208 records · Page 12

Surviving nanoscale interfacial stability in extreme thermal expansion contrast Zn(CN) 2 -epoxy resin matrix composites

Here, we report the remarkable stability at the nanoscale matrix-filler interface in a series of overall low coefficient of thermal expansion (CTE) zinc cyanide (ZC)/epoxy resin composites. These interfaces demonstrate the stability of highly contrasting materials. These composites are designed to optimize the properties of both materials: epoxy resins are valued for their high strength, superb chemical resistance, low dielectric properties, and adhesive abilities. ZC, a model flexible framework, exhibits negative thermal expansion (NTE) behavior and compensates for the epoxy resin’s detrimentally large thermal expansion values. Filled resins minimize the native 65 ppm/°C CTE values to 19 ppm/° C over a wide temperature range while maintaining linearity, yielding composites compatible with typical metal and ceramic substrates’—commonly bonded to the resin— 0–20 ppm/° C CTE values. Additionally, with significant intrinsic differences in the materials, we use wide-angle X-ray diffraction and atomic force microscopy to elucidate thermal movement. The ZC/epoxy interface is surprisingly resilient over 1,000 cycles between -55° C and 75° C, extremes typical to aerospace applications. Further, we show that the resin viscosity remains less than 21 Pa*s at up to 30 vol% ZC, an important consideration for workability. We also discuss settling distribution, glass transition temperature, flexural strength, and longevity. All results point favorably towards practical implementation in low thermal expansion application needs: filling the gap in component design.

42 ENGINEERING↗

Silicon carbide fiber composite receiver tubes manufactured by PIP process

The performance of SiC fiber composites made by a polymer infiltration and pyrolysis (PIP) process was investigated. Two types of tubular composites were manufactured using Hi-Nicalon and Nicalon-CG silicon carbide fibers infiltrated with SMP10 silicon carbide matrix. The fiber content in both composites was about 25 vol.% with an average density of 2.39 g/cc. The tubular SiC composites showed stable solar absorptance and emittance of 0.97 and 0.91, respectively, at 800 °C. The composites were thermally shocked at 900, 1000, and 1100 °C with a waterjet simulating raindrops. As a result, the hoop tensile strength of the composites revealed no loss of mechanical strength due to the thermal shock experiments up to 1100 °C.

14 SOLAR ENERGY↗

Carbon Additive Manufacturing with a Near-Replica “Green-to-Brown” Transformation

Nanocomposites containing nanoscale materials offer exciting opportunities to encode nanoscale features into macroscale dimensions, which produces unprecedented impact in material design and application. However, conventional methods cannot process nanocomposites with a high particle loading, as well as nanocomposites with the ability to be tailored at multiple scales. A composite architected mesoscale process strategy that brings particle loading nanoscale materials combined with multiscale features including nanoscale manipulation, mesoscale architecture, and macroscale formation to create spatially programmed nanocomposites with high particle loading and multiscale tailorability is reported. The process features a low-shrinking (<10%) “green-to-brown” transformation, making a near-geometric replica of the 3D design to produce a “brown” part with full nanomaterials to allow further matrix infill. Here, this demonstration includes additively manufactured carbon nanocomposites containing carbon nanotubes (CNTs) and thermoset epoxy, leading to multiscale CNTs tailorability, performance improvement, and 3D complex geometry feasibility. The process can produce nanomaterial-assembled architectures with 3D geometry and multiscale features and can incorporate a wide range of matrix materials, such as polymers, metals, and ceramics, to fabricate nanocomposites for new device structures and applications.

36 MATERIALS SCIENCE↗

Understanding the Influence of Li 7 La 3 Zr 2 O 12 Nanofibers on Critical Current Density and Coulombic Efficiency in Composite Polymer Electrolytes

Composite polymer electrolytes (CPEs)are attractive materials for solid-state lithium metal batteries, owing to their high ionic conductivity from ceramic ionic conductors and flexibility from polymer components. As with all lithium metal batteries, however, CPEs face the challenge of dendrite formation and propagation. Not only does this lower the critical current density (CCD) before cell shorting, but the uncontrolled growth of lithium deposits may limit Coulombic efficiency (CE) by creating dead lithium. Here, we present a fundamental study on how the ceramic components of CPEs influence these characteristics. CPE membranes based on poly-(ethylene oxide) and lithium bis-(trifluoro methane sulfonyl)-imide(PEO-LiTFSI) with Li 7 La 3 Zr 2 O 12 (LLZO) nanofibers were fabricated with industrially relevant roll-to-roll manufacturing techniques. Galvanostatic cycling with lithium symmetric cells shows that the CCD can be tripled by including 50 wt % LLZO, but half-cell cycling reveals that this comes at the cost of CE. Varying the LLZO loading shows that even a small amount of LLZO drastically lowers the CE, from 88% at 0 wt % LLZO to 77% at just 2 wt % LLZO. Mesoscale modeling reveals that the increase in CCD cannot be explained by an increase in the macroscopic or microscopic stiffness of the electrolyte; only the microstructure of the LLZO nanofibers in the PEO-LiTFSI matrix slows dendrite growth by presenting physical barriers that the dendrites must push or grow around. This tortuous lithium growth mechanism around the LLZO is corroborated with mass spectrometry imaging. In conclusion, this work highlights important elements to consider in the design of CPEs for high-efficiency lithium metal batteries.

36 MATERIALS SCIENCE↗

Corrosion Testing of Refractory inContact with Molten Glasses Designed for Waste Vitrification - VSL Touchpoint Matrix Glasses

It is known that the predictive life of the refractory ceramic liner of nuclear waste glass melters is conservative, as demonstrated by performance of these materials such as in the Defense Waste Processing Facility (DWPF). The motivation for this task is to maximize the useful life of the melters that will be operated at the Waste Treatment and Immobilization Plant (WTP), which will in turn minimize procurement and disposal costs and melter outage times, as well as to identify maximum loadings in the waste glass of those species that corrode melter components. This task was initiated jointly with Pacific Northwest National Laboratory (PNNL) with the objective to develop a methodology and model to enable more accurate prediction of refractory service life under prototypic conditions from laboratory-scale material corrosion tests. Refractory corrosion is generally reported as physical material loss, measured in units of distance (e.g., inch) or as physical material loss rate, measured in units of distance per time (e.g., inch/day). In post-operational melters, the refractory corrosion is measured directly, sometimes reported as corrosion depth. Crucible tests are used in the laboratory to accelerate the refractory corrosion to facilitate a meaningful measurement in a commensurate amount of time. Crucible tests are particularly useful in understanding refractory corrosion across a large glass composition space, where operational testing would be prohibitive. Some of the critical parameters that are known to influence refractory corrosion by molten glass in a crucible test are temperature, system redox, molten salt phases, glass chemistry, and test duration. The majority of data collected for Monofrax® K-3 (hereafter referred to as K-3) corrosion is from crucible tests, but a small amount comes directly from scaled and production melters. Crucible test data has been collected under varying conditions, whereas data collected from operational melters is relatively fewer and represents conditions specific to the melter campaign. The result is that the published data can be grouped and analyzed in multiple ways, not all of which are readily comparable. The Standard Test Method for Isothermal Corrosion Resistance of Refractories to Molten Glass (ASTM C621) outlines the general guidelines used across industry. That method describes a sealed, static test in which the surface area of the refractory coupon and the volume of glass are fixed. A significant portion of the crucible data pertaining to nuclear waste glasses has been collected in a modified configuration; the most notable differences being the surface area of the refractory coupon to volume of the glass and use of a method for bubbling the melt. To our knowledge, the influence of those parameters on the refractory corrosion has not been quantified. In this work, it was determined that static tests and bubbled tests would be performed. Savannah River National Laboratory (SRNL) was tasked with setting up and performing static testing while PNNL was tasked with setting up and performing bubbled testing. Initial activities were performed to establish laboratory methods that reproduce data comparable to existing data sets of K-3 refractory corrosion by low activity waste (LAW) and high-level waste (HLW) glass compositions. Later activities were focused on refining the test parameters to establish a standard test practice to be used between Laboratories and collecting additional data to be used in the enhanced waste glass model development. This document serves primarily to convey the refractory loss measurement results from corrosion testing of K-3 refractory with waste glass compositions developed for use in the WTP melters. The data will be used in the enhanced property/composition models being developed for waste glass vitrification and melter operations.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Multicomponent pyrochlore solid solutions with uranium incorporation – A new perspective of materials design for nuclear applications

Multicomponent pyrochlore solid solutions with and without uranium incorporation were fabricated and their thermal-mechanical properties were characterized. Multicomponent pyrochlore solid solutions without uranium exhibit comparable thermal conductivity and higher mechanical strength compared to baseline single component rare-earth titanate pyrochlore (A 2 Ti 2 O 7 ). Uranium incorporation reduces hardness as compared with single component compositions. High entropy pyrochlore with uranium displays the highest thermal conductivity within multicomponent pyrochlore solid solutions with significantly better mechanical properties than UO 2 . The measured thermal conductivity correlates well with A-site cation mixing entropy and a modified size disorder parameter, and thus the size disorder and mixing entropy could be good indicators for predicting thermal conductivity of multicomponent pyrochlore solid solutions. This work opens up the possibility of designing multicomponent oxide solid solutions by controlling their chemical disorder/mixing entropy to achieve acceptable thermal-mechanical properties, desired radiation and corrosion performance for potential nuclear waste form and inert matrix fuel applications.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Structural Origins of High MoO 3 Solubility in Peraluminous Borosilicate Glasses

Molybdenum (Mo) imposes strict loading limits in conventional borosilicate nuclear waste glasses due to the tendency of tetrahedral molybdate [MoO 4 ] 2− species to phase-separate and crystallize as alkali molybdates. Here, we demonstrate an unprecedented 13.96 wt % (7.51 mol %) MoO 3 solubility in peraluminous sodium aluminoborosilicate glasses a ∼15× increase over their peralkaline counterparts. Using Raman spectroscopy, multinuclear and dipolarcorrelation magic angle spinning nuclear magnetic resonance (MAS NMR), electron paramagnetic resonance (EPR), and scanning transmission electron microscopy (STEM)-energy dispersive spectroscopy (EDS), we reveal that Nadeficient, low optical basicity conditions stabilize octahedral MoO 6 units, which polymerize into molybdite-like Mo−O clusters dispersed within the glass matrix. These Mo-rich clusters suppress the formation of depolymerized [MoO 4 ] 2− environments typically responsible for Na 2 MoO 4 precipitation and instead promote the formation of Na 2 Mo 2 O 7 as the saturation phase. Concurrently, Mo solubility drives the conversion of AlO 4 − to higher-coordination AlO 5 species, liberating Na + that is subsequently sequestered in molybdate-rich domains. The combined evolution of Mo coordination, modifier redistribution, and network depolymerization provides a mechanistic basis for the markedly enhanced Mo solubility in peraluminous compositions. These findings establish new structural guidelines for designing aluminoborosilicate waste forms with substantially greater capacity to incorporate Mo-rich nuclear waste streams.

Amorphous materials↗

Validation of a Custom Ball-on-Ring Apparatus and Consideration of Common Issues for Use in Further Testing (SULI Deliverables)

Ceramic materials are well-known for their high hardness and strength but are limited in their application due to low toughness and sudden failure. As a potential solution, inspiration can be taken from dental enamel nanostructure, where undulating rods cause cracks to branch or deflect, increasing the energy needed to cause total fracture of a ceramic part. Following the dental enamel structure, a novel ceramic which uses 3D printed Yttria stabilized Zirconia rods in an alumina matrix was developed. To test this bio-inspired ceramic material, a proper testing apparatus needed to be created and tested to verify its accuracy. For this project, a bespoke ball on ring testing apparatus was created and tested using both conventionally sintered alumina disks and purchased alumina disks to validate its accuracy. By comparing the Weibull distribution of rupture strengths measured by the tests to literature values, it was shown that the testing frame had a wide distribution of strength which did not align with literature values on the lower end. Through fractography, it was found that some samples fractured from the contact stress induced by the ball indenter, which could not be used to calculate rupture strength. This fracture was often linked to low stress to failure, which was initiated by a flaw on the surface near the indenter which acted as a stress concentrator. Removal of these samples from the data set increased the accuracy of the reported rupture strength values for the ceramic. Considering the equations for the magnitude of contact and flexural strength, along with observations of initiating flaws, several measures can be taken for testing the bio-inspired composite. These measures include proper polishing of both sides of the sample, reducing sample thickness, and potentially using a softer indenter material.

36 - MATERIALS SCIENCE↗

Accurate additive manufacturing of lightweight and elastic carbons using plastic precursors

Despite groundbreaking advances in the additive manufacturing of polymers, metals, and ceramics, scaled and accurate production of structured carbons remains largely underdeveloped. This work reports a simple method to produce complex carbon materials with very low dimensional shrinkage from printed to carbonized state (less than 4%), using commercially available polypropylene precursors and a fused filament fabrication-based process. The control of macrostructural retention is enabled by the inclusion of fiber fillers regardless of the crosslinking degree of the polypropylene matrix, providing a significant advantage to directly control the density, porosity, and mechanical properties of 3D printed carbons. Using the same printed plastic precursors, different mechanical responses of derived carbons can be obtained, notably from stiff to highly compressible. This report harnesses the power of additive manufacturing for producing carbons with accurately controlled structure and properties, while enabling great opportunities for various applications.

36 MATERIALS SCIENCE↗

Chemical compatibility of hollow ceramic cenospheres as thermal insulation for high-temperature thermal energy storage applications with molten nitrate salt

An effective insulation material that is both thermally and chemically stable in molten salts could transform the design of molten-salt-based thermal energy storage (TES) tanks. Most current molten salt TES tanks hold the metallic tank structure in direct contact with hot salt inventory, a design which leads to thermal expansion of the tank and triggers stresses that can lead to thermomechanical failures. With an internal insulation to lower the temperature at the tank structure, the extent of thermal expansion can be reduced, thereby reducing expansion-induced stresses and allowing for consideration of lower-cost tank structure materials. Conventional insulation materials are either 1) too porous and allow molten salts to permeate into the matrix, which significantly increases the thermal conductivity or 2) too dense and have a thermal conductivity that cannot provide sufficient thermal insulation. This paper presents an alternative thermal insulation concept using cenospheres which have an alumino-silicate structure. The cost analysis suggests that the low-density cenospheres can be one of the cheapest materials to provide cost-effective thermal insulation. The chemical compatibility of cenospheres is investigated in molten 60 wt% NaNO3/40 wt% KNO3 salt which is close to industrial-grade Solar Salt. This paper shows that diffusion of the sodium and potassium cations from the salt into the cenospheres occurs based on weight analysis, energy dispersive spectroscopy (EDS), X-ray diffraction (XRD) and Fourier-transform infrared (FTIR) spectroscopy. The cation diffusion breaks the bridging oxygen bonds and causes volume expansion of the microstructure which is responsible for the failure of the cenosphere particles. The chemical composition of the cenospheres is found to affect their compatibility with molten nitrate salt. A cenosphere product with low iron content showed the best compatibility with an average survival rate of 77.9% +/- 9.8% after 7 days of immersion in the molten nitrate salt. While even the low-iron cenospheres appear to require protection from direct molten salt contact, their slow degradation rate, closed-cell porosity, and low cost hold potential for effective use as internal tank insulation.

14 SOLAR ENERGY↗