Data on Cu- and Ni-Si-Mn-rich solute clustering in a neutron irradiated austenitic stainless steel

The data presented in this article is supplementary to the research article “Phase instabilities in austenitic steels during particle bombardment at high and low dose rates” (Levine et al.). Needle-shaped samples were prepared with focused ion beam milling from a 304L stainless steel that was irradiated with fast neutrons (E 0.1 MeV) in the BOR-60 reactor at 318 °C to 47.5 dpa. Atom probe tomography (APT) experiments in voltage mode were then conducted on a Cameca LEAP 5000X HR. Atom position, range, and mass spectrum files after reconstruction with Cameca’s IVAS software are included. Cu- and Ni-Si-Mn-rich solute nanoclusters were identified and analyzed using the Open Source Characterization of APT Reconstructions (OSCAR) program. Python code for OSCAR, information on the program’s underlying algorithm, and sample output files are provided. A proximity histogram of a Ni-Si-Mn-rich cluster and a 1D density/solute concentration profile of a Cu-rich cluster are given to demonstrate OSCAR’s analytical functionalities. The provided APT dataset is valuable for benchmarking phase instabilities in neutron-irradiated austenitic stainless steels that occur at high doses. The OSCAR program can be reused to process other APT data sets where solute nanoclustering is of interest.

42 ENGINEERING↗

Irradiation hardening and ductility loss of Eurofer97 steel variants after neutron irradiation to ITER-TBM relevant conditions

Ten Eurofer97 steel variants, produced by non-standard fabrication-processing routes and modified alloying chemistries, were studied by neutron irradiations in the high flux isotope reactor. The irradiations were performed to ITER-TBM relevant conditions of ~255–350 °C, 2.94–3.24 dpa. We quantified the irradiation-induced degradation of the steels using mechanical property tests. All the steels suffered from irradiation hardening, where a significant increase in Vickers microhardness and yield stress (σ YS ) occurred, accompanied with severe loss of tensile elongation. The extent of hardening was material dependent. For T irr = 300±30 °C, most steels showed σ YS increase in the range of ~30% to as high as ~66%, except for a low temperature tempered steel with σYS increase below 15%. Despite large losses in elongation, most failures were ductile. Significant post-necking ductility was retained with reduction in area (RA) between 65–75%, but <50% for low temperature tempered steels. The ultimate tensile stress to yield stress (σ UTS /σ YS ) ratios decreased significantly after irradiation, highlighting irradiation-induced strain hardening capacity reduction. No major effect of irradiation on the plastic instability stress (σ PIS ) and true fracture stress of the steels was observed. By comparing the tensile stresses in true stress units and with literature, the results suggest that RAFM steel designing should target materials with a large separation between σ PIS and σ YS , to ensure the materials can maintain large work hardening and uniform deformation capability after irradiation. The tensile data of the steels additionally revealed a compelling evidence of an inverse trend between the change in RA and increase in σ YS of the neutron irradiated Eurofer97 type steels.

36 MATERIALS SCIENCE↗

A methodology for corrosion testing ODS steels in liquid tin under reactor conditions in HFIR

Liquid metal–based divertor concepts have promising attributes for application in fusion reactors. Liquid tin is being considered as one of those liquid metals due to its excellent thermophysical properties. However, tin is extremely corrosive to steels at elevated temperatures, and the coupled effects of corrosion with neutron irradiation for application in fusion reactors have not been quantified. Researchers at Oak Ridge National Laboratory (ORNL) have designed and irradiated a series of capsules in the High Flux Isotope Reactor (HFIR) to help address gaps in the literature with respect to coupled corrosion and neutron irradiation effects. The capsules are filled with solid tin designed to melt due to the gamma heating in HFIR and allow interaction with the specimens. The capsules contain a SiC thermometer for post-irradiation temperature verification. Five capsules were irradiated in HFIR for 10.5 days, accumulating 0.93 dpa in the FeCrAl specimens. Post-irradiation temperature verification was performed on the SiC thermometers, and temperatures were observed to be higher than what was expected from thermal models. An explanation for the model underprediction is given herein. In conclusion, the capsules described within this article are the first to irradiate liquid metal within the HFIR flux trap and demonstrated the safety basis for continued liquid coolant studies in HFIR.

FeCrAl↗

Preliminary neutronic and thermal analysis of Inertial Fusion Energy systems with a focus on thick liquid wall concepts

This paper provides an assessment of the neutronic behavior of Inertial Fusion Energy systems using the Serpent 2 Monte Carlo code. The study explores different types of reactor concepts, including dry-wall and thick liquid wall systems. In particular, it characterizes the tritium breeding and energy multiplication performance, as well as the effect of long-term irradiation on structural materials. For this purpose, the displacement per atom (DPA) and the gas production rate in structural materials are calculated. A simplified geometry with varying geometrical parameters is used as a representation for the different kinds of devices. Additionally, the case of the HYLIFE-II concept is used to assess modeling inaccuracies arising from certain approximations. A comparison between the simplified geometry and a realistic one is performed, thanks to Serpent’s capability to run transport calculations on unstructured meshes. The study then addresses the impact of these discrepancies on the temperature distribution in the first wall using the GeN-Foam code for conjugate heat transfer analysis. The results highlight the necessity to consider the heterogeneous nature of the liquid wall, as simplified models tend to underestimate radiation damage metrics and heat loads.

Conjugate heat transfer↗

Neutron irradiation-enhanced grain growth in tungsten and tungsten alloys

Herein, to understand the microstructural stability of candidate plasma-facing materials under fusion-relevant environments, neutron irradiation of W and W-3%Re alloys with and without K and La dopants was performed in the mixed-spectrum High Flux Isotope Reactor at nominal temperatures of ~850 °C and ~1100 °C to calculated doses between 0.42 and 0.47 dpa. To the best of our knowledge, this study presents the first experimental evidence of radiation-enhanced recrystallization in W and undoped W–Re alloys at ~850 °C, conditions where thermal annealing does not cause any grain growth in a similar timescale. Potassium- or lanthanum-doped tungsten alloys showed more resistance to radiation-enhanced grain growth. We explain the acceleration of grain growth by analyzing the self-diffusion constant under atomic displacement environments. The microstructural observations of the studied W variants suggest that La doping is more effective than K doping for mitigating recrystallization. This study also found that radiation-enhanced recrystallization is an important consideration when designing and applying W to plasma-facing components in future nuclear fusion reactors.

36 MATERIALS SCIENCE↗

Lattice response to ambient self-irradiation of δ-phase 239 Pu-Ga alloys exposed to cryogenic temperatures

Self-irradiation in plutonium is a continuous process that introduces radiation damage ranging from point defects to nanoscale radiation damage as well as decay daughter product impurities that require to be accommodated by the host material. These changes are affecting the structure and properties of the material by lattice swelling, mechanical strengthening, and other alterations. X-ray diffraction and dilatometry studies have shown that the room temperature self-irradiation of δ-phase Pu-Ga alloys (2 and 7 at%Ga) results in swelling of the lattice that saturates after 0.1–0.2 displacement per atom (dpa) of accumulated lattice damage. Here, for a better understanding of these self- irradiation processes, defect accumulation and damage evolution, this time-of-flight neutron diffraction study investigates the impact of ambient self-irradiation effects on the structural evolution of δ-phase 239 Pu-Ga alloys exposed to cryogenic temperatures (<120 K), associated with a varied history of storage time and thermal treatments. Two key behaviors were observed in the lattice evolution after exposure to cryogenic temperatures with respect to room-temperature accumulated self-irradiation damage. Samples with no self- irradiation damage accumulation under ambient conditions showed swelling of the lattice at the end of the measurement, while samples that accumulated significant self-irradiation damage under ambient conditions showed only a partial recovery of the lattice parameter value upon completion of the measurements (cooling followed by heating back to room temperature). Possible causes of the behavior are proposed, and their associated effects are discussed.

36 MATERIALS SCIENCE↗

Bulk synthesis of radiation resistant W – Ti – Cr – V compositionally complex alloys

Refractory compositionally complex alloys are candidate material systems for next generation advanced nuclear reactors. This work showcases the first successful bulk synthesis of low activation W–Ti based refractory compositionally complex alloys using arc melting and provides insights on using additive manufacturing for these compositions using directed energy deposition. Both techniques produce equiaxed grains composed of a tungsten matrix with Ti–V–Cr dendritic boundaries. The arc melted specimen possesses a multi-modal grain size distribution, while the directed energy deposition specimen possesses a more gaussian distribution of grain size. Both arc melted and directed energy deposition specimens demonstrate high thermal stability up to 900 °C, as well as promising radiation resistance with low loop formation and the presence of homogeneously distributed helium cavities maintaining small diameters at ≥10 dpa under simultaneous light (helium) and heavy (krypton) ion irradiation at 900 °C.

Arc melting (AM)↗

Defect evolution in Ni and solid-solution alloys of NiFe and NiFeCoCr under ion irradiation at 16 and 300 K

Single-phase concentrated solid-solution alloys (SP-CSAs) have shown unique chemical complexity at the levels of electrons and atoms, and their defect evolution is expected to be different from conventional dilute alloys. Single crystals of Ni, NiFe and NiFeCoCr are chosen as model systems to understand the chemical complexity on defect formation and damage accumulation in SP-CSAs under ion irradiation. The high-quality crystals were irradiated at 16 and 300 K to different ion fluences, to form irradiated region with little to heavy damages. Additionally, the ion-induced damage was determined using Rutherford backscattering spectrometry technique along a channeling direction (RBS/C) and the level of lattice damage in irradiated Ni and SP-CSAs was quantified from Monte Carlo (MC) simulations. The results are interpreted using the Multi Step Damage Accumulation model to reveal material damage accumulation kinetics. Key findings of the study are that in case of room temperature irradiations the damage level measured for complex alloys at the highest irradiation fluence of 2 × 10 15 cm -2 (~3 dpa) is significantly higher than that obtained for pure nickel samples and suggest two-step damage accumulation process with a defect transformation taking place at a fluence of about 1.5 × 10 15 cm -2 . Furthermore, structural and damage kinetic differences clearly imply that, with increasing degree of chemical complexity and high solid-solution strengthening effects from Ni to NiFe and to NiFeCoCr, the enhanced lattice stiffness resists to randomization of atomic configurations and inhibits the growth of extended defects.

36 MATERIALS SCIENCE↗

Dislocation loop evolution and radiation hardening in nickel-based concentrated solid solution alloys

Effects of chemical composition, ion irradiation dose and temperature on unfaulting of irradiation induced Frank dislocation loops to perfect loops in two nickel based single-phase solid solution alloys, Ni–20Fe and NiFe–20Cr, have been studied. The fraction of Frank loops decreases with irradiation dose from 7.2 to 38.4 dpa at 500°C, but with more Frank loops remaining in the ternary alloy. However, perfect loops and dislocation networks become the dominant features of defects at 580°C in both alloys. The results indicate a thermally assisted loop unfaulting process that may be hindered by more sluggish defect motion in the alloy with more chemical components. Nano-indentation with both continuous stiffness method and single indentation method are used to measure radiation hardening. Loop unfaulting in both alloys irradiated at 580°C reduced radiation hardening while significant hardening is observed after irradiation at 500°C. The quasi-static single indentation method exhibits lower hardness results compared to continuous stiffness method, because dislocations induced from the cyclic loading in the latter method get relaxed and stabilized, resulting in higher resistance to the indenter.

36 MATERIALS SCIENCE↗

Disordering of helium gas bubble superlattices in molybdenum under ion irradiation and thermal annealing

Self-organization of gas bubbles causes the formation of an ordered array of nanoscale gas bubbles (a gas bubble superlattice), a highly efficient mechanism for gas storage under irradiation. Here, the stability of helium (He) gas bubble superlattices in molybdenum (Mo) under krypton (Kr) ion irradiation and thermal annealing has been investigated. The He gas bubble superlattices gradually become disordered under Kr ion irradiation at 300° C, and the order-disorder transformation process completes at 2.5 dpa. Both transmission electron microscopy (TEM) and synchrotron-based small-angle X-ray scattering (SAXS) reveal that the order-disorder transformation of He gas bubble superlattices is associated with a slight increase in the average bubble size. Phase-field modeling indicates that the inhomogeneous growth and coarsening of bubbles/voids cause the disordering of imperfect superlattices under irradiation and implies that highly ordered superlattices could potentially exhibit much stronger resistance to irradiation damage. Under thermal annealing, the He gas bubble superlattices in Mo become unstable and disordered at 1000° C with the bubble size increasing from ~1.1 to ~1.6 nm. The finding in this research provides insights into the disordering mechanisms of defect superlattices as well as guidance for designing stable defect superlattices in harsh environments.

73 NUCLEAR PHYSICS AND RADIATION PHYSICS↗

D retention and depth profile behavior for single crystal tungsten with high temperature neutron irradiation

Single crystalline W (tungsten) samples irradiated at 633, 963 and 1073 K by neutrons to a damage level of 0.1 dpa were exposed to a high-flux D (deuterium) plasma at 673, 873 and 973 K, respectively, in TPE (Tritium Plasma Experiment) at INL (Idaho National Laboratory). Deuterium desorption was analyzed by TDS (Thermal Desorption Spectroscopy), and D depth profiles were determined by NRA (Nuclear Reaction Analysis) at SNL (Sandia National Laboratories). HIDT (Hydrogen Isotope Diffusion and Trapping) simulation code was applied to evaluate D behavior for neutron-damaged W at higher temperature. The D retention at depths up to 3 f.tm for the neutron-damaged sample at 673 K was two orders of magnitude larger than that for undamaged tungsten, and its D desorption spectrum had a single broad stage at around 900 K. As the neutron irradiation/plasma exposure temperature increased, D retention was largely reduced, and the desorption temperature was increased to higher temperatures above 1100 K. The D depth profiles by NRA also showed D migration toward bulk by higher temperature irradiation, compared to undamaged W. The HIDT simulation indicated that the major binding energy of D was changed from 1.43 eV to 2.07 eV at higher neutron irradiation and plasma exposure temperatures, suggesting that some vacancies and small vacancy clusters would aggregate to form larger voids, or depopulation of weak traps at high D plasma exposure temperatures. It can be said that more stable trapping sites played dominant roles in the D retention at higher neutron irradiation and plasma exposure temperature. The binding energy by HIDT simulation was almost consistent with the reported value by TMAP, but the consideration of not only total D retention measured by TDS but also D depth profile by NRA led to the more accurate D behavior in neutron-damaged W.

36 MATERIALS SCIENCE↗

Irradiation effects on Al 0.3 CoCrFeNi and CoCrMnFeNi high-entropy alloys, and 316H stainless steel at 500 °C

To evaluate the potential of high entropy alloys (HEAs) for nuclear applications, two HEAs, Al 0.3 CoCrFeNi and CoCrFeMnNi, and a conventional Type 316H stainless steel (SS) were irradiated with 1 MeV krypton ions at 500 degrees C up to 1 dpa, and examined in-situ with a transmission electron microscope (TEM). After irradiation, a high density of ordered L1 2 nanoparticles was observed in Al 0.3 CoCrFeNi. In contrast, no phase transformation was observed in CoCrFeMnNi and 316H SS. In the thin foil regions of TEM samples, stacking-fault tetrahedra were observed in the HEAs. In the thick foil regions, interstitial dislocation loops were observed for all alloys, and the areal loop density increased linearly with foil thickness. The Al 0.3 CoCrFeNi had the largest loop size (the lowest density), followed by the CoCrFeMnNi and then the 316H SS. The higher loop nucleation rate in the 316H SS was attributed to carbon content. Finally, the degree of irradiation hardening was slightly lower for the HEAs than for the 316H SS, which is a promising sign for the nuclear application of HEAs at high temperatures.

36 MATERIALS SCIENCE↗

Dislocation loop evolution in F/M steel T91 under in-situ ion irradiation: Influence of the presence of initial dislocations

Ferritic/Martensitic (F/M) steel T91 was irradiated in-situ to 4 and 10 dpa at 470 °C using 1 MeV Kr 2+ . Additionally, the microstructure evolution under irradiation was followed and characterized by in-situ Transmission Electron Microscopy (TEM), in terms of dislocation loop Burgers vector, average size and density as a function of dose. Furthermore, the influence of the presence of dislocations in the pre-irradiated matrix was investigated by comparing the radiation induced defect evolution in grains with and without initial dislocations.

36 MATERIALS SCIENCE↗

Irradiation Damages of Structural Materials under Different Irradiation Environments

For the advancement and development of nuclear systems used in heavy irradiation environments such as fusion DEMO reactors, fission reactors, fast reactors, and accelerator driven target systems, it is necessary to fully understand the changes of mechanical properties and the other properties of the materials induced by irradiation and to clarify the synergistic effect of displacement damage and helium generation. In this study the mechanical property changes and microstructural development induce by displacement damage and helium production have been mainly examined in austenitic stainless steels, 316FR and type304, and ferritic/martensitic steel, HCM12A, irradiated at around 550oC in JRR-3M reactor and/or JOYO fast reactor. At 550°C, 316FR steel was superior to 304 steel in terms of the amount of ductility and strength with respect to irradiation resistance. It is noteworthy that at 550 °C as well as room temperature, the higher fracture strength of the 316FR steels is a remarkable result. It is found that helium atoms strongly influenced on creep lifetime of the irradiated austenitic stainless steel, 316FR. It was found that the ratio of creep rupture time is slightly lower than the lower limit of previous study’s Miyaji and co-workers in the region from 0.01 appm to 1 appm. It is also found that the lower limit of reduction ratio of creep rupture time (irradiation specimen to unirradiation one) does not decrease linearly with the helium production above 10 appm up to about 33 appm. dpa enhanced the reduction of creep lifetime. Recent R&D of high-energy accelerator driven target systems used under heavy irradiation environment is also introduced and discussed for high radiation resistance materials such as Ti alloys with very high number density of nano size precipitate, which have been studying under RaDIATE collaboration, from points of view of irradiation damage and materials development.

radiation damage, structural alloys, neutron irrad↗

Tensile properties of powder-metallurgical-processed tungsten alloys after neutron irradiation near recrystallization temperatures

The tensile properties of powder-metallurgical-processed Pure W, K-doped W, W-3%Re, and K-doped W-3%Re were examined after neutron irradiation up to 0.7 dpa at 910–1020 °C with a thermal neutron shield in the High Flux Isotope Reactor (HFIR). After irradiation, recrystallized Pure W (R) exhibited a brittle fracture mode, while recrystallized K-doped W-3%Re (R) exhibited a ductile fracture mode at 500 °C. K-doped W-3%Re (R) has fine grains, and hence, contains a considerable number of grain boundaries that act as sinks for irradiation defects. Solid solute Re in the W matrix could improve not only the mechanical properties of W, but also its resistance to neutron irradiation. At 500 °C, the ductility of K-doped W-3%Re after irradiation was significantly higher than that of Pure W. The irradiation at ~1000 °C did not induce hardening of stress-relieved (SR) W materials, but SR W materials tended to exhibit a decrease in the ultimate tensile strength (UTS) and an increase in total elongation (TE). Here, the softening due to the recovery and recrystallization of SR W materials and the hardening due to the formation of irradiation defect clusters were balanced during irradiation at ~1000 °C, and ductility was exhibited without an increase in strength.

36 MATERIALS SCIENCE↗

Thermal diffusivity of irradiated tungsten and tungsten-rhenium alloys

The Japan-US PHENIX project irradiated tungsten materials in the RB-19J capsule experiment in the High Flux Isotope Reactor (HFIR). A gadolinium (Gd) shielding was used to absorb the thermal neutrons and reduce rhenium and osmium generation in tungsten. Pure tungsten and K-doped W-3% Re samples were irradiated at 532 – 662 °C to dose of 0.21-0.46 dpa, with the grain orientation perpendicular or parallel to the disk surface. Thermal diffusivity measurements were performed from 100 °C to 500 °C. Furthermore, additional measurements followed after annealing up to 900 °C. Irradiated pure tungsten specimens showed similar thermal diffusivity results compared with an unirradiated W-1% Re specimen in another study. The transmutation amount of Re was calculated to be about 0.52% for those specimens that showed good agreement with this study. Specimens irradiated in this study to different doses presented almost the same thermal diffusivity. Annealing up to 800 °C resulted in no recovery of thermal diffusivity. These results show that the contribution of crystalline defects to degradation of thermal diffusivity is quite limited. In addition, the thermal diffusivity of the irradiated specimens was getting close to that of the unirradiated specimens at elevated temperature.

36 MATERIALS SCIENCE↗

Void shrinkage in 21Cr32Ni austenitic model alloy during in-situ ion irradiation

Austenitic 21Cr32Ni model alloy thin foils, previously irradiated with 5 MeV Fe ++ ions in bulk to create voids, were re-irradiated in-situ in the Intermediate Voltage Electron Microscope Facility (IVEM). The voids which had been formed under bulk-ion irradiation shrank and disappeared after in-situ Kr ion irradiation in the temperature range 50 K-713 K to an additional dose of 1 dpa. The voids were unaffected by eithersuccessive thermal annealing to 673 K and by prolonged exposure to the 200 keV electron beam at the irradiation temperature. The high void shrinkage rate observed did not change significantly for irradiation temperatures between 50 K and 713 K, suggesting that the void shrinkage process in thin foils during in-situ heavy-ion irradiation results from the interactions of displacement cascades with the voids. Finally, possible void shrinkage mechanisms under thin foil irradiation are discussed in this study.

36 MATERIALS SCIENCE↗

Oxide dispersoid coherency of a ferritic-martensitic 12Cr oxide-dispersion-strengthened alloy under self-ion irradiation

Ferritic-martensitic oxide-dispersion-strengthened (ODS) alloy has shown excellent mechanical property and high radiation tolerance. However, the stability of dispersoids during displacive irradiation in the individual ferritic and martensitic phases is unclear. In this work, the correlation among dispersoid coherency, size, density, and matrix phase are studied in dual-phase 12Cr ODS after 100 peak displacements-per-atom (dpa) irradiation at 475°C, using 3.5 MeV Fe 2+ self-ions. The size and density changes of coherent and incoherent dispersoids were analyzed as a function of irradiation depth. The average dispersoid size decreased after irradiation in both phases, and the large incoherent dispersoids in the tempered martensite phase underwent a more dramatic change than those in the ferrite phase. The dispersoid density significantly increased in the ferrite phase within the irradiated region, mostly resulting in an increase in coherent dispersoid density. On the other hand, only a small change in density was observed in the tempered martensite phase for both coherent and incoherent dispersoids. This study shows that dispersoid evolution is dramatically different in ferrite and tempered martensite phases.

36 MATERIALS SCIENCE↗