Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “CLADDING”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 217 records · Page 12

Functionally graded coatings and claddings

A shear assisted extrusion process for producing cladded materials wherein a cladding material and a material to be cladded are placed in sequence with the cladded material positioned to contact a rotating scroll face first and the material to be cladded second. The two materials are fed through a shear assisted extrusion device at a preselected feed rate and impacted by a rotating scroll face to generate a cladded extrusion product. This process allows for increased through wall strength and decreases the brittleness in formed structures as compared to the prior art.

36 MATERIALS SCIENCE↗

Evaluating the Effects of Hydride Embrittlement and Pulse Width on Zircaloy Cladding Transient Performance

Pellet Cladding Mechanical Interaction is the primary failure mode for high burnup Zircaloy claddings in Light Water Reactor Reactivity Initiated Accidents. This failure mode is not seen in fresh and lower burnup fuels and is the result of environmental degradation of the cladding material and the unique loading condition on the cladding as a result of the sudden contact forces with the pellet. This paper describes work that is underway at the Idaho National Laboratory to better understand this failure mode by pre-hydriding fresh Zircaloy cladding. The pre-hydrided cladding is being mechanically characterized and will ultimately be used as part of an in-pile testing campaign at the TREAT reactor that will simulate the unique transient loading and heating conditions present in a Reactivity Initiated Accident. A description of the pre-hydriding and mechanical testing processes being followed, and initial results are presented followed by a description of the planned transient testing

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

A review of cladding failure thresholds in RIA conditions based on transient reactor test data and the need for continued testing

Transient reactor experiments on light water reactor (LWR) fuel pins had been conducted since the beginning of the nuclear era to help determine core coolability and cladding failure thresholds. During one such test in November of 1993 at the CABRI transient test reactor on a test involving a high burnup fuel rod with a corroded Zircaloy-4 cladding it was first observed that cladding failures could occur prior to a departure from nucleate boiling (pre-DNB) at lower-than-expected peak radial average enthalpies. Thirteen additional tests would be performed in the CABRI reactor over the next decade on fuel rods with higher burnups [1]. Additionally, a larger testing program at the NSRR reactor in Japan with high burnup fuel would uncover a similar trend of pre-DNB ruptures in high burnup test rods at lower-than-expected peak enthalpies [2]. Numerous out of pile testing programs involving a variety of innovative mechanical testing techniques have been employed in an attempt to better quantify the failure thresholds of corroded zirconium alloy cladding in these rapid heating and loading conditions [3][4][5]. While previously interim guidance had been issued, in June of 2020 the NRC officially published updated regulatory guidance to account of these pre-DNB failures in Regulatory Guide 1.236 [6]. This paper will present an independent review of the publicly available transient reactor test database on higher burnup LWR pins conducted at the CABRI and NSRR reactors as well as review of a selection of published out of pile mechanical testing methods. The purpose of the review is to determine how well the new regulatory limits are supported by experimental data. The review will identify if additional transient reactor tests could provide additional support for the NRC guidance or identify the need for revisions. The evaluation will consider how far the existing database can be extrapolated when considering low hydrogen zirconium alloy claddings (with and without protective coatings) containing very high burnup (> 70 MWd/kgU) UO2 fuel pellets. Finally, the authors will suggest how out of pile mechanical tests can be used in conjunction with a limited number of transient reactor tests to develop cladding specific failure thresholds in RIA type transients.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Method of making an annular radioisotope target having a helical coil-shaped foil ribbon between cladding tubes

An annular radioisotope target and method therefor that includes an inner cladding tube and a helical coil-shaped foil ribbon disposed over the inner cladding tube. The helical coil-shaped foil ribbon has a first end, a second end, a first edge and a second edge. An outer cladding tube is disposed over the helical coil-shaped foil ribbon and inner cladding tube, and end caps are attached to the outer cladding tube and the inner cladding tube.

Ripley, Edward B.↗

Cladding Alloys for Fluoride Salt Compatibility Final Report

This interim report provides an overview of several candidate technologies for cladding nickel-based corrosion protection layers onto high-temperature structural alloys. The report also provides a brief overview of the welding and weld performance issues associated with joining nickel-clad nickel-based alloys. From the available techniques, two cladding technologies were selected for initial evaluation. The first technique is a line-of-sight method that would be useful for coating large structures such as vessel interiors or large piping. The line-of-sight method is a laser-based surface cladding technique in which a high-purity nickel powder mixed into a polymer binder is first sprayed onto the surface, baked, and then rapidly melted using a high power laser. The second technique is a vapor phase technique based on the nickel-carbonyl process that is suitable for coating inaccessible surfaces such as the interior surfaces of heat exchangers. The final project report will feature an experimental evaluation of the performance of the two selected cladding techniques.

36 MATERIALS SCIENCE↗

Fuel performance of chromium-coated zirconium alloy and silicon carbide accident tolerant fuel claddings

The U.S. Department of Energy’s Accident Tolerant Fuel program is focused on extending the time for fuel failure during postulated severe accidents compared to the standard UO2-Zr alloy fuel system. This research investigates the feasibility of two different chromium-coated cladding concepts, one of which is zirconium-alloy based and the other is composite-SiC based. Both claddings had 50µm coatings, deducted from the base layer thicknesses. The claddings were reported on, using the multi- physics fuel performance tool BISON, under steady-state PWR operating conditions as well as two transients: power ramp and a loss-of-coolant accident (LOCA). The chromium-coated claddings showed comparable thermo-mechanical performance to the reference Zircaloy-4 cladding. As chromium is reported to provide an order of magnitude improvement in oxidation resistance, it is expected to be a better alternative in accident scenarios. Simulation results for both concepts call for further experimental investigation as well as modeling of beyond design-basis accidents.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Fuel performance analysis of Cr-coated Zircaloy-4 cladding during a prototypical LOCA event using BISON

Here, deformation and failure of chromium (Cr) coated Zircaloy-4 (Zry-4) were studied in loss-of-coolant accident (LOCA) conditions using the BISON fuel performance code. The BISON validation model simulating Halden research reactor experiments was extended to include Cr coatings and higher rod internal pressures to simulate high-burnup fuel. The transient simulations show Cr coatings help relieve stress in the Zry-4 substrate during the transient, delaying the onset of high-temperature creep, which leads to ballooning and bursting of the cladding. A nominal Cr coating thickness of 30 µm delays clad failure by 26 seconds and increases the clad burst temperature by 40 K. A parametric study showed that time to failure and burst temperature both increase with coating thickness, and Cr-coated cladding offers burst resistance under a wide range of rod internal pressures simulating high-burnup fuel. Results indicate that a thin Cr coating provides resistance against ballooning and bursting of cladding during LOCA events.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Fabrication and testing of U–7Mo monolithic plate fuel with Zircaloy cladding

The Materials Management and Minimization program is developing fuel designs to replace highly enriched fuel with fuels of low enrichment. In the most challenging cases, U–(7–10wt%)Mo monolithic plate fuel are proposed. The chosen design includes aluminum-alloy cladding, which provides some challenges in fabrication and fuel/cladding interaction in service. We investigated zircaloy cladding, specifically Zry–4as an alternative cladding, and development of a fabrication method was performed by researchers with the Comisión Nacionalde Energia Atómica (CNEA) in Argentina, resulting in test fuel plates (Zry–4 clad U–7Mo) which were subsequently tested in the Advanced Test Reactor in Idaho. Because Zry–4 and U–(7–10)Mo have similar high-temperature mechanical properties, fabrication was simplified in that the fuel foil and cladding could be co-rolled and bonded. The challenge was to prevent a thermal-expansion mismatch which could destroy the fuel/cladding bond before complete bonding was achieved; the solution was to prevent the composites from cooling significantly between roll passes. Our final product performed very well in-reactor, showing good bonding, very little fuel/cladding interaction, either from fabrication or in-reactor testing, and little swelling, especially no detectable heterogeneous bubble formation at the fuel/cladding interface tested to a fission density of up to 2.54E+21

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Thermo-mechanical assessment of full SiC/SiC composite cladding for LWR applications with sensitivity analysis

SiC/SiC composites are considered among leading candidates for accident tolerant fuel cladding in light water reactors. However, when SiC-based materials are exposed to neutron irradiation, they experience significant changes in dimensions and physical properties. Under a large heat flux application (i.e. fuel cladding), the non-uniform changes in the dimensions and physical properties will lead to build-up of stresses in the structure over the course of time. To ensure reliable and safe operation of such a structure it is important to assess its thermo-mechanical performance under in-reactor conditions of irradiation and elevated temperature. In this work, the foundation for 3D thermo-mechanical analysis of SiC/SiC cladding is put in place and a set of analyses with simplified boundary conditions has been performed. The analyses were carried out with two different codes that were benchmarked against one another and prior results in the literature. A constitutive model is constructed and solved numerically to predict the stress distribution and variation in the cladding under normal operating conditions. The dependence of dimensions and physical properties variation with irradiation and temperature has been incorporated. These robust models may now be modified to take into account the axial and circumferential variation in neutron and heat flux to fully account for 3D effects. Here, the results from the simple analyses show the development of high tensile stresses especially in the circumferential and axial directions at the inner region of the cladding. Based on the results obtained, design guidelines are recommended. For lack of certainty in or tailor-ability for the physical and mechanical properties of SiC/SiC composite material a sensitivity analysis is conducted. The analysis results establish a precedence order of the properties based on the extent to which these properties influence the temperature and the stresses.

Accident tolerant fuel↗

Formation and characterization of hydride rim structures in Zircaloy-4 nuclear fuel cladding tubes

Zirconium alloy tubes used as nuclear fuel cladding are subject to oxidation and subsequent hydrogen pickup during their long service in commercial light water reactors. The hydrogen picked up in the cladding can precipitate as a brittle hydride rim feature on the cladding outer surface. Here, to better understand the effect of hydride rims on the fracture behavior of stress-relieved zirconium alloy cladding tubes, a procedure to produce these rim-like structures has been developed and is described herein. Extensive characterization of the ‘as hydrided’ tubes is performed. The hydrogen charging apparatus consists of a tube furnace with a quartz chamber that is connected to a vacuum pump as well as a bottle of pure hydrogen gas. The charging station uses a static charge of hydrogen as opposed to a flowing gas. The chief advantage of this approach is the ability to monitor the pressure drop in the hydriding chamber and correlate this pressure drop to a known rate of hydrogen pickup in the cladding tube. It was found that the hydrogen partial pressure, metal temperature, and surface treatment all clearly played a role in whether a hydride rim was formed. Extensive characterization of the hydride rims shows they consist of needle like platelets of δ phase hydrides (ZrH1.66) oriented in the circumferential direction with a radial spacing of several microns in a sandwich-like structure.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Improved damage tolerance of SiC-based nuclear fuel cladding with novel multi-layered SiC coating design at 1200 °C

Continuous SiC fibre reinforced SiC matrix composites (SiC f -SiC m ) with monolithic SiC outer coatings are considered as a damage-tolerant cladding design for loss of coolant accident (LOCA) conditions in light water reactors. However, monolithic SiC coatings are brittle and prone to catastrophic failure. In this study, a SiC f -SiC m cladding with a novel multi-layer SiC outer coating (11 sub-layers, ∼260 µm in total thickness) was investigated under C-ring compression at room temperature and 1200 °C in argon environment. Real-time synchrotron X-ray computed tomography (XCT) was employed to capture crack initiation and propagation processes. Compared to conventional monolithic SiC outer coatings, the multi-layer coating structure facilitated crack deflection and bifurcation enhancing its damage tolerance at both temperatures. Despite pre-existing surface cracks, claddings exhibited stable mechanical-performance at both temperatures. These initial cracks did not critically affect the failure processes as they were not aligned with the maximum stress direction. Furthermore, the microstructure, distribution of residual stresses, and local properties of individual components in the material were thoroughly characterized, and compared with open literature on conventional claddings with monolithic outer coatings. These results provide new insights into the failure mechanisms of multi-layer SiC coatings and offer guidance for the future design of accident-tolerant nuclear fuel claddings.

36 - MATERIALS SCIENCE↗

$\mathrm{REX}$: An analytical tool for reactor operating envelope expansion through fuel-clad thermo-mechanics

Here REX, an analytical reactor design tool for the identification and expansion of reactor operating envelopes, is introduced and detailed. Written in MATLAB, REX takes core geometries and axially discretized detector and depletion output from the Serpent neutron transport code and performs full-core, pin-specific thermal-hydraulic and thermo-mechanical calculations. REX identifies the operating envelopes of advanced, solid-fuel nuclear reactors on the basis of their fuel-cladding, fuel-gas, and coolant-cladding interfacial thermo-mechanics. It iteratively pushes coolant inlet temperatures and modifies fuel pin geometries to induce mechanical failure in their original cladding materials at the fullest extent of their fuel cycle lengths and permissible coolant inlet temperatures. It then attempts to expand their operating envelopes by determining the mechanical responses of alternative cladding materials under the same geometric conditions. The result of the REX calculation sequence is a set of 5-D variables describing the temperatures, pressures, geometries, and mechanics of the core as functions of assembly, fuel pin, axial zone, depletion step, and coolant inlet temperature for each candidate cladding material with the limiting fuel pin geometry for the original material.

22 GENERAL STUDIES OF NUCLEAR REACTORS↗

Unveiling damage mechanisms of chromium-coated zirconium-based fuel claddings at LWR operating temperature by in-situ digital image correlation

Here, we investigate the coupled thermomechanical fracture mechanisms of coated nuclear fuel claddings at Light Water Reactor (LWR) operating temperatures. These coated claddings are a highly attractive, near-term solution, which addresses the demands for accident-tolerant fuel systems and provide greater oxidation resistance. However, the fracture mechanisms of these coatings, which may create channels for oxidation ingression, must be fully understood prior to implementation. Thus, high-temperature expanding plug experiments were conducted on coated cladding specimens at a temperature of 315 °C, consistent with the operating environment of LWRs. Furthermore, in-situ thermomechanical deformation was measured with stereo digital image correlation during heating and mechanical testing to separately resolve contributions of thermal and mechanical strain. Digital image correlation, supported by acoustic emissions (AE) detection, was also leveraged to track cracking activity during loading. Coating fracture was found to initiate at total hoop strains of 0.34%. The thermal deformation of the coated claddings was investigated via finite element simulations, revealing a bidirectional stress-state within the coating with axial and circumferential strains of 0.026 and 0.031%. This bidirectional stress-state was attributed with the generation of off-axis fracture pattern within the coating as identified via post-experiment scanning electron microscopy. Thus, this study unveiled critical, coupled thermomechanical mechanisms governing the coating fracture of coated claddings at LWR temperatures.

36 MATERIALS SCIENCE↗

Properties and features of structure formation CuCr-contact alloys in electron beam cladding

The microstructure and properties of the contact CuCr alloy produced by electron-beam cladding have been investigated. The effect of the electron beam cladding parameters and preheating temperature of the base metal on the structure and the properties of the coatings has been determined. The bimodal structure of the cladding coating has been established. The short circuit currents tests have been carried out according to the Weil-Dobke synthetic circuit simulating procedure developed for vacuum circuit breakers (VCB) test in real electric circuits. Test results have shown that the electron beam cladding (EBC) contact material has better breaking capacity than that of commercially fabricated sintered contact material. The application of the technology of electron beam cladding for production of contact material would significantly improve specific characteristics and reliability of vacuum switching equipment.

36 MATERIALS SCIENCE↗

Evolution of pores in the fuel cladding of the electrogenerating channel

The results of reactor tests of carbonitride fuel in a monocrystalline cladding from a molybdenum-based alloy that were carried out earlier on an experimental setup Ya-82 for 8 to 300 h at a temperature of ∼1500°C can be used in order to prove the operational reliability of fuel elements in the design of a megawatt nuclear power plant for a spacecraft. A raster image of the surface of a sample of cladding shows that the interfaces between the layers are decorated by pores. This result is explained in this work by the theory of coalescence. The mechanisms responsible for the evolution of pores taking place at the parameters of a Ya-82 setup are considered. The effect of decoration by pores of the interfaces between the layers of a sample of cladding of the electrogenerating channel by carrying out reactor tests is explained. The dependence of the average radius of pores on the duration of the experiment is obtained. An evaluation of the average sizes of pores arising under the conditions of the experiment gives a value of ∼2 μm, which is in agreement with the experimental data. A computational study of swelling of the cladding material in the process of irradiation is performed. Predictive estimates of the behavior of the porous system and swelling of the cladding material for a megawatt class nuclear power plant are made.

21 SPECIFIC NUCLEAR REACTORS AND ASSOCIATED PLANTS↗

High-temperature secondary hydriding experiments with E110 and E110G claddings - 2016-0031

Secondary hydriding can take place during a loss-of-coolant accident event after the ballooning and burst of the zirconium alloy cladding. The oxidation and hydrogen uptake in the ballooned section can produce the weakest segment of the rod. This phenomenon was investigated in the past mainly for Zircaloy-4 cladding. We investigated the effect of secondary hydriding in VVER reactors with E110 and E110G alloys. A high-temperature facility was built to carry out high-temperature treatment of fuel cladding samples. The burst of tubes was reached with inner pressurization at 750 and 800 C. After burst the samples were oxidized in the same furnace for different periods and at different temperatures. The oxidized samples were tested in a tensile test machine with four-point bending tests. The microstructure of the samples was analyzed by optical and scanning electron microscopy. The hydrogen content of the cladding was measured by heat extraction, prompt gamma activation analyses, and neutron radiography methods. The experiments indicated that the ballooned section after oxidation became the weakest segment of the VVER fuel. According to the mechanical testing, the cladding samples were brittle even after a short oxidation time (200 s at 1,000 C) without any sign of ductile behavior. The comparison of E110 and E110G samples showed that the E110 tubes lost their load-bearing capability or even integrity much earlier than the E110G samples treated under similar conditions. (authors)

36 MATERIALS SCIENCE↗

Post-quench ductility of zirconium alloy cladding materials - 2016-0088

The ductility of zirconium-based alloys after steam oxidation at high temperatures, followed by quenching in water, is of significant interest for the nuclear industry. High-temperature steam oxidation and quenching of nuclear fuel cladding occurs during postulated loss-of-coolant accidents. The industry is currently establishing in-reactor operation limits for peak cladding temperature and time at temperature based on the measured ductile-to-brittle transition of different cladding materials, both in the as-fabricated condition and using hydrogen charging as a surrogate for in-reactor operation. Aiming to study possible differences in post-quench ductility caused by differences in chemical composition, extensive testing on Zircaloy-4, ZIRLO{sup R}, and Optimized ZIRLO{sup TM} cladding materials as a function of hydrogen content, extent of oxidation, and peak cladding temperature was performed. The results showed similar ductile-to-brittle transition for the alloys studied despite differences in chemical composition, with a decrease in the extent of oxidation to reach the ductile to brittle transition with increasing hydrogen content. Microstructural characterization was performed to investigate the evolution of the oxygen-enriched layer that forms underneath the oxide, both during the time at high temperatures and during cooling. Significantly different morphologies of the oxygen-enriched layer were observed with different cooling rates, particularly for alloys containing niobium. Possible mechanisms for the development of the oxygen-enriched layer are discussed. (authors)

36 MATERIALS SCIENCE↗

Results of U-xMo (x=7, 10, 12 wt.%) Alloy Versus Al-6061 Cladding Diffusion Couple Experiments Performed at 500, 550 and 600°C

The Reduced Enrichment for Research and Test Reactors (RERTR) program has been developing low enrichment fuel systems encased in Al 6061 for use in research and test reactors. U–Mo alloys in contact with Al and Al alloys can undergo diffusional interactions that can result in the development of interdiffusion zones with complex fine-grained microstructures composed of multiple phases. A monolithic fuel currently being developed by the RERTR program has local regions where the U–Mo fuel plate is in contact with the Al 6061 cladding and, as a result, the program finds information about interdiffusion zone development at high temperatures of interest. In this study, the microstructural development of diffusion couples consisting of U-7wt.%Mo, U-10wt.%Mo, and U-12wt.%Mo vs. Al 6061 (or 6061 aluminum) cladding, annealed at 500, 550, 600 degrees C for 1, 5, 20, 24, or 132 hours, was analyzed by backscatter electron microscopy and x-ray energy dispersive spectroscopy on a scanning electron microscope. Concentration profiles were determined by standardized wavelength dispersive spectroscopy and standardless x-ray energy dispersive spectroscopy. The results of this work shows that the presence of surface layers at the U–Mo/Al 6061 interface can dramatically impact the overall interdiffusion behavior in terms of rate of interaction and uniformity of the developed interdiffusion zones. It further reveals that relatively uniform interaction layers with higher Si concentrations can develop in U–Mo/Al 6061 couples annealed at shorter times and that longer times at temperature result in the development of more non-uniform interaction layers with more areas that are enriched in Al. At longer annealing times and relatively high temperatures, U–Mo/Al 6061 couples can exhibit more interaction compared to U–Mo/pure Al couples. The minor alloying constituents in Al 6061 cladding can result in the development of many complex phases in the interaction layer of U–Mo/Al–6061 cladding couples, and some phases in the interdiffusion zones of U–Mo/Al–6061 cladding couples are likely similar to those observed for U–Mo/pure Al couples.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗