Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “COLD WORKING”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 217 records · Page 12

ASSESSMENT OF RESIDUAL STRESSES IN SRS AND HANFORD 3013 INNER AND CONVENIENCE CANS

Chloride stress corrosion cracking (SCC) is a plausible corrosion mechanism for the stainless steel 3013 containers during their lifetime for plutonium material storage if sufficient electrolyte is present within the container. Contributing factors for SCC, such as fabrication and welding residual stresses, are present in the 3013 cans. Convenience and inner cans from both Hanford and SRS are made by a flow form process, which cold works the stainless steel during fabrication. Additionally, the inner cans also are sealed at the can top with a closure weld to the sealing plug. Only SRS and Hanford were tested since moisture levels were significant for SCC. As part of the 3013 corrosion plan for FY09, testing in a boiling magnesium chloride solution was performed on actual 3013 convenience and inner cans to determine if the residual stresses were sufficient for the initiation and propagation of SCC. Additional testing in a 40% calcium chloride solution was also performed on 304L stainless steel SCC coupons, i.e. stressed teardrop-shaped samples (teardrops), and an inner can welded top to provide comparative results and to assess the effect of residual stresses in a less aggressive environment. The testing performed under this task consisted of 3013 inner and convenience cans and 304L teardrops exposed to a boiling magnesium chloride solutions per ASTM G36 and a 40% calcium chloride solution at 100 C following the guidance of ASTM G123. Cracking occurred in all can types including the inner can bottom and welded top and the bottoms of the SRS and Hanford convenience cans when exposed to the boiling magnesium chloride solution at 155 C. Cracking occurred at different times indicative of the residual stress levels in the cans. 304L teardrops cracked in the shortest time interval and therefore provide a conservative estimate for can performance. Testing in a 40% calcium chloride solution at 100 C demonstrated that cracking occurs in a less aggressive environment but at significantly longer times than in the boiling magnesium chloride. Vapor space cracking was also found to occur in the inner can welded top exposed over the boiling magnesium chloride solution and on 304L teardrops exposed over a hot calcium chloride solution.

36 MATERIALS SCIENCE↗

Improving 6061-Al Grain Growth and Penetration across HIP-Bonded Clad Interfaces in Monolithic Fuel Plates: Initial Studies

Grain penetration across aluminum-aluminum cladding interfaces in research reactor fuel plates is desirable and was obtained by a legacy roll-bonding process, which attained 20-80% grain penetration. Significant grain penetration in monolithic fuel plates produced by Hot Isostatic Press (HIP) fabrication processing is equally desirable but has yet to be attained. The goal of this study was to modify the 6061-Al in such a way as to promote a much greater extent of crossinterface grain penetration in monolithic fuel plates fabricated by the HIP process. This study documents the outcomes of several strategies attempted to attain this goal. The grain response was characterized using light optical microscopy (LOM) electron backscatter diffraction (EBSD) as a function of these prospective process modifications done to the aluminum prior to the HIP cycle. The strategies included (1) adding macroscopic gaps in the sandwiches to enhance Al flow, (2) adding engineering asperities to enhance Al flow, (3) adding stored energy (cold work), and (4) alternative cleaning and coating. Additionally, two aqueous cleaning methods were compared as baseline control conditions. The results of the preliminary scoping studies in all the categories are presented. In general, none of these approaches were able to obtain >10% grain penetration. Recommended future work includes further development of macroscopic grooving, transferred-arc cleaning, and combinations of these with one another and with other processes.

36 MATERIALS SCIENCE↗

Technical Letter Report on the Cracking of Irradiated Stainless Steels in Low-Corrosion-Potential Environments

Irradiation-assisted stress corrosion cracking (IASCC) is a major degradation mechanism for reactor internal components of austenitic stainless steels (SSs) in light water reactors. Crack growth rate (CGR) and fracture toughness J-R curve tests were performed on four irradiated SS specimens in high-purity water with low dissolved oxygen and in a simulated pressurized water reactor (PWR) environment. The samples had been previously irradiated from ~5 to 8 dpa in the BOR-60 reactor. The materials were cold-worked (CW) 316 and solution-annealed (SA) 304L SSs, which are commonly used in PWR core internals. Cyclic and constant-load CGRs were obtained from these samples to assess their cracking behaviors in low-corrosion-potential environments. A Ti-stabilized specimen, CW 316-Ti SS, was found to be highly vulnerable to IASCC, and its cracking susceptibility increased with neutron dose between ~5 and 8 dpa. The CW 316 and SA 304L SSs showed moderate cracking susceptibilities in the low-corrosion potential environments up to ~7 dpa. Periodic partial unloading (PPU) had a significant impact on the crack growth behavior of all irradiated specimens, and the measured CGRs were more than one order of magnitude higher in the test periods with than without PPU. A “stair-step” crack growth behavior was also observed for all irradiated specimens during the test periods with PPU, suggesting a strong effect of dynamic loading on IASCC. The SA 304L SS showed the best fracture resistance, and the CW 316 SS was the most brittle among the tested specimens. The fracture toughness J values of the two CW 316-Ti SS specimens were nearly identical at ~5 and ~8 dpa.

Chen, Y.↗

Stainless Steel Microstructure and Mechanical Properties Evaluation

A nitrogen strengthened 21-6-9 stainless steel plate was spinformed into hemispherical test shapes. A battery of laboratory tests was used to characterize the hemispheres. The laboratory tests show that near the pole (axis) of a spinformed hemisphere the yield strength is the lowest because this area endures the least “cold-work” strengthening, i.e., the least deformation. The characterization indicated that stress-relief annealing spinformed stainless steel hemispheres does not degrade mechanical properties. Stress-relief annealing reduces residual stresses while maintaining relatively high mechanical properties. Full annealing completely eliminates residual stresses, but reduces yield strength by about 30%.

36 MATERIALS SCIENCE↗

Report on Status of Shipment of High Fluence Austenitic Steel Samples for Characterization and Stress Corrosion Crack Testing

The goal of the Mechanisms of Irradiation Assisted Stress Corrosion Cracking (IASCC) task in the LWRS Program is to conduct experimental research into understanding how multiple variables influence the crack initiation and crack growth in materials subjected to stress under corrosive conditions. This includes understanding the influences of alloy composition, radiation condition, water chemistry and metallurgical starting condition (i.e., previous cold work or heat treatments and the resulting microstructure) has on the behavior of materials. Testing involves crack initiation and growth testing on irradiated specimens of single-variable alloys in simulated Light Water Reactor (LWR) environments, tensile testing, hardness testing, microstructural and microchemical analysis, and detailed efforts to characterize localized deformation. Combined, these single-variable experiments will provide mechanistic understanding that can be used to identify key operational variables to mitigate or control IASCC, optimize inspection and maintenance schedules to the most susceptible materials/locations, and, in the long-term, design IASCC-resistant materials. In support of this research, efforts are currently underway to arrange shipment of “free” high fluence austenitic alloys available through Électricité de France (EDF) for post irradiation testing at the Oak Ridge National Laboratory (ORNL) and IASCC testing at the University of Michigan. These high fluence materials range in damage values from 45 to 125 displacements per atom (dpa). The samples identified for transport to the United States, which include nine, no-cost, 304, 308 and 316 tensile bars, were relocated from the Research Institute of Atomic Reactors (RIAR) in Dimitrovgrad, Ulyanovsk Oblast, Russia, and received at the Halden Reactor in Halden, Norway, on August 23, 2016. ORNL has been notified that a significant amount of work is required to prepare the samples for further shipment to Oak Ridge, Tennessee. The preliminary work for sample shipment between Halden and Oak Ridge includes fabrication of an inner cask sample container, decontamination and preparation of a Type A container, preparation of new activity calculations, all necessary paperwork, and handling. ORNL will continue to work to track progress of sample preparation and shipment status, and to work toward an agreement that covers material shipping costs between the Halden Reactor and the Oak Ridge National Laboratory.

36 MATERIALS SCIENCE↗

Nanoindentation Characterization of FeCrAl C26M tubes

The present report summarizes the nanoindentation characterization of a FeCrAl alloy, C26M in both tube and bar form. Microstructural analysis on the tube using electron backscatter diffraction showed a textured system with the cross-section favoring orie ntations near the [110] and the tube surface near the [111]. The bar cross-section showed a texture with orientation favoring those near the [100]. A large amount of in-grain misorientation was observed in the tube specimen with very little in the bar, indicating cold-work from tube processing steps. Nanoindentation with a Berkovich tip measured a similar modulus for all specimens of ~220 GPa. The bar specimens had a hardness of ~3.9 GPa, significantly lower than the 4.8 GPa and 5.2 GPa for the tube cross-section and surface, respectively. Spherical nanoindentation was performed on all specimens and orientations. Indentation with a 100 μm tip resulted in a measured modulus value of ~220 GPa for all specimens, in agreement with the Berkovich indentation results. The nanoindentation yield strength for the bar was found to be ~0.8 - 0.9 GPa, nearly 0.5 GPa less than the C26M tube.

36 MATERIALS SCIENCE↗

Neutron Fluences for EBR-II Reflector Assemblies U9902, U9003, U9005, U9006 and U9027

There are currently five complete Experimental Breeder Reactor No. 2 (EBR-II) reflector assemblies being stored in the Hot Fuel Examination Facility (HFEF) pits at Idaho National Laboratory (INL); these are reflector assemblies U9902, U9003, U9005, U9006 and U9027. Reflector assembly U9027 was fabricated with a 12% cold-worked Type 316 steel can and Type 304 steel blocks, while the other assemblies had Type 304 steel cans and blocks. There has been interest at INL in using these irradiated reflector (steel) assemblies to correlate observed material damage to exposure (fluence, i.e., flux times time), and to do this, spatial neutron fluence levels for each of these reflector assemblies needs to be known. The irradiation histories of these five reflector assemblies, in terms of EBR-II grid positions and Run cycles, are shown in Table 1. This data was obtained from the “SASBLY” file in the EBR-II Physics Analysis Database (PADB) which gives positional and run information for each assembly irradiated in the EBR-II. Except for short-term storage in the blanket region (position 13D8), all relevant reflector assemblies were irradiated in either EBR-II hex-row 9 or 10.

21 SPECIFIC NUCLEAR REACTORS AND ASSOCIATED PLANTS↗

Intermediate-Term Thermal Aging Effect Evaluation for Grade 92 and 316L at The LWR Relevant Temperature

Life extension of the existing nuclear reactors imposes accumulated damages, such as higher fluences and longer period of corrosion, to structural materials, which would result in significant challenges to the traditional reactor materials such as type 304 and 316 stainless steels. Advanced alloys with superior radiation resistance will increase safety margins, design flexibility, and economics for not only the life extension of the existing fleet but also new builds with advanced reactor designs. The Electric Power Research Institute (EPRI) teamed up with Department of Energy (DOE) on the Advanced Radiation Resistant Materials (ARRM) program, aiming to develop and test degradation resistant alloys from current commercial alloy specifications by 2021 to a new advanced alloy with superior degradation resistance in light water reactor (LWR)-relevant environments by 2024. Based on a comprehensive microstructure and property screening performed in Phase-1 of the ARRM program, a total of five alloys, together with 316L and X-750 as references, were down-selected for Phase-2 neutron irradiation studies. Because thermal aging could exert a synergistic effect on neutron irradiation due to the low neutron damage rate on the order of 10 –7 displacements per atom per second (dpa/s), Grade 92 (one of the five down-selected alloys) and two heats of 316L were selected in this task to study the effect of aging at 350°C for 12.5–12.7 kh on microstructure and mechanical properties. The aging time is approximately corresponding to 5 dpa neutron irradiation, which can be served as a reference for the 5-dpa-irradiated samples of the alloys to help understand the independent neutron damage influence on microstructure and mechanical properties. Optical microscopy and scanning electron microscopy were used for microstructural characterization. Hardness, tensile, Charpy impact toughness, and fracture toughness in the ductile regime of the aged samples were examined. The aging of Grade 92 led to the formation of many Laves phase in sizes of ~100–200 nm and resulted in some reduction in hardness and yield/ultimate tensile strength with some increases in uniform and total plastic elongations, which may have helped the enhancement of Charpy impact toughness, e.g., ~4 J increase in upper-shelf energy and 20.5°C reduction in ductile-brittle transition temperature compared with the unaged condition. The fracture toughness of the aged Grade 92 showed decent toughness of ~303 MPa√m (K Jq ) with ~87 tearing modulus at 22°C, which reduced to ~241 MPa√m (~20% reduction) with ~75 tearing modulus at 300°C. The two heats of 316L are differentiated by their amounts of δ-ferrite, i.e., ~1 vol% in heat T1103 and ~4 vol% in heat N5B8. The two heats of 316L were subjected to 15% cold work (CW) as this condition is often used in nuclear reactors to help trapping radiation-induced defects and thus postpone the steady state swelling stage. The aging did not result in any noticeable microstructure changes, except for possible segregations at grain boundaries that need to be further investigated. The aging resulted in slight reduction in hardness of 316L-T1103 and slight increase in hardness of 316L-N5B8, which is consistent with their tensile testing results. The 15%CW might have introduced some inhomogeneity, resulting in large standard deviations in hardness, which were reduced after the aging. The aged 316L followed the same trend as the unaged condition for the strength and elongation results from the tensile testing. Minimum elongations appeared within ~300–600°C, above which the elongations seem to increase. Unlike the negligible or minor changes in microstructure, hardness and tensile results of the two heats of 316L, their fracture toughness showed noticeable difference. The aged 316L-T1103 showed good toughness of ~350 MPa√m with ~80 tearing modulus at 22°C, which reduced to ~271 MPa√m (~23% reduction) with ~83 tearing modulus at 300°C. In contrast, the aged 316L-N5B8 showed lower toughness of ~244 MPa√m with ~53 tearing modulus at 22°C, which reduced to ~180 MPa√m (~26% reduction) with ~31 tearing modulus at 300°C. The preliminary results indicate that the presence of high volume of δ-ferrite would noticeable impair fracture toughness although it may not influence hardness and tensile properties.

22 GENERAL STUDIES OF NUCLEAR REACTORS↗

Innovative Method for Welding in Generation 3 CSP to Enable Reliable Manufacturing of Solar Receivers to withstand Daily Cycling at Temperatures Above 700°C (Final Technical Report)

Inconel® Alloy 740H® (alloy 740H) was the first age-hardenable nickel-based alloy approved by the ASME Boiler & Pressure Vessel Code for use in pressure-boundary applications. Over the past ~20 years the alloy has been optimized for weldability and high-temperature stability, approved for use in different applications. Development of a supply chain combined with the advantageous properties of the alloy (high-temperature creep strength, oxidation and corrosion resistance, etc.) have resulted in the alloy being applied to new high-temperature power cycle demonstration projects, and of particular interest are applications to concentrating solar power (CSP) to enable higher-efficiency Generation 3 CSP systems and the corresponding supercritical CO 2 (sCO 2 ) power cycle components (heat exchangers, piping, etc.). The high allowable stresses of alloy 740H also make it a desirable material for current Generation 2 CSP solar power receivers to improve cyclic capability and/or reduce receiver height. Recent experiences in demonstration projects utilizing alloy 740H identified cracking issues during welding and fabrication. In this project, a detailed study was done to confirm and clarify the Stress Relaxation Cracking (SRxC) mechanism, also known as stress relief cracking or strain-age cracking (SAC), during post-weld heat-treatment (PWHT). This involved detailed microscopy and advanced characterization to understand the root cause(s) of three failures obtained from industry. Based in-part on these findings, a targeted laboratory based SRxC test method was utilized to evaluate variables such as heat-to-heat variations, strain level, PWHT temperature, and starting material condition on three heats of alloy 740H. Industrial shop welding of cold-worked plates was also conducted. The research showed the following: SRxC was confirmed as the cracking mechanism for all field failures; Stress state (from residual stresses, constraint, deformation, and local stress concentrations) was playing a significant role in field failures and laboratory testing confirmed increasing susceptibility for all heats with increasing strain levels. High levels of microstructural strain were identified at crack initiation locations, in some cases leading to local recrystallization; Precipitate free zones (PFZs) at grain boundaries were found at relaxation cracks and crack initiation locations uniquely associated with SRxC in alloy 740H. Laboratory testing reproduced this microstructural feature which had only previously been reported in long-term creep testing of weldments. Advanced nano-scale characterization confirmed the presence of a moving boundary leading to coarsening of precipitates and PFZs where damage accumulated; The research suggested heat-to-heat variations due to local chemistry and processing may influence SRxC susceptibility, but more work is needed to fully clarify these effects. To disseminate the key learnings from this research to the scientific and engineering communities and alloy 740H end users, multiple technical publications and presentations were made, an industrial alloy 740H users meeting was held, and a new industry guideline specification document which can be directly implemented by end-users of alloy 740H was produced.

14 SOLAR ENERGY↗

PIE of Cycle 13 316SS Cladding Using Aberration Corrected STEM Image and Analys

Optical, SEM and TEM analysis confirmed the presence of moderate sensitization in the 20% cold worked 316SS after the iron aluminide coating was applied. The Cr depletion occurs on the grain boundaries between the closely spaced carbides, and at the interface between the carbides and matrix. Cr depletion varied from locally along the grain boundaries, in many cases showing levels down to 15 wt%, but a few isolated regions had depletion levels down to 12.5 wt%. Optical and SEM images taken from a weld heat affected zone revealed the recrystallization occurred after an end plug cap had been welded to the coated cladding. Irradiation did not affect the carbides in a noticeable manner, but radiation-induced segregation/depletion altered the Cr depletion profiles by removing the wide Cr depletion profile, and replacing it with a much deeper, more narrow profile. Cr levels were depleted to 8-10 wt%, Ni and Si were enriched to levels of 40 wt% and 12 wt% respectively. Substantial precipitation formed in the matrix, and on line dislocations in the matrix and on grain boundary dislocations. Voids were observed in the upper region of the TPBAR where the irradiation temperature exceeds 320C. The levels of Cr depletion and Ni/Si enrichment indicate a material in a state susceptible to irradiation assisted stress corrosion cracking.

316SS cladding↗

Analysis of Deformation and Fracture Mechanisms in the Harvested Low-Dose Baffle Former Bolt via Advanced Mechanical Tests

This report details the production of tensile specimens from in-service irradiated baffle former bolts (BFBs) and presents the results of a pilot in-situ SEM/EBSD test conducted at Oak Ridge National Laboratory’s Low Activation Materials Development and Analysis (LAMDA) facility. The SEM/EDS results confirmed that the material is AISI 316L steel, not AISI 347, and that no Nb addition was detected in several analyzed locations. EBSD analysis of the microstructure revealed in-grain misorientation gradients indicative of cold work, likely caused by material processing, and no retained ferrite was identified. During straining, dislocation channel formation was the primary deformation mechanism, with twinning also observed in favorably oriented grains at local strains as small as ~1.5%. No strain-induced phase instability was observed, likely due to the fact that the Ni and Cr content reached the upper limits for the 316L steel specification. Multiple microfracture events were observed during the tensile test. Fine strain-induced pores formed at the channel-grain boundary intersection points, while coarser microcracks were associated with non-metallic inclusions. Data analysis is ongoing, and additional tests are planned in the near future to provide more statistics and details.

36 MATERIALS SCIENCE↗

Examination of the 1970 National Bureau of Standards Underground Corrosion Test Welded Stainless STeel Coupons from Site D

A 1970 study initiated by the National Bureau of Standards (NBS), now known as the National Institute of Standards and Technology (NIST), buried over 6000 corrosion coupons or specimens of stainless steel Types 201, 202, 301, 304, 316, 409, 410, 430, and 434. The coupons were configured as sheet metal plates, coated plates, cross-welded plates, U-bend samples, sandwiched materials, and welded tubes. All coupons were of various heat-treatments and cold worked conditions and were buried at six distinctive soil-type sites throughout the United States. The NBS scientists dug five sets of two trenches at each of the six sites. In each pair of trenches, they buried duplicate sets of stainless steel coupons. The NBS study was designed to retrieve coupons after one year, two years, four years, eight years, and x years in the soil. During the first eight years of the study, four of five planned removals were completed. After the fourth retrieval, the NBS study was abandoned, and the fifth and final set of specimens remained undisturbed for over 33 years. In 2003, an interdisciplinary research team of industrial, university, and national laboratory investigators were funded under the United States Department of Energy’s Environmental Management Science Program (EMSP; Project Number 86803) to extract part of the remaining set of coupons at one of the test sites, characterize the stainless steel underground corrosion rates, and examine the fate and transport of metal ions into the soil. Extraction of one trench at one of the test sites occurred in April 2004. This report details only the characterization of corrosion found on the 14 welded coupons–two cross welded plates, six U-bends, and six welded tubes–that were retrieved from Site D, located near Wildwood, NJ. The welded coupons included Type 301, 304, 316, and 409 stainless steels. After 33 years in the soil, corrosion on the coupons varied according to alloy. This report discusses the stress corrosion cracking and crevice corrosion cracking of the U-bend coupons; the minimal corrosion found on the cross-bead plates; and the general, pitting, and crevice corrosion found on the welded tubes. In general, the austenitic Type 301, 304 and 316 samples showed little if any corrosion after 33+-years in the soil, whereas the ferritic alloys-Type 409 and 434– showed a spectrum of corrosion.

36 MATERIALS SCIENCE↗

A Comprehensive Review on Finite Element Analysis of Laser Shock Peening

Laser shock peening (LSP) is a formidable cold working surface treatment that provides high-energy precision to enhance the mechanical properties of materials. This paper delves into the intricacies of the LSP process, offering insights into its methodology and the simulation thereof through the finite element method. This review critically examines various points, such as laser energy, overlapping of shots, effect of LSP on residual stress, effect of LSP on grain refinement, and algorithms for simulation extrapolated from finite element analyses conducted by researchers, shedding light on the nuanced considerations integral to this technique. As the significance of LSP continues to grow, the collective findings underscore its potential as a transformative technology for fortifying materials against mechanical stress and improving their overall performance and longevity. The discourse encapsulates the evolving landscape of the LSP, emphasizing the pivotal role played by finite element analysis in advancing our understanding and application of this innovative surface treatment.

36 MATERIALS SCIENCE↗

Evaluation of Hydrogen Gettering Rates Correlated to Surface Composition and Texture of Nickel-Plated Zircaloy Getters of Different Heat Treatment Procedures

Coatings of metal specimens are known to have an impact on hydrogen gettering (hydrogen absorption). The coating can have one or more functions, such as enhancing gettering, preventing gettering and/or preventing oxidation of the metal substrate. It is known that contaminants and surface texture can impact hydrogen gettering/absorption performance, but has not previously been thoroughly explored. This study evaluated the role of different post-plating heat treatments of nickel-plated zircaloy-4 getters (NPGs) and the role of the heat treatments on gettering rates, surface composition and texture. Nickel plating is applied to prevent oxidation of the Zircaloy-4 surface and also enhances gettering. The nickel plating must be heat treated before desirable gettering can occur. Our NPG getters with historically known satisfying performance were pre-heat treated in air followed by activation heat treatment in a vacuum at a higher temperature. In this study, we were interested in finding out if both heat treatment steps were necessary to obtain a desirable gettering performance, or if one step could be omitted. XPS analysis showed that if the nickel surface is not heat treated before bonding the nickel to the zirconium in the activation step, there will be carbon contaminants on the surface, which significantly reduces gettering. We studied the texture of Zircaloy-4 using SEM/EBSD to compare NPGs with both heat treatment steps with NPGs that had no post-plating heat treatment to learn if the degree of cold work could be impacted by the heat treatment steps. We did not observe any differences in texture between them. We measured gettering rates of both pretreated and activated NPGs and NPGs that had been activated without first being pre-heat treated. We found that the NPGs without the first post-plating heating step had up to a seven times slower gettering rate and obtained higher plateau pressures due to the contaminated surface. Thus, the pre-heat treatment in air before activation is necessary to avoid slower gettering rates and higher plateau pressures.

36 MATERIALS SCIENCE↗

Forming blocks speed production of strain gage grids

A tool is designed which facilitates the forming of wire grids used in manufacturing strain gage grids. Flattening the grid wire by a cold working process produces a stabilized grid which can be readily handled for storage or shipment.

Bonn, J. L.↗