher temperature. The D retention at depths up to 3 f.tm for the neutron-damaged sample at 673 K was two orders of magnitude larger than that for undamaged tungsten, and its D desorption spectrum had a single broad stage at around 900 K. As the neutron irradiation/plasma exposure temperature increased, D retention was largely reduced, and the desorption temperature was increased to higher temperatures above 1100 K. The D depth profiles by NRA also showed D migration toward bulk by higher temperature irradiation, compared to undamaged W. The HIDT simulation indicated that the major binding energy of D was changed from 1.43 eV to 2.07 eV at higher neutron irradiation and plasma exposure temperatures, suggesting that some vacancies and small vacancy clusters would aggregate to form larger voids, or depopulation of weak traps at high D plasma exposure temperatures. It can be said that more stable trapping sites played dominant roles in the D retention at higher neutron irradiation and plasma exposure temperature. The binding energy by HIDT simulation was almost consistent with the reported value by TMAP, but the consideration of not only total D retention measured by TDS but also D depth profile by NRA led to the more accurate D behavior in neutron-damaged W.

36 MATERIALS SCIENCE↗

Irradiation effects on Al 0.3 CoCrFeNi and CoCrMnFeNi high-entropy alloys, and 316H stainless steel at 500 °C

To evaluate the potential of high entropy alloys (HEAs) for nuclear applications, two HEAs, Al 0.3 CoCrFeNi and CoCrFeMnNi, and a conventional Type 316H stainless steel (SS) were irradiated with 1 MeV krypton ions at 500 degrees C up to 1 dpa, and examined in-situ with a transmission electron microscope (TEM). After irradiation, a high density of ordered L1 2 nanoparticles was observed in Al 0.3 CoCrFeNi. In contrast, no phase transformation was observed in CoCrFeMnNi and 316H SS. In the thin foil regions of TEM samples, stacking-fault tetrahedra were observed in the HEAs. In the thick foil regions, interstitial dislocation loops were observed for all alloys, and the areal loop density increased linearly with foil thickness. The Al 0.3 CoCrFeNi had the largest loop size (the lowest density), followed by the CoCrFeMnNi and then the 316H SS. The higher loop nucleation rate in the 316H SS was attributed to carbon content. Finally, the degree of irradiation hardening was slightly lower for the HEAs than for the 316H SS, which is a promising sign for the nuclear application of HEAs at high temperatures.

36 MATERIALS SCIENCE↗

Dislocation loop evolution in F/M steel T91 under in-situ ion irradiation: Influence of the presence of initial dislocations

Ferritic/Martensitic (F/M) steel T91 was irradiated in-situ to 4 and 10 dpa at 470 °C using 1 MeV Kr 2+ . Additionally, the microstructure evolution under irradiation was followed and characterized by in-situ Transmission Electron Microscopy (TEM), in terms of dislocation loop Burgers vector, average size and density as a function of dose. Furthermore, the influence of the presence of dislocations in the pre-irradiated matrix was investigated by comparing the radiation induced defect evolution in grains with and without initial dislocations.

36 MATERIALS SCIENCE↗

Irradiation Damages of Structural Materials under Different Irradiation Environments

For the advancement and development of nuclear systems used in heavy irradiation environments such as fusion DEMO reactors, fission reactors, fast reactors, and accelerator driven target systems, it is necessary to fully understand the changes of mechanical properties and the other properties of the materials induced by irradiation and to clarify the synergistic effect of displacement damage and helium generation. In this study the mechanical property changes and microstructural development induce by displacement damage and helium production have been mainly examined in austenitic stainless steels, 316FR and type304, and ferritic/martensitic steel, HCM12A, irradiated at around 550oC in JRR-3M reactor and/or JOYO fast reactor. At 550°C, 316FR steel was superior to 304 steel in terms of the amount of ductility and strength with respect to irradiation resistance. It is noteworthy that at 550 °C as well as room temperature, the higher fracture strength of the 316FR steels is a remarkable result. It is found that helium atoms strongly influenced on creep lifetime of the irradiated austenitic stainless steel, 316FR. It was found that the ratio of creep rupture time is slightly lower than the lower limit of previous study’s Miyaji and co-workers in the region from 0.01 appm to 1 appm. It is also found that the lower limit of reduction ratio of creep rupture time (irradiation specimen to unirradiation one) does not decrease linearly with the helium production above 10 appm up to about 33 appm. dpa enhanced the reduction of creep lifetime. Recent R&D of high-energy accelerator driven target systems used under heavy irradiation environment is also introduced and discussed for high radiation resistance materials such as Ti alloys with very high number density of nano size precipitate, which have been studying under RaDIATE collaboration, from points of view of irradiation damage and materials development.

radiation damage, structural alloys, neutron irrad↗

Tensile properties of powder-metallurgical-processed tungsten alloys after neutron irradiation near recrystallization temperatures

The tensile properties of powder-metallurgical-processed Pure W, K-doped W, W-3%Re, and K-doped W-3%Re were examined after neutron irradiation up to 0.7 dpa at 910–1020 °C with a thermal neutron shield in the High Flux Isotope Reactor (HFIR). After irradiation, recrystallized Pure W (R) exhibited a brittle fracture mode, while recrystallized K-doped W-3%Re (R) exhibited a ductile fracture mode at 500 °C. K-doped W-3%Re (R) has fine grains, and hence, contains a considerable number of grain boundaries that act as sinks for irradiation defects. Solid solute Re in the W matrix could improve not only the mechanical properties of W, but also its resistance to neutron irradiation. At 500 °C, the ductility of K-doped W-3%Re after irradiation was significantly higher than that of Pure W. The irradiation at ~1000 °C did not induce hardening of stress-relieved (SR) W materials, but SR W materials tended to exhibit a decrease in the ultimate tensile strength (UTS) and an increase in total elongation (TE). Here, the softening due to the recovery and recrystallization of SR W materials and the hardening due to the formation of irradiation defect clusters were balanced during irradiation at ~1000 °C, and ductility was exhibited without an increase in strength.

36 MATERIALS SCIENCE↗

Thermal diffusivity of irradiated tungsten and tungsten-rhenium alloys

The Japan-US PHENIX project irradiated tungsten materials in the RB-19J capsule experiment in the High Flux Isotope Reactor (HFIR). A gadolinium (Gd) shielding was used to absorb the thermal neutrons and reduce rhenium and osmium generation in tungsten. Pure tungsten and K-doped W-3% Re samples were irradiated at 532 – 662 °C to dose of 0.21-0.46 dpa, with the grain orientation perpendicular or parallel to the disk surface. Thermal diffusivity measurements were performed from 100 °C to 500 °C. Furthermore, additional measurements followed after annealing up to 900 °C. Irradiated pure tungsten specimens showed similar thermal diffusivity results compared with an unirradiated W-1% Re specimen in another study. The transmutation amount of Re was calculated to be about 0.52% for those specimens that showed good agreement with this study. Specimens irradiated in this study to different doses presented almost the same thermal diffusivity. Annealing up to 800 °C resulted in no recovery of thermal diffusivity. These results show that the contribution of crystalline defects to degradation of thermal diffusivity is quite limited. In addition, the thermal diffusivity of the irradiated specimens was getting close to that of the unirradiated specimens at elevated temperature.

36 MATERIALS SCIENCE↗

Void shrinkage in 21Cr32Ni austenitic model alloy during in-situ ion irradiation

Austenitic 21Cr32Ni model alloy thin foils, previously irradiated with 5 MeV Fe ++ ions in bulk to create voids, were re-irradiated in-situ in the Intermediate Voltage Electron Microscope Facility (IVEM). The voids which had been formed under bulk-ion irradiation shrank and disappeared after in-situ Kr ion irradiation in the temperature range 50 K-713 K to an additional dose of 1 dpa. The voids were unaffected by eithersuccessive thermal annealing to 673 K and by prolonged exposure to the 200 keV electron beam at the irradiation temperature. The high void shrinkage rate observed did not change significantly for irradiation temperatures between 50 K and 713 K, suggesting that the void shrinkage process in thin foils during in-situ heavy-ion irradiation results from the interactions of displacement cascades with the voids. Finally, possible void shrinkage mechanisms under thin foil irradiation are discussed in this study.

36 MATERIALS SCIENCE↗

Oxide dispersoid coherency of a ferritic-martensitic 12Cr oxide-dispersion-strengthened alloy under self-ion irradiation

Ferritic-martensitic oxide-dispersion-strengthened (ODS) alloy has shown excellent mechanical property and high radiation tolerance. However, the stability of dispersoids during displacive irradiation in the individual ferritic and martensitic phases is unclear. In this work, the correlation among dispersoid coherency, size, density, and matrix phase are studied in dual-phase 12Cr ODS after 100 peak displacements-per-atom (dpa) irradiation at 475°C, using 3.5 MeV Fe 2+ self-ions. The size and density changes of coherent and incoherent dispersoids were analyzed as a function of irradiation depth. The average dispersoid size decreased after irradiation in both phases, and the large incoherent dispersoids in the tempered martensite phase underwent a more dramatic change than those in the ferrite phase. The dispersoid density significantly increased in the ferrite phase within the irradiated region, mostly resulting in an increase in coherent dispersoid density. On the other hand, only a small change in density was observed in the tempered martensite phase for both coherent and incoherent dispersoids. This study shows that dispersoid evolution is dramatically different in ferrite and tempered martensite phases.

36 MATERIALS SCIENCE↗

Heavy ion irradiation response of an additively manufactured 316LN stainless steel

Additive manufacturing has become an appealing technique to fabricate three-dimensional metallic materials and components for nuclear reactors. However, response of additively manufactured alloys to high-dose heavy ion irradiations at elevated temperatures is still not well understood. Here, an additively manufactured 316LN austenitic stainless steel with high-density solidification cells was irradiated using 3.5 MeV Fe ion to a peak dose of 220 dpa at 450 °C. Microscopy studies show a lower Frank loop density and smaller size in the additively manufactured sample compared with its cold worked counterpart, and the cellular structures may largely suppress the formation of perfect loops and dislocation networks and reduce the magnitude of solute segregations comparing with high angle grain boundaries. In conclusion, the present work advances the understanding on the high-temperature irradiation response of additively manufactured steels for nuclear reactor applications.

36 MATERIALS SCIENCE↗

High-throughput ion irradiation of additively manufactured compositionally complex alloys

Several advanced nuclear reactor designs promise efficiency and safety improvements over the current reactor fleet but are limited by the current set of ASME code-qualified materials. Novel alloys including high-entropy alloys (HEAs), and more broadly compositionally complex alloys (CCAs), have shown promising irradiation-tolerance. However, the vast range of alloy compositions adds to an already time-consuming alloy development process. In this study, to accelerate the development of novel alloys for nuclear applications, a high-throughput (HTP) methodology has been employed. Additive manufacturing has been used to produce a compositional array of unary, binary, ternary, and quaternary alloys, including several CCAs, which span the Cr-Fe-Mn-Ni composition space. Additionally, the compositional array was homogenized at 1000°C for 24 hours and each sample was irradiated using 4-MeV Ni2+ ions at room temperature to a peak damage of 50 dpa, as estimated using SRIM, at the University of Wisconsin Ion Beam Laboratory. A custom XY stage was built to accommodate the large compositional array and half of each sample was masked during irradiation enabling both the irradiated and unirradiated properties of each alloy to be characterized side-by-side. Each alloy was characterized using X-ray fluorescence (XRF), X-ray diffraction (XRD), scanning electron microscopy (SEM), energy dispersive spectroscopy (EDS), and nanoindentation. CALPHAD simulations spanning the entire Cr-Fe-Mn-Ni composition space at 1000°C were performed to compare predicted equilibrium phases with phases identified experimentally from the unirradiated regions of each alloy. Nanoindentation measurements indicate radiation-induced hardening ranging from ~1-1.5 GPa in each of Cr-Fe-Mn-Ni CCAs, which is relatively insensitive to modest changes in alloy composition and comparable to hardening observed in neutron irradiated Cr-Fe-Mn-Ni CCAs in the literature. Overall, a substantial time savings was realized by employing HTP synthesis, irradiation, and characterization in this study compared to conventional techniques, the implications of which are discussed.

36 MATERIALS SCIENCE↗

Deconvoluting the Effect of Chromium and Aluminum on the Radiation Response of Wrought FeCrAl Alloys After Low-Dose Neutron Irradiation

FeCrAl alloys have been extensively investigated over the past decade as a candidate material for accident-tolerant fuel cladding in light water reactors. Here, we have completed a first of its kind study where Al and Cr concentrations are varied systematically under neutron irradiation to elucidate the post irradiation microstructural and mechanical response as a direct result of alloying content. Neutron irradiations were performed on alloys with composition Fe-(10-13)Cr-(5-7)Al in wt.% at temperatures of 214, 357, and 557°C to a dose of ~1.8 dpa (displacements per atom). Dislocation loop sizes and dispersion characteristics did not show strong compositional dependence. However, there were noticeable effects of composition on the dispersion of Cr-rich α'-precipitates, particularly a decrease in number density with increasing Al content or a decrease in Cr content. The present results confirm previous studies indicating the Cr concentration in these precipitates is lower than that expected in binary FeCr alloys and that Al can act as a destabilizing alloying element for the deleterious α'-phase.

36 MATERIALS SCIENCE↗

Mechanical behavior of additively manufactured and wrought 316L stainless steels before and after neutron irradiation

Fabrication of nuclear reactor components using additive manufacturing (AM) methods is now a practical option since the AM technologies have advanced to allow for building of complex parts with high quality materials. To assess the mechanical performance of printed components in reactor-relevant conditions and to build a property database for the AM 316L stainless steel (SS), mechanical testing and characterization were performed before and after neutron irradiation. In this work, miniature tensile specimens were irradiated at the High Flux Isotope Reactor (HFIR) to 0.2 and 2 displacements per atom (dpa) at 300 and 600°C. The AM 316L SS was tested in the as-built, stress-relieved, and solution-annealed conditions, and the wrought (WT) 316L SS in solution-annealed condition as a reference alloy. The baseline test result showed that the AM 316L SS, regardless of the post-build heat treatment, had higher strength than the WT 316L SS, but similar ductility. Post-irradiation tensile testing was conducted at RT, 300°C, and 500°C for selected irradiation conditions. Neutron irradiation induced significant changes in the mechanical behavior of the AM stainless steels, including both hardening and softening. Although the as-built 316L steel after 300°C irradiation showed necking just after yielding, the overall property changes of the as-printed alloy became less significant after 600°C irradiation. Irradiation-induced ductilization was also observed after the higher temperature irradiation. In general, the strength change was smaller in the relatively stronger as-built and stress-relieved AM SSs than in the solution-annealed AM and WT SSs. These relatively lower strength 316L SSs overall retained higher ductility in the irradiation conditions tested, but the stronger 316L SSs demonstrated a similar level of ductility after the higher temperature (600°C) irradiation. It is a positive assessment for the AM 316L materials that no embrittlement was observed within the test and irradiation conditions of the experiment.

36 MATERIALS SCIENCE↗

A microscopic and crystallographic study of proton irradiated alloy 718

Solution annealing and age hardening are important processes for achieving good engineering and chemical properties of alloy 718. The composition of alloy 718 also plays an important role as it can affect both mechanical (γ”- and γ’-phase formation) and irradiation behaviors. Therefore, in this study five different sets of alloy 718 samples with two different chemical compositions were fabricated using different processing conditions and irradiated up to 4 dpa. Based on the effects of irradiation on the microstructural data of γ”- and γ’-phases, irradiation-induced dislocation statistics, and crystallographic data, it can be inferred that the samples processed at high solution annealing temperature (1093°C) behave better under irradiation compared to the samples processed at low solution annealing temperatures (945 and 1065°C).

36 MATERIALS SCIENCE↗